Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “joint”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 109 records · Page 6

Phase Field Modeling of Corrosion for Design of Next-Generation Magnesium-Aluminum Vehicle Joints

In this study, WPI and its partners sought to understand galvanic corrosion in Mg-Al friction stir weld (FSW) joints. Unlike fusion welds, FSW is done in the solid state. This limits (but does not eliminate) the formation of brittle Al-Mg intermetallics, resulting in better joint strength and corrosion resistance. This study aimed to understand corrosion behavior of Mg-Al FSW joints by using a Cahn-Hilliard phase field electrochemistry model based on the work of Pongsaksawad et al. Its context challenge problem was an ultra-light door designed by Magna with 6061-Al sheet outer and ZEK100-Mg sheet inner panels, joined by an adhesive and FSW. Unlike most FSW joints, which weld through the softer material into the harder one, the Al sheet’s hem joint around Mg required the FSW tool to through the harder Al into the softer Mg, which was itself a challenge. Despite this challenge, PNNL succeeded in consistently making very strong FSW lap joints, by using a triflute tool and power control. Characterization showed mostly separate Al and Mg regions in the weld, usually with a hook protruding from Al into Mg, which likely contributed to high joint strength. Nanohardness mapping showed higher hardness in thin Mg swirls into the Al nugget, likely due to the intermetallics. The study used the industry standard SAE J2334 Cyclic Corrosion Test (CCT) to simulate corrosion conditions over the life of a vehicle, as well as linear polarization testing and ASTM G71 pitting corrosion testing. Corrosion reactions were: H 2 O + ½O 2 + 2e - → 2OH - at the Al cathode, and either Mg → Mg 2+ + 2e - or Mg + 2OH - → Mg(OH) 2 + 2e - at the Mg anode, with electron transfer through the joint. Mass loss increased with Al section length, supporting the hypothesis that galvanic corrosion in Al-Mg joints is limited by the cathodic reaction. Both pitting corrosion (first anode reaction) and hydroxide film formation (second reaction) were observed. The J2334 CCT test method was slightly modified, adding a chromium solution cleaning step after each week of corrosion testing, in order to remove Mg oxides and hydroxides and accurately measure mass loss over time. That said, FSW joints treated in this way did not did not exhibit significant reduction in lap shear strength of the joints vs. newly welded samples which had not undergone corrosion. Corrosion appeared to consist mainly of pitting in Mg in a way which did not directly affect the bond between the materials where the joints failed. A Cahn-Hilliard phase field model coupled with electrical potential described the electronically mediated galvanic corrosion electrochemical reactions described above in the four-component Al-Mg-H 2 O-(H 2 O+½O 2 ) system. This 2-D model successfully predicted Mg(OH)₂ formation at the anode in some circumstances, and Mg pitting corrosion in others, and showed the correct electric field directions in both cases. The model predicted Mg pit corrosion depth within a factor of two of measured pits.

32 ENERGY CONSERVATION, CONSUMPTION, AND UTILIZATI↗

Effects of joints in truss structures

The response of truss-type structures for future space applications, such as Large Deployable Reflector (LDR), will be directly affected by joint performance. Some of the objectives of research at BAC were to characterize structural joints, establish analytical approaches that incorporate joint characteristics, and experimentally establish the validity of the analytical approaches. The test approach to characterize joints for both erectable and deployable-type structures was based upon a Force State Mapping Technique. The approach pictorially shows how the nonlinear joint results can be used for equivalent linear analysis. Testing of the Space Station joints developed at LaRC (a hinged joint at 2 Hz and a clevis joint at 2 Hz) successfully revealed the nonlinear characteristics of the joints. The Space Station joints were effectively linear when loaded to plus or minus 500 pounds with a corresponding displacement of about plus or minus 0.0015 inch. It was indicated that good linear joints exist which are compatible with errected structures, but that difficulty may be encountered if nonlinear-type joints are incorporated in the structure.

