Molten Target Sputtering: Non-Conventional Method for High Mobility Si0.15Ge0.85 Growth at 500°C

Since electrons travel over 100 times faster in Silicon-Germanium (SiGe) than in pure Si due to the low effective masses associated with Ge and SiGe-based devices continue to replace Si-based solid-state electronic devices. SiGe thin film on sapphire was successfully grown at 890°C, using a magnetron sputtering system within heteroepitaxial framework. However, SiGe growth at 890oC is a costly and difficult process to produce as a uniform wafer for semiconductor device manufacturing due to thermal soak times, and geometric thermal shadowing from the wafer holder. To leverage the semiconducting capabilities of SiGe, novel processing techniques for SiGe film growth with decreased thermal loading are required. This paper introduces the Molten Target Sputtering (MTS) method that produces high mobility SiGe on sapphire below 500°C. This non-conventional method has the advantage of high kinetic energy, high-energy latency, and high flux density of sputtered atoms by combining benefits of both magnetron sputtering and thermal evaporation. For the MTS method, a 1~2 mm (depth and width) ring-shaped groove was cut between the center magnet and surrounded by electromagnets creating a circular cavity between the copper plate and source target materials that melt the target material. The SiGe grown from the MTS shows continuous morphology and 99.7% single crystal Si0.15Ge0.85 films. The Hall electron mobilities of the Si0.15Ge0.85 are 456 sq. cmV(exp -1)s(exp -1) and 123.9 sq. cmV(exp -1)s(exp -1) at 5.59 x 10(exp 18) cubic cm and 3.5 x 10(exp 20) cubic cm carrier concentration at 22.38°C, respectively. This is approximately 5.5 times higher than that of Si and similar to the Ge value at equivalent carrier concentrations and temperatures.

High mobility SiGe↗

Radiofrequency-sputtered coatings for lubrication system components and other complex surfaces

Irregularly shaped surfaces, such as lubrication system components (ball bearings, seals, gears, etc.), can be coated on all surfaces, including irregular shapes, when radiofrequency sputtering is used. When the specimen is properly located with respect to the sputtering target, the sputtered material covers the entire surface of the object irrespective of its geometrical configuration. An adherent, dense film is formed. The film thickness varies from 20 to 50 percent on, for example, a hearing cage or race depending on its geometry. When sputtered solid film lubricants such as molybdenum disulfide are used, a film thickness only of the order of 10 to the minus 7th power m (thousands of angstroms) is required at the contacting areas. It is only essential to determine the required film thickness at the critical areas in need of lubrication. The sections outside the areas to be lubricated fall within the thickness deviation range of 20 to 50 percent, which still constitutes a negligible change respect to tolerance requirements.

Spalvins, T.↗

Sputtering and ion plating

The proceedings of a conference on sputtering and ion plating are presented. Subjects discussed are: (1) concepts and applications of ion plating, (2) sputtering for deposition of solid film lubricants, (3) commercial ion plating equipment, (4) industrial potential for ion plating and sputtering, and (5) fundamentals of RF and DC sputtering.

Source record↗

Change in transmittance of fused silica as a means of detecting material sputtered from components on a 5-cm ion thruster

Two endurance tests of a 5-cm mercury bombardment thruster are reported. Both tests used a translational screen-grid system with the beam vectored 10 degrees. The first test lasted 141 hours and the second test operated for 2026 hours. In each test two fused silica samples (solar cell covers), 2.0 cm by 2.1 cm, were placed in shielded holders to detect materials sputtered from the thruster. Spectral optical properties between 0.398 and 2.16 microns were measured on each sample, both before and after the endurance tests. The deposition on each sample was spectrographically analyzed to determine the type of materials sputtered from the thruster. It was found that sputtering from the neutralizer is highly dependent on its position with respect to the beam edge. The sputtering from the accelerator grid of the translational screen-grid system of the 2026 hour test was sufficient to form an opaque film on the sample located in the direction opposite to the vectored beam.

Weigand, A. J.↗

Structure of molybdenum disulfide films sputtered on substrates at various temperatures

Molybdenum disulfide films 300 to 400 A thick were rf sputtered on aluminum and nickel surfaces at elevated, ambient, and liquid nitrogen temperatures. Electron transmission micrographs and electron diffraction patterns were taken to determine the structural growth. These transmission micrographs revealed that sputtered MoS2 films at ambient and elevated temperatures (320 and 150 C) formed an irregular network of ridges. The electron diffraction patterns of these films showed relatively sharp diffraction rings, indicating crystallinity. The transmission micrographs of sputtered films at liquid nitrogen temperatures revealed a continuous featureless film. The electron diffraction patterns showed broad, diffused rings indicating an amorphous film. The transmission micrographs of a post-annealed (425 C) MoS2 film sputtered at liquid-nitrogen temperature revealed the tendency for ridge formation. Electron diffraction patterns also showed increased sharpness of the diffraction rings. Friction tests showed that MoS2 films deposited at ambient and elevated temperatures exhibited good lubricating properties. The MoS2 films deposited at cryogenic temperatures had no lubricating characteristics.

