133 records · Page 2

Advanced LiFSI-LiPF6 Electrolyte for Wide-Temperature and Thermally Stable Lithium-Ion Batteries

A new optimized LiFSI–LiPF6 dual-salt controlled-solvation electrolyte (E-DS) is demonstrated to enable practical graphite||LiNi0.8Mn0.1Co0.1O2 cells (˜4.0 mAh cm?²) to achieve exceptional performance and safety under extreme conditions. By optimizing anion coordination with the smaller, more dissociating FSI? anion, the E-DS forms ultrathin, dense, and inorganic-rich electrode/electrolyte interphases that dramatically suppress solvent decomposition, transition-metal dissolution, and surface reconstruction compared to the conventional LiPF6/carbonate electrolyte. Consequently, E-DS cells deliver >78% capacity retention after 300 cycles at 60 °C, retain fast discharging capacity at 30 °C, and operate effectively at -20 °C. Most strikingly, fully charged full cells with E-DS, even under overcharging to 4.8 V, show a lower heat evolution in stable formulations — transforming a traditionally unstable high-voltage/high-temperature configuration into an intrinsically safe state. This work establishes a new benchmark for carbonate-containing electrolytes, simultaneously achieving high energy density, fast-discharging capability, wide-temperature operation (-20 to 60 °C), and outstanding thermal safety in nickel-rich lithium-ion batteries.

electrode/electrolyte interphase

Complex-Concentrated Anion Doping Enables Ultra-Stable Lattice Oxygen and Structural Integrity in Lithium-Rich Layered Oxide Cathodes

Lithium- and manganese-rich layered oxides (LMR) stand out as next-generation lithium-ion cathode chemistries, which harness both transition-metal and lattice-oxygen redox processes to deliver exceptional capacity and energy density. However, their full potential is hindered by intrinsic oxygen instability and structural degradation, resulting in pronounced voltage fade and capacity decay. Here, we present a complex-concentrated anion-doping paradigm in which multiple anions, F, Br, and S, are incorporated into the oxygen sublattice to enhance oxygen-redox and structural stability. X-ray absorption spectroscopy and aberration-corrected scanning transmission electron microscopy confirm ultra-stable local oxygen coordination environments during long-term cycling, with detrimental phase transformations and oxygen-loss-induced cavitation dramatically inhibited. Notably, we show that the characteristic LiTM6 transition metal (TM) honeycomb ordering is preserved even after electrochemical cycling. Concurrently, this strategy yields an unprecedented volume change of only 0.63% upon charging to 4.8 V vs. Li+/Li, achieving the first zero-strain LMR cathode. The resulting LMR cathode delivers ultralow voltage fade (1 mV per cycle during the first 100 cycles and becomes negligible in subsequent cycles) and outstanding energy retention (93% after 200 cycles) in a pouch cell configuration. Our complex-concentrated anion-doping concept establishes a broadly applicable strategy for resolving chemo-mechanical failure mechanisms in ceramic intercalation electrodes for next-generation energy storage.

Li-ion batteries

Highly Porous Polyimide Gel for Use as Battery Separator with Room Temperature Ionic Liquid Electrolytes

Advanced aerospace vehicular concepts require advances in many existing technologies, including space power and energy storage systems. Batteries represent one of the major areas in need of improvement, both in terms of energy density and safety, with growing concerns over the fire safety of commercial lithium-ion batteries. This has prompted efforts to develop nonflammable battery components, namely the electrolyte and separator. Existing commercial lithium-ion batteries utilize polyolefin microporous membranes as separators with an electrolyte consisting of a lithium salt dissolved in a mixture of cyclic carbonate solvents. This separator/electrolyte combination has ionic conductivities in the range of 10 −2 to 10 −3 S/cm. However, the cyclic carbonate solvents are inherently flammable. Room-temperature ionic liquids (RTILs) appear to be a safer alternative. They offer good ionic conductivities and are inherently nonvolatile and nonflammable, giving them a safety advantage. However, many promising RTILs for battery electrolytes are not compatible with commercial polyolefin separator materials. Alternative separator materials, such as polyimides, are non-flammable and are capable of accepting RTILs into their structure. Polyimide gels, with a composition of 4,4′-oxydianiline, 3,3′,4,4′-tetracarboxylic dianhydride and cross-linked with Desmodur N3300A, possess an open-porous, fibrillar network architecture which offers a high degree of porosity (typically greater than 85% porosity) for lithium-ion transport and conduction, as well as good mechanical properties. Furthermore, these polyimide gels are compatible with selected imidazolium-based RTILs. Nonflammable separator/electrolyte systems with room-temperature conductivities in the range of 10 −3 S/cm have been evaluated. It has been demonstrated that 1-ethyl-3-methylimidazolium bis(trifluoromethylsulfonyl)imide was the most promising among six RTILs screened, in terms of both ionic conductivity and constant current cycling.

