Highly Accelerated UV Stress Testing for Transparent Flexible Frontsheets
Not Available
Engineering topics
Publications and source records attributed to Hacke, Peter.
Not Available
Combined-accelerated stress testing (C-AST) simultaneously combines stress factors of the natural environment (including UV radiation, temperature, humidity, electrical current, and external mechanical force) into a single test that requires fewer modules, fewer chambers, and makes it possible to discover weaknesses in new designs that are not known a-priori. C-AST reduces risk, accelerates time to market, and improves bankability by reducing costly overdesign using test levels not exceeding those seen in the natural environment. This project seeks to evaluate strengths and weaknesses of modern cell interconnect designs with combined-accelerated stress testing (C-AST) to screen multiple climates along with finite element and failure analysis to determine the potential for a 50-year life. Supporting this, we seek to develop methods of characterization to assess the degradation of interconnects, enable predictive rate models with material forensics and FEA and show C-AST's ability to find interconnect failures and benchmark it relative to other accelerated stress test methods like temperature cycling and cyclic dynamic mechanical loading. Examples of modern interconnect designs covered are Canadian Solar Hetero Technology ribbon enabling closer cell interconnections, SmartWire (eg. Meyer-Berger technology), and shingled cells with new interconnect materials.
The direct current bias for photovoltaic (PV) modules interconnected in series-strings may include both high voltage negative (“HV-”) and positive (“HV+”) polarity with respect to the electrical ground. Multiple degradation modes, resulting in quantifiable optical loss, were found to occur during HV-/HV+ sequential stress, including corrosion of the external glass surface, encapsulant delamination (at its interfaces with the glass and the PV cell), internal haze formation (resulting from a chemical interaction between the glass and the encapsulant), corrosion and migration of the gridlines, and corrosion of the silicon nitride (Si x N y ) antireflective coating on the cell. The effects of these separate modes were examined using monolithic (e.g., glass or PV cell) and laminated-coupon (glass/encapsulant/glass or glass/encapsulant/cell/encapsulant/backsheet) specimens. Characterizations during and after unbiased accelerated testing at 85°C/85% relative humidity included spectrophotometry, optical microscopy, electron microscopy, and ellipsometry. For some module components (i.e., the glass and the Si x N y coating), the optical performance was determined through iterative analysis of empirical measurements. Concentrating on just their spectral effect, a novel model was then developed to estimate the transfer of light to the PV cell and the return of light from the PV module with simultaneous degradation mechanisms, which was compared with a mini-module previously subjected to HV-/HV+ stress. Here the model suggests that one third of the current loss observed for the mini-module can be attributed to the optical degradation of the packaging materials. The dominant degradation modes include encapsulant delamination and corrosion of the Si x N y coating. Recommendations are given so that the optical model may be improved relative to accelerated testing and validated relative to field aging.
The effect of cracks in solar cells on the long-term degradation of photovoltaic (PV) modules remains to be determined. To investigate this effect in future studies, it is necessary to quantitatively describe the crack features (e.g., length) and correlate them with module power loss. Electroluminescence (EL) imaging is a common technique for identifying cracks. However, it is currently challenging and time-consuming to identify cracks in a large number of EL images and quantify complex crack features by human inspection. This article introduces a fast semantic segmentation method (~0.18 s/cell) to automatically segment cracks from EL images and algorithms to extract crack features. Here we fine-tuned a UNet neural network model using pretrained VGG16 as the encoder and obtained an average F1 score of 0.875 and an intersection over union score of 0.782 on the testing set. With cracks and busbars segmented, we developed algorithms for extracting crack features, including the crack-isolated area, the brightness inside the isolated area, and the crack length. We also developed an automatic preprocessing tool for cropping individual cell images from EL images of PV modules (~0.72 s/module). Our codes are published as open-source an software, and our annotated dataset composed of various types of cells is published as a benchmark for crack segmentation in EL images.
