At least 145 records · Page 8

Molecular design principles of Lysine-DOPA wet adhesion

The mussel byssus has long been a source of inspiration for the adhesion community. Recently, adhesive synergy between flanking lysine (Lys, K) and 3,4-Dihydroxyphenylalanine (DOPA, Y ) residues in the mussel foot proteins (Mfps) has been highlighted. However, the complex topological relationship of DOPA and Lys as well as the interfacial adhesive roles of other amino acids have been understudied. Herein, we study adhesion of Lys and DOPA-containing peptides to organic and inorganic substrates using single-molecule force spectroscopy (SMFS). We show that a modest increase in peptide length, from K Y to (K Y ) 3 , increases adhesion strength to TiO 2. Surprisingly, further increase in peptide length offers no additional benefit. Additionally, comparison of adhesion of dipeptides containing Lys and either DOPA (K Y ) or phenylalanine (KF) shows that DOPA is stronger and more versatile. We furthermore demonstrate that incorporating a nonadhesive spacer between (K Y ) repeats can mimic the hidden length in the Mfp and act as an effective strategy to dissipate energy.

59 BASIC BIOLOGICAL SCIENCES↗

Adhesion of impure ice on surfaces

The undesirable buildup of ice can compromise the operational safety of ships in the Arctic to high-flying airplanes, thereby having a detrimental impact on modern life in cold climates. The obstinately strong adhesion between ice and most functional surfaces makes ice removal an energetically expensive and dangerous affair. Hence, over the past few decades, substantial efforts have been directed toward the development of passive ice-shedding surfaces. Conventionally, such research on ice adhesion has almost always been based on ice solidified from pure water. However, in all practical situations, freezing water has dissolved contaminants; ice adhesion studies of which have remained elusive thus far. Here, in this work, we cast light on the fundamental role played by various impurities (salt, surfactant, and solvent) commonly found in natural water bodies on the adhesion of ice on common structural materials. We elucidate how varying freezing temperature & contaminant concentration can significantly alter the resultant ice adhesion strength making it either super-slippery or fiercely adherent. The entrapment of impurities in ice changes with the rate of freezing and ensuing adhesion strength increases as the cooling temperature decreases. We discuss the possible role played by the in situ generated solute enriched liquid layer and the nanometric water-like disordered ice layer sandwiched between ice and the substrate behind these observations. Our work provides useful insights into the elementary nature of impure water-to-ice transformation and contributes to the knowledge base of various natural phenomena and rational design of a broad spectrum of anti-icing technologies for transportation, infrastructure, and energy systems.

36 MATERIALS SCIENCE↗

Exploring Failure of Adhesively-Bonded Joints with Different Void Sizes at the Same Void Volume Fraction through A Micro-scale Numerical Modeling

This paper studied the effects of void sizes on the failure behavior of adhesively-bonded materials under global shear via micro-scale computational modeling. The numerical results indicate that large void sizes with increased distances between them at the same void volume fraction can alleviate the reduced joint strength of a weaker adherend-adhesive interface caused by interfacial voids. However, this is not the case for an adherend-adhesive interface with the interfacial tensile strength being sufficiently higher than the adhesive strength, showing the negligible effect on the joint strength due to various void sizes and the amount of interfacial voids. This preliminary investigation provides insightful information for scaling up the void size in the macro-scale computational modeling of joints, and enhances the understanding of the micro-mechanical adhesion in adherend-adhesive interfaces with different levels of bonding.

Qiao, Yao↗

Adhesion and transfer of polytetrafluoroethylene to tungsten studied by field ion microscopy

Mechanical contacts between polytetrafluoroethylene (PTFE) and tungsten field ion tips were made in situ in the field ion microscope. Both load and force of adhesion were measured for varying contact times and for clean and contaminated tungsten tips. Strong adhesion between the PTFE and clean tungsten was observed at contact times greater than 2.5 min (forces of adhesion were greater than three times the load). For times less than 2.5 min, the force of adhesion was immeasurably small. The increase in adhesion with contact time after 2.5 min can be attributed to the increase in true contact area by creep of PTFE. No adhesion was measurable at long contact times with contaminated tungsten tips. Neon field ion micrographs taken after the contacts show many linear and branched arrays which appear to represent PTFE that remains adhered to the surface even at the high electric fields required for imaging.

Brainard, W. A.↗

Characterization of Adhesives for Attaching Reusable Surface Insulation on Space Shuttle Vehicles

An extensive development and testing program on adhesive systems shows that: (1) A closed cell silicone rubber sponge bonded to substrates with thin bond lines of glass filled adhesive exhibits density and modulus values approximately one third that of solid silicone adhesives; (2) utilization of glass or phenolic microballoons as fillers in silicone adhesives reduces density but increases moduli of the vulcanized materials; (3) the silicone elastomer based adhesives appear to be complex systems rather than homogeneous, isotropic materials. Tensile, shear, and compression properties plotted versus temperature verify this conjecture; and (4) constant strain-stress relaxation tests on glass-filled adhesive show that stress relaxation is most pronounced near the glass transition temperature.

