Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “WEAR”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 127 records · Page 7

Effect of annealing treatment on the dry sliding wear behavior of copper

We report the effect of annealing on the wear behavior of commercial grade pure copper (Cu) was evaluated by performing unlubricated pin-on-disc wear tests of as-received and annealed samples under 0.1-10 kgf normal load. It was found that annealing at 800 °C for 24 h led to an increase of grain size of Cu from ~ 6.7 to ~ 15.3 μm and a decrease in hardness. Wear rates of both samples increased while the friction coefficients decreased with increasing normal load. Subsurface microstructure evolution and wear debris were characterized by high resolution electron backscattered diffraction (EBSD) and transmission electron microscopy (TEM) after wear tests. Dynamic recrystallization and abnormal subsurface grain growth were observed in both samples under high load. Finally, the effect of annealing on the microstructure evolution and wear resistance of Cu were discussed.

36 MATERIALS SCIENCE↗

Carbon nanotube (CNT) reinforced 316L stainless steel composites made by laser powder bed fusion: Microstructure and wear response

Carbon nanotube (CNT) reinforced 316L stainless steel (SS) composites were fabricated by laser powder bed fusion (LPBF) additive manufacturing (AM). This study focuses on microstructure evolution, hardness, and wear behavior. The wear behavior for AM 316L SS and 1 wt% CNT/316L SS was studied by a dry sliding test under normal loads of 10, 15, and 25 N. The addition of CNT to 316L SS led to the change of solidification mode from cellular/columnar to dendritic growth, producing grain refinement. Nanoscale dendrites were observed. Although TEM characterization confirmed the existence of CNT in cell interior, most CNT were damaged, resulting in carbon material segregation along cellular/dendritic boundaries. The wear rate was found dramatically decreased due to the improved hardness. Compared to the adhesive and abrasive wear in AM 316L SS, the wear mechanism of CNT/316L composite was adhesion and oxidative wear. Furthermore, enhanced cellular/dendritic boundary strengthening by carbon segregation was the main strengthening mechanism of CNT/316L composite.

36 MATERIALS SCIENCE↗

Estimation of cutting tool wear using an elastomeric tactile sensor

Machining performance of cutting tools and part quality are affected by the geometric condition of the cutting edge, which is influenced by thermomechanical loads experienced during the process. Tool condition monitoring (TCM) systems provide insight for timely replacement of cutting tools. However, existing TCM systems are expensive and require specialized equipment or sensors, hindering widespread adoption. A novel TCM system is developed herein using an elastomeric tactile sensor. Sensor images of the cutting edge are used to quantify wear using two distinct algorithms. In the first algorithm, the unworn and worn edges are identified based on Canny edge detect. In the second, the unworn edge is identified using edge detection while the region of wear is identified using a relative intensity method. In both cases, the maximum wear width is calculated based on an experimentally determined pixel to-physical distance scale. The TCM system is first used to estimate flank wear on a solid carbide helical end mill before evaluating its robustness by employing it to estimate insert wear of an indexable helical end mill. Measurements are also performed manually using an optical microscope and a high-resolution focus variation microscope for verification. The novel technique estimates flank wear in the solid carbide tool with a high accuracy of 98%. Larger discrepancies are observed for the inserts, however, with overlapping uncertainties. In conclusion, the technique shows promise in adaptability, automation, and closed loop control of machine tools.

Machining↗

Wear Mechanism Analysis of a New Rotary Shear Biomass Comminution System

A new biomass comminution system, Crumbler rotary shear, was developed to process fuel-grade biomass. The rotary shear is more efficient than the traditional hammer mill in comminuting high-moisture biomass and producing more uniform particles with minimal fines. However, the milling unit experiences significant wear in processing dirty woodchips. This study investigated the wear mechanisms of the rotary shear system based on analysis of the minerals carried by woodchips and characterization of actual worn components. Abrasive wear was found to be the dominant effect, and localized adhesive wear (material transfer), microfracture (chipping), and plastic deformation were additional effects. Connections have been made between the wear progression of key cutting components and the particle size change of biomass extrinsic minerals. On the basis of the wear mechanism understanding, mitigations based on advanced tool materials and optimized tool geometric designs are being developed for improving the tool life and cutting efficiency.

