Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “irradiation tolerance”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 91 records · Page 5

Reliability Characterization of TaOx-Based Commercial ReRAM in Combination with Radiation

We present reliability data combined with total dose gamma radiation for one of the first commercially available resistive memory devices. These Tantalum Oxide (TaOX)-based resistive memory chips demonstrate operation in dynamic program and erase testing up to ~130 Krad(Si) of 60Co gamma dose. In static and unbiased conditions, the stored data in the memory cells were able to withstand up to 50Mrad(Si) of exposure. The access circuitry, though, seemed less robust to gamma radiation and was able to operate only up to a total dose of 3Mrad(Si). Post exposure reliability as indicated by endurance, cycling error rate, and data retention tests showed no detectable impact from the combination with prior gamma irradiation. Overall, the total dose radiation tolerance of the commercial TaOx-based resistive memory chip appears to be higher than flash memory chips and in agreement with prior tests conducted with single cell resistive memories.

total ionizing dose↗

Screening and qualification methodology for SiC end plug processing methods

Deployment of SiC-ceramic-based fuel cladding for light water reactors requires a hermetic end plug–to–cladding joint that can withstand neutron irradiation during normal operation and maintain integrity during design-basis accidents. Reactor experiments have shown that some SiC composite tubes with SiC end plugs can retain hermeticity after irradiation. However, achieving consistent joint performance under irradiation remains a key challenge. Resolving this issue is essential to enable integral irradiation testing and to demonstrate fuel integrity under commercial-reactor irradiation conditions. This report aims to: (1) provide guidance for designing radiation-tolerant end plug joints for SiC cladding; (2) demonstrate experimental methods to detect processing defects that are unstable under neutron irradiation at light-water-reactor-relevant temperatures and doses; and (3) outline a step-by-step approach for designing and conducting reactor experiments to screen joining methods. The resulting data will be used to improve joint processing and to define critical defect types and sizes that must be detected and eliminated through non-destructive evaluation for quality assurance. Based on prior irradiation experiments at the High Flux Isotope Reactor, differential swelling among the cladding, bonding layer, and end plug was identified as an underlying mechanism for irradiation-induced joint degradation. Accordingly, this effect must be considered in the design of radiation-tolerant joining techniques. In this work, miniature SiC end plug joint specimens irradiated during the previous project were analyzed using X-ray computed tomography to characterize the joint microstructure. Digital volume correlation of the tomography data quantified radiation-induced microstructural changes and enabled evaluation of defect-related risks. Finally, ongoing neutron irradiation efforts using larger specimen volumes are presented. These efforts aim to statistically assess joint performance and to build a microstructure–performance (e.g., leak-tightness) dataset to inform processing improvements and quality control.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

In situ study on heavy ion irradiation induced microstructure evolution in single crystal Cu with nanovoids at elevated temperature

Understanding the response of nanovoids to irradiation damage advances our capability to design radiation tolerant materials. Recent in situ studies reveal the shrinkage of hexagon-shaped nanovoids in (110) textured Cu. However, the evolution of voids with irregular geometries under irradiation is less well understood. Here, in situ Kr ion irradiation was performed at 100 °C on single-crystal Cu (112) that possesses nanovoids with high aspect ratio. In situ studies show these elongated voids fragment into smaller voids and shrink gradually with increasing dose. Phase field simulations confirm that fragmentation of the void is governed by the competing kinetics between atoms diffusing toward and away from the elongated nanovoid. In conclusion, cost irradiation analysis reveals the formation of high-density defect clusters.

38 RADIATION CHEMISTRY, RADIOCHEMISTRY, AND NUCLEA↗

Fracture Toughness Characterization of Generation II FeCrAl Alloys after ~18 dpa Irradiation