Owen, H. P.↗

Cryogenic/high temperature structural adhesives

Results are described of the work performed to develop a structural adhesive system which possesses useful properties over a 20K (-423 F) to 589 K (600 F) temperature range. Adhesives systems based on polyimide, polyphenylquinoxaline polyquinoxaline, polybenzothiazole and polybenzimidazole polymers first were screened for suitability. Detailed evaluation of two polyimide adhesive sytems, Br34/FM34 and P4/A5F or P4A/A5FA, and one polyphenylquinoxaline adhesive system, PPQ II (IMW), then was performed. Property information was generated over the full temperature range for shear strength, stressed and unstressed thermal aging, thermal shock and coefficient of thermal expansion. Both polyimide adhesive systems were identified as being capable of providing structural adhesive joints for cryogenic/high temperature service.

Vaughan, R. W.↗

Effect of Various Material Properties on the Adhesive Stage of Fretting

Various properties of metals and alloys were studied with respect to their effect on the initial stage of the fretting process, namely adhesion. Crystallographic orientation, crystal structure, interfacial binding energies of dissimiliar metal, segregation of alloy constituents and the nature and structure of surface films were found to influence adhesion. High atomic density, low surface energy grain orientations exhibited lower adhesion than other orientations. Knowledge of interfacial surface binding energies assists in predicting adhesive transfer and wear. Selective surface segregation of alloy constituents accomplishes both a reduction in adhesion and improved surface oxidation characteristics. Equivalent surface coverages of various adsorbed species indicate that some are markedly more effective in inhibiting adhesion than others.

Buckley, D. H.↗

Cryogenic/high temperature structural adhesives

Studies were conducted to develop a structural adhesive system possessing useful properties over a 20 to 589 K temperature range. Adhesive systems based on polyimide, polyphenylquinoxaline, polyquinoxaline, polybenzothiazole and polybenzimidazole polymers first were screened for suitability. Detailed evaluation of two polyimide adhesive systems, BR34/FM34 and P4/A5F or P4A/A5FA, and one polyphenylquinoxaline adhesive system, PPQ (IMW), then was performed. Property information was generated over the full temperature range for shear strength, stressed and unstressed thermal aging, thermal shock, and coefficient of thermal expansion. Both polyimide adhesive systems were identified as being capable of providing structural adhesive joints for cryogenic/high temperature service.

Vaughan, R. W.↗

NR-150B2 adhesive development

Adhesive based polyimide solutions which are more easily processed than conventional aromatic polyimide systems and show potential for use for extended times at 589K are discussed. The adhesive system is based on a solution containing diglyme as the solvent and 2,2 bis(3',4'-dicarboxyphenyl)hexafluoropropane, paraphenylenediamine, and oxydianiline. The replacement of N-methylpyrrolidone with diglyme as the solvent was found to improve the adhesive strengths of lap shear samples and simplify the processing conditions for bonding both titanium and graphite fiber/polyimide matrix resin composites. Information was obtained on the effects of various environments including high humidity, immersion in jet fuel and methylethylketone on aluminum filled adhesive bonds. The adhesive was also evaluated in wide area bonds and flatwise tensile specimens using titanium honeycomb and composite face sheets. It was indicated that the developed adhesive system has the potential for use in applications requiring long term exposure to at least 589K (600 F).

Blatz, P. S.↗

Thermophysical and flammability characterization of phosphorylated epoxy adhesives

Some of the thermophysical and flammability properties of a phosphorylated epoxy adhesive, which has potential applications in aircraft interior panels, are described. The adhesive consists of stoichiometric ratios of bis(3-glycidyloxphenyl)methylphosphine oxide and bis(3-aminophenyl)methylphosphine oxide containing approximately 7.5% phosphorus. Preliminary data are presented from adhesive bonding studies conducted utilizing this adhesive with polyvinyl fluoride (PVF) film and phenolic-glass laminates. Limiting oxygen index and smoke density data are presented and compared with those of the tetraglycidyl methylene dianiline epoxy resin-adhesive system currently used in aircraft interiors. Initial results indicate that the phosphorylated epoxy compound has excellent adhesive properties when used with PVF film and that desirable fire-resistant properties are maintained.