The direct current bias for photovoltaic (PV) modules interconnected in series-strings may include both high voltage negative ("HV-") and positive ("HV+") polarity with respect to the electrical ground. Multiple degradation modes, resulting in quantifiable optical loss, were found to occur during HV-/HV+ sequential stress, including: corrosion of the external glass surface, encapsulant delamination (at its interfaces with the glass and the PV cell), internal haze formation (resulting from a chemical interaction between the glass and the encapsulant), corrosion and migration of the gridlines, and corrosion of the silicon nitride (SixNy) antireflective coating on the cell. The effects of these separate modes were examined using monolithic (e.g., glass or PV cell) and laminated-coupon (glass/encapsulant/glass or glass/encapsulant/cell/encapsulant/backsheet) specimens. Characterizations during and after unbiased accelerated testing at 85 degrees C/85% relative humidity included: spectrophotometry, optical microscopy, electron microscopy, and ellipsometry. For some module components (i.e., the glass and the SixNy coating), the optical performance was determined through iterative analysis of empirical measurements. Concentrating on just their spectral effect, a novel model was then developed to estimate the transfer of light to the PV cell and the return of light from the PV module with simultaneous degradation mechanisms, which was compared to a mini-module previously subjected to HV-/HV+ stress. The model suggests one-third of the current loss observed for the mini-module can be attributed to the optical degradation of the packaging materials. The dominant degradation modes include encapsulant delamination and corrosion of the SixNy coating. Recommendations are given so that the optical model may be improved relative to accelerated testing and validated relative to field aging.
Abstract This paper analyzes the mechanisms and pathways for leakage current flow observed in Si photovoltaic modules subjected to high temperature and humidity and a large voltage bias with respect to ground. The current inside of the frame is in the form of electron motion, but in the glass and polymer, it is in at least a large part attributable to the movement of ions. When the mode of current flow changes from electronic to ionic conduction, electrochemical reactions will take place at the interface. This can include reactions that produce volatile chemical species like H 2 , CO x , and O 2 , along with ionic species such as OH − and H 3 O + . Here, we see evidence of the importance of different charge carriers with different diffusion rates and the influence of electrochemical processes involved. The application of negative voltage to the cell circuit affects the resistivity of glass producing surfaces with poor conductivity but with some increases in the electrochemical potential producing complicated interactions that are important when the voltage is changed. In the polymer, there is the development of a space charge region and a chemical gradient providing two oppositional forces to current flow, which when released create a complicated discharge process. Here, we give a basic understanding of the charge/discharge of PV cells highlighting how the specific mechanisms are important in understanding some of the degradation processes in PV modules. We find that there is evidence of multiple significant charge carrier species with different diffusion time scales. The glass/polymer interface forms a depleted region of higher resistance after prolonged exposure to current. Charge also builds up at the polymer to cell antireflective coating interface and mostly flows to the gridlines to experience electrochemical reactions. These complexities result in non‐linear behavior where the apparent resistivities of the different layers change during charge/discharging processes, making the modeling of the current flow extremely difficult.
Bifacial modules are increasingly deployed in the field and are expected to represent half of the market share within 10 years. Their rear structure differs from monofacial modules to allow additional light absorption. However, it brings new reliability challenges to address. In particular, the risk of potential-induced degradation (PID) is increased as both module sides are impacted. Different PID processes have been identified in the literature: shunting type (PID-s), polarization type (PID-p), Na penetration type, and corrosion type (PID-c). Their occurrence depends on the photovoltaic system configuration as well as the module's materials. Apart from PID-s, PID processes are not well understood and extensive research is needed to elucidate the PID scenario and underlying mechanisms. Herein, current knowledge about PID processes and their impact on the main bifacial modules in the market are gathered with the aim to guide future research. Bifacial module technologies and leakage current paths leading to PID are described. Indoor and outdoor PID testing methods are detailed. For each bifacial module technology, the PID processes are investigated with their indicators, mechanism and recovery process. Furthermore, PID-impacting factors and limitation solutions are finally reported and a state of the art on PID modeling is presented.
This paper presents the indoor extended accelerated stress testing (EAST) results of glass/glass (GG), glass/backsheet (GB) and glass/transparent backsheet (GT) modules having identical cells and two different encapsulant types, ethyl-vinyl-acetate (EVA) and polyolefin-elastomer (POE). Six 4-cell modules having the above-mentioned construction combinations were subjected to extended ultraviolet (UV; 600 kWh/m2), damp-heat (DH; 2000 hours) and thermal-cycling (TC; 600 cycles) tests. The post-stress UV fluorescent imaging, electroluminescent imaging, reflectance spectrophotometry and colorimetry results indicated that the grid finger degradation and encapsulant browning are slightly higher in the GG modules compared to the GB modules. The post-stress IV test results indicated, in general, that the GG/EVA modules tend to perform inferior to the GG/POE modules with the EAST evaluation.
