Relative fraction of sp{sup 3} bonding in boron incorporated amorphous carbon films determined by X-ray photoelectron spectroscopy
Boron incorporated amorphous carbon (a-C:B) films were deposited by a filtered cathodic vacuum arc system using various percentage of boron mixed graphite cathodes. X-ray photoelectron spectroscopy (XPS) was employed to determine the properties of the films as a function of boron concentration. Deconvolutions of the XPS C 1s core level spectra were carried out using four different components. The relative fraction of sp{sup 3} bonding was then evaluated from the area ratio of the peaks at 285.0, 284.1 eV which were individually attributed to sp{sup 3} C-C, sp{sup 2} C=C hybridizations. The results showed that the sp{sup 3} content of a-C:B film decreases from 73.8 to 58.6% for the films containing boron from 0.59 to 2.13 at.%, and then gradually reduced to 42.5% at a slower rate with boron concentration up to 6.04 at.%. Furthermore, a series of a-C:B films with fixed boron content (2.13 at.%) were prepared to identify the relationship between sp{sup 3} bonding and substrate bias. It was found that the fraction of sp{sup 3} bonding increased from 50.28% at the bias voltage of 0 V and reached a maximum value of 66.3% at -150 V. As the bias voltage increased up to -2000 V, the sp{sup 3} content decreased sharply to 43.9%.