FCCI Barrier Coating on U-10Zr Fuel
Explore the source record for details and available documents.
SEARCH · Engineering Papers
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Explore the source record for details and available documents.
Fuel clad chemical interaction (FCCI) is a pervasive issue for metallic nuclear fuels. FCCI can damage cladding, reduce thermal efficiency, and compromise the structural integrity of the fuel rod. In this study, we evaluated the FCCI mitigation capabilities of electrophoretically-deposited Zr nanoparticle coatings on ferritic-martensitic stainless-steel cladding (HT9). Zr was deposited on the internal surface of 6 mm outer diameter cladding using electrophoretic deposition (EPD). Thickness varied among samples with similar EPD conditions. A uniformly coated sample was selected and sent to the Argonne Tandem Linac Accelerator System (ATLAS) to simulate the coating's behavior under irradiation conditions. Furthermore, the coating prevented FCCI in diffusion couple studies. Results of this study confirm that Zr could potentially make an effective FCCI barrier in metallic fuel rods but the deposition process needs improvement.
Novel fuel form fabrication efforts have focused on casting of smaller diameter fuels in order to show the feasibility of the FAST test and the incorporation of a FCCI barrier either integral to the fuel or within the cladding tube. Casting of small diameter fuel slugs proved to be feasible at least one pin at a time using vacuum assisted arc casting. Integration of an integral FCCI barrier is also feasible although additional refinement will be necessary. If a sodium bonded fuel is employed, a more simple FCCI barrier may be to incorporate a thin barrier of material in the cladding before the sodium and fuel are loaded. Experiments have shown that sodium bonding of the barrier material and fuel is feasible.
Nuclear fuels using alloys of uranium, or metallic fuels, have many beneficial properties. The classical metallic fuel design uses a loose fitting cylindrical “slug” of fuel placed inside stainless-steel cladding tubes where the gap is filled with sodium. This sodium bond is liquid at operating temperature and conducts heat from the slug to the cladding, especially in early life before fuel swells into contact with the cladding. Despite the benefits of sodium bonding, there is a desire to develop metallic fuel technologies without it chiefly to reduce chemical reaction hazards in spent fuel storage from sodium fast reactors operating on once-through fuel cycles. Elimination of the sodium bond may also help unlock potential benefits for fuel fabrication, reactor neutronics, and compatibility with other types of reactors. Creating a sodium-free metallic fuel revolves around the problem of manufacturing fuel slug geometries which are in close contact with the cladding at beginning of life to facilitate heat transport while alleviating fuel-cladding chemical interactions (FCCI) at this interface and providing enough free volume to accommodate fuel swelling. Accelerating development and qualification of this fuel system will require careful selection of design and manufacturing options. To this end, a design trade-off study was performed to evaluate candidate options. Several design and manufacturing options were assessed, weighted, scored, and ranked with respect to fabrication, normal reactor operation, off-normal scenarios, and back-end considerations. This effort was performed both for “baseline” needs, which represented a once-through fuel cycle at temperatures and burnups known to be viable for sodium-bonded metallic fuel, and for “enhanced” needs to represent opportunities for closed fuel cycles and/or more aggressive temperatures/burnups. The outcomes of this study prioritized a baseline technology using U-Zr alloy with additives to mitigate FCCI, produced in annular slug geometry by continuous casting, clad in austenitic stainless-steel alloy, and followed by a final step to swage the cladding down to close the gap. This study prioritized an enhanced fuel technology using U-Mo alloy, also produced by continuous casting into an annular geometry, followed by coating/plating with an FCCI barrier on the slug, again with a final step to swage the cladding diameter down using oxide dispersion strengthened steel. It was noted that development of the enhanced fuel technology would entail more risk, thus U-Zr alloy was put forth as a backup to U-Mo if challenges are encountered with FCCI barriers, and advanced ferritic/martensitic steels are put forth as a backup to oxide dispersion strengthened steels if swaging and welding are found unworkable.