09 BIOMASS FUELS↗

Mechanical and wear properties of aluminum coating prepared by cold spraying

In this study, aluminum (Al) powders were deposited onto Al substrates using cold spray to form a coating. The main objective is to investigate and compare the microstructure, mechanical and wear properties of Al coating to that of the Al substrate. The microstructure of the coating and substrate were observed using Scanning Electron Microscope (SEM). Hardness was evaluated using the Vickers Hardness test and wear properties were investigated using a pin-on-disk wear test machine. The elemental composition of the coating and substrate was determined using Energy-dispersive X-ray spectroscopy (EDX). Results showed that the friction coefficient and specific wear rate decreased while wear rate increased linearly with increasing load. It was found that the coating exhibit slightly better mechanical and wear properties compared to the substrate.

36 MATERIALS SCIENCE↗

Analysis of Cutter Blade Wear in Rotary Shear Mills

Following development of an analytical abrasive wear model to predict wear of components in a rotary shear mill, the team used a finite element analysis (FEA) approach to calculate forces and loads acting on particles responsible for abrasive wear. The analytical model related critical rotary shear process parameters (shear geometry and rotational speed) to critical material attributes of inorganic mineral species in feedstock (density, size, and aspect ratio) and substrate (hardness and elastic modulus) that enabled us to model the wear of shear cutters in a rotary shear milling system developed by Forest Concepts. With proper knowledge of the forces acting between abrasive particles and cutter components built into it, the model can accurately predict wear of the cutters and provides a quality by design (QbD) approach to predict component reliability based on scientific engineering principles in lieu of trial-and-error approaches. During this reporting period, researchers at Oak Ridge National Laboratory applied an FEA package to simulate the local stresses and forces between an abrasive silica particle and two rotary shear cutters as the distance between the cutters decreases. The output of the FEA was used to provide more accurate projections of the loads applied to the particles in the analytical wear model. Comparison of the FEA force calculations are in good agreement with the loads assumed in the analytical predictions.

36 MATERIALS SCIENCE↗

Friction and Wear of Unlubricated NiTiHf with Nitriding Surface Treatments

The unlubricated friction and wear properties of the superelastic materials NiTi and NiTiHf, treated by either gas nitriding or plasma nitriding, have been investigated. Pin on disk testing of the studied materials was performed at sliding speeds from 0.01 to 1m/s at normal loads of 1, 5 or 10N. For all of the studied friction pairs (NiTiHf pins vs. NiTi and NiTiHf disks) over the given parameters, the steady-state coefficients of friction varied from 0.22 to 1.6. Pin wear factors ranged from approximately 1E-6 against the NiTiHf and plasma nitrided disks to approximately 1E-4 for the gas nitrided disks. The plasma nitrided disks provided wear protection in several cases and tended to wear by adhesion. The gas nitrided treatment generated the most pin wear but had essentially no disk wear except at the most severe of the studied conditions (1N load and 1m/s sliding speed). The results of this study are expected to provide guidance for design of components such as gears and fasteners.

friction↗

Influence of steel type on the propensity for tribochemical wear in boundary lubrication with a wind turbine gear oil

Tribochemical wear may occur at the interface between a surface and a lubricant as a result of chemical and mechanical interactions in a tribological contact. Understanding the onset of tribochemical wear damage on component surfaces requires the use of high resolution techniques such as transmission electron microscopy (TEM). In this study, two steel types, case carburized AISI 3310 and through-hardened AISI 52100, were wear tested using a ball-on-disk rolling/sliding contact tribometer in fully formulated commercial wind turbine gearbox oil under boundary lubrication conditions with 10% slip. With the exception of steel type, all other test conditions were held constant. Conventional tribofilm analysis in the wear tracks was performed using X-ray photoelectron spectroscopy, and no significant composition differences were detected in the tribofilms for the different steel disk types. However, TEM analysis revealed significant tribochemical wear differences between the two steel types at multiple length scales, from the near-surface material microstructure (depth < 500 nm) to the tribofilm nanostructure. Nanometer-scale interfacial cracking and surface particle detachment was observed for the AISI 52100 case, whereas the tribofilm/substrate interface was abrupt and undamaged for the AISI 3310 case. Differences in tribofilm structure, including the location and orientation of MoS{sub 2} single sheet inclusions, were observed as a function of steel type as well. It is suggested that the tribochemical wear modes observed in these experiments may be origins of macroscopic surface-initiated damage such as micropitting in bearings and gears.