Ikegami, R.↗

Joints in deployable space truss structures

Since the response of deployable structural concepts being considered for the Large Deployable Reflector (LDR) backup structure will be dominated by the response of joints, the joint characteristics are significant. An overview is given of the research activities at LaRC on the static behavior of joints for deployable space truss structures. Since a pin-clevis-type joint will be utilized in deployable structures, an experimental research program to characterize the joint parameters which affect stiffness was conducted. An experimental research program was conducted on a second type of joint, referred to as a near-center latch joint. It was used in the center of members on the deployable truss structure for the Control of Flexible Structures (COFS) flight experiment. The test results of the near-center latch joint and the member with the joints indicated that the stiffness of the near-center joint is linear and stiffer than the stiffness of the total member, and that non-linearities in the stiffness characteristics of the total member were due to bending introduced at the ends of the member. The resulting data indicates that stiff linear folding joints can be designed and that bending load paths should be avoided whenever possible. In summary, for deployable structures, special attention to the joint and the structure design is required to minimize the undesirable structural non-linearities.

Rhodes, M.↗

Axisymmetric shell analysis of the space shuttle solid rocket booster field joint

The Space Shuttle Challenger (STS 51-L) accident led to an intense investigation of the structural behavior of the solid rocket booster (SRB) tang and clevis field joints. Results are presented of axisymmetric shell analyses that parametrically assess the structural behavior of SRB field joints subjected to quasi-steady-state internal pressure loading for both the original joint flown on mission STS 51-L and the redesigned joint flown for the first time after the STS 51-L accident on the Space Shuttle Discovery. Discussion of axisymmetric shell modeling issues and details is presented and a generic method for simulating contact between adjacent shells of revolution is described. Results are presented that identify the performance trends of the joints for a wide range of joint parameters. An important finding is that the redesigned joint exhibits significantly smaller O-ring gap changes and much less sensitivity to joint clearances than the original joint. For a wide range of joint parameters, the result presented indicate that the redesigned joint provides a much better pressure seal than the original joint.

Nemeth, Michael P.↗

A Single-Lap Joint Adhesive Bonding Optimization Method Using Gradient and Genetic Algorithms

A natural process for any engineer, scientist, educator, etc. is to seek the most efficient method for accomplishing a given task. In the case of structural design, an area that has a significant impact on the structural efficiency is joint design. Unless the structure is machined from a solid block of material, the individual components which compose the overall structure must be joined together. The method for joining a structure varies depending on the applied loads, material, assembly and disassembly requirements, service life, environment, etc. Using both metallic and fiber reinforced plastic materials limits the user to two methods or a combination of these methods for joining the components into one structure. The first is mechanical fastening and the second is adhesive bonding. Mechanical fastening is by far the most popular joining technique; however, in terms of structural efficiency, adhesive bonding provides a superior joint since the load is distributed uniformly across the joint. The purpose of this paper is to develop a method for optimizing single-lap joint adhesive bonded structures using both gradient and genetic algorithms and comparing the solution process for each method. The goal of the single-lap joint optimization is to find the most efficient structure that meets the imposed requirements while still remaining as lightweight, economical, and reliable as possible. For the single-lap joint, an optimum joint is determined by minimizing the weight of the overall joint based on constraints from adhesive strengths as well as empirically derived rules. The analytical solution of the sin-le-lap joint is determined using the classical Goland-Reissner technique for case 2 type adhesive joints. Joint weight minimization is achieved using a commercially available routine, Design Optimization Tool (DOT), for the gradient solution while an author developed method is used for the genetic algorithm solution. Results illustrate the critical design variables as a function of adhesive properties and convergences of different joints based on the two optimization methods.

Smeltzer, Stanley S., III↗

Low-Friction, High-Stiffness Joint for Uniaxial Load Cell

A universal-joint assembly has been devised for transferring axial tension or compression to a load cell. To maximize measurement accuracy, the assembly is required to minimize any moments and non-axial forces on the load cell and to exhibit little or no hysteresis. The requirement to minimize hysteresis translates to a requirement to maximize axial stiffness (including minimizing backlash) and a simultaneous requirement to minimize friction. In practice, these are competing requirements, encountered repeatedly in efforts to design universal joints. Often, universal-joint designs represent compromises between these requirements. The improved universal-joint assembly contains two universal joints, each containing two adjustable pairs of angular-contact ball bearings. One might be tempted to ask why one could not use simple ball-and-socket joints rather than something as complex as universal joints containing adjustable pairs of angularcontact ball bearings. The answer is that ball-and-socket joints do not offer sufficient latitude to trade stiffness versus friction: the inevitable result of an attempt to make such a trade in a ball-and-socket joint is either too much backlash or too much friction. The universal joints are located at opposite ends of an axial subassembly that contains the load cell. The axial subassembly includes an axial shaft, an axial housing, and a fifth adjustable pair of angular-contact ball bearings that allows rotation of the axial housing relative to the shaft. The preload on each pair of angular-contact ball bearings can be adjusted to obtain the required stiffness with minimal friction, tailored for a specific application. The universal joint at each end affords two degrees of freedom, allowing only axial force to reach the load cell regardless of application of moments and non-axial forces. The rotational joint on the axial subassembly affords a fifth degree of freedom, preventing application of a torsion load to the load cell.

