Polyimide adhesives

A process was developed for preparing aromatic polyamide acids for use as adhesives by reacting an aromatic dianhydride to an approximately equimolar amount of an aromatic diamine in a water or lower alkanol miscible ether solvent. The polyamide acids are converted to polyimides by heating to the temperature range of 200 - 300 C. The polyimides are thermally stable and insoluble in ethers and other organic solvents.

Progar, D. J.↗

High-temperature adhesives for polyimide films

Linear condensation polyimides which are high-temperature polymers show promise as adhesives which form flexible film coatings compatible with polyimide films. Materials are advantageous since they can be supplied as flexible tape, already B-staged and ready for bonding.

St. Clair, A. K.↗

Heat-shrinkable film improves adhesive bonds

Pressure is applied during adhesive bonding by wrapping parts in heat-shrinkable plastic film. Film eliminates need to vacuum bag or heat parts in expensive autoclave. With procedure, operators are trained quickly, and no special skills are required.

Johns, J. M.↗

Phosphorylated epoxy adhesives

Fire retardant adhesives for aircraft interiors are developed. Monomers, epoxy synthesis, diamine synthesis, acrylic modified epoxy, and phosphorylated amine epoxy blends are examined.

Bilow, N.↗

Adhesive material transfer in the erosion of an aluminum alloy

In order to study the basic mechanisms of erosion, hardened steel balls were shot into annealed 6061 Al alloy targets at velocity of up to 150 m/sec. The projectiles were collected and examined by a scanning electron microscope combined with energy-dispersive X-ray analyzer and it was found that target material in substantial amounts is adhesively transferred to the projectile. The transferred material forms on the projectile surface a layer the thickness of which increases with increases in impact velocity.

Salik, J.↗

Adhesives for bonding RSI tile to Gr/Pi structure for advanced space transportation systems

An adhesive was developed having improved high-temperature capability while retaining the ideal processing characteristics of RTV silicones. After evaluating several possibilities, mixtures of RTV with glass resins were selected as most promising. While results are not conclusive, tests of the final mixture evaluated, designated RA59, indicated capability of performing as a tile bonding agent to temperatures approaching 370C (700F) during repeated cycling.

Smith, K. E.↗

Development of LARC-13 adhesive systems

Various adhesive formulations were evaluated and the effects of various environments upon different titanium bond surface treatments were noted. Initial data show LARC-13 to possess good 589K (600 F) stability as compared to other high temperature stable systems.

Hoggatt, J. T.↗

Strength of adhesive-bonded hybrid structures

Structures prepared from materials with different thermal and mechanical properties by means of fiber-strengthened binders can fail in a number of ways. The present lecture is focused on failures through debonding at the metal or at the fiber-reinforced plastic. A method for calculating the stress distribution in adhesive layers as a function of the load is outlined, and its usefulness in providing insight into the behavior of bonds in hybrid structures is noted. Means of eliminating the unfavorable effects of temperature, humidity, creep and relaxation on the bonds in the manufacture of hybrid structures are examined, along with test methods developed for such structures.

Kirschke, L.↗

High temperature adhesives for bonding Kapton

Experimental polyimide resins have been developed and evaluated as potential high temperature adhesives for bonding Kapton polyimide film. Lap shear strengths of 'Kapton'/'Kapton' bonds were obtained as a function of test temperature, adherend thickness, and long term aging at 575K (575 F) in vacuum. Glass transition temperatures of the polyimide/'Kapton' bondlines were monitored by thermomechanical analysis.

Saint Clair, A. K.↗

Room-temperature adhesive for high-temperature use

PPQ (polyphenylquinoxaline) cures at room temperature, but withstands temperatures between -186 and +402 deg C. Adhesive is applied in chloroform solution. Bond forms as solvent evaporates.

Brooks, J. L.↗

Investigation into the effect of plasma pretreatment on the adhesion of parylene to various substrates

A procedure is described for using argon and oxygen plasmas to promote adhesion of parylene coatings upon many difficult-to-bond substrates. Substrates investigated were gold, nickel, kovar, teflon (FEP), kapton, silicon, tantalum, titanium, and tungsten. Without plasma treatment, 180 deg peel tests yield a few g/cm (oz/in) strengths. With dc plasma treatment in the deposition chamber, followed by coating, peel strengths are increased by one to two orders of magnitude.