Slides containing updated PIE results for AFC-4C-R5 (MNT20E)
Advanced fuel cladding is critical for fast reactors, offering sufficient thermal conductivity, mechanical and dimensional stability and radiation tolerance of the cladding base material. Additionally, it must provide corrosion resistance and high temperature coolant compatibility on the cladding outer surface, as well as chemical stability on the cladding inner wall against fuel cladding chemical interaction (FCCI). TiN ceramic coating has been considered an effective diffusion barrier for inner and outer cladding-walls for enhanced performance. The TiN-metal interface microstructure and chemistry play a critical role in coating bond strength and integrity under harsh conditions. High-resolution transmission electron microscopy characterization of ceramic-metal interface at atomic resolution in unirradiated, irradiated and thermal cycled conditions were performed. The interface remained intact after irradiation up to 200 dpa or thermal cycling five times up to 550 °C. In conclusion, this work discusses the potential impact of these results on coating performance and design for advanced claddings.
The diffusion of lanthanide fission products plays an important role in the growth of the fuel-cladding chemical interaction (FCCI) region in metallic fuels. The use of a Zr interdiffusion barrier may mitigate the transport of lanthanides from the fuel to the cladding, but the efficacy of such a liner is not yet known. In this paper, the stability and vacancy-mediated diffusion of La, Ce, Pr, and Nd in hexagonal close-packed (HCP) Zr is investigated via density functional theory (DFT) calculations and self-consistent mean field (SCMF) analysis. DFT is used to calculate the formation, binding, and migration energies of vacancies and vacancy-solute pairs. The DFT energetics are used in the KineCluE code to calculate the Onsager transport coefficients. La is found to be the fastest diffusing species in HCP Zr and experiences an almost isotropic diffusion behavior. The other three species (Ce, Pr, and Nd) demonstrate anisotropic diffusion where the diffusion in the basal planes is significantly faster than that along the c-axis. Further, the calculated lanthanide diffusivities in HCP Zr are fitted to an Arrhenius relation and the activation energies and prefactors are reported for the first time. Furthermore, the vacancy drag and the segregation tendencies were analyzed using the calculated off-diagonal transport coefficients. According to our vacancy-mediated diffusion model, lanthanides are expected to be enriched at vacancy sinks at low temperatures, while at high temperatures, lanthanides are depleted at sinks and will preferably diffuse into the bulk. The enrichment/depletion transition temperature depends on the diffusion direction (basal or axial) and hence will be controlled by the grain texture and orientation.
Advanced cladding is critical for fast reactors with the adequate thermal conductivity, mechanical stability and radiation tolerance of the cladding base material, corrosion resistance and high temperature coolant compatibility of the cladding surface, and chemical stability of the cladding inner wall against fuel cladding chemical interaction (FCCI). The preliminary results of recent ion irradiation studies of two diffusion-couple samples of cerium (Ce)/oxide-dispersion strengthened steel (ODS) and Ce/TiN/ODS, irradiated with 80 MeV xenon (Xe) ions to 100 displacements per atom (dpa) at 500°C, are summarized. Significant Ce-Fe interaction occurred in the Ce/ODS sample, and no noticeable Ce-Fe interaction was found in the Ce/TiN/ODS sample. It shows the effectiveness of 1-µm TiN diffusion barrier coated by the pulsed laser deposition on suppressing Ce-Fe interaction, a major contributor to FCCI in cladding. Here, density function theory (DFT) calculations of the impurity diffusivities of Ce and Fe within the Ti sublattice of TiN were performed to assist a mechanistic understanding of the experimental results.
