Mapping the Microhardness of Al Matrix in U-7Mo/Al Dispersion Fuels at Medium and High Burn-up by in situ Nanoindentation

The mechanical degradation of the Al matrix in U-7Mo dispersion fuels was detected after irradiation in previous studies, but more details of the degradation mechanism are not clear yet to clarify the root cause. In this study, microhardness mapping in fresh and irradiated U-7Mo dispersion fuels coated with ZrN, with burn-up of 3.35 × 10 21 and 6.28 × 10 21 f/cm 3 , are measured to reveal the hardening of the Al matrix as a function of distance to fuel particles. Micro cubes were pulled by plasma focused ion beam scanning electron microscopy and tested by in situ nanoindenter with Berkovitch tip. Size effects are measured in medium and high burn-up samples. The higher burn-up specimen exhibits a more pronounced size effect when indent load is lower than 20 mN. Size effect correction models are also calculated by plots fitting, which predicts the true microhardness without size effect. Results shows that the hardness of the Al matrix near the ZrN coating has the highest value, then decreases moving away from the coating and become stable when the distance reaches ∼10 µm. The hardness starts increasing again getting closer to the next fuel particle, which makes the hardness distribution between two fuel particles to be “U” shape.

36 - MATERIALS SCIENCE

Thick graded interfaces increase wear resistance in Ti/TiN nanolayered thin films

Multilayered composites with nanoscale layer thickness incorporating titanium and titanium nitride (Ti/TiN) are used as a model system to study the effects of heterophase interface structure on elastic and plastic deformation, as well as wear behavior. Here, in this work, hardness, modulus, and wear rate under dry reciprocating sliding contact are quantified as a function of Ti-TiN heterophase interfacial nitrogen gradient thickness for Ti/TiN multilayers with 10–80 nm layer thickness. Hardness and modulus are found to be inversely proportional to layer thickness and independent of interface gradient for most specimens. Wear rate is found to be inversely proportional to interface gradient thickness at constant layer thickness, demonstrating that control of nanoscale interface structure is a valid approach to enhancing wear behavior. The materials studied in this work wear comparably or slower than other Ti- and TiN-based composites in the literature, providing a promising avenue for engineering wear-resistant materials for use in industrially relevant applications.

Graded interfaces

Boron Nitride-Driven Strengthening of Aluminum Composites via Friction Stir Processing

Friction stir welding and processing (FSW/P) has emerged as an effective solid-state joining technique for fabricating metal matrix composites (MMCs), offering improved mechanical properties through refined microstructural evolution. In this study, an aluminum-boron nitride nanoparticle (Al-BNNP) composite was synthesized via FSW, and its indentation-based mechanical properties were systematically evaluated. Microhardness mapping across the weld cross-section revealed a progressive increase in hardness toward the stir zone (SZ), attributed to severe plastic deformation, dynamic recrystallization (DRX), and the reinforcing effect of BNNPs. Profilometry-based indentation plastometry (PIP) inferred yield strength (YS) demonstrates a 47.8% increase compared to the base metal (BM) and a 75% improvement compared to FSP pure aluminum reported in literature. This enhancement is attributed to strengthening mechanisms, including grain boundary pinning, load transfer, and increased dislocation density. The strain rate sensitivity (SRS) measurements at the nanoscale demonstrated a substantial decrease in the SZ, correlated with ultrafine grain structures and strong BNNP-matrix interactions. Activation volume analysis revealed a significant reduction in the SZ, suggesting that dislocation motion is increasingly restricted by dislocation-dislocation and dislocation-particle interactions. These findings suggest that incorporating BNNPs in FSW/P enables tailoring the microstructure without thermal degradation of the secondary particles, thereby significantly enhancing the mechanical performance of aluminum composites, particularly for structural applications in aerospace and automotive industries.

Aluminum

Thermal stability of 3D interface Cu/Nb nanolaminates

Nanocrystalline alloys are promising structural materials yet lack thermal stability in many cases. Recent work shows that interface structure has an outsize effect on the thermal behavior of nanostructured alloys. Here, this work focuses on the role of controlled heterophase interface structure in the thermal evolution of model Cu/Nb nanolaminates. We introduce 3D interfaces containing nanoscale heterogeneities in all spatial dimensions between Cu and Nb, forming 3D Cu/Nb. TEM, nanoindentation, and DSC are used in tandem to establish thermal stability and to identify shifts in microstructure as a function of static annealing temperature. 3D interfaces are shown to survive annealing to 300 °C for 1 hr., while 3D Cu/Nb microstructure evolves to form low-density and voided regions correlating to the onset of layer pinch-off between 500 and 600 °C annealing temperatures. A diffusivity- and vacancy energetics-based mechanism is developed to explain void formation driven by 3D interface degradation at elevated temperature.

3D interfaces