Module-Level Solutions For Degradation by Ionization Damage

After years of improving module efficiency while targeting mean degradation rates of 0.5 to 0.6 %/y for crystalline silicon technology, there is much evidence that the degradation rates are now increasing significantly. Contributing factors include:Radiation damage (UV-Light Induced Degradation): Trina solar: -4.5%/y degradation rate in Singapore, DOE National Laboratory Regional Test Centers showed degradation of -1% < r < -2%/y in crystalline silicon modules, Jinko Solar: -4% < r < -7% efficiency loss from 540 MJ/m-2 of UV-A light, ISFH: 15% relative power loss during of 1.8 GJ/m-2 UV exposure, attributed to H+. Electrical bias from positive system voltage (e.g., +1000 V, +1500 V) can drive ions and metallization through the encapsulation, NREL: Ion transport can affect the cell passivation, resulting in power loss of 5% to 40% in p-PERC+ (bifacial), NREL: Damage at cell rear with up to 17% power at cell fronts in n-PERT modules. Delamination can also occur due to cell surface reactions driven by light and bias.

module efficiency↗

Silicon Heterojunction Field Performance

The market share of silicon heterojunction (SHJ) modules are expected to increase in the following years. The presentation discusses field performance of SHJ and compares it to other high-efficiency modules. In-depth materials characterization is used to understand the origins of degradation in these type of modules.

ENGINEERING,SOLAR ENERGY↗

A study of degradation mechanisms in PVDF-based photovoltaic backsheets

Abstract Commercial backsheets based on polyvinylidene fluoride (PVDF) can experience premature field failures in the form of outer layer cracking. This work seeks to provide a better understanding of the changes in material properties that lead to crack formation and find appropriate accelerated tests to replicate them. The PVDF-based backsheet outer layer can have a different structure and composition, and is often blended with a poly(methyl methacrylate) (PMMA) polymer. We observed depletion of PMMA upon aging with sequential (MAST) and combined (C-AST) accelerated stress testing. In field-aged samples from Arizona and India, where PVDF crystallizes in its predominant α-phase, the degree of crystallinity greatly increased. MAST and C-AST protocols were, to some extent, able to replicate the increase in crystallinity seen in PVDF after ~ 7 years in the field, but no single-stress test condition (UV, damp heat, thermal cycling) resulted in significant changes in the material properties. The MAST regimen used here was too extreme to produce realistic degradation, but the test was useful in discovering weaknesses of the particular PVDF-based outer layer structure studied. No excessive β-phase formation was observed after aging with any test condition; however, the presence of β-phase was identified locally by Fourier transform infrared spectroscopy (FTIR). We conclude that both MAST and C-AST are relevant tests for screening outdoor failure mechanisms in PVDF backsheets, as they were successful in producing material degradation that led to cracking.

14 SOLAR ENERGY↗

UV‐induced degradation of high‐efficiency silicon PV modules with different cell architectures

Abstract Degradation from ultraviolet (UV) radiation has become prevalent in the front of solar cells due to the introduction of UV‐transmitting encapsulants in photovoltaic (PV) module construction. Here, we examine UV‐induced degradation (UVID) in various commercial, unencapsulated crystalline silicon cell technologies, including bifacial silicon heterojunction (HJ), interdigitated back contact (IBC), passivated emitter and rear contact (PERC), and passivated emitter rear totally diffused (PERT) solar cells. We performed UV exposure tests using UVA‐340 fluorescent lamps at 1.24 W·m −2 (at 340 nm) and 45°C through 4.02 MJ·m −2 (2000 h). Our results showed that modern cell architectures are more vulnerable to UVID, leading to a significant power decrease (−3.6% on average; −11.8% maximum) compared with the conventional aluminum back surface field (Al‐BSF) cells (<−1% on average). The power degradation is largely caused by the decrease in short‐circuit current and open‐circuit voltage. A greater power decrease is observed in bifacial cells with rear‐side exposure compared with those with front‐side exposure, indicating that the rear side is more susceptible to UV damage. Secondary ion mass spectroscopy (SIMS) confirmed an increase in hydrogen concentration near the Si/passivation interface in HJ and IBC cells after UV exposure; the excess of hydrogen could result in hydrogen‐induced degradation and subsequently cause higher recombination losses. Additionally, surface oxidation and hot‐carrier damage were identified in PERT cells. Using a spectral‐based analysis, we obtained an acceleration factor of 5× between unpackaged cells (containing a silicon nitride antireflective coating on the front) in the UV test and an encapsulated module (with the front glass and encapsulant blocking 90% of the UV at 294 nm and 353 nm, respectively) in outdoor conditions. From the analytical calculations, we show that a UV‐blocking encapsulant can reduce UV transmission in the module by an additional factor of ~50.