In view of the increasing interest and market share of bifacial cells and modules, suitable substrates such as glass and transparent backsheets along with ethylene vinyl acetate (EVA) and polyolefin elastomer (POE) encapsulants were examined in combined-accelerated stress testing (C-AST) to evaluate and compare degradation modes. Testing with both monofacial and bifacial cells, we found glass-glass modules with monofacial cells led to greater grid finger breakage than those with polymeric backsheets. This is attributed to previous x-ray topography work showing higher stress in cells in glass-glass modules than glass backsheet modules. Consistent with the objectives of C-AST, which stresses modules at levels corresponding to the limits seen in the natural environment, we observed the UV-fluorescence signatures of modules tested in C-AST (considering the degradation associated with developing chromophores, moisture penetration and photobleaching effects) to be like those in fielded modules, more so than other chamber stress testing implemented for comparison. Finally, among multiple cell degradation modes that we observed such as light-induced degradation (LID), we differentiated susceptibility to potential-induced degradation (PID) on the back of the bifacial Passivated Emitter Back Cells (PERC) in C-AST. Confirming with ex-situ tests, we found polarization-type PID most prevalent in glass/glass modules with EVA as would be anticipated considering the greater leakage current through such module encapsulation. Unlike PID tests performed in the dark, which can lead to false positive PID test results, field-representative illumination is experienced by the modules on the front and back side while -1200 V system voltage is applied in C-AST, supporting the conclusion that this module type would be susceptible to PID in the field.
The degradation of photovoltaic (PV) balance of systems (BoS) components is not well-studied, but the consequences include offline modules, strings, and inverters; system shutdown; arc faults; and fires. A utility provider experienced a ~30% failure rate in their power transfer chain, originally attributed to branch connectors. Field-failed specimen assemblies were therefore examined, consisting of cable connector, branch connector, and discrete fuse components. In this study, unused field-vintage specimens are examined using combined-accelerated stress testing (C-AST) to clarify the most influential environmental stressors as well as the effect of external mechanical perturbation. A benchtop prototype fixture was used to develop the perturbation capability for the C-AST chamber. The benchtop experiments were also used to develop the in-situ data acquisition of specimen current, voltage, and temperature. A significant increase in operating temperature (~100 degrees C from ~40 degrees C) and a different failure mode were observed promptly once periodic mechanical perturbation was applied. The current at failure was decreased from 35 A (with failure in the fuses) to 15 A (failure at the male/female metal pin connection). After initial examination using X-ray computed tomography, the external plastic was machined away from failed specimens to allow for failure analysis, including the extraction of the internal convolute springs for morphological examination (optical and electron microscopy).
In the near future, grid operators are expected to regularly use advanced distributed energy resource (DER) functions, defined in IEEE 1547-2018, to perform a range of grid-support operations. Many of these functions adjust the active and reactive power of the device through commanded or autonomous modes, which will produce new stresses on the grid-interfacing power electronics components, such as DC/AC inverters. In previous work, multiple DER devices were instrumented to evaluate additional component stress under multiple reactive power setpoints. We utilize quasi-static time-series simulations to determine voltage-reactive power mode (volt-var) mission profile of inverters in an active power system. Mission profiles and loss estimates are then combined to estimate the reduction of the useful life of inverters from different reactive power profiles. It was found that the average lifetime reduction was approximately 0.15% for an inverter between standard unity power factor operation and the IEEE 1547 default volt-var curve based on thermal damage due to switching in the power transistors. For an inverter with an expected 20-year lifetime, the 1547 volt-var curve would reduce the expected life of the device by 12 days. This framework for determining an inverter's useful life from experimental and modeling data can be applied to any failure mechanism and advanced inverter operation.