Kourtides, D. A.↗

Evaluation of high-temperature structural adhesives for extended service

Candidate high-temperature stable resin formulations were evaluated for adhesive properties when bonded to titanium treated with various surface preparations. The adhesive formulations included LARC-13, NR150 A2, NR150 B2, NR056X, FM-34, HR-602, and polyphenylquinoxaline. Eight titanium surface preparations were compared for resulting bond strength with the candidate adhesives. After initial evaluation, three adhesive systems (comprised of adhesive, primer, and titanium surface preparation) were selected for further screening. The screening (still in progress) includes cure-cycle optimization and bond properties from 219 K (-65 F) to 505 K (450 F), after isothermal aging at 505 K (450 F) up to 15,000 hours, and after humidity aging at 322 K 9120 F)/ 95 percent R. H. for up to 2000 hours. Larger-area bond capability of the three adhesive system can be demonstrated by fabrication of 30.5 cm (12 in) square titanium honeycomb sandwich and metal-to-metal bonded panels.

Hendricks, C. L.↗

Recent developments in polyimide adhesives at NASA-Langley Research Center

Adhesive development is directed towards elevated temperature applications (200-300 C). Because of thermal stability considerations, the most attractive adhesives for this temperature range are linear and addition polyimides. The linear polymide adhesive research encompassed basic structure-property relationships, solvent studies and formulations to meet various requirements. The most recent research in linear polyimide systems was in the development of thermoplastic systems in an effort to eliminate the undesirable evolution of water classically associated with the cure going through an amide-acid intermediate step in the cure process. Addition polyimide adhesive research was undertaken in order to avoid water evolution during cure. Basic structure-property relationships for these materials led to an adhesive which was used extensively for high temperature adhesive needs. Since addition systems are of a highly crosslinked nature, they are not as resistant to impact as their linear counterparts. In order to overcome this problem, research was done in the area of elastomer-toughening these polymers.

St.clair, T. L.↗

Develop, demonstrate, and verify large area composite structural bonding with polyimide adhesives

The technology required to produce graphite-polyimide structural components with operational capability at 598 K (600 F) is considered. A series of polyimide adhesives was screened for mechanical and physical properties and processibility in fabricating large midplane bonded panels and honeycomb sandwich panels in an effort to fabricate a structural test component of the space shuttle aft body flap. From 41 formulations, LaRC-13, FM34B-18, and a modified LaRC-13 adhesive were selected for further evaluation. The LaRC-13 adhesive was rated as the best of the three adhesives in terms of availability, cost, processibility, properties, and ability to produce void fee large area (12" x 12") midplane bonds. Surface treatments and primers for the adhesives were evaluated and processes were developed for the fabrication of honeycomb sandwich panels of very good quality which was evidenced by rupture in the honeycomb core rather than in the facesheet bands on flatwise tensile strength testing. The fabrication of the adhesively bonded honeycomb sandwich cover panels, ribs, and leading edge covers of Celion graphite/LARC-160 polyimide laminates is described.

Bhombal, B. D.↗

Characterization of mode 1 and mixed-mode failure of adhesive bonds between composite adherends

A combined experimental and analytical investigation of an adhesively bonded composite joint was conducted to characterize both the static and fatigue beyond growth mechanism under mode 1 and mixed-mode 1 and 2 loadings. Two bonded systems were studied: graphite/epoxy adherends bonded with EC 3445 and FM-300 adhesives. For each bonded system, two specimen types were tested: a double-cantilever-beam specimen for mode 1 loading and a cracked-lapshear specimen for mixed-mode 1 and 2 loading. In all specimens tested, failure occurred in the form of debond growth. Debonding always occurred in a cohesive manner with EC 3445 adhesive. The FM-300 adhesive debonded in a cohesive manner under mixed-mode 1 and 2 loading, but in a cohesive, adhesive, or combined cohesive and adhesive manner under mode 1 loading. Total strain-energy release rate appeared to be the driving parameter for debond growth under static and fatigue loadings.

Mall, S.↗

Adhesion and wear resistance of materials

Recent studies into the nature of bonding at the interface between two solids in contact or a solid and deposited film have provided a better understanding of those properties important to the adhesive wear resistance of materials. Analytical and experimental progress are reviewed. For simple metal systems the adhesive bond forces are related to electronic wave function overlap. With metals in contact with nonmetals, molecular-orbital energy, and density of states, respectively can provide insight into adhesion and wear. Experimental results are presented which correlate adhesive forces measured between solids and the electronic surface structures. Orientation, surface reconstruction, surface segregation, adsorption are all shown to influence adhesive interfacial strength. The interrelationship between adhesion and the wear of the various materials as well as the life of coatings applied to substrates are discussed. Metallic systems addressed include simple metals and alloys and these materials in contact with themselves, both oxide and nonoxide ceramics, diamond, polymers, and inorganic coating compounds, h as diamondlike carbon.