FeCrAl alloys are promising candidate materials for the accident tolerant fuel (ATF) cladding applications due to their excellent corrosion resistance to the elevated temperature steam environment. Currently, the handbook on FeCrAl material properties contains only limited data regarding the fracture toughness properties of any FeCrAl alloy. This includes alloys currently under investigation within the Advanced Fuels Campaign (AFC) at Oak Ridge National Laboratory (ORNL). In this project, a series of irradiation capsules have been irradiated in the High Flux Isotope Reactor (HFIR) at ORNL with two Generation II FeCrAl candidate alloys, i.e., C06M and C36M, to assess the fracture response of these alloys after neutron irradiation. These alloys represent the “book-end” compositions for C26M, the alloy currently being developed as the leading candidate for LWR cladding. A total of six irradiation capsules were irradiated in HFIR at target temperatures of 200°C, 330°C, and 500°C up to target damage doses of 8 displacements per atom (dpa) and 16 dpa. These damage doses represent the expected middle and end of life damage levels for typical LWR cladding while the irradiation temperature regimes will provide insight into the role of varying microstructural features on the fracture toughness properties of neutron irradiated FeCrAl alloys. To date, irradiation of all capsules has been completed in HFIR. This report summarizes the latest results of microhardness and fracture toughness PIE for the 16 dpa capsules (FCAB2, FCAB4, and FCAB6), for which the measured irradiation conditions were: 204°C/17.6dpa, 343°C/18.3dpa, and 507°C/18.6dpa. The main conclusions of this study can be summarized as follows: 1) After the 204°C/17.6dpa irradiation, both C06M and C36M exhibited significant irradiation hardening and embrittlement 2) After the 343°C/18.3dpa irradiation, both C06M and C36M exhibited small irradiation hardening without irradiation embrittlement 3) After the 507°C/18.6dpa irradiation, both C06M and C36M exhibited irradiation softening without irradiation embrittlement 4) Comparing the microhardness and Master Curve reference temperature T 0q before and after neutron irradiation, we did not observe a linear correlation between the two parameters for both C06M and C36M. This should be mainly due to a flat response of the Master Curve reference temperature T 0q to the irradiations at 166-204°C and 315-343°C ranges 5) C06M showed a lower T 0q , meaning better toughness, than C36M at the unirradiated condition and such trend was kept even after neutron irradiation except for the 166-204°C irradiation where both materials had similar T 0q . 6) In terms of hardening and embrittlement, the irradiation effect on both C06M and C36M appeared to saturate after an irradiation dose of 7 dpa.

36 MATERIALS SCIENCE↗

Processing of silicon solar cells by ion implantation and laser annealing

Methods to improve the radiation tolerance of silicon cells for spacecraft use are described. The major emphasis of the program was to reduce the process-induced carbon and oxygen impurities in the junction and base regions of the solar cell, and to measure the effect of reduced impurity levels on the radiation tolerance of cells. Substrates of 0.1, 1.0 and 10.0 ohm-cm float-zone material were used as starting material in the process sequence. High-dose, low-energy ion implantation was used to form the junction in n+p structures. Implant annealing was performed by conventional furnace techniques and by pulsed laser and pulsed electron beam annealing. Cells were tested for radiation tolerance at Spire and NASA-LeRC. After irradiation by 1 MeV electrons to a fluence of 10 to the 16th power per sq cm, the cells tested at Spire showed no significant process induced variations in radiation tolerance. However, for cells tested at Lewis to a fluence of 10 to the 15th power per sq cm, ion-implanted cells annealed in vacuum by pulsed electron beam consistently showed the best radiation tolerance for all cell resistivities.

Minnucci, J. A.↗

Radiation effects in Mn+1AXn phases

M n+1 AX n phases exhibit unique laminated atomic structures that result in properties typical of both ceramics and metals. Due to their unusual characteristics, these materials have been proposed for use in a wide variety of industrial applications, including in nuclear reactors—both fission and fusion systems—where they will be exposed to extreme irradiation conditions and high temperatures. Recently, numerous studies have investigated radiation effects on the M n+1 AX n phases, revealing complex behavior—phase transformations, surface modification, and mechanical property changes—induced by ion or neutron irradiation over a range of temperatures. This review summarizes recent experimental and theoretical work on the response of the M n+1 AX n phases to irradiation and discusses the intrinsic controls on the radiation tolerance of these materials. Based on the review of the present body of work, a comprehensive understanding of the mechanisms of irradiation-induced structural modification and defect evolution in M n+1 AX n phases is developed, as well as proposed strategies for designing novel M n+1 AX n phases with enhanced performance under extreme irradiation conditions.

73 NUCLEAR PHYSICS AND RADIATION PHYSICS↗

Electromagnetic Radiation Effects on MgO-Based Magnetic Tunnel Junctions: A Review