Polyimide

Phase Stability and Electrochemical Performance of La-Site-Doped Li6La3Zr0.5Nb0.5Ta0.5Hf0.5O12 High-Entropy Garnets

We investigate La-site substitution in the high-entropy garnet Li6La3Zr0.5Nb0.5Ta0.5Hf0.5O12 (LLZNTH) using Ba2+, Sr2+, and Sm3+ to elucidate how dopant governs phase stability, Li-site distribution, and electrochemical behavior. X-ray diffraction shows that Sr2+ is incorporated homogeneously into the garnet lattice, whereas the larger Ba2+ and smaller Sm3+ ions partially exceed the structural tolerance, generating secondary phases. Nevertheless, the Sm-doped composition (x = 0.05) exhibits the highest room-temperature ionic conductivity (2.7 × 10–4 S cm–1). Neutron powder diffraction reveals that Sm substitution drives a redistribution of Li+ from the tetrahedral 24 d sites into the higher-mobility 96 h positions, enhancing the connectivity of the three-dimensional Li-ion migration network. A Sm-doping series (x = 0.01–0.05) further shows that only sufficiently high Sm levels induce this redistribution, whereas lower concentrations retain Li arrangements similar to the undoped garnet. Critical current density measurements demonstrate that La-site dopants also influence interfacial stability against Li metal, underscoring a trade-off between bulk transport enhancement and mechanical robustness. Collectively, these findings reveal that in high-entropy garnets improved ionic conductivity can originate not only from phase-pure structures but also from targeted modification of the Li sublattice, even when accompanied by secondary phases, offering a compositional design principle for garnet electrolytes.

Li, Chang [Mechanical Engineering, School of Scien

Revealing key structures for reversible sulfur redox in amorphous polymeric sulfur

Amorphous polymeric sulfur cathodes, such as sulfurized polyacrylonitrile (SPAN), enable high-energy lithium-sulfur batteries without cobalt or nickel, leveraging abundant sulfur. However, the limited in situ understanding of their synthesis and electrochemistry has impeded targeted optimization. Here, in this study, we integrate operando high-energy total scattering with sulfur K-edge X-ray absorption spectroscopy to monitor SPAN's formation and cycling in real time. Our results show that S-C bond formation halts further fusion of cyclized polyacrylonitrile, fostering π-π stacking and a transition from long-chain to short-chain sulfur-critical for reversible sulfur redox. These features synergistically minimize polysulfide dissolution and charge-transfer resistance, enabling optimized SPAN to achieve high capacity retention over 1,000 cycles. Operando X-ray absorption spectroscopy reveals that residual protons drive thiol-thione tautomerism, with lithium replacement during the first discharge causing ~20% irreversible capacity loss. To enhance performance, minimizing -NH groups and expanding pyridine networks are key. These findings transform SPAN optimization from empirical tuning to mechanism‑guided engineering and point the way towards sulfur loadings and energy densities competitive with state‑of‑the‑art Li‑ion cathodes.

25 ENERGY STORAGE

Unraveling interphase-driven failure pathways in LiMn0.6Fe0.4PO4/graphite pouch cells