Lewis, James L.↗

Seal Joint Analysis and Design for the Ares-I Upper Stage LOX Tank

The sealing capability of the Ares-I Upper Stage liquid oxygen tank-to-sump joint is assessed by analyzing the deflections of the joint components. Analyses are performed using three-dimensional symmetric wedge finite element models and the ABAQUS commercial finite element software. For the pressure loads and feedline interface loads, the analyses employ a mixed factor of safety approach to comply with the Constellation Program factor of safety requirements. Naflex pressure-assisted seals are considered first because they have been used successfully in similar seal joints in the Space Shuttle External Tank. For the baseline sump seal joint configuration with a Naflex seal, the predicted joint opening greatly exceeds the seal design specification. Three redesign options of the joint that maintain the use of a Naflex seal are studied. The joint openings for the redesigned seal joints show improvement over the baseline configuration; however, these joint openings still exceed the seal design specification. RACO pressure-assisted seals are considered next because they are known to also be used on the Space Shuttle External Tank, and the joint opening allowable is much larger than the specification for the Naflex seals. The finite element models for the RACO seal analyses are created by modifying the models that were used for the Naflex seal analyses. The analyses show that the RACO seal may provide sufficient sealing capability for the sump seal joint. The results provide reasonable data to recommend the design change and plan a testing program to determine the capability of RACO seals in the Ares-I Upper Stage liquid oxygen tank sump seal joint.

Phillips, Dawn R.↗

Strength Variation of Parachute Joints

A parachute joint is defined as a location where a component is sewn or connected to another component. During the design and developmental phase of a parachute system, the joints for each structural component are isolated and tested through a process called seam and joint testing. The objective of seam and joint testing is to determine the degradation on a single component due to interaction with other components; this data is then used when calculating the margin of safety for that component. During the engineering developmental phase of CPAS (Capsule Parachute Assembly System), the parachute system for the NASA Orion Crew Module, testing was completed for every joint of the six subsystems: the four parachutes (main, drogue, pilot, and FBCP [forward bay cover parachute]), the retention release bridle, and the retention panels. The number of joint tests for these subsystems totaled 92, which provides a plethora of data and results for further analysis. In this paper, the data and results of these seam and joint tests are examined to determine the effects, if any, of different operators and sewing machines on the strength of parachute joints. Other variables are also studied to determine their effect on joint strength, such as joint complexity, joint strength magnitude, material type, and material construction. Findings reveal that an optimally-run seam and joint test program could result in an increased understanding of the structure of the parachute; this should lead to a parachute built with optimal components, potentially saving system weight and volume.

Mollmann, Catherine↗

Development of the bus joint for the ITER Central Solenoid

The terminations of the Central Solenoid (CS) modules are connected to the bus extensions by joints located outside the CS in the gap between the CS and Torodial Field (TF) assemblies. These joints have very strict space limitations. Low resistance is a common requirement for all ITER joints. In addition, the CS bus joints will experience and must be designed to withstand significant variation in the magnetic field of several tenths of a Tesla per second during initiation of plasma. The joint resistance is specified to be less than 4 nOhm. The joints also have to be soldered in the field and designed with the possibility to be installed and dismantled in order to allow cold testing in the cold test facility. We have developed coaxial joints that meet these requirements and have demonstrated the feasibility to fabricate and assemble them in the vertical configuration. We introduced a coupling cylinder with superconducting strands soldered to the surface of the cable that can be installed in the ITER assembly hall and at the Cold Test Facility. This cylinder serves as a transition area between the CS module and the bus extension. We made two racetrack samples and tested four bus joints in our Joint Test Apparatus. Resistance of the bus joints was measured by a decay method and by a microvoltmeter; the value of the current was measured by the Hall probes. This measurement method was verified in the previous tests. The resistance of the joints varied insignificantly from 1.5 to 2 nOhm. One of the challenges associated with a soldered joint is the inability to use corrosive chemicals that are difficult to clean. This paper describes our development work on cable preparation, chrome removal, compaction, soldering, and final assembly and presents the test results.