Magnetic tunnel junctions (MTJs) have been widely utilized in sensitive sensors, magnetic memory, and logic gates due to their tunneling magnetoresistance. Moreover, these MTJ devices have promising potential for renewable energy generation and storage. Compared with Si-based devices, MTJs are more tolerant to electromagnetic radiation. In this review, we summarize the functionalities of MgO-based MTJ devices under different electromagnetic irradiation environments, with a focus on gamma-ray radiation. We explore the effects of these radiation exposures on the MgO tunnel barriers, magnetic layers, and interfaces to understand the origin of their tolerance. This review enhances our knowledge of the radiation tolerance of MgO-based MTJs, improves the design of these MgO-based MTJ devices with better tolerances, and provides information to minimize the risks of irradiation under various irradiation environments. This review starts with an introduction to MTJs and irradiation backgrounds, followed by the fundamental properties of MTJ materials, such as the MgO barrier and magnetic layers. Then, we review and discuss the MTJ materials and devices’ radiation tolerances under different irradiation environments, including high-energy cosmic radiation, gamma-ray radiation, and lower-energy electromagnetic radiation (X-ray, UV–vis, infrared, microwave, and radiofrequency electromagnetic radiation). In conclusion, we summarize the radiation effects based on the published literature, which might benefit material design and protection.

42 ENGINEERING↗

Irradiation-induced swelling of pure chromium with 5 MeV Fe ions in the temperature range 450–650 °C

A surface coating using pure chromium has been proposed to increase the accident tolerance of Zircaloy cladding in pressurized water reactors. However, there is not much irradiation experience with Cr alloys and especially pure Cr. In the present study, pure chromium was irradiated with 5 MeV Fe ions to 50 peak dpa (displacements per atom) at temperatures of 450, 500, 550, 600 and 650 °C. Then irradiation at the peak swelling temperature of 550 °C was conducted to 50, 100, 150 peak dpa. Swelling at 50 dpa was observed over the entire temperature range studied, 450–650 °C, but appeared to be decreasing strongly at the temperature boundaries of the experiment. After an initial transient of rapid swelling, chromium was observed to swell at a rate of ~0.03–0.04%/dpa (up to 120 local dpa), which is much lower than pure Fe at 0.2%/dpa. This low swelling rate was found to be relatively insensitive to dpa rate, which varied by a factor of ~2 over the depth of data collection. Here, swelling was observed to begin quickly with an incubation period less than 10 dpa. Self-organization in the form of void ordering was observed to be developing at 50 dpa, becoming better defined with increasing dose. The void alignment direction is determined to be the $\langle$111$\rangle$ axial direction.

36 MATERIALS SCIENCE↗

Growth and tuberization of potato (Solanum tuberosum L.) under continuous light

The growth and tuberization of potatoes (Solanum tuberosum L.) maintained for 6 weeks under four different regimes of continuous irradiance were compared to plants given 12 hours light and 12 hours dark. Treatments included: (a) continuous photosynthetic photon flux of 200 micromoles per square meter per second cool-white fluorescent (CWF); (b) continuous 400 micromoles per square meter per second CWF; (c) 12 hours 400 micromoles per square meter per second CWF plus 12 hours dim CWF at 5 micromoles per square meter per second; (d) 12 hours [400] micromoles per square meter per second CWF plus 12 hours dim incandescent (INC) at 5 micromoles per square meter per second and a control treatment of 12 hours light at 400 micromoles per square meter per second CWF and 12 hours dark. The study included five cultivars ranging from early- to late-season types: 'Norland,' 'Superior,''Norchip,' 'Russet Burbank,' and 'Kennebec,' Tuber development progressed well under continuous irradiation at 400 micromoles per square meter per second and under 12 hours irradiance and 12 hours dark, while tuber development was suppressed in all other light treatments. Continuous irradiation at 200 or 400 micromoles per square meter per second resulted in severe stunting and leaf malformation on 'Superior' and 'Kennebec' plants, but little or no injury and vigorous shoot growth in the other cultivars. No injury or stunting were apparent under 12-dim light or 12-dark treatments. Plants given 12 hours dim INC showed significantly greater stem elongation but less total biomass than plants in other treatments. The continuous light encouraged shoot growth over tuber growth but this trend was overridden by providing a high irradiance level. The variation among cultivars for tolerance to continuous lighting indicates that potato may be a useful species for photoinhibition studies.

NASA Program CELSS↗

In-Situ Helium Implantation and TEM Investigation of Radiation Tolerance to Helium Bubble Damage in Equiaxed Nanocrystalline Tungsten and Ultrafine Tungsten-TiC Alloy

The use of ultrafine and nanocrystalline materials is a proposed pathway to mitigate irradiation damage in nuclear fusion components. Here, we examine the radiation tolerance of helium bubble formation in 85 nm (average grain size) nanocrystalline-equiaxed-grained tungsten and an ultrafine tungsten-TiC alloy under extreme low energy helium implantation at 1223 K via in-situ transmission electron microscope (TEM). Helium bubble damage evolution in terms of number density, size, and total volume contribution to grain matrices has been determined as a function of He+ implantation fluence. The outputs were compared to previously published results on severe plastically deformed (SPD) tungsten implanted under the same conditions. Large helium bubbles were formed on the grain boundaries and helium bubble damage evolution profiles are shown to differ among the different materials with less overall damage in the nanocrystalline tungsten. Compared to previous works, the results in this work indicate that the nanocrystalline tungsten should possess a fuzz formation threshold more than one order of magnitude higher than coarse-grained tungsten.