LiMnxFe1−xPO4 (LMFP) is a promising high-voltage, thermally stable, and earth-abundant cathode material, yet its practical application is limited by interphase instability and Mn dissolution. In this work, we systematically evaluate LiMn0.6Fe0.4PO4/graphite pouch cells using three electrolyte formulations including control carbonate electrolyte, control + 2 wt% vinylene carbonate (VC), and control + 2 wt% VC + 1 wt% 1,3,2-dioxathiolane 2,2-dioxide (DTD), to establish how electrolyte composition governs interphase chemistry and long-term degradation. Electrochemical testing shows that both additives are preferentially reduced prior to ethylene carbonate (EC) during cell formation, generating robust cathode-electrolyte interphase (CEI) and solid-electrolyte interphase (SEI) layers that suppress gas evolution and raise the first-cycle coulombic efficiency to 89.3%. Additionally, the dual-additive electrolyte delivers the most stable performance, retaining over 85% capacity after 600 cycles while minimizing impedance growth under long-term cycling at C/3 and 40 °C. Soft X-ray absorption spectroscopy confirms that VC + DTD effectively suppresses electrolyte oxidation at the cathode surface, and micro-X-ray fluorescence shows substantially reduced Mn dissolution and deposition on the graphite anode. Density functional theory simulations further provided insights into the structural and energetic influences of alkoxide species on the cathode surface, proposing a Mn2+ extraction mechanism. The combined experimental and computational findings establish a mechanistic link between electrolyte composition and interphase evolution, highlighting the effectiveness of electrolyte engineering for extending the operational lifetime of LMFP-based lithium-ion batteries.

Chak, Chanmonirath Michael

Observation of N-rich solid-electrolyte interphase by ToF-SIMS.

Formation of a stable solid electrolyte interphase (SEI) between lithium electrodes and electrolyte upon multiple charge/discharge cycles is crucial to a long-term lithium-ion battery performance. Addition of LiNO3 to lithium bis (fluorosulfonyl) imide/poly(ethylene oxide) (LiFSI/PEO) electrolyte leads to a durable SEI that is electrically insulating yet highly conductive to Li ions, chemically and electrochemically stable, physically uniform, and mechanically robust. ToF-SIMS was used here in combination with sputtering by a gaseous cluster ion beam (GCIB) to examine how the addition of a small proportion of LiNO3 to the LiFSI/PEO electrolyte affects the SEI composition. Negative ion ToF-SIMS spectra of the cycled samples display an intense m/z 26 peak associated with the SEI. Exact mass assignments and isotopic ratios indicate that this peak should be assigned as (CN-)-C-12, with little to no negative secondary ion signal arising from (LiF-)-Li-7. This CN- signal appears to arise from an N-rich portion of the SEI adjacent to the Li electrode that is depleted in LiF relative to the bulk electrolyte. The dearth of LiF- (and LiF+ from the positive ion spectra) is unexpected because LiF has been identified in the SEI in similar samples. Finally, GCIB sputtering indicates that the SEI adheres more strongly to the Li electrode than to the LiFSI/PEO electrolyte.

Shavandi, Seyedeh Reyhaneh

Sodium-Ion Battery Cathode with Dominating Copper and Oxygen Redox Chemistry

Sodium-ion batteries offer low-cost energy storage solutions for the grid and electric vehicles, leveraging the established "rocking-chair" Li-ion design and the natural abundance of sodium. However, SIBs face challenges such as relatively lower voltage and capacity than lithium-ion batteries, as well as dependence on nickel resources. Here, in this work, a new nickel-free cathode material, Na 0.75 Li 0.08 Cu 0.25 Mn 0.66 O 2 , was designed and synthesized. This material has a capacity of ~125 mAh/g and an average discharge voltage of 3.5 V. Notably, more than one-third of the capacity arises from lithium substitution of Cu (~8 mol.%) and high voltage activation to 4.6 V. Multimodal synchrotron x-ray characterization combining spectroscopy, microscopy, and scattering reveal the capacity is primarily from the redox of copper and oxygen, with a minor contribution from the manganese redox. Lithium substitution alters the phase transition mechanism from a two-phase transition in P3-Na 2/3 Cu 1/3 Mn 2/3 O 2 to a solid-solution in Na 0.75 Li 0.08 Cu 0.25 Mn 0.66 O 2 , enhancing the reversibility of this material.