Spalvins, T.↗

On the sputtering of binary compounds

A simple physical model is presented to describe some aspects of the sputtering of compound targets. In particular, expressions are developed for the partial sputtering yields for binary systems in terms of the elemental sputtering rates, the stoichiometric concentrations and surface binding energy. The partial yields depend non-linearly on the bulk target concentrations. Comparison of the theoretical predictions with the data on sputtering of PtSi, NiSi and Cu3Au indicates that the general features are well described.

Haff, P. K.↗

Microstructural and wear properties of sputtered carbides and silicides

Sputtered Cr3C2, Cr3Si2, and MoSi2 wear-resistant films (0.05 to 3.5 microns thick) were deposited on metal and glass surfaces. Electron transmission, electron diffraction, and scanning electron microscopy were used to determine the microstructural appearance. Strong adherence was obtained with these sputtered films. Internal stresses and defect crystallographic growth structures of various configurations within the film have progressively more undesirable effects for film thicknesses greater than 1.5 microns. Sliding contact and rolling element bearing tests were performed with these sputtered films. Bearings sputtered with a duplex coating (0.1-micron-thick undercoating of Cr3Si2 and subsequently 0.6-micron coating of MoS2) produced marked improvement over straight MoS2 films.

Spalvins, T.↗

X-Ray photoelectron spectroscopy study of radiofrequency-sputtered titanium, carbide, molybdenum carbide, and titanium boride coatings and their friction properties

Radiofrequency sputtered coatings of titanium carbide, molybdenum carbide and titanium boride were tested as wear resistant coatings on stainless steel in a pin on disk apparatus. X-ray photoelectron spectroscopy (XPS) was used to analyze the sputtered films with regard to both bulk and interface composition in order to obtain maximum film performance. Significant improvements in friction behavior were obtained when properly biased films were deposited on deliberately preoxidized substrates. XPS depth profile data showed thick graded interfaces for bias deposited films even when adherence was poor. The addition of 10 percent hydrogen to the sputtering gas produced coatings with thin poorly adherent interfaces. Results suggest that some of the common practices in the field of sputtering may be detrimental to achieving maximum adherence and optimum composition for these refractory compounds.

Brainard, W. A.↗

On the sputtering of binary compounds

A simple physical model is presented to describe some aspects of the sputtering of compound targets. In particular, expressions are developed for the partial sputtering yields for binary systems in terms of the elemental sputtering rates, the stoichiometric concentrations, and surface binding energy. The partial yields depend nonlinearly on the bulk target concentrations. Comparison of the theoretical predictions with the data on sputtering of PtSi, NiSi, and Cu3Au indicates that the general features are well described.

Haff, P. K.↗

Ion beam sputter etching and deposition of fluoropolymers

Fluoropolymer etching and deposition techniques including thermal evaporation, RF sputtering, plasma polymerization, and ion beam sputtering are reviewed. Etching and deposition mechanism and material characteristics are discussed. Ion beam sputter etch rates for polytetrafluoroethylene (PTFE) were determined as a function of ion energy, current density and ion beam power density. Peel strengths were measured for epoxy bonds to various ion beam sputtered fluoropolymers. Coefficients of static and dynamic friction were measured for fluoropolymers deposited from ion bombarded PTFE.

Banks, B. A.↗

Ion beam sputter etching and deposition of fluoropolymers

Fluoropolymer etching and deposition techniques including thermal evaporation, RF sputtering, plasma polymerization, and ion beam sputtering are reviewed. Etching and deposition mechanisms and material characteristics are discussed. Ion beam sputter etch rates for polytetrafluoroethylene (PTFE) were determined as a function of ion energy, current density and ion beam power density. Peel strengths were measured for epoxy bonds to various ion beam sputtered fluoropolymers. Coefficients of static and dynamic friction were measured for fluoropolymers deposited from ion bombarded PTFE.

Banks, B. A.↗

Adherence of sputtered titanium carbides

Sputtered coatings of the refractory metal carbides are of great interest for applications where hard wear-resistant materials are desired. The usefulness of sputtered refractory carbides is often limited, in practice, by spalling or interfacial separation. In this work improvements in the adherence of refractory carbides on iron, nickel and titanium based alloys were obtained by using oxidation, reactive sputtering or sputtered interlayers to alter the coating-substrate interfacial region. X-ray photoelectron spectroscopy and argon ion etching were used to characterize the interfacial regions, and an attempt was made to correlate adherence as measured in wear tests with the chemical nature of the interface.

