Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Oxidation Testing”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 163 records · Page 9

Effects of silicon additions on oxidation and mechanical behavior of the nickel-base superalloy B-1900

Test specimens with nominal additions of Si were tested in oxidation, thermal fatigue, sulfidation, tension, and stress rupture, and were also extensively studied metallographically. Alloy B-1900 modified with 0.6- or 1.2-wt% Si exhibited oxidation resistance equivalent to that of aluminide-coated B-1900 during cyclic, high-gas-velocity oxidation tests. Resistances to thermal fatigue and sulfidation were improved by the Si additions, but were not superior to aluminide-coated B-1900. Stress-rupture tests at 1000 C of specimens given the standard heat treatment to simulate an aluminide coating cycle showed Si to be detrimental. However, application of another heat treatment increased the rupture life of the alloy with 0.6-wt% Si to that of the unmodified B-1900 given the standard heat treatment.

Miner, R. V., Jr.↗

A High Temperature Cyclic Oxidation Data Base for Selected Materials Tested at NASA Glenn Research Center

The cyclic oxidation test results for some 1000 high temperature commercial and experimental alloys have been collected in an EXCEL database. This database represents over thirty years of research at NASA Glenn Research Center in Cleveland, Ohio. The data is in the form of a series of runs of specific weight change versus time values for a set of samples tested at a given temperature, cycle time, and exposure time. Included on each run is a set of embedded plots of the critical data. The nature of the data is discussed along with analysis of the cyclic oxidation process. In addition examples are given as to how a set of results can be analyzed. The data is assembled on a read-only compact disk which is available on request from Materials Durability Branch, NASA Glenn Research Center, Cleveland, Ohio.

Barrett, Charles A.↗

Dynamic Nuclear Polarization of Metal-Doped Oxide Glasses: A Test of the Generality of Paramagnetic Metal Polarizing Agents

Nuclear magnetic resonance (NMR) spectroscopy can provide unique, atomic-level insights into the structure and dynamics of materials, but its applications are impeded by the intrinsically low sensitivity. Dynamic nuclear polarization (DNP) is poised to overcome this limitation, and indeed has revolutionized the study of surfaces; however, the current approaches are ill-suited for bulk solids. One potential pathway toward the hyperpolarization of bulk solids by DNP is through the inclusion of paramagnetic metal ions that can serve as polarizing agents. Here, we compared the relative performance of two such dopants, Mn 2+ and Gd 3+ , in three series of oxide glasses having chemical environments representative of those found in other crystalline and amorphous solids. In our studies, Gd 3+ outperformed Mn 2+ , consistently providing more than one order of magnitude greater time savings. We attributed this difference mainly to the lack of hyperfine interaction to 55 Mn.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Testing of UV Oxidation Process for Acetonitrile Destruction

The Hanford Site Effluent Treatment Facility (ETF) currently treats aqueous waste streams that include condensates from the 242-A evaporator, leachate from the Environmental Restoration Disposal Facility (ERDF), as well as laboratory wastes and, in the future, will treat liquid effluents from the Hanford Waste Treatment and Immobilization Plant (WTP) and Integrated Disposal Facility (IDF) leachate. Liquid effluents from the WTP will have significant concentrations of acetonitrile. Acetonitrile is formed by reaction of nitrates and sugar in the WTP low activity waste (LAW) melters and is prevalent in the submerged bed scrubber (SBS) and wet electrostatic precipitator (WESP) liquid effluents from WTP off-gas treatment. When these liquids are concentrated in the WTP Effluent Management Facility (EMF) evaporator in the direct feed low activity waste (DFLAW) flow-sheet, testing has shown that the majority of the acetonitrile partitions to the evaporator condensate. Since the evaporator condensate is directed to the ETF, this creates a potential issue with the ETF waste acceptance criteria and, specifically, the ETF Delisting Modification treatability envelope limits. Consequently, there is a need to assess possible mitigation approaches, one of which involves identification and assessment of potential treatment processes to destroy the acetonitrile, which is the subject of the present report.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Leak test for solid oxide fuel cells and solid oxide electrolysis cells