17 WIND ENERGY↗

Laser-Hardened and Ultrasonically Peened Surface Layers on Tool Steel AISI D2: Correlation of the Bearing Curves’ Parameters, Hardness and Wear

This paper is focused on the effects of the separately applied laser heat treatment (LHT) and ultrasonic impact treatment (UIT) and the combined LHT + UIT process on the wear and friction behaviors of the hardened surface layers of the tool steel AISI D2. In comparison with the initial state, wear losses of the treated specimens after long-term wear tests were decreased by 68, 41, and 77% at the LHT, UIT, and combined LHT + UIT processes, respectively. The Abbott–Firestone bearing curves were used to analyze the material ratio and functional characterization (bearing capacity and oil capacitance) of the studied surface specimens. The wear losses registered after short (15 min) tests correlate well with the changes in experimental surface roughness Ra, and the predictive Rpk, and bearing capacity B{sub C} parameters, respectively, evaluated using the Abbott–Firestone curves and Kragelsky–Kombalov formula. The wear losses after the long-term (45 min) tests are in good correlation with the reciprocal surface microhardness HV and with the W{sub L} and W{sub P} wear parameters, respectively, estimated using Archard–Rabinowicz formula and complex roughness-and-strength approach. The observed HV increase is supported by nanotwins (LHT), by dense dislocation nets (UIT), and by dislocation cells/nanograins fixed with fine carbides (LHT + UIT) formed in the surface layers of the steel.

36 MATERIALS SCIENCE↗

Thermal Wear Sensing System: Proof of the Concept

A technique for wear sensing using a sacrificial layer with specific material properties has been developed successfully. This is achieved by recording the temperature evolution underneath the sacrificial organic layer during sliding tests, and by correlating the recorded temperature with a wear depth. Finite element modeling was used to calculate the contact temperature which spreads through the sacrificial layer under different sliding test conditions. Numerical simulation was used to determine the optimal parameters for the best correlation between temperature and wear depth. These parameters were used to select the appropriate sacrificial layer for wear sensing. Thus, an epoxy layer was implemented and experimental measurements were carried out to check the correlation between the measured temperature underneath the epoxy layer and wear depth. It was found that a low thermal conductivity of the sacrificial layer of less than 1 W/m K and a relative high thermal conductivity of the substrate, namely more than 4 W/m K are the optimal parameters for our thermal wear sensing system. The thickness of the sacrificial layer is also a crucial parameter and has to be taken into account when designing such a sensing system.

36 MATERIALS SCIENCE↗

Wear Mechanisms in Contacts Involving Slippers in Axial Piston Pumps: A Multi-Technical Analysis

Axial piston pumps are widely used in actuation as power conversion systems, especially in aeronautics. Even though they combine compactness and efficiency, wear of their parts reduces their lifespan. Studies on these pumps often consist in analytic or numerical analyses of lubricated contact between their components. Piston slippers are in tribological contacts with swashplate, pistons and slipper retainer. This study aims to understand wear mechanisms in the contacts involving this central component. An experimental multi-technical analysis of helicopter pumps parts after several functioning times is presented. To determine wear mechanisms, worn surfaces are observed with SEM. 3D surface roughness measurements provide surface topography. Contact conditions and consequently wear severity and mechanisms differ from one contact to another. Detached coarse carbides from the swashplate surface act as an abrading third-body against slippers and swashplate. Debris generated in this contact is carried by the fluid to the other contacts. Although pistons are made of the same steel as swashplate, there is no carbide detachment and wear comes from debris polluting the fluid. Slipper retainer is almost not worn, and debris causes abrasive wear and craters generation in the slippers.