Martovetsky, Nicolai N↗

PRELIMINARY ASSESSMENT OF NDE METHODS ON INSPECTION OF HDPE BUTT FUSION PIPING JOINTS FOR LACK OF FUSION WITH VALIDATION FROM MECHANICAL TESTING

Studies at the Pacific Northwest National Laboratory (PNNL) in Richland, Washington, are being conducted to evaluate nondestructive examinations (NDE) coupled with mechanical testing of butt fusion joints in high density polyethylene (HDPE) pipe for assessing lack of fusion. The work provides information to the United States Nuclear Regulatory Commission (NRC) on the effectiveness of volumetric inspection techniques of HDPE butt fusion joints in Section III, Division 1, Class 3, buried piping systems in nuclear power plants. This paper describes results from preliminary assessments using ultrasonic and microwave nondestructive techniques and mechanical testing with the high speed tensile impact test and the bend test for determining joint integrity. A series of butt joints were fabricated in 3408, 12 inch (30.5 cm) IPS DR-11 HDPE material by varying the fusion parameters to create good joints and joints containing a range of lack of fusion conditions. Six of these butt joints were volumetrically examined with time of flight diffraction (TOFD), phased array (PA) ultrasound, and the Evisive microwave system. The outer diameter (OD) weld beads were removed for microwave evaluation and the pipes ultrasonically re-evaluated. In two of the six pipes both the outer and inner diameter (ID) weld beads were removed and the pipe joints re-evaluated. Several of the pipes were sectioned and the joints destructively evaluated with the following techniques: high speed tensile test, bend test, and focused immersion ultrasound on a joint section removed from the pipe coupled with slicing through the joint and examining the revealed surfaces. The fusion parameters, nondestructive, and destructive evaluation results will be correlated to validate the effectiveness of what each NDE technology detects and what each does not detect. This is an initial limited study which will aid in identifying key future work.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

PRELIMINARY ASSESSMENT OF NDE METHODS ON INSPECTION OF HDPE BUTT FUSION PIPING JOINTS FOR LACK OF FUSION

Studies at the Pacific Northwest National Laboratory in Richland, Washington, are being conducted to evaluate nondestructive examination approaches for inspecting butt fusion joints in high density polyethylene (HDPE) pipe for lack of fusion (LOF). The work provides information to the United States Nuclear Regulatory Commission on the effectiveness and need for volumetric inspection techniques of HDPE butt fusion joints in Section III, Division 1, Class 3, buried piping systems in nuclear power plants. This paper describes results from preliminary assessments using ultrasonic nondestructive techniques and high-speed tensile impact testing for determining joint integrity. A series of butt joints were fabricated in 3408, 12-inch IPS DR-11 material by varying the fusion parameters in attempts to provide good joints and joints containing LOF. These butt joints were visually examined and volumetrically examined with time-of-flight diffraction (TOFD) and phased-array (PA) ultrasound. A limited subset of pipe joint material was destructively analyzed by either slicing through the joint and visually examining the surface or by employing a standard high-speed tensile impact test. Initial correlation of the fusion parameters, nondestructive, and destructive evaluations have shown that areas with gross LOF were detected with both TOFD and PA ultrasound and that the tensile impact test showed a brittle failure at the joint. There is still some ambiguity in results from the less obvious LOF conditions. Current work is targeted on assessing the sensitivity of the ultrasonic volumetric examinations and validating the results with a destructive analysis. It is expected that on-going and future work will lead to quantifying the ultrasonic responses in terms of joint integrity.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Mechanisms of degradation in adhesive joint strength: Glassy polymer thermoset bond in a humid environment

The degradation in the strength of napkin-ring (NR) joints bonded with an epoxy thermoset is evaluated in a humid environment. While adherend composition (stainless steel and aluminum) and surface preparation (polished, grit blasted, primed, coupling agent coated) do not affect virgin (time=0) joint strength, they can significantly affect the role of moisture on the strength of the joint. Adherend surface abrasion and corrosion processes are found to be key factors in determining the reliability of joint strength in humid environments. In cases where surface specific joint strength degradation processes are not active, decreases in joint strength can be accounted for by the glass transition temperature, T g , depression of the adhesive associated with water sorption. Under these conditions, joint strength can be rejuvenated to virgin strength by drying. In addition, the decrease in joint strength associated with water sorption can be predicted by the Simplified Potential Energy Clock (SPEC) model by shifting the adhesive reference temperature, T ref , by the same amount as the T g depression. When surface specific degradation mechanisms are active, they can reduce joint strength below that associated with adhesive T g depression, and joint strength is not recoverable by drying. Furthermore, a critical relative humidity (or, potentially, critical water sorption concentration), below which the surface specific degradation does not occur, appears to exist for the polished stainless steel joints.