A simple, fast, and economical alcohol penetration method for assessing the solid oxide cell to metal window frame seal in a typical planar design is presented. An alcohol such as ethanol or isopropanol is placed into the cavity of a cell sealed to the window frame. Within 3–5 min, one can determine if the glass seal is hermetic by visual observation along the seal edges on the side of the sealed frame. Cross bubbling and open circuit voltage methods for determining whether the seal failed or cracked at high temperature after final stack firing are also discussed.

25 ENERGY STORAGE↗

Organic Evaporation, Oxidation, and Hydrolysis Testing in Support of Hanford Sample-and-Send

The Hanford site has approximately 54 to 56 million gallons of radioactive mixed waste stored in 156 unretrieved underground storage tanks. The Hanford Waste Treatment and Immobilization Plant (WTP) is being built to treat and immobilize the tank waste. The baseline method for immobilization of Low Activity Waste (LAW) through the WTP is vitrification, but additional immobilization capacity is needed to supplement the initial LAW melters. An alternative cementitious waste form is being investigated for that future immobilization method. However, one impediment to a cementitious waste form is the presence of Land Disposal Restricted (LDR) organic chemicals in tank waste, which are regulated on a concentration based standard in the final waste form. Hence, if the quantity of organics in LAW is high enough, they must be destroyed or removed to make a waste form compatible with disposal in a mixed low level waste landfill. This work evaluates potential avenues for treatment of LDR organics to eliminate the impediment and permit possible use of a cementitious waste form. Vacuum evaporation testing to remove LDR organics consisted of preparing a non-radioactive LAW simulant, spiking that simulant with organic chemicals, and evaporating the mixture via differential distillation. The apparatus was a laboratory-scale vacuum evaporator operated at 60 ±5 torr absolute (vacuum evaporation). The LAW simulant represented the liquid expected to be retrieved from the Hanford tank farms at approximately 4.0 M [Na+] total sodium ion concentration. The concentration of the organic chemicals added was significantly higher than typically found in the tank waste samples since the higher levels were necessary to assist in analytical measurement and tracking of the spiked species.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Organic Evaporation, Oxidation, and Hydrolysis Testing in Support of Hanford Sample-and-Send

The Hanford site has approximately 56 million gallons of radioactive mixed waste stored in 156 unretrieved underground storage tanks. The Hanford Waste Treatment and Immobilization Plant (WTP) is being built to treat and immobilize the tank waste. The baseline method for immobilization of Low Activity Waste (LAW) through the WTP is vitrification, but additional immobilization capacity is needed to supplement the initial LAW melters. An alternative cementitious waste form is being investigated for that future immobilization method. However, one impediment to a cementitious waste form is the presence of Land Disposal Restricted (LDR) organic chemicals in tank waste, which are regulated on a concentration-based standard in the final waste form. Hence, if the quantity of organics in LAW is high enough, they must be destroyed or removed to make a waste form compatible with disposal in a mixed low level waste landfill. This work evaluates potential avenues for treatment of LDR organics to eliminate the impediment and permit possible use of a cementitious waste form.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Hypersonic test facility using nitrous oxide

A high enthalpy and low-cost Hypersonic Test Facility (HTF), which employs nitrous oxide to generate clean air-like gas; and a method of decomposing nitrous oxide in the presence of a catalyst in a catalytic decomposition chamber in a HTF.

