Advanced LiFSI-LiPF6 Electrolyte for Wide-Temperature and Thermally Stable Lithium-Ion Batteries

Abstract

A new optimized LiFSI–LiPF6 dual-salt controlled-solvation electrolyte (E-DS) is demonstrated to enable practical graphite||LiNi0.8Mn0.1Co0.1O2 cells (˜4.0 mAh cm?²) to achieve exceptional performance and safety under extreme conditions. By optimizing anion coordination with the smaller, more dissociating FSI? anion, the E-DS forms ultrathin, dense, and inorganic-rich electrode/electrolyte interphases that dramatically suppress solvent decomposition, transition-metal dissolution, and surface reconstruction compared to the conventional LiPF6/carbonate electrolyte. Consequently, E-DS cells deliver >78% capacity retention after 300 cycles at 60 °C, retain fast discharging capacity at 30 °C, and operate effectively at -20 °C. Most strikingly, fully charged full cells with E-DS, even under overcharging to 4.8 V, show a lower heat evolution in stable formulations — transforming a traditionally unstable high-voltage/high-temperature configuration into an intrinsically safe state. This work establishes a new benchmark for carbonate-containing electrolytes, simultaneously achieving high energy density, fast-discharging capability, wide-temperature operation (-20 to 60 °C), and outstanding thermal safety in nickel-rich lithium-ion batteries.

Explore related subjects

Keep this discovery

BibTeXRIS

Kautz, David Joseph J., Lim, Hyung-Seok (ORCID:0000000225990405), Faruk, Omar, Gao, Peiyuan, Xu, Yaobin (ORCID:0000000299453514), Kim, Un-Hyuck, Zhong, Lirong, Buyuker, Isiksu, Zhou, Hui, Zhang, Dongshe, Fan, Jiang, Whittingham, M. S., Wang, Chongmin (ORCID:0000000333270958), Xu, Wu (ORCID:0000000226858684). 2026-03-25. Advanced LiFSI-LiPF6 Electrolyte for Wide-Temperature and Thermally Stable Lithium-Ion Batteries. https://doi.org/10.1149/1945-7111/ae5348

Cite the original work for its findings. Save a collection to share your selection of sources.

Discover connections

Connections use source metadata and explicit phrase matches, not verified experimental comparisons.

KEEP EXPLORING

Related reports

Observation of N-rich solid-electrolyte interphase by ToF-SIMS.

Formation of a stable solid electrolyte interphase (SEI) between lithium electrodes and electrolyte upon multiple charge/discharge cycles is crucial to a long-term lithium-ion battery performance. Addition of LiNO3 to lithium bis (fluorosulfonyl) imide/poly(ethylene oxide) (LiFSI/PEO) electrolyte leads to a durable SEI that is electrically insulating yet highly conductive to Li ions, chemically and electrochemically stable, physically uniform, and mechanically robust. ToF-SIMS was used here in combination with sputtering by a gaseous cluster ion beam (GCIB) to examine how the addition of a small proportion of LiNO3 to the LiFSI/PEO electrolyte affects the SEI composition. Negative ion ToF-SIMS spectra of the cycled samples display an intense m/z 26 peak associated with the SEI. Exact mass assignments and isotopic ratios indicate that this peak should be assigned as (CN-)-C-12, with little to no negative secondary ion signal arising from (LiF-)-Li-7. This CN- signal appears to arise from an N-rich portion of the SEI adjacent to the Li electrode that is depleted in LiF relative to the bulk electrolyte. The dearth of LiF- (and LiF+ from the positive ion spectra) is unexpected because LiF has been identified in the SEI in similar samples. Finally, GCIB sputtering indicates that the SEI adheres more strongly to the Li electrode than to the LiFSI/PEO electrolyte.

Shavandi, Seyedeh Reyhaneh

Heterogeneous Solid Electrolyte Interphase Interactions Dictate Interface Instability in Sodium Metal Electrodes

Sodium (Na) metal batteries have attracted recent attention due to their low cost and high abundance of Na. However, the advancement of Na metal batteries is impeded due to key challenges such as dendrite growth, solid electrolyte interphase (SEI) fracture, and low Coulombic efficiency. This study examines the coupled electro‐chemo‐mechanical interactions governing the electrodeposition stability and morphological evolution at the Na/electrolyte interface. The SEI heterogeneities influence transport and reaction kinetics leading to the formation of current and stress hotspots during Na plating. Further, it is demonstrated that the heterogeneity‐induced Na metal evolution and its influence on the stress distribution critically affect the mechanical overpotential, contributing to a faster SEI failure. The analysis reveals three distinct failure mechanisms—mechanical, transport, and kinetic—that govern the onset of instabilities at the interface. Finally, a comprehensive comparative study of SEI failure in Na and lithium (Li) metal anodes illustrates that the electrochemical and mechanical characteristics of the SEI are crucial in tailoring the anode morphology and interface stability. This work delineates mechanistic stability regimes cognizant of the SEI attributes and underlying failure modes and offers important guidelines for the design of artificial SEI layers for stable Na metal electrodes.

25 ENERGY STORAGE

Mechanistic Understanding of Interphase-driven Aging in Silicon Anodes

Conventional solid electrolyte interphases (SEIs) strongly adhere to micro-silicon (µ-Si) and crack under volume changes, causing poor cycling performance. Nano-silicon improves cycling performance but remains costly with limited calendar life. Here potentiostatic ageing tests demonstrate that both calendar and cycle ageing are governed by SEI cracking and dissolution with different relative contributions. When the system is not dominated by SEI dissolution, the relative calendar life of Si anodes could correlates positively with their cycle life. LiF-rich SEI that enables long cycle life in µ-Si is therefore expected to enhance calendar life as well. Using this framework, we screened electrolytes, SEIs and electrodes and validated them with full-cell storage. LiF-rich SEI minimizes cracking and dissolution, enabling μ-Si to achieve excellent calendar life, whereas nano-silicon suffers from SEI dissolution and needs reduced electrolyte–electrode contact for better calendar life. This work clarifies calendar-ageing behaviour and accelerates electrolytes and SEI development for long-life Si anodes.

Johnson, Christopher S.