The market share for bifacial modules is projected to be doubled from 30% to 60% in the next ten years. For the monofacial crystalline silicon glass/backsheet (G/B) modules, extensive reliability data has been available for over 40 years. However, practically little/no long-term field or accelerated reliability test data is available for the new generation glass/glass (G/G) bifacial modules and glass/transparent (G/T) bifacial modules. Therefore, the primary motivation of this project was to identify the reliability strengths and weaknesses of new generation G/G modules compared to G/B modules. In this 3-year project, the goal was to objectively recommend the best construction materials for the new generation G/G (bifacial) modules through a systematic experimental approach with appropriate tasks including: Evaluation of field retrieved old-generation G/G modules; Inspection of new-generation G/G modules installed in the plants; Evaluation of new-generation G/G, G/B and G/T modules using EAST (Extended Accelerated Stress Testing), CAST (Combined Accelerated Stress Testing) and FAST (Field Accelerated Stress Testing); and, dynamic literature search and review. Major accomplishments and outcomes of this project are: Accomplishments: Evaluated more than 60 field retrieved modules and constructed and characterized more than 135 mini-modules with three substrate types (G, B, and T), two encapsulant types (EVA and POE), and two cell types (monofacial and bifacial) as well as evaluated more than 30 commercial G/G and G/B modules; Subjected all the modules to multitude characterization tests and various indoor and outdoor accelerated stress tests including FAST (Field Accelerated Stress Testing), EAST (Extended Accelerated Stress Testing), and CAST (Combined Accelerated Stress Testing) to identify and correlate the failure modes in both field and lab tests. Outcomes: Based on the accelerated test results and handling/mounting experience obtained in this project, the recommended best construction for the glass/glass modules is: “Framed GG modules with cut-cells and POE encapsulant (UVpass front; UVpass back).” However, from a statistical and manufacturing point of view (along with stakeholders surveys), the following cautionary notes are added to the above-mentioned recommendation: (i) Cut cells could introduce a higher level of manufacturing issues, including a higher number of cell interconnects; (ii) POE encapsulant is more expensive than EVA and could present a delamination risk and lower throughput during manufacturing due to lower adhesion strength. Other encapsulants, such as coextruded EPE (EVA/POE/EVA), are also recommended to be investigated. The potential public benefit of the proposed project is to present the strengths and weaknesses of glass/glass modules, so an informed procurement decision can be made.
In view of the increasing interest and market share of bifacial cells and modules, suitable substrates such as glass and transparent backsheets along with ethylene vinyl acetate (EVA) and polyolefin elastomer (POE) encapsulants were examined in combined-accelerated stress testing (C-AST) to evaluate and compare degradation modes. Testing with both monofacial and bifacial cells, we found glass-glass modules with monofacial cells led to greater grid finger breakage than those with polymeric backsheets. Furthermore, this is attributed to previous X-ray topography and modeling work showing higher stress in cells and interconnections in glass-glass modules than glass-backsheet modules. Consistent with the objectives of C-AST, which stresses modules at levels corresponding to the limits seen in the natural environment, we observed the UV-fluorescence signatures of modules tested in C-AST (considering the degradation associated with developing chromophores, moisture penetration and photobleaching effects) to be like those in fielded modules, more so than other chamber stress testing implemented for comparison. We found light-induced degradation (LID) in module types with regenerated (inactive) cells with C-AST, suggesting the possibility of LID destabilization in some field conditions. We could also distinguish potential-induced degradation (PID) on the back of the bifacial passivated emitter and rear cells (PERC) in C-AST. Confirming with ex-situ tests, we found polarization-type PID most prevalent in glass-glass modules with EVA as would be anticipated considering the greater leakage current through such module encapsulation. Unlike PID tests performed in the dark, which can lead to false positive PID test results, field-representative illumination is experienced by the modules on the front and back side while –1200 V system voltage is applied in C-AST, supporting the conclusion that this module type with glass-glass construction would be susceptible to PID in the field.
The degradation of photovoltaic (PV) balance of systems (BoS) components is not well-studied, but the consequences include offline modules, strings, and inverters; system shutdown; arc faults; and fires. A utility provider experienced a ~30% failure rate in their power transfer chain, originally attributed to branch connectors. Field-failed specimen assemblies were therefore examined, consisting of cable connector, branch connector, and discrete fuse components. Previous papers and presentations have focused on the development of the test method using a benchtop prototype. This presentation covers the early results of C-AST aging of static and dynamic specimens.
The degradation of photovoltaic (PV) balance of systems (BoS) components is not well-studied, but the consequences include: offline-modules, -strings, -inverters; system shutdown; arc-faults; and fires. A utility provider experienced a ~30% failure rate in their power transfer chain, originally attributed to branch connectors. Field-failed specimen assemblies were therefore examined, consisting of cable connector, branch connector, and discrete fuse components. Unused field-vintage specimens are presently being examined using combined-accelerated stress testing (C-AST) to clarify the most influential environmental stressors as well as the effect of external mechanical perturbation. A benchtop prototype fixture was used to develop the perturbation capability for the C-AST chamber. The benchtop experiments were also used to develop the in-situ data acquisition of specimen: current, voltage, and temperature. A significant increase in operating temperature, ~100 deg C from ~40 deg C, and a different failure mode was observed promptly once periodic mechanical perturbation was applied. The current at failure was decreased from 35 A (with failure in the fuses) to 15 A (failure at the male/female metal pin connection). After initial examination using X-ray computed tomography, the external plastic was machined away from failed specimens to allow failure analysis, including the extraction of the internal convolute springs for morphological examination (optical- and electron-microscopy).