Pourpoint, Timothee L.↗

Metal Oxide Varistor (MOV) Lifetime Estimation with Impulse-Based Testing in PV Inverter Systems

Surges caused by lightning strikes could damage electrical components in photovoltaic (PV) systems. Metal oxide varistors (MOVs) are commonly used to protect PV systems from lightning strikes. This paper proposes a holistic impulse-based MOV lifetime estimation framework. The impacts of peak current and fault duration induced by lightning events are considered in the MOV lifetime estimation framework. Moreover, the impact of different parameter combinations on MOV lifetime estimation is analyzed. The effectiveness of the proposed work is validated in a PV inverter test system developed in MATLAB/Simulink.

lifetime estimation↗

High Temperature Steam Oxidation of Irradiated FeCrAl in the Severe Accident Test Station

FeCrAl-UO2 test capsules were fabricated at Oak Ridge National Laboratory (ORNL) and irradiated at the Advanced Test Reactor. Following irradiation, samples were sectioned from the irradiated rod and oxidation kinetics were evaluated to access the candidate cladding high-temperature oxidation performance following irradiation. The irradiation was performed at approximately 400°C to a burnup of 10 GWd/MT. The high-temperature oxidation tests were conducted in the ORNL Severe Accident Test Station at 1200 and 1300°C. Weight measurements were taken before and after oxidation testing. Cross-sections of the cladding were metallographically mounted and optical microscopy was performed. Measurements of the oxidation layer before and after high-temperature testing were collected. The results indicate the irradiated FeCrAl C35M alloy provided good thermal stability up to 1200°C.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Hot-Fire Test Results of an Oxygen/RP-2 Multi-Element Oxidizer-Rich Staged-Combustion Integrated Test Article

As part of the Combustion Stability Tool Development project funded by the Air Force Space and Missile Systems Center, the NASA Marshall Space Flight Center was contracted to assemble and hot-fire test a multi-element integrated test article demonstrating combustion characteristics of an oxygen/hydrocarbon propellant oxidizer-rich staged-combustion engine thrust chamber. Such a test article simulates flow through the main injectors of oxygen/kerosene oxidizer-rich staged combustion engines such as the Russian RD-180 or NK-33 engines, or future U.S.-built engine systems such as the Aerojet-Rocketdyne AR-1 engine or the Hydrocarbon Boost program demonstration engine. For the thrust chamber assembly of the test article, several configurations of new main injectors, using relatively conventional gas-centered swirl coaxial injector elements, were designed and fabricated. The design and fabrication of these main injectors are described in a companion paper at this JANNAF meeting. New ablative combustion chambers were fabricated based on hardware previously used at NASA for testing at similar size and pressure. An existing oxygen/RP-1 oxidizer-rich subscale preburner injector from a previous NASA-funded program, along with existing and new inter-connecting hot gas duct hardware, were used to supply the oxidizer-rich combustion products to the oxidizer circuit of the main injector of the thrust chamber. Results from independent hot-fire tests of the preburner injector in a combustion chamber with a sonic throat are described in companion papers at this JANNAF conference. The resulting integrated test article - which includes the preburner, inter-connecting hot gas duct, main injector, and ablative combustion chamber - was assembled at Test Stand 116 at the East Test Area of the NASA Marshall Space Flight Center. The test article was well instrumented with static and dynamic pressure, temperature, and acceleration sensors to allow the collected data to be used for combustion analysis model development. Hot-fire testing was conducted with main combustion chamber pressures ranging from 1400 to 2100 psia, and main combustion chamber mixture ratios ranging from 2.4 to 2.9. Different levels of fuel film cooling injected from the injector face were examined ranging from none to about 12% of the total fuel flow. This paper presents the hot-fire test results of the integrated test article. Combustion performance, stability, thermal, and compatibility characteristics of both the preburner and the thrust chamber are described. Another companion paper at this JANNAF meeting includes additional and more detailed test data regarding the combustion dynamics and stability characteristics.

Hulka, J. R.↗

Oxidizer heat exchanger component testing

As part of the RL10 Rocket Engine Product Improvement Program, Oxidizer Heat Exchanger (OHE) stages 1, 2, and 3 were designed and fabricated during late 1983 and early 1984. The purpose of the OHE is to provide gaseous oxygen to the propellant injector for stable engine operation at tank head idle and pumped idle operating modes. This report summarizes the OHE stages 1 and 3 rig testing, and includes the separation of the stage 1-and-2 assembly and the remanifolding of stage 1. The OHE performance analysis and analytical model modifications for both stages are also presented. The flow tests were accomplished during the time period from 9 October 1984 to 12 November 1984.