14 SOLAR ENERGY↗

Automating Component-Level Stress Measurements for Inverter Reliability Estimation

In the near future, grid operators are expected to regularly use advanced distributed energy resource (DER) functions, defined in IEEE 1547-2018, to perform a range of grid-support operations. Many of these functions adjust the active and reactive power of the device through commanded or autonomous operating modes which induce new stresses on the power electronics components. In this work, an experimental and theoretical framework is introduced which couples laboratory-measured component stress with advanced inverter functionality and derives a reduction in useful lifetime based on an applicable reliability model. Multiple DER devices were instrumented to calculate the additional component stress under multiple reactive power setpoints to estimate associated DER lifetime reductions. A clear increase in switch loss was demonstrated as a function of irradiance level and power factor. This is replicated in the system-level efficiency measurements, although magnitudes were different—suggesting other loss mechanisms exist. Using an approximate Arrhenius thermal model for the switches, the experimental data indicate a lifetime reduction of 1.5% when operating the inverter at 0.85 PF—compared to unity PF—assuming the DER failure mechanism thermally driven within the H-bridge. If other failure mechanisms are discovered for a set of power electronics devices, this testing and calculation framework can easily be tailored to those failure mechanisms.

Flicker, Jack (ORCID:0000000212232154)↗

Failure Mode and Effects Analysis for a Photovoltaic Inverter

While PV panel reliability continues to increase, PV inverters become the limiting factor for PV system reliability. Consequently, it is critical to have a generic tool from a third party for PV inverter reliability assessment to help 1) utilities/PV farm operators schedule maintenance in advance, and 2) inverter developers improve the next-generation design. However, these two things cannot be accomplished without first understanding the reasons behind inverter failure. Following this idea, as the first step, it is essential to identify and investigate the most failure-prone components within a PV inverter system. After all, any system is only as reliable as the components that are contained within it. This motivates the failure mode and effects analysis (FMEA) work presented for this workshop. The FMEA is conducted as follows: first, the overview of the methodology on the development of the FMEA is presented; then, based on a top-down approach starting from the PV inverter system, critical inverter components with high failure rates are identified and summarized; afterward, a thorough FMEA study at a component-level is performed and its results, including failure modes, failure mechanisms, and critical stressors, are tabulated; finally, according to three rankings (chance of occurrence, severity of occurrence, and ease of detection prior to failure) for each failure mechanism provided by the FMEA, risk priority numbers are calculated and the failure mechanisms along with the critical stressors are ranked in terms of their potentially detrimental effect on the PV inverter.

Brown, Buck↗

Evaluating the Durability of Balance of Systems Components Using C-AST

The testing of branch- and cable-connectors, and fuses in C-AST is introduced. A significant effect was observed when mechanical actuation was introduced to the benchtop prototype testing. Therefore, this presentation emphasizes the mechanical test fixture, data acquisition system, failure analysis of the components used in specimen assemblies, and the validation of the results relative to field failed samples.

components↗

Potential-induced degradation of Cu(In,Ga)Se 2 can occur by shunting the front i-ZnO and by damaging the p-n junction

In this work we test field-relevant potential-induced degradation (PID) behavior by encapsulating laboratory Cu(In,Ga)Se 2 (CIGS) solar cells and applying +1000 V uniformly on the face of the front glass. In this configuration, we find that K-rich borosilicate glass reduces the extent of PID relative to Na-rich soda-lime glass. We also find that the standard testing protocol of stressing cells at short-circuit leads to faster PID than stressing cells at open-circuit. We characterize two types of CIGS PID: The first, front shunting PID, is driven by front-glass stress and occurs when alkali metal cations accumulate in the i-ZnO buffer, where they increase shunt conductance to reduce fill factor. The second, p-n junction PID, results from back-glass stress as alkali metal cations pile up near the CIGS surface/CdS buffer, where they reduce charge carrier concentration, open-circuit voltage, and fill factor to degrade efficiency ~160 times faster than front shunting PID.