Buckley, D. H.↗

Status of high temperature adhesives

The status of high temperature organic adhesives is reviewed. These materials are defined by having usable adhesive properties at temperatures ranging from 232 C (after hundreds of hours at 232 C) to 538 C (after a few minutes at 538 C). The search for high temperature adhesives began in the 1960s, primarily under government funding. Since then, many high temperature polymers have undergone evaluation as adhesives. In spite of this effort, only a few are commercially available because of an elusive market and an unfavorable combination of price, processability and performance. The principal adhesives to be discussed will be addition and condensation polyimides, polyquinoxalines, polybenzimidazoles, and addition, condensation, and cross-linked polyphenylquinoxalines. The synthesis, processability, adhesive performance, and availabiity of these materials are addressed.

Hergenrother, P. M.↗

Characterization of mode I and mixed-mode failure of adhesive bonds between composite adherends

A combined experimental and analytical investigation of an adhesively bonded composite joint was conducted to characterize both the static and fatigue beyond growth mechanism under mode 1 and mixed-mode 1 and 2 loadings. Two bonded systems were studied: graphite/epoxy adherends bonded with EC 3445 and FM-300 adhesives. For each bonded system, two specimen types were tested: a double-cantilever-beam specimen for mode 1 loading and a cracked-lapshear specimen for mixed-mode 1 and 2 loading. In all specimens tested, failure occurred in the form of debond growth. Debonding always occurred in a cohesive manner with EC 3445 adhesive. The FM-300 adhesive debonded in a cohesive manner under mixed-mode 1 and 2 loading, but in a cohesive, adhesive, or combined cohesive and adhesive manner under mode 1 loading. Total strain-energy release rate appeared to be the driving parameter for debond growth under static and fatigue loadings.

Mall, S.↗

Enhancing Adhesion: Relative Merits of Different Approaches

Adhesive performance is improved mainly by manipulation of the bimaterials interface zone, which is only a few molecules thick. There are three approaches to enhancement of interfacial adhesion at the molecular level. They are 1) changing the nonchemically bonded interactions across the interface from weak ones to strong ones, 2) making the true interfacial area much larger than the simple geometric area, and 3) inducing chemical bonding between the two materials forming the interface. Our goal this summer was to question some of the built-in assumptions contained within these approaches and to determine the most promising approach, both theoretically and practically, for enhancing adhesion in NASA structures. Our computations revealed that all three of these approaches have, in theory, the potential to enhance molecular adhesion approximately ten-fold. Experiments, however, revealed that this excellent level of enhancement is not likely to be reached in practice. Each approach was found to be severely limited by practical problems. In addition, some of the built-in assumptions associated with these approaches were found to be insufficient or inadequate. The first approach, changing the nonchemically bonded interactions from weak to strong, Is an example of one containing inadequate assumptions. The extensive literature on intermolecular interactions, based on solution studies, shows that certain functional group pairs interact much more strongly than others. It has always been assumed that these data can be reliably extended to systems where only one member of the pair is in solution and the other Is contained in a solid surface. Our experiments this summer demonstrated that solution data do not adequately predict the strength of functional group interaction at the solid-liquid interface. Furthermore, the strong solvents needed to dissolve the monomers or polymers to which the functional groups of interest are attached compete successfully with the solid surface for the functional group. As a result, functional groups in solution cannot pair with the complementary groups in the solid surface, and the expected enhancement of nonchemically bonded interactions is not realized. The second approach, increasing the true interfacial area, is an example of one containing inadequate assumptions and suffering from numerous practical problems. First, practitioners have assumed that material removal, such as bead blasting or etching, increases true surface area (and therefore interfacial area) in a meaningful way. Our geometric analysis demonstrated that removal methods increase area by a factor of two at most. To increase interfacial area by an order of magnitude or more. a thin layer of high porosity must be added to the substrate surface prior to application of the adhesive phase. Consistent with this finding, we attempted to create a thin layer of rigid, highly porous glass on the surface of our smooth glass substrate by means of sol-gel technology. We were unable to surmount a wide variety of practical problems and obtained only collapsed, nonporous layers. Thus this approach, appealing in principle, would require long term development and is not promising in the near term. The third approach, inducing chemical bonding at the interface, is an example of one having neither inadequate assumptions nor insurmountable practical problems. When silicate glass is the substrate, there are only a few chemical reactions that can be successfully conducted to create these chemical bonds, and these reactions usually involve silicon-containing reagents. We compared the silazane reagents to the silane reagents and found through experiment that the silazanes react with the glass surface much more readily, and under milder conditions, than the silanes. The functional groups attached to the glass surface by silazane reactions were not able to be removed by solvent extraction, elevated temperature exposure, or mechanical action. This clearly indicates that the formation of chemical bonds at the interface is the most effective approach for enhancing molecular adhesion.

Penn, L. S.↗