36 MATERIALS SCIENCE↗

Mechanical end joint system for connecting structural column elements

A mechanical end joint system is presented that eliminates the possibility of free movements between the joint halves during loading or vibration. Both node joint body (NJB) and column end joint body (CEJB) have cylindrical engaging ends. Each of these ends has an integral semicircular tongue and groove. The two joint halves are engaged transversely - the tongue of the NJB mating with the groove of the CEJB and vice versa. The joint system employs a spring loaded internal latch mechanism housed in the CEJB. During mating, this mechanism is pushed away from the NJB and enters the NJB when mating is completed. In order to lock the joint and add a preload across the tongue and groove faces, an operating ring collar is rotated through 45 deg causing an internal mechanism to compress a Belleville washer preload mechanism. This causes an equal and opposite force to be exerted on the latch bolt and the latch plunger. This force presses the two joint halves tightly together. In order to prevent inadvertent disassembly, a secondary lock is also engaged when the joint is closed. Plungers are carried in the operating ring collar. When the joint is closed, the plungers fall into tracks on the CEJB, which allows the joint to be opened only when the operating ring collar and plungers are pushed directly away from the joining end. One application of this invention is the rapid assembly and disassembly of diverse skeletal framework structures which is extremely important in many projects involving the exploration of space.

Bush, Harold G.↗

Microstructure and Mechanical Properties of Reaction-Formed Joints in Reaction Bonded Silicon Carbide Ceramics

A reaction-bonded silicon carbide (RB-SiC) ceramic material (Carborundum's Cerastar RB-SIC) has been joined using a reaction forming approach. Microstructure and mechanical properties of three types of reaction-formed joints (350 micron, 50-55 micron, and 20-25 micron thick) have been evaluated. Thick (approximately 350 micron) joints consist mainly of silicon with a small amount of silicon carbide. The flexural strength of thick joints is about 44 plus or minus 2 MPa, and fracture always occurs at the joints. The microscopic examination of fracture surfaces of specimens with thick joints tested at room temperature revealed the failure mode to be typically brittle. Thin joints (<50-55 micron) consist of silicon carbide and silicon phases. The room and high temperature flexural strengths of thin (<50-55 micron) reaction-formed joints have been found to be at least equal to that of the bulk Cerastar RB-SIC materials because the flexure bars fracture away from the joint regions. In this case, the fracture origins appear to be inhomogeneities inside the parent material. This was always found to be the case for thin joints tested at temperatures up to 1350C in air. This observation suggests that the strength of Cerastar RB-SIC material containing a thin joint is not limited by the joint strength but by the strength of the bulk (parent) materials.

Singh, M.↗

Development of Thermal Barriers For Solid Rocket Motor Nozzle Joints

Joints in the Space Shuttle solid rocket motors are sealed by O-rings to contain combustion gases inside the rocket that reach pressures of up to 900 psi and temperatures of up to 5500 F. To provide protection for the O-rings, the motors are insulated with either phenolic or rubber insulation. Gaps in the joints leading up to the O-rings are filled with polysulfide joint-fill compounds as an additional level of protection. The current RSRM nozzle-to-case joint design incorporating primary, secondary, and wiper O-rings experiences gas paths through the joint-fill compound to the innermost wiper O-ring in about one out of every seven motors. Although this does not pose a safety hazard to the motor, it is an undesirable condition that NASA and rocket manufacturer Thiokol want to eliminate. Each nozzle-to-case joint gas path results in extensive reviews and evaluation before flights can be resumed. Thiokol and NASA Marshall are currently working to improve the nozzle-to-case joint design by implementing a more reliable J-leg design that has been used successfully in the field and igniter joint. They are also planning to incorporate the NASA Glenn braided carbon fiber thermal barrier into the joint. The thermal barrier would act as an additional level of protection for the O-rings and allow the elimination of the joint-fill compound from the joint.