The degradation of photovoltaic (PV) balance of systems (BoS) components is not well studied, but the consequences include offline modules, strings, and inverters; system shutdown; arc faults; and fires. A utility provider experienced a ~30% failure rate in their power transfer chain, originally attributed to branch connectors. Field-failed specimen assemblies were, therefore, examined, consisting of cable connector, branch connector, and discrete fuse components. In this study, unused field-vintage specimens are examined using a benchtop prototype fixture to identify the most influential environmental stressors on BoS components as well as the effect of external mechanical perturbation. The prototype fixture was used to develop a perturbation capability for future use in the combined-accelerated stress testing chamber. The benchtop experiments were also used to develop the in-situ data acquisition of specimen current, voltage, and temperature. A significant increase in operating temperature (~100 °C from ~40 °C) and a different failure mode (arcing at the metal pins rather than overheating of the fuse filament) were observed promptly once periodic mechanical perturbation was applied. The current at failure was decreased from 35 A (measured for static specimens, with failure occurring in the fuses) to 15 A (for tests with mechanical perturbation, with failure at the male/female metal pin connection). After initial examination using X-ray computed tomography, the external plastic was machined away from failed specimens to allow for failure analysis, including the extraction of the internal convolute springs for morphological examination (optical and electron microscopy). Chemical composition analysis included energy-dispersive X-ray spectroscopy, differential scanning calorimetry, and Fourier transform infrared spectroscopy.
The degradation of photovoltaic (PV) balance of systems (BoS) components is not well-studied, but the consequences include: offline-modules, -strings, -inverters; system shutdown; arc-faults; and fires. A utility provider experienced a ~30% failure rate in their power transfer chain, attributed to branch connectors. Field-failed specimen assemblies were therefore examined, consisting of cable connector, branch connector and discrete fuse components. Unused field-vintage specimens are presently being examined using combined-accelerated stress testing (C-AST) to clarify the most influential environmental stressors as well as the effect of external mechanical perturbation. A benchtop prototype fixture was used to develop the perturbation capability for C-AST. The benchtop experiments were also used to develop the in-situ data acquisition of specimen: current, voltage, and temperature. A significant increase in operating temperature, ~100 deg C from ~40 deg C, and a different failure mode was observed immediately once periodic mechanical perturbation was applied. The current at failure was decreased from 35 A (with failure occurring in the fuses) to 15 A (failure at the male/female metal pin connection). After initial examination using X-ray computed tomography, the external plastic was machined away from failed specimens to allow failure analysis, including the extraction of the internal convolute springs for morphological examination (optical- and electron-microscopy). Chemical composition analysis included: energy-dispersive X-ray spectroscopy, differential scanning calorimetry, and Fourier transform infrared spectroscopy.
Various common crystalline silicon cell technologies were exposed to UVA radiation (1.24 Wm-2 nm-1 at 340 nm peak) on the front and back faces at 45 degrees Celsius for periods up to 3000 h, representing about 3 y of solar exposure in Phoenix, Arizona, USA. The resulting degradation of the open-circuit voltage and short-circuit current is presented. Of the various cell types examined, significant levels of degradation were seen in all cases. Less degradation was generally found after UV irradiation of cell fronts and older cell types, whereas a bifacial PERC type exposed on the rear showed about 25% degradation in short circuit current, attributable to lack of a diffused surface field. Selected cells were exposed to UV irradiation with the addition of long pass UV filters to replicate UV-absorbers in encapsulants. Modern cell designs are sensitive to UV-ID because of reduced or eliminated front and back surface field and increased dependence on high quality surface passivation. Single transformation of the independent variable (t, kW h/m^2) could be used to achieve a linear model of the data to extrapolate to 50 y. Solar Advisor Model (SAM) shows appropriate filtering of UV-irradiation can improve LCOE and net present value of plant. Some advanced cell types are seen to be UV-resistant (cell level solutions also exist). Solutions therefore exist on the cell, glass, and encapsulant level. Changes over time in each of these would also need to be considered (solarization, encapsulant browning...).