36 MATERIALS SCIENCE↗

Modeling of complex wear behavior associated with grid-to-rod fretting in light water nuclear reactors

One significant concern in the operation of light water nuclear reactors is the fretting wear damage to fuel cladding from flow-induced vibrations. For years, research on the grid-to-rod fretting (GTRF) phenomena has been underway in countries where nuclear power production is a significant industry. Under the auspices of the U.S. Department of Energy Consortium for Advanced Simulation of Light Water Reactors, an effort has been underway to develop and test an engineering wear model for zirconium alloy fuel rod cladding against a supporting grid. Furthermore, the multi-stage model accounts for oxide layers and wear rate transitions. Our paper describes the basis for a GTRF engineering wear model, the physical significance of the wear factor it contains, and recent progress toward model validation based on a fretting wear testing apparatus that accounts for coolant temperature, pressure, and the presence of periodic impacts (gaps) in grid/rod contact.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Graphene - MoS 2 ensembles to reduce friction and wear in DLC-Steel contacts

Recent demonstration of two dimensional (2D) solid lubricant materials to minimize friction to unmeasurable levels (superlubricity) and reduce wear at macroscale propelled further research investigations in the direction of exploring their potential in industrially relevant material combinations such as steel and diamond-like-carbon (DLC) in sliding contact. In this study, we have used a combination of 2D materials i. e. Graphene and MoS 2 as a solid lubricant to reduce friction and wear in steel-hydrogenated DLC contacts even at high contact pressures and sliding speed. Sliding friction tests conducted under dry nitrogen conditions shows a reduction of friction and wear by 16 and 29 times, respectively as compared to Steel vs H-DLC (baseline) experiments and friction and wear by a factor of 43 and 434, respectively, compared to self-mated steel vs steel experiments. In conclusion, optical and Raman investigations of the material pairs and the wear debris analysis in TEM indicated the formation of amorphous carbon mixed graphene layers at the sliding interface leading to such dramatic reductions in friction and wear.

36 MATERIALS SCIENCE↗

Hybrid data-driven and model-informed online tool wear detection in milling machines

Precision machining tool wear is responsible for low product throughput and quality. Monitoring the tool wear online is vital to prevent degradation in machining quality. However, direct real-time tool wear measurement is not practical. This paper presents residual-based anomaly detection models, combining a hybrid model comprised of a physics-based model and a data-driven model (a decision tree or a neural network) to predict signals of interest (e.g., power or forces) under nominal conditions, followed by Page’s cumulative sum test for detecting tool wear on-line using the computer numerical control machine measurements. The most informative features are ranked using dynamic programming and its approximation variants from real-time measurements and machine settings, such as the width of cut, depth of cut, feed rate and spindle speed, that serve as inputs to the predictive models. The baseline nominal model is incrementally updated with experimental data via a gradient boosted adaptation model to generate the residuals that account for discrepancies between the actual machine data under normal conditions and the baseline nominal model predictions. The hybrid model is validated against 20 Mazak milling machine experimental tests and one Haas run-to-failure experiment. The proposed anomaly detector is applied to synthetic data from simulations of the physics-based model at different operating conditions, measurement noise levels, and tool wear levels, and the methods were able to achieve an overall 92% accuracy in data with 1% noise. The anomaly detection methods based on hybrid model reduced the false alarms of either the data-driven or physical-based models alone, and are found to be capable of good online detection of tool wear.

42 ENGINEERING↗

Thick graded interfaces increase wear resistance in Ti/TiN nanolayered thin films

Multilayered composites with nanoscale layer thickness incorporating titanium and titanium nitride (Ti/TiN) are used as a model system to study the effects of heterophase interface structure on elastic and plastic deformation, as well as wear behavior. Here, in this work, hardness, modulus, and wear rate under dry reciprocating sliding contact are quantified as a function of Ti-TiN heterophase interfacial nitrogen gradient thickness for Ti/TiN multilayers with 10–80 nm layer thickness. Hardness and modulus are found to be inversely proportional to layer thickness and independent of interface gradient for most specimens. Wear rate is found to be inversely proportional to interface gradient thickness at constant layer thickness, demonstrating that control of nanoscale interface structure is a valid approach to enhancing wear behavior. The materials studied in this work wear comparably or slower than other Ti- and TiN-based composites in the literature, providing a promising avenue for engineering wear-resistant materials for use in industrially relevant applications.