Kmiec, T.↗

Silicon device performance measurements to support temperature range enhancement

Testing of the metal oxide semiconductor (MOS)-controlled thyristor (MCT) has uncovered a failure mechanism at elevated temperature. The failure appears to be due to breakdown of the gate oxide. Further testing is underway to verify the failure mode. Higher current level inverters were built to demonstrate 200 C operation of the N-MOSFET's and insulated-gate-bipolar transistors (IGBT's) and for life testing. One MOSFET failed early in testing. The origin of this failure is being studied. No IGBT's have failed. A prototype 28-to-42 V converter was built and is being tested at room temperature. The control loop is being finalized. Temperature stable, high value (10 micro-F) capacitors appear to be the limiting factor in the design at this time. In this application, the efficiency will be lower for the IGBT version due to the large V sub(cesat) (3.5-4 V) compared to the input voltage of 28 V. The MOSFET version should have higher efficiency; however, the MOSFET does not appear to be as robust at 200 C. Both versions are built for comparison.

Bromstead, James↗

Oxidation and Associated Pore Structure Modification During Experimental Alteration of Granite

Weathering plays a crucial role in a number of environmental processes, and the microstructure and evolution of multi-scale pore space is a critically important factor in the weathering of geological formations. In igneous rocks the infiltration of meteoric water into initially relatively dry material can cause the rock to begin to disaggregate, increasing porosity and surface area, and allowing further disaggregation and weathering to occur. These processes, in turn, allow biota to colonize the rock, further enhancing the weathering rate. In some igneous rocks this may be driven by oxidation of primary minerals. One such mineral, biotite, has been repeatedly mentioned as a cause of cracking during oxidation. However, the scale-dependence of the processes by which this occurs are poorly understood. We cannot, therefore, accurately extrapolate laboratory reaction rates to the field in predictive numerical models. In order to better understand the effects of oxidation and test the hypothesis that fracture and disaggregation are initiated by swelling of oxidizing biotites, we reacted granite cores in a selenic acid-rich aqueous solution at 200°C for up to 438 days. Elevated temperatures and selenic acid were used to provide relatively fast reaction rates and highly oxidizing conditions in sealed reaction vessels. These experiments were analyzed using a combination of imaging, X-ray diffraction, Mössbauer spectroscopy, and small- and ultra-small angle neutron scattering to interrogate porosity and microfracture formation. The experimental results show little observable biotite swelling, but significant transport and growth of iron oxides and/or clays along grain boundaries throughout the sample. Significant increases in porosity were also observed at the sample rim, likely associated with feldspar alteration. Fractures and transport were observed throughout the core, suggesting that stresses due to crystallization pressures caused by the growing iron phases may be the initiating factors in granite weathering, possibly followed by biotite swelling after sufficient permeability is achieved.

Anovitz, Lawrence M.↗

Thermal and oxidative degradation studies of formulated C-ethers by gel-permeation chromatography

Gel-permeation chromatography was used to analyze C-ether lubricant formulations from high-temperature bearing tests and from micro-oxidation tests. Three mu-styragel columns (one 500 and two 100 A) and a tetrahydrofuran mobile phase were found to adequately separate the C-ether degradation products. The micro-oxidation tests yielded degradation results qualitatively similar to those observed from the bearing tests. Micro-oxidation tests conducted in air yielded more degradation than did tests in nitrogen. No great differences were observed between the thermal-oxidative stabilities of the two C-ether formulations or between the catalytic degradation activities of silver and M-50 steel. C-ether formulation I did yield more degradation than did formulation II in 111- and 25-hour bearing tests, respectively.

Jones, W. R., Jr.↗