36 MATERIALS SCIENCE↗

Kinetic interplay between chemical short-range order and grain boundaries in NiCoCr alloys under irradiation

Chemical short-range order (CSRO) and grain boundary (GB) engineering are routes to enhance radiation damage tolerance in alloys. Here, we reveal that CSRO and GB interact in a sink-strength-dependent manner under irradiation in NiCoCr. Near a weak sink (Σ3 GB), CSRO reduces defect cluster growth by slowing interstitial diffusion and enhancing vacancy-interstitial recombinations. In contrast, near strong sinks such as Σ5 GBs, CSRO and GB act competitively for interstitial accumulation but synergistically to suppress large stacking-fault tetrahedra growth via enhanced recombination. Such mechanistic duality underscores the need for coordinated control of CSRO stability and GB sink strength to enhance radiation damage tolerance.

36 MATERIALS SCIENCE↗

Installation and Demonstration of CNC Machining for Mechanical Test Specimens in the IFEL Hot Cell

This report documents the installation and demonstration of computer numerical control (CNC) machining capabilities in the Irradiated Fuels Examination Laboratory hot cell facility at Oak Ridge National Laboratory (ORNL). A modified Tormach PCNC 440 mill was integrated into the hot cell with custom fixturing, fines management, and manipulator-compatible interfaces to enable the fabrication of axial tension test (ATT) and ring tension test (RTT) specimens from irradiated cladding. The first irradiated specimens machined included ATT and RTT geometries harvested from the high-burnup 6XV fuel rod. Dimensional inspections confirmed that machined specimens met the ±0.025 mm tolerance envelope established in prior development; deviations were consistent with expected measurement scatter and inherent specimen variability, such as wall thickness gradients and eccentricity. Comparisons with out-of-cell metrology confirmed that in-cell machining performance aligns with baseline scatter observed under ideal conditions. This work establishes reproducible, end-to-end specimen preparation at ORNL, directly supporting the US Department of Energy’s Accident-Tolerant Fuel program by enabling reliable, traceable mechanical testing of irradiated cladding.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Irradiation creep measurement and microstructural analysis of chromium nitride–coated zirconium alloy using pressurized tubes

Environmental barrier coatings for Zr-based materials are currently under development to reduce oxidation and embrittlement in light-water reactors. Chromium nitride is one such candidate for this application, particularly as accident-tolerant fuel cladding. However, quantifying the impact of coatings on the irradiation-induced creep of zircaloy (Zry) is critical as this mechanism often exceeds thermal creep rates under light-water reactor operating conditions and can be a limiting design characteristic. Additionally, examining irradiation effects in the microstructure at the coating interface is key to understanding the compatibility of the material system. Here, to accelerate the experimental measurement of irradiation creep and microstructure evolution in CrN-Zry, compact, pressurized creep tubes were fabricated and irradiated in the High Flux Isotope Reactor (HFIR) at Oak Ridge National Laboratory. Miniature, thin-walled rodlets fabricated from annealed Zr-Sn barstock were coated with CrN using physical vapor deposition (PVD) to nominal thicknesses of 4 and 8 μm. Coated and uncoated rodlet specimens were internally pressurized and welded, generating nominal circumferential hoop stresses of 0, 90, or 180 MPa under 300°C irradiation conditions. Twelve specimens were measured diametrically prior to irradiation using a low-cost, automated, contactless laser profilometer developed for this work. Specimens were irradiated in sealed capsules for one 25-day HFIR cycle, accumulating approximately 1.8 $\times$ 10 21 n/cm 2 fast fluence (E n > 10 MeV). The irradiated samples were retrieved and remeasured using the same profilometry system in a shielded hot cell facility. Irradiation creep between specimens was compared using standard statistical tests and showed that both thicknesses of CrN coating had a negligible effect on the irradiation creep strain of the Zry material. Microstructure characterization of pre- and post-irradiated CrN-Zry specimens showed minimal changes due to irradiation but did show a substantial O-rich region at the Zry-CrN interface.

36 MATERIALS SCIENCE↗

FeCrAl fuel/clad chemical interaction in light water reactor environments

This article investigates the fuel-cladding chemical interaction (FCCI) behavior of two commercial FeCrAl alloys, APMT composition (Fe-21Cr-5Al-3Mo wt.%) and C35M (Fe-13Cr-5Al-2Mo-0.2Si-0.03Y wt.%), after neutron irradiation. “H-cup” diffusion multiples of FeCrAl alloys and ceramic UO 2 fuel were irradiated at a temperature of ~300 °C to a total estimated burnup of 26 GWd/tHM. Post-irradiation Examination results demonstrate the excellent degradation resistance of FeCrAl alloys as accident tolerant fuel (ATF) cladding materials in light water reactor conditions. The study concludes that there was no irradiation-induced defects observed in either of the two commercial FeCrAl claddings. The formation of amorphous Al/U mixed oxide was observed at the fuel-clad interface, which can serve as a tritium permeation barrier and protect against potential chemical attack from the fuel. Finally, the study attributed the formation of amorphous Al/U mixed oxide to the low temperature and limited time of neutron irradiation. APMT forms more distinct Cr and Cr-Fe intermetallic at the FeCrAl-UO 2 interface than C35M due to the higher bulk Cr:Al ratio.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Properties and microstructure evolution of silicon nitride and zirconium nitride following Ni ion irradiation

We report that silicon nitride and zirconium nitride have been proposed as potential materials for multiple nuclear applications (inert matrix fuels, accident tolerant fuels, space nuclear power, fusion reactor design), yet knowledge on their behavior under irradiation remains limited. Ion irradiations were performed using 15 MeV Ni 5+ ions on Si 3 N 4 and ZrN samples, with midrange doses (around 3 µm) from 1 to 50 dpa and temperatures from 300 to 700°C. Volumetric lattice swelling was determined by grazing incidence X-ray diffraction, defect production and evolution were tracked using Transmission Electron Microscopy, and nanoindentation was performed to quantify the ceramics’ mechanical properties evolution. The results from these irradiation studies on nitride ceramics help fill the current gap present in the literature. Behavior consistent with past work on irradiated Si 3 N 4 was observed with respect to mechanical properties and defect formation up to 15 dpa and 500°C. Failure of the grain boundary sintering aid in Si 3 N 4 was observed above these conditions. Different behavior was observed in both nitrides at 50 dpa and 700°C, where lattice swelling increased past potential saturation values. Unreported cavity formation was witnessed in both materials under all irradiation conditions, with stable number density and slight size increase above 15 dpa. The mechanism for the cavity formation remains to be determined.

36 MATERIALS SCIENCE↗

ATF-2 Sensitivity M&C 2023 (Slides)

Irradiation experiments in the Idaho National Laboratory's Advanced Test Reactor are typically assumed to have little effect on one another. This assumption does not hold true for certain experiments in close proximity. To evaluate the impacts on safety and programmatic parameters of experiments in the center flux trap, the contents of the adjacent H and inner-A positions are modeled with a range of possible irradiation targets. First, neutron flux maps with experiments in those positions are compared to those of a water-filled configuration. Then, several safety and programmatic parameters for a generic accident-tolerant fuel test train are calculated. It is shown that these parameters can exhibit considerable sensitivity to the contents of the H and A experiment positions.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Establishing defect-property relationships for 2D-nanomaterials (Final technical report)

Studies of new families of two-dimensional nanomaterials (2DNMs) have established that they possess unique properties that diverge from those of their bulk counterparts. This project aimed to determine how tolerant 2DNMs are to extreme photon and particle fluxes and to identify the mechanisms governing their radiation response. Early work indicated that graphene is not as representative of other 2DNMs as previously assumed; however, the origin of this difference remained unclear. To address these knowledge gaps, this project investigated the physical processes occurring at multiple length scales in transition metal dichalcogenides (TMDs) and quantified their structural stability and property evolution under far-from-equilibrium conditions. In-situ and ex-situ ion and electron irradiations were performed to directly control and monitor defect formation in TMDs. Complementary density functional theory (DFT) and molecular dynamics (MD) simulations were employed to elucidate the mechanisms of defect generation and evolution. The outcomes of this work established mechanistic understanding of irradiation-induced defect formation in 2DNMs, quantified the radiation tolerance of TMDs, and built a fundamental knowledge base for correlating defect structures with material properties. Collectively, these results provide new insights into the stability of low-dimensional materials in extreme environments and enable the predictive design of radiation-tolerant 2DNMs.

2D materials↗