Riley, T.↗

High-temperature adhesives for bonding polyimide film

Experimental polyimide resins were developed and evaluated as potential high temperature adhesives for bonding Kapton polyimide film. Lap shear strengths of Kapton/Kapton bonds were obtained as a function of test temperature, adherend thickness, and long term aging at 575 K (575 F) in vacuum. Glass transition temperatures of the polyimide/"Kapton" bondlines were monitored by thermomechanical analysis.

St.clair, A. K.↗

Investigation into the effect of plasma pretreatment on the adhesion of parylene to various substrates

An experimental effort has been undertaken to examine the effect of plasma pretreatment of various substrate materials coated with a polymer in the parylene family. This report describes the procedure and discusses initial data which indicate using plasmas of argon and oxygen to promote adhesion of parylene coatings upon many difficult-to-bond substrates. Substrates investigated were gold, nickel, kovar, teflon (FEP), kapton, silicon, tantalum, titanium, and tungsten. Without plasma treatment, 180 deg peel tests yield a few g/cm (oz/in) strengths. With dc plasma treatment in the deposition chamber, followed by coating, peel strengths are increased by one to two orders of magnitude.

Riley, T.↗

An analysis of interface crack in adhesively bonded lap shear joints

This paper presents an analytical study of interface crack problems in adhesively bonded lap shear joints. A convenient and accurate method of analysis is developed on the basis of conservation laws in elasticity and of the fundamental relationships in fracture mechanics of interface crack problems. The problem is eventually reduced to a system of linear algebraic equations of mixed-mode stress intensity factor solutions. One of the salient features of the present approach is that the interface crack-tip stress intensity solutions can be determined accurately and directly by the information extracted from the far field. Solutions of the interface crack problems in lap shear joints have been obtained for the cases of various adhesive/adherend material systems and geometric configurations of the crack and the joint. Of particular interest is the evaluation of the mixed-mode stress intensity factors and the associated energy release rates. They are determined explicitly to illustrate the fundamental nature of the joint fracture problem.

Wang, S. S.↗

High temperature adhesives for bonding composites

Selection and evaluation of candidate adhesives for bonding composites are described. These are based on mechanical property tests (lap shear and flatwise tensile) and processibility. Consideration is given to composite-to-composite, composite-to-titanium, and honeycomb sandwich structures.

Progar, D. J.↗

Elastomer-Toughened Polyimide Adhesives

T-Peel strengths of adhesive/Titanium bonds are compared for LARC-13 with and without elastomer additives. Elastomer toughening (incorporation of small amounts of rubber into polymer matrix) has been one of the most successful methods for modifying polymer toughness. Addition polyimides are currently under consideration as high-temperature adhesives for bonding composite materials such as titanium.

St. Clair, A. K.↗

Adhesion and friction of transition metals in contact with nonmetallic hard materials

Sliding friction experiments were conducted with the metals yttrium, titanium, tantalum, zirconium, vanadium, neodymium, iron, cobalt, nickel, tungsten, platinum, rhenium, ruthenium, and rhodium in sliding contact with single crystal diamond, silicon carbide, pyrolytic boron nitride, and ferrite. Auger electron spectroscopy analysis was conducted with the metals and nonmetals to determine the surface chemistry and the degree of surface cleanliness. The results of the investigation indicate the adhesion and friction of the transition metals in contact with diamond, silicon carbide, boron nitride, and ferrite are related to the relative chemical activity of the metals. The more chemically active the metal, the higher the coefficient of friction and the greater amount of transfer to the nonmetals.

Miyoshi, K.↗

Tool Severs Hidden Adhesive Bonds

New tool enters narrow gap between fragile materials and removes adhesively bonded filler without damage to adjacent surfaces. Reaches deep into narrow crevices to reach hidden bond lines. Tool originally developed to remove ceramic filler from between Space Shuttle surface-insulation tiles.

Keir, A. R.↗