A unified large language model–based framework for heterogeneous PV image diagnosis

With advances in imaging technologies, modern photovoltaic (PV) systems generate large volumes of heterogeneous image data, including visible, electroluminescence (EL), and infrared (IR) images. Existing PV image analysis models, particularly deep learning approaches, are typically task-specific and lack cross-modality generalization. To address this limitation, this paper proposes an open-source large language model (LLM)–based unified framework for heterogeneous PV image diagnostics. Through task-aware diagnostic prompting, the framework enables analysis of visible, EL, and IR images within a single pipeline, supporting both zero-shot and few-shot inference and binary and multiclass classification. It is compatible with state-of-the-art multimodal LLMs, including ChatGPT, Gemini, Claude, Qwen, and CLIP. The framework is evaluated on PV module condition classification (clean, soiling, snow, hail, and bird droppings) using visible images, cell crack detection using EL images, and hotspot detection using IR images. GPT-5.1 in few-shot mode achieves the best performance, with classification accuracy exceeding 97.3%. Open-source models such as Qwen and CLIP also deliver competitive results on visible images (around 90% accuracy), though their performance is more limited on EL and IR modalities. On the full ELPV dataset, the framework achieves 83.5% zero-shot accuracy, within 2.8% of the supervised CNN baseline, confirming scalability to larger benchmarks. Practical aspects such as reproducibility, response latency, and confidence estimation are systematically analyzed. The framework operates across PV image modalities without modality- or task-specific training, making it well suited as a rapid pre-screening tool to support downstream detailed diagnostics. A benchmark dataset of diverse labeled PV images is also released.

Li, Baojie↗

Control of Excitonic Energy Transfer in RGB Quantum Dot:Polymer Composites for Tunable White Emission

Tint-controlled white light is crucial for both illumination systems and display applications. Here, in this study, we demonstrate solution-processed quantum-dot light-emitting diodes (QD-LEDs) featuring a red–green–blue (RGB) QD–poly(methyl methacrylate) (PMMA) composite emissive layer (EML) for tunable white electroluminescence (EL). In this composite EML, PMMA functions as a dispersion matrix that modulates the interdot spacing (d), thereby controlling Förster resonance energy transfer (FRET) between QDs. By adjustment of the PMMA content, the balance of R, G, and B emissions is controlled, enabling systematic and continuous tuning of the EL color from greenish to reddish white at a fixed RGB ratio and constant driving bias. Time-resolved photoluminescence measurements confirm that the variation in the exciton lifetime with the PMMA fraction is the primary factor for tuning the EL color. Notably, nearly pure white EL with CIE coordinates close to (0.33, 0.33) is achieved using a diluted PMMA matrix without significant degradation of the electrical properties. Our results demonstrate d as an independent design parameter for decoupling color tuning from RGB composition and electrical operation, providing a versatile design framework for high-quality white- or tint-controlled QD-LEDs toward advanced solid-state lighting and display technologies.

36 MATERIALS SCIENCE↗

Light-Matter Interaction in Ultrastable Tunneling Nanogaps

Light emission and detection through tunnel junctions have emerged as a promising platform for studying nanoscale light–matter interactions, including electroluminescence and photoassisted transport. However, controlling these interactions in the tunneling regime has been challenging due to complex underlying mechanisms that remain poorly understood. A major obstacle is the difficulty in forming stable junctions that can function reliably over extended periods. In this study, we fabricate ultrastable tunneling junctions consisting of epitaxial indium–tin-oxide, epitaxial lutetium oxide, and gold. With their stable and consistent tunneling currents, we investigate photon-assisted transport phenomena using simple direct-current detection. Our results demonstrate that optical rectification is the primary contributor to the laser-induced current, alongside thermal effects and hot-electron currents. Furthermore, owing to their epitaxial nature and high breakdown threshold, this ultrastable platform holds promise for future real-world applications, including nanoscale light sources and multifunctional photodetectors.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Emissive Colloidal GaAs Quantum Dots

Colloidal quantum dots offer tunable optical properties for optoelectronic applications, but the synthesis of high-quality III–V quantum dots (QDs) other than indium pnictides, and particularly GaAs, has remained elusive due to synthetic challenges. Colloidal GaAs QDs have been reported very recently and have shown only weak band-edge photoluminescence. Here, we demonstrate a large-scale synthesis of colloidal GaAs QDs in molten salts, followed by a high-temperature surface treatment with K 2 S, which removes native oxide and enables uniform zinc chalcogenide shell growth on GaAs. These QDs demonstrate bright band-edge photoluminescence and electroluminescence in QD LED devices. Low-temperature spectroscopy reveals a well-resolved exciton fine structure with distinct bright-state splitting and temperature-independent decay dynamics from 4 to 100 K. These results establish a practical pathway for the preparation of high-quality colloidal GaAs QDs from molten salts with potential applications in quantum technologies and optoelectronics.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Quantum barriers engineering toward radiative and stable perovskite photovoltaic devices

Efficient photovoltaic devices must be efficient light emitters to reach the thermodynamic efficiency limit. Here, we present a promising prospect of perovskite photovoltaics as bright emitters by harnessing the significant benefits of photon recycling, which can be practically achieved by suppressing interfacial quenching. We have achieved radiative and stable perovskite photovoltaic devices by the design of a multiple quantum well structure with long (~3 nm) organic spacers with oleylammonium molecules at perovskite top interfaces. Our L-site exchange process (L: barrier molecule cation) enables the formation of stable interfacial structures with moderate conductivity despite the thick barriers. Compared to popular short (~1 nm) Ls, our approach results in enhanced radiation efficiency through the recursive process of photon recycling. This leads to the realization of radiative perovskite photovoltaics with both high photovoltaic efficiency (in-lab 26.0%, certified to 25.2%) and electroluminescence quantum efficiency (19.7 % at peak, 17.8% at 1-sun equivalent condition). Furthermore, the stable crystallinity of oleylammonium-based quantum wells enables our devices to maintain high efficiencies for over 1000 h of operation and >2 years of storage.

14 SOLAR ENERGY↗

Surface-binding molecular multipods strengthen the halide perovskite lattice and boost luminescence

Reducing the size of perovskite crystals to confine excitons and passivating surface defects has fueled a significant advance in the luminescence efficiency of perovskite light-emitting diodes (LEDs). However, the persistent gap between the optical limit of electroluminescence efficiency and the photoluminescence efficiency of colloidal perovskite nanocrystals (PeNCs) suggests that defect passivation alone is not sufficient to achieve highly efficient colloidal PeNC-LEDs. Here, we present a materials approach to controlling the dynamic nature of the perovskite surface. Our experimental and theoretical studies reveal that conjugated molecular multipods (CMMs) adsorb onto the perovskite surface by multipodal hydrogen bonding and van der Waals interactions, strengthening the near-surface perovskite lattice and reducing ionic fluctuations which are related to nonradiative recombination. The CMM treatment strengthens the perovskite lattice and suppresses its dynamic disorder, resulting in a near-unity photoluminescence quantum yield of PeNC films and a high external quantum efficiency (26.1%) of PeNC-LED with pure green emission that matches the Rec.2020 color standard for next-generation vivid displays.

36 MATERIALS SCIENCE↗

Predicting the single-site and multi-site event discrimination power of dual-phase time projection chambers

Dual-phase xenon time projection chambers (TPCs) are widely used in searches for rare dark matter and neutrino interactions, in part because of their excellent position reconstruction capability in 3D. Despite their millimeter-scale resolution along the charge drift axis, xenon TPCs face challenges in resolving single-site (SS) and multi-site (MS) interactions in the transverse plane. In this paper, we build a generic TPC model with an idealized signal readout, and use Fisher Information (FI) to predict its theoretical capability of differentiating SS and MS events using the electroluminescence signal. We also demonstrate via simulation that, when only statistical photon noise is present, the theoretical limits can be approached with conventional reconstruction algorithms like maximum likelihood estimation, and with a convolutional neural network classifier. The implications of this study on future TPC experiments will be discussed.

Physics↗

Characterization of Field-Exposed Photovoltaic Modules Featuring Signs of Contact Degradation

Here, this work investigates several photovoltaic (PV) modules that have shown signs of metal contact corrosion due to field exposure in a hot and humid climate. This includes two multicrystalline silicon aluminum back surface field systems with 10 and 14 years of exposure and one monocrystalline silicon passivated emitter and rear cell system with four years of exposure. A comprehensive, multiscale characterization process is used to evaluate these PV modules in great detail. Current–voltage (I−V), Suns-V OC measurements, electroluminescence imaging, infrared imaging, and ultraviolet fluorescence imaging were performed, and locations of interest were cored and analyzed using cross-sectional scanning electron microscopy (SEM). A rigorous, quantitative analysis procedure for the cross-sectional SEM images is proposed and implemented. Careful characterization does reveal that some of these PV modules do indeed exhibit the same classic signs of acetic-acid-based corrosion of the glass frit that is present at the silver/silicon interface, which have been observed previously in PV modules exposed to damp heat in an environmental chamber.

14 SOLAR ENERGY↗

Diagnosis of PV Cell Antireflective Coating Degradation Resulting From Hot-Humid High-Voltage Potential Aging

Corrosion of the antireflective coating on a photovoltaic cell ("ARc corrosion") has previously been observed in studies using hot-humid test conditions with external high-voltage (HV) bias. This study primarily focuses on known vulnerable legacy aluminum back surface field cells in mini-modules (MiMos) put through comparative stepped stress tests. Each cell type had MiMos at +1500 V, -1500 V, or unbiased ("Voc") potential, which were sequentially subjected to test conditions of 60 degrees C/60% relative humidity (RH) for 96 h, as in International Electrotechnical Commission Technical Specification 62804-1; 70 degrees C/70% RH for 200 h; and 85 degrees C/85% RH for 200 h. Characterizations at each step included visual camera and electroluminescence (EL) imaging, colorimetry, and current-voltage curve tracing. Final characterizations included: Suns-Voc, spatial mapping of external quantum efficiency, high-resolution photoluminescence, EL, and dark lock-in thermography imaging. Forensics were performed on extracted cores, including scanning electron microscopy (SEM) with energy-dispersive X-ray spectroscopy (EDS), X-ray photoelectron spectroscopy, and scanning Auger microscopy (SAM). Forensics were also conducted on MiMos from previous studies that underwent stepped HV aging and separate outdoor aged full-sized modules. ARc corrosion was specifically seen for the glass/encapsulant/cell side of the +1500 V (HV+) stressed MiMos and modules. Appearance, color, and reflectance were the most distinguishing characteristics relative to glass corrosion, gridline corrosion and delamination, and other concurrent degradation modes. SEM/EDS and SAM identified the conversion of silicon nitride to hydrated silica, hydrous silica, or hydrated amorphous silica, which preferentially occurred at the edges and tips of the pyramidal textured cell surface.

14 SOLAR ENERGY↗

A New UV Spot Test for Quality Control

Here, we present a fast, low-cost ultraviolet (UV) spot test to screen photovoltaic modules for UV-induced degradation (UVID). The measurement is based on a fiber-coupled arc lamp that delivers a highly accelerated local UV dose-approximately five years of equivalent field exposure in less than a day. Spot-exposed areas are evaluated using electroluminescence imaging. We test a “known bad” product, which was observed to experience UVID in the field, and a “known good” product which did not exhibit UVID in the field. Results indicate that the method may be useful as a quick and relatively inexpensive quality control screening tool for customers and manufacturers.

14 SOLAR ENERGY↗

Extended Accelerated Stress Testing of Lamination-Free Edge-Sealed Photovoltaic Minimodules

Lamination-free minimodules are constructed with silicon solar cells between glass sheets and an edge seal of polyisobutylene and silicone. These samples are stressed using a repeated sequential testing sequence including ultraviolet-containing simulated solar spectrum light exposure at elevated temperature, damp heat, humidity freeze, and thermal cycling adapted from the International Electrotechnical Commission (IEC) TS 63209-2:2022. The minimodule performance throughout the stressing is characterized by flash testing and electroluminescence imaging. Results are compared to conventional laminated minimodules using the same type of solar cells. The lamination-free minimodules experience up to 8% power loss compared to roughly 3% for the laminated versions. However, those losses, dominated by current and fill factor, are caused by glass soiling and busbar ribbon separation on the cells. When glass is replaced and the stressed cells are contacted with probes bypassing the delaminated ribbons, the initial performance is recovered, and overall losses of the lamination-free samples become negligible.

14 SOLAR ENERGY↗

Different Damp-Heat-Induced Series Resistance Degradation Behaviors in Fielded Crystalline Silicon Photovoltaic Modules Due to Difference in Bill of Materials

This case study investigates mono-crystalline silicon modules from underperforming portions of a utility-scale photovoltaic power plant. Field-collected I-V curves and electroluminescence imaging suggested that increased series resistance was a primary factor driving module degradation. Selected modules were removed from the field for further analysis, including incremental damp heat accelerated testing, which confirmed a progression in series resistance degradation. Two distinct cell degradation behaviors became apparent during the investigation. Cross-sectional scanning electron microscopy (with elemental analysis) and scanning spreading resistance microscopy identified key differences between the two degradation mechanisms, primarily grid finger width and contact resistance. Additionally, the study highlights the reliability implications of retest requirements in International Electrotechnical Commission 61215 for material changes and how they may have mitigated the degradation observed at this site.

14 SOLAR ENERGY↗

Diagnosis of PV Cell Passivation Degradation Resulting from Hot-Humid, High Voltage Potential Aging

Corrosion of the antireflective coating on the cell ("AR c corrosion") was previously observed in studies using hot-humid test conditions with external high voltage (HV) bias. Because AR c corrosion is not well understood, mini-modules (MiMos) were examined in a comparative experiment using PERC and PERT as well as legacy Al-BSF cells. For separate MiMos with the cell circuit electrical at +1500 V, -1500 V, or unbiased "V oc", test conditions in the comparative study included 60degrees C/60% RH for 96 h, as in IEC TS 62804-1; 70degrees C/70%RH for 200 h; and 85degrees C/85% RH for 200 h. Characterizations at each read point included: camera and electroluminescence (EL) imaging, colorimetry, and I-V curve tracing. Characterizations at the final read point included: SunsVoc; spatially mapping external quantum efficiency (EQE); high resolution: photoluminescence (PL), EL, and dark lock-in thermographic (DLIT) imaging. Forensics were performed on extracted cores, including scanning electron microscopy (SEM) with energy-dispersive X-ray spectroscopy (EDS) and scanning Auger microscopy (SAM). Forensics were also conducted on MiMos (stepped HV aging) and full-sized modules (outdoor aging) from previous studies. AR c corrosion was specifically observed for the glass/encapsulant/cell side of +1500 V (HV+) stressed MiMos, where appearance, color, and reflectance were the characteristics most distinguished relative to simultaneously occurring degradation modes. SEM/EDS and SAM identified conversion of silicon nitride to silicon oxide or hydrous silica, preferentially occurring at the edges and tips of the pyramidal textured cell surface.

aging↗

Exploring Capability of Multimodal Foundation Model for Image-based Fault Detection of Photovoltaic Modules

Multimodal