14 SOLAR ENERGY↗

Impact of illumination and encapsulant resistivity on polarization-type potential-induced degradation on n-PERT cells

Power loss caused by polarization-type potential-induced degradation (PID-p) in a variety of high-performance photovoltaic cell types has been observed to be recoverable via subsequent illumination and in some cases preventable via simultaneous illumination. In this report, we describe the results of a study in which the front faces of n-PERT cells encapsulated in polymers with a broad range of electrical resistivity were exposed to varying and controlled irradiance during PID testing. For a low resistivity ethylene-vinyl acetate copolymer encapsulant, no reduction in the rate or extent of power loss was observed for irradiance as high as 1,000 W/m 2 , whereas for high and intermediate resistivity polyolefin encapsulants, 100 and 300 W/m 2 , respectively, prevented power loss. We introduce a simple model based on charge accumulation that facilitates interpretation of these results whereby degradation via charge accumulation under voltage stress and recovery due to light exposure are opposing and interdependent phenomena that describe the susceptibility of a module to power loss.

14 SOLAR ENERGY↗

Development of Mission Profiles for Humidity Models in the Reliability Testing of PV Inverters: Preprint

To understand the impacts of humidity on PV inverters, mission profiles were developed to accurately describe the different processes and rates based on the environmental factors of temperature, relative humidity, and irradiance. The operating environment of the device introduces stress factors dependent on component temperature, relative humidity, and component voltage. The development of profiles started from looking at historical climate conditions at Cocoa, Florida, a hot and humid location. The profile developed from field location was compared with existing humidity test profiles in industrial and military standards to determine acceleration factors. Prior to the evaluation of the mission profiles, critical components in the PV inverter were identified based on vendor discussions along with failure modes of interest. The profiles considered in this study was demonstrated using a 4-kVA string inverter. The measurements from the devices were substituted in device manufacturer specified equation to determine the severity of each test. The severity of each test was compared against the severity of the 24-hour result to determine the acceleration factor of each test. The acceleration factors were determined to be over a range of 1.2-6 for the existing humidity tests from standards, when compared against the mission profile developed from field data. This optimal humidity/thermal profile will be passed to the IEC standards development for inverter qualification testing.

humidity models↗

Assessing UV-Induced Degradation in Bifacial Modules of Different Cell Technologies

Bifacial technology enables solar cells to offer higher power output and lower levelized cost of energy compared to their monofacial counterparts. Here, we examined the adverse effects of ultraviolet-induced degradation (UVID) on a variety of high-efficiency silicon wafer-based bifacial cell technologies, including silicon heterojunction (SHJ), interdigitated back contact (IBC), passivated emitter rear contact (PERC), and passivated emitter rear totally-diffused (PERT). Both the front and rear sides of bifacial cells without any encapsulation were exposed to an artificially accelerated UV exposure test. After 2000 h of UV irradiation, the bifacial cells exhibited greater power loss with backside exposure indicating potential sensitivity of the rear passivation to UV. The highest power degradation is observed in SHJ cells, followed by p-PERC and n-PERT cell technologies. The degradation in SHJ cells is attributed to the reduction in V oc and FF, while the degradation in p-PERC and n-PERT cells is correlated with a significant drop in I sc . This suggests that each cell type/make degrades via different degradation pathways.

bifacial cells↗

Failure Analysis of a New Polyamide-Based Fluoropolymer-Free Backsheet After Combined-Accelerated Stress Testing

The viability of novel coextruded, fluoropolymer-free backsheets for photovoltaic (PV) modules has been questioned as a result of a large number of early-life backsheet failures in PV installations containing one of the earliest co-extruded polyamide (PA)-based backsheet to reach the market, “AAA.” New PV reliability testing protocols have been recently developed and applied to backsheets to reproduce failures observed in the field and evaluate the durability of novel backsheet materials and designs prior to commercialization. A new co-extruded PA-based backsheet was tested using combined-accelerated stress testing (C-AST) and demonstrated a greater lifetime than AAA, and some other fluoropolymer-based backsheets such as polyvinylidene fluoride. The improved PA-based backsheet also eventually failed by through-thickness cracking. Using surface and bulk material characterization techniques, we performed a comprehensive study of material properties before and after the stress testing. Aging of the backsheet resulted in an increase of surface roughness by erosion of the outer PA layer. However the failure is more likely related to an increase in crystallinity of the polyolefin core layer reducing the backsheet tearing energy. The analysis can ultimately inform on the specific weaknesses of the materials so that the manufacturer can improve the backsheet design to extend its lifetime.