Brainard, W. A.↗

Tribological properties of sputtered MoS sub 2 films in relation to film morphology

Thin sputter deposited MoS2 films in the 2000 to 6000 A thickness range have shown excellent lubricating properties, when sputtering parameters and substrate conditions are properly selected and precisely controlled. The lubricating properties of sputtered MoS2 films are strongly influenced by their crystalline-amorphous structure, morphology and composition. The coefficient of friction can range from 0.04 which is effective lubrication to 0.4 which reflects an absence of lubricating properties. Visual screening and slight wiping of the as-sputtered MoS2 film can identify the integrity of the film. An acceptable film displays a black-sooty surface appearance whereas an unacceptable film has a highly reflective, gray surface and the film is hard and brittle.

Spalvins, T.↗

A thermalized ion explosion model for high energy sputtering and track registration

A velocity spectrum of neutral sputtered particles as well as a low resolution mass spectrum of sputtered molecular ions was measured for 4.74 MeV F-19(+2) incident of UF4. The velocity spectrum is dramatically different from spectra taken with low energy (keV) bombarding ions, and is shown to be consistent with a hot plasma of atoms in thermal equilibrium inside the target. A thermalized ion explosion model is proposed for high energy sputtering which is expected to describe track formation in dielectric materials. The model is shown to be consistent with the observed total sputtering yield and the dependence of the yield on the primary ionization rate of the incident ion.

Seiberling, L. E.↗

Improved adhesion of sputtered refractory carbides to metal substrates

Sputtered coatings of the refractory metal carbides are of great interest for applications where hard wear-resistant materials are desired. The usefulness of sputtered refractory carbides is often limited in practice by spalling or interfacial separation. In this work improvements in the adherence of refractory carbides on iron, nickel and titanium base alloys were obtained by using oxidation, reactive sputtering or sputtered interlayers to alter the coating-substrate interfacial region. X-ray photoelectron spectroscopy and argon ion etching were used to characterize the interfacial regions, and an attempt was made to correlate adherence as measured in wear tests with the chemical nature of the interface.

Wheeler, D. R.↗

Development of RF sputtered chromium oxide coating for wear application

The radio frequency sputtering technique was used to deposite a hard refractory, chromium oxide coating on an Inconel X-750 foil 0.1 mm thick. Optimized sputtering parameters for a smooth and adherent coating were found to be as follows: target-to-substrate spacing, 41.3 mm; argon pressure, 5-10 mTorr; total power to the sputtering module, 400 W (voltage at the target, 1600 V), and a water-cooled substrate. The coating on the annealed foil was more adherent than that on the heat-treated foil. Substrate biasing during the sputter deposition of Cr2O3 adversely affected adherence by removing naturally occurring interfacial oxide layers. The deposited coatings were amorphous and oxygen deficient. Since amorphous materials are extremely hard, the structure was considered to be desirable.

Bhushan, B.↗

Deposition of reactively ion beam sputtered silicon nitride coatings

An ion beam source was used to deposit silicon nitride films by reactively sputtering a silicon target with beams of Ar + N2 mixtures. The nitrogen fraction in the sputtering gas was 0.05 to 0.80 at a total pressure of 6 to 2 millionth torr. The ion beam current was 50 mA at 500 V. The composition of the deposited films was investigated by auger electron spectroscopy and the rate of deposition was determined by interferometry. A relatively low rate of deposition of about 2 nm. one-tenth min. was found. AES spectra of films obtained with nitrogen fractions higher than 0.50 were consistent with a silicon to nitrogen ratio corresponding to Si3N4. However the AES spectra also indicated that the sputtered silicon nitride films were contaminated with oxygen and carbon and contained significant amounts of iron, nickel, and chromium, most probably sputtered from the holder of the substrate and target.

Grill, A.↗

Possible isotopic fractionation effects in material sputtered from minerals

A model is presented which predicts isotope fractionation in material sputtered from mineral surfaces. According to the model, the fractionation is a function of the fractional abundances of each isotope, the low-energy collision cross sections and the atomic masses, and the fractionation pattern can be nonlinear. Calculations are illustrated for all sets of isotopes in the minerals perovskite, anorthite, akermanite, enstatite and troilite, and it is found that while O is always positively fractionated, with heavier isotopes sputtered preferentially, heavier elements are generally negatively fractionated. It is noted that the model may be tested by experiments on a system such as CaF2, CaI2, in which the Ca sputtered from CaF2 is predicted to be strongly fractionated in a negative sense and that sputtered from CaI2 is predicted to be strongly fractionated in a positive sense.