Graded interfaces↗

The characterization of wear-causing particles and silica sand in particular

Erodants and abradants are two types of wear-causing particles (WCP). Despite their effects on the severity and rate of wear, WCP are inadequately characterized in a surprising number of publications, especially those involving impingement erosion and three-body abrasion. That shortfall makes it difficult to correlate features of WCP with the details of worn surfaces, or to develop wear models that account for those features. It is argued that the documentation of WCP should go beyond simply reporting their composition and mean particle size. In late 1985, ASTM Committee G2 on Wear and Erosion established a task group on the characterization of WCP. At that time, image analysis was slower and less sophisticated than it is today. While that ASTM task group failed to produce a consensus standard, computerized particle characterization methods were developing in fields other than tribology, fields like geoscience, heavy sand mining, materials processing, and pharmaceuticals. A notable exception to this is ferrography, which is a widely-used diagnostic for lubricated tribosystems. In the context of dry wear, it is useful to identify which features of WCP would be beneficial to document, and to identify some techniques and scales of detail appropriate to particular tribosystems. In this paper, examples are presented for the morphological and mechanical characterization of silica sand grains, as prompted by a triboanalysis of the abrasive and erosive wear of biomass pre-processing equipment. The authors propose a minimum level of documentation for WCP, one that can enrich tribosystem analysis both in laboratory tests and field studies.

36 MATERIALS SCIENCE↗

Anti-Wear Performance and Mechanism of an Oil-Miscible Ionic Liquid as a Lubricant Additive

An ionic liquid (IL) trihexyltetradecylphosphonium bis(2-ethylhexyl) phosphate has been investigated as a potential anti-wear lubricant additive. Unlike most other ILs that have very low solubility in non-polar fluids, this IL is fully miscible with various hydrocarbon oils. In addition, it is thermally stable up to 347 oC, showed no corrosive attack to cast iron in ambient environment, and has excellent wettability on solid surfaces (e.g., contact angle on cast iron <8o). Most importantly, this phosphonium-based IL has demonstrated effective anti-scuffing and anti-wear characteristics when blended with lubricating oils. For example, a 5 wt.% addition into a synthetic base oil eliminated the scuffing failure experienced by the neat oil and, as a result, reduced the friction coefficient by 60% and the wear rate by three orders of magnitude. A synergistic effect on wear protection was observed with the current anti-wear additive when added into a fully-formulated engine oil. Nanostructure examination and composition analysis revealed a tribo-boundary film and subsurface plastic deformation zone for the metallic surface lubricated by the IL-containing lubricants. This protective boundary film is believed to be responsible for the IL s anti-scuffing and anti-wear functionality.

36 MATERIALS SCIENCE↗

Recoil-Implantation Of Multiple Radioisotopes Towards Wear Rate Measurements And Particle Tracing In Prosthetic Joints

This study demonstrates a new method of radioisotope labeling of ultra-high molecular weight polyethylene inserts in prosthetic joints for wear studies. The radioisotopes {sup 97}Ru, {sup 100}Pd, {sup 100}Rh, and {sup 101m}Rh are produced in fusion evaporation reactions induced by {sup 12}C ions in a {sup 92}Zr target foil. The fusion products recoil-implant into ultra-high molecular weight polyethylene plugs, machined to fit into the surface of the inserts. During laboratory simulations of the joint motion, a wear rate of the labeled polyethylene may be measured and the pathways of wear debris particles can be traced by detecting characteristic gamma-rays. The concentration profiles of the radioisotopes extend effectively uniformly from the polyethylene surface to a depth of about 4 {mu}m. The multiplicity of labeling and the use of several gamma-ray lines aids with avoiding systematic measurement uncertainties. Two polyethylene plugs were labeled and one was fitted into the surface of the tibial insert of a knee prosthesis, which had been worn in. Actuation over close to 100,000 cycles with a 900 N axial load and a 24 deg. flexion angle removed (14{+-}1)% of the gamma-ray activity from the plug. Most of this activity dispersed into the serum lubricant identifying this as the important debris pathway. Less than 1% activity was transferred to the femoral component of the prosthesis and the measured activity on the tibial tray was insignificant. Assuming uniform wear across the superior surface of the insert, a wear rate of (12{+-}3) mm{sup 3}/Megacycle was determined. This is consistent with wear rate measurements under similar conditions using other techniques.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