14 SOLAR ENERGY↗

Understanding interfacial chemistry of positive bias high-voltage degradation in photovoltaic modules

Photovoltaic module degradation from a high system voltage is a prevalent degradation mode in the field, where the enabling degradation mechanisms are inherently dependent on the voltage bias polarity of the installed system. In this study, the effects of positive bias on module performance are confirmed and the underlying chemical degradation processes are more thoroughly investigated to reveal different degradation pathways from those previously reported in negative bias studies. When cells are under +1000 V stress, crystalline silicon mini-modules with poly(ethylene-co-vinyl acetate) (EVA) encapsulant demonstrated a significant photocurrent loss due to EVA discoloration and delamination from increased chemical reactivity at the front-side EVA/cell metallization interface. Brown discoloration of the EVA encapsulant near the cell gridlines is linked to an electrochemical reaction at the Ag gridlines under hot and humid conditions (85 °C, 85% relative humidity). Chemical compositional analysis using X-ray photoelectron spectroscopy (XPS) confirmed that the discoloration is attributed to the formation of silver sulfide (Ag 2 S) and/or silver oxide (Ag 2 O) species at the EVA/Ag gridline interface. The subsequent migration of Ag ions from the cell gridlines into the bulk of the EVA was evident from XPS depth profiling and optical microscopy. However, the Ag signal was not detected at the EVA/glass interface, inferring limited ionic transport through the nominally 0.45 mm thick encapsulant. For the samples studied herein, the sulfur is believed by the process of elimination to come from the ambient air, diffusing into the module through the permeable polymer backsheet.

14 SOLAR ENERGY↗

Towards validation of combined-accelerated stress testing through failure analysis of polyamide-based photovoltaic backsheets

Abstract Novel methods for advancing reliability testing of photovoltaic (PV) modules and materials have recently been developed. Combined-accelerated stress testing (C-AST) is one such method which has demonstrated reliable reproduction of some field-failures which were not reproducible by standard certification tests. To increase confidence and assist in the development of C-AST, and other new testing protocols, it is important to validate that the failure modes observed and mechanisms induced are representative of those observed in the field, and not the product of unrealistic stress conditions. Here we outline a method using appropriate materials characterization and modelling to validate the failure mechanisms induced in C-AST such that we can increase confidence in the test protocol. The method is demonstrated by applying it to a known cracking failure of a specific polyamide (PA)-based backsheet material. We found that the failure of the PA-based backsheet was a result of a combination of stress factors. Photo-oxidation from ultra-violet (UV) radiation exposure caused a reduction in fracture toughness, which ultimately lead to the cracking failure. We show that the chemical and structural changes observed in the backsheet following C-AST aging were also observed in field-aged samples. These results increase confidence that the conditions applied in C-AST are representative of the field and demonstrates our approach to validating the failure mechanisms induced.

14 SOLAR ENERGY↗

Highly Accelerated UV Stress Testing for Transparent Flexible Frontsheets

There are many photovoltaic (PV) applications where lighter weight and/or bendable PV power would be beneficial. This includes the curved surfaces of buildings, buildings with weight limitations, boats, automobiles, or other portable applications. In many of these cases, the bending will be only a single occurrence at installation or the amount of bending, even if repeated, is not dramatic. This allows for crystalline silicon modules to be used. For flexible applications, the dominant material for the frontsheet is polyethylene tetrafluoroethylene (PETFE). As a fluoropolymer it resists soiling, is UV stable, and PETFE is a more mechanically durable fluoropolymer. However, in the interests of keeping costs down, less expensive alternative polymers are desirable. In this study, highly accelerated ultraviolet light and heat stresses are applied to candidate materials and the degradation kinetics are determined to provide information to evaluate their suitability for use in a PV application.

41 EE - Solar Energy Technologies Office (EE-4S)↗