Steinetz, Bruce M.↗

Ultrasonic Measurement and Monitoring of Loads in Bolts used in Structural Joints

The paper is an overview of work by the author in measuring and monitoring loads in bolts using an ultrasonic extensometer. A number of cases of bolted joints are covered. These include, a clamped joint with clearance fit between the bolt and hole, a clamped joint with the bolt in an interference fit with the hole, a flanged joint which allows the flange and bolt to bend; and a shear joint in a clevis and tang configuration. These applications were initially developed for measuring and monitoring preload in the NASA Space Shuttle Orbiter critical joints but are also applicable for monitoring loads in other critical bolted joints of structures such as transportation bridges and other aerospace structures. The paper explains how to set‐up a model to estimate the load factor and accuracy for the ultrasonic preload application in a clamped joint with clearance fit. The ultrasonic preload application for clamped joint with bolt in an interference fit can also be used to measure diametrical interference between the bolt shank and hole; and interference pressure on the bolt shank. Model and experimental data are given to demonstrate use of ultrasonic measurements in a shear joint. A bolt in a flanged joint experiences both tensile and bending loads. This application involves measurement of bending and tensile preload in a bolt. The ultrasonic beam bends due to the bending load on the bolt. A numerical technique to compute the trace of ultrasonic ray is presented.

Koshti, Ajay↗

CD206 + Trem2 + macrophage accumulation in the murine knee joint after injury is associated with protection against post-traumatic osteoarthritis in MRL/MpJ mice

Post-traumatic osteoarthritis (PTOA) is a painful joint disease characterized by the degradation of bone, cartilage, and other connective tissues in the joint. PTOA is initiated by trauma to joint-stabilizing tissues, such as the anterior cruciate ligament, medial meniscus, or by intra-articular fractures. In humans, ~50% of joint injuries progress to PTOA, while the rest spontaneously resolve. To better understand molecular programs contributing to PTOA development or resolution, we examined injury-induced fluctuations in immune cell populations and transcriptional shifts by single-cell RNA sequencing of synovial joints in PTOA-susceptible C57BL/6J (B6) and PTOA-resistant MRL/MpJ (MRL) mice. We identified significant differences in monocyte and macrophage subpopulations between MRL and B6 joints. A potent myeloid-driven anti-inflammatory response was observed in MRL injured joints that significantly contrasted the pro-inflammatory signaling seen in B6 joints. Multiple CD206 + macrophage populations classically described as M2 were found enriched in MRL injured joints. These CD206 + macrophages also robustly expressed Trem2 , a receptor involved in inflammation and myeloid cell activation. These data suggest that the PTOA resistant MRL mouse strain displays an enhanced capacity of clearing debris and apoptotic cells induced by inflammation after injury due to an increase in activated M2 macrophages within the synovial tissue and joint space.

60 APPLIED LIFE SCIENCES↗

Assessment of NDE Methods on Inspection of HDPE Butt Fusion Piping Joints for Lack of Fusion with Validation from Mechanical Testing

Studies at the Pacific Northwest National Laboratory (PNNL) in Richland, Washington, are being conducted to evaluate nondestructive examinations (NDE) coupled with mechanical testing of butt fusion joints in high-density polyethylene (HDPE) pipe for assessing lack of fusion. The work provides information to the U.S. Nuclear Regulatory Commission (NRC) on the effectiveness of volumetric inspection techniques of HDPE butt fusion joints in Section III, Division 1, Class 3, buried piping systems in nuclear power plants. This paper describes results from preliminary assessments using ultrasonic and microwave nondestructive techniques and mechanical testing with the high-speed tensile impact test and the side-bend test for determining joint integrity. A series of butt joints were fabricated in 3408, 12-in. IPS DR-11 HDPE material by varying the fusion parameters to create good joints and joints containing a range of lack-of-fusion conditions. Six of these butt joints were volumetrically examined with time-of-flight diffraction (TOFD), phased-array (PA) ultrasound, and the Evisive microwave system. The outer-diameter weld beads were removed for the microwave inspection. In two of the four pipes, both the outer and inner weld beads were removed and the pipe joints re-evaluated. The pipes were sectioned and the joints destructively evaluated with the side-bend test by cutting portions of the fusion joint into slices that were planed and bent. The last step in this limited study will be to correlate the fusion parameters, nondestructive, and destructive evaluation results to validate the effectiveness of what each NDE technology detects and what each does not detect. The results of the correlation will be used in identifying any future work that is needed.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