Innovative thin film multilayer metal/ceramic barrier coatings have been developed by Argonne National Laboratory to protect fuel cladding against different phenomena that can be encountered under the harsh operating conditions of advanced nuclear reactors. One phenomenon is Fuel-Cladding Chemical Interaction (FCCI), which can represent a challenge to the performance of steel-clad metallic fuels in sodium-cooled fast reactors (SFRs), especially when operating to high burnups at elevated cladding temperatures, and long fuel residence time. Another phenomenon is the corrosion of zirconium-based cladding under prototypic boiling water reactor (BWR) conditions and associated cladding during off normal conditions, including loss of coolant accidents (LOCA). This work provides details of the development and testing of a thin film (few microns) multilayer metal/ceramic (CrY/Y 2 O 3 ) coatings on steel cladding and its performance against FCCI. The coating architecture evolved through systematic mechanical testing, radiation tolerance assessments, and high-temperature diffusion studies from a preliminary multilayer concept to an optimized high-performance design. The optimized structure leverages stoichiometric Y 2 O 3 for its exceptional radiation stability, chemical inertness, and ultra-low fission product diffusivity (e.g., Ce diffusivity ~10 -20 m 2 /s in irradiated Y 2 O 3 at 650 °C). This is paired with ductile chromium-rich interlayers (Cr 95 Y 5 ), which significantly enhance fracture toughness and mechanical resilience. Design refinements, including increased ceramic layer thickness and optimized Cr–Y interlayer composition, eliminated fracture propagation and preserved coating integrity under extreme mechanical stress (>10× typical reactor conditions) and prolonged radiation exposure (~300 dpa). Those conditions are well beyond expected conditions during normal operations in SFR, and cover some of the transient conditions as well. In addition, the coating deposition was demonstrated to be applied uniformly to the inner surface of steel tubes representing prototypic SFR cladding. Another phenomenon under consideration in this work is the corrosion of zirconium-based cladding under prototypic boiling water reactor (BWR) conditions and associated off normal conditions including loss of coolant accident (LOCA). Another multilayer thin film coating is considered for mitigation of this phenomenon, where a coating of yttrium aluminum and yttrium aluminum ceramic/metal thin film coating. Preliminary results on the coating performance during high temperature thermal cycling (up to 1000 C) have shown promising performance of the coating. On-going optimization of the coating will continue in FY26.
Fuel-Cladding Chemical Interaction (FCCI) poses significant challenges in nuclear reactors, where fission products from nuclear fuel interact with Fe-based cladding materials, potentially compromising their structural integrity. This study investigates the diffusion behavior of oversized fission products, Pr, Nd, Ce, and La, within bcc Fe cladding using density functional theory (DFT), nudged elastic band (NEB) method, and self-consistent mean field (SCMF) theory. Our results reveal significant long-range vacancy binding energies, particularly up to the 6th nearest neighbor, with La exhibiting the strongest binding affinity, followed by Nd, Ce, and Pr. The NEB calculations indicate significant high barriers for the dissociation of 1nn vacancy-solute pairs for all fission products. The tracer diffusion coefficients of these fission products was derived in Arrhenius form. The significant trapping effect of vacancies by a very dilute amount of fission products reduces vacancy mobility, leading to an oversaturation of point defects, void nucleation, and swelling. These are critical issues for irradiated cladding materials. The tracer diffusion coefficients indicate that Nd diffuses the fastest, followed by La, Ce, and Pr. This study provides essential insights for developing advanced cladding materials and design strategies to mitigate FCCI, ultimately enhancing nuclear reactor safety and performance.
This article investigates the fuel-cladding chemical interaction (FCCI) behavior of two commercial FeCrAl alloys, APMT composition (Fe-21Cr-5Al-3Mo wt.%) and C35M (Fe-13Cr-5Al-2Mo-0.2Si-0.03Y wt.%), after neutron irradiation. “H-cup” diffusion multiples of FeCrAl alloys and ceramic UO 2 fuel were irradiated at a temperature of ~300 °C to a total estimated burnup of 26 GWd/tHM. Post-irradiation Examination results demonstrate the excellent degradation resistance of FeCrAl alloys as accident tolerant fuel (ATF) cladding materials in light water reactor conditions. The study concludes that there was no irradiation-induced defects observed in either of the two commercial FeCrAl claddings. The formation of amorphous Al/U mixed oxide was observed at the fuel-clad interface, which can serve as a tritium permeation barrier and protect against potential chemical attack from the fuel. Finally, the study attributed the formation of amorphous Al/U mixed oxide to the low temperature and limited time of neutron irradiation. APMT forms more distinct Cr and Cr-Fe intermetallic at the FeCrAl-UO 2 interface than C35M due to the higher bulk Cr:Al ratio.