25 ENERGY STORAGE

Atomic- and Molecular-Scale Interphase Engineering for High-Performance Solid-State Batteries

Solid-state batteries (SSBs) promise a decisive advance beyond conventional Li-ion systems, yet their development remains constrained by persistent solid–solid interfacial instabilities that degrade performance and durability. Interfaces between solid electrolytes and both cathodes and Li metal often exhibit poor wettability, limited physical contact, and high charge–transfer resistance, leading to chemical decomposition, mechanical failure, and impedance growth. Overcoming these limitations requires interphase engineering with atomic-scale precision—capabilities that conventional coating methods cannot reliably deliver. Atomic layer deposition (ALD) and molecular layer deposition (MLD) uniquely meet this need by enabling ultrathin, conformal, and composition-tunable films that stabilize reactive surfaces, suppress parasitic reactions, and regulate Li-metal morphology. Importantly, this Perspective highlights ALD/MLD systems that have already demonstrated effectiveness in liquid-electrolyte cells and discusses how these validated strategies can be deliberately translated to solid-state architectures. By grounding future directions in experimentally proven concepts rather than speculative hypotheses, we outline how atomic- and molecular-scale design principles can accelerate the development of robust, high-performance SSB technologies.

atomic and molecular layer deposition

Probing Operando Electrochemical Strain Generation in α-NaFeO 2 Composite Cathodes during Cycling of Na-Ion Batteries

The transition metal oxide (TMO) cathodes in Na-ion batteries suffer from low-capacity retention. Chemo-mechanical instabilities lead to the deterioration of the electrochemical performance of TMO cathodes in Li-ion batteries. However, there is not much known about the chemo-mechanical instabilities in the TMO cathodes for Na-ion batteries. Understanding the governing forces behind the interplay between the electrochemical performance and mechanical stability in TMO cathodes is critical for the development of Na-ion batteries. Here, we synchronize the digital image correlation (DIC) technique with electrochemical analysis to capture the real-time deformation behavior of the α-NaFeO 2 cathodes during cycling. When the charge cutoff voltage is 3.6 V, the cathode experiences reversible deformations (except for the first cycle). There is negative strain (shrinkage) generation during Na extraction and positive strain (expansion) generation during the subsequent Na insertion. A detailed analysis of the potential-dependent strain rate evolution points out complicated phase transformations and nonequilibrium conditions in the α-NaFeO 2 cathodes during cycling. When the charge cutoff voltage was increased to 4.2 V, there was a rapid capacity loss and large plastic deformations in the α-NaFeO 2 cathodes. We provide an in-depth discussion about the possible mechanisms behind the chemo-mechanical instabilities in the α-NaFeO 2 . In conclusion, the correlation is critical to develop material-based strategies to mitigate instability mechanisms in TMO cathodes for Na-ion batteries.

Wable, Minal [University of Maryland Baltimore Cou

Probing the role of local tunnel variations in early-stage lithiation of α-MnO₂ nanowires via in situ TEM

Understanding lithium-ion transport in tunnel-structured manganese oxides is essential for designing high-performance lithium-ion battery electrode materials. Here, we elucidate the early-stage lithiation mechanism of potassium-stabilized α-MnO 2 nanowires using in situ transmission electron microscopy (TEM) coupled with electron energy-loss spectroscopy (EELS), high-resolution TEM (HRTEM), and geometric phase analysis (GPA). Real-time TEM imaging reveals clear volume expansion at the reaction front, while EELS analysis uncovers lithium-ion diffusion far beyond this region, where no visible expansion is observed, indicating fast, defect-assisted transport. GPA and HRTEM analyses show that localized tensile and compressive strain fields, originating from pre-existing local tunnel structural variations, persist after lithiation. The tensile-strained regions enable lithium-ion insertion with minimal lattice distortion, offering additional free volume that facilitates rapid lithium-ion accommodation ahead of the structural transformation. Our results demonstrate a local tunnel variation-mediated fast diffusion pathway that precedes bulk reaction, underscoring the critical role of local strain in enabling early-stage lithium transport. Given the structural versatility of MnO 2 and its ability to accommodate diverse atomic arrangements beyond the well-known tunnel phases (β-, γ-, δ-, λ-, R-phases), our findings highlight the importance of understanding and engineering local structural environments. This work provides fundamental insights into the interplay between defects, strain, and ion dynamics, and presents defect engineering as a promising approach to enhance both rate performance and structural stability in manganese-based cathodes.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND

Manganese‐Based Spinel Cathodes: A Promising Frontier for Solid‐State Lithium‐Ion Batteries

Recently, all-solid-state lithium-ion batteries (ASSLIBs), which exhibit improved safety and enhanced energy density compared to conventional commercialized lithium-ion batteries (LIBs), thereby have garnered extensive research interest. Among the promising cathode candidates, Mn-based spinel cathodes LiMn 2 O 4 (LMO) and LiNi 0.5 Mn 1.5 O 4 (LNMO), with the unique characteristics of low cost, structural stability, and 3D Li-ion diffusion channels, have demonstrated excellent performance in LIBs and presented great potential in ASSLIBs applications. However, several challenges, including structural degradations, poor interfacial contact, large interfacial resistance, and Mn-dissolution/diffusion during the electrochemical cycling, hinder their practical applications and commercialization in the ASSLIBs. Particularly, the high-voltage LNMO cathodes suffer from the challenge of electrochemical incompatibility with most of the solid-state electrolytes (SSEs). Herein, the spinel structure, the electrochemical behavior, and the structural degradation of the LMO/LNMO are explored. The characteristics and recent progress of the mitigating strategies to the challenges of various SSEs, including polymer-, oxide-, composite-, sulfide-, halide-, and LiPON-based SSEs, are introduced when paired with LMO/LNMO. Finally, the directions for future research to advance Mn-based spinel cathodes and fulfill the requirements of the next-generation ASSLIBs are also discussed.

Dou, Yu [Concordia University, Montreal, QC (Canad

Unveiling the lithium-ion transport mechanism in Li{sub 2}ZrCl{sub 6} Solid-State Electrolyte {ital via} deep learning-accelerated molecular dynamics simulations.

Lithium zirconium chlorides (LZCs) present a promising class of cost-effective solid electrolytes for next-generation all-solid-state batteries. The unique crystal structure of LZCs plays a crucial role in facilitating lithium-ion mobility, which further affects the electrochemical performance. To understand the underlying mechanism governing ion transport, we employed deep learning-accelerated molecular dynamics simulation on Li2ZrCl6 (trigonal alpha- and monoclinic beta-LZC), focusing specifically on the zirconium coordination environment. Our results reveal that disordered alpha-LZC exhibits the highest ionic conductivity, while beta-LZC demonstrates significantly lower conductivity, closely aligning with experimental findings. The study confirms that across all phases, lithium migration proceeds via the site-to-site hopping mechanism, where variations in site residence times critically impact the overall ionic conductivity. In alpha-LZCs, lithium ions prefer to anisotropically diffuse across interlayers as the result of a lower energy barrier, driven primarily by collective diffusion. In contrast, lithium ions in beta-LZC primarily isotropically diffuse within the intralayer, hindered by higher energy barriers and determined by individual diffusion. The variation in ZrCl6 2- octahedral unit softening, induced by the specific layered arrangement of zirconium atoms, emerges as a critical determinant of the energy barriers across the LZC phases. These atomic-scale insights into the transport processes provide valuable guidance for the rational design and optimization of LZCs-based electrolytes, accelerating their practical application in advanced energy storage technologies.

Guo, Hanzeng

Review on Preprocessing Strategies, Deactivation, Thermal Safety, and Future Perspectives in Lithium-Ion Battery Recycling

The rapid growth in the use of lithium-ion batteries (LIBs) in electric vehicles, consumer electronics, and renewable energy storage has made effective end-of-life management essential. Recycling LIBs is critical not only for resource recovery and environmental protection but also for ensuring safety and economic viability. This review focuses on the preprocessing technologies that precede typical recovery processes, including disassembly, sorting, discharging, electrolyte removal, dismantling, thermal treatment, separation, and flotation. These steps play a foundational role in determining the efficiency, safety, and environmental impact of LIB recycling. LIBs pose substantial fire and explosion risks due to residual charge, flammable electrolytes, and reactive materials. The conditions and successive progression of the exothermic reactions which lead to thermal runaway has been discussed. It also explores secure deactivation techniques such as external circuit discharge, saline immersion, and thermomechanical methods, alongside fire prevention strategies including the use of flame retardants, elimination of oxidants, and reduction of heat generation and accumulation. Challenges and future directions are outlined, highlighting the need for standardized designs, automation, and safer, more sustainable recycling infrastructure. Furthermore, this review is distinguished by its focused analysis of preprocessing and deactivation steps, with particular attention to the thermal safety engineering aspects of LIB recycling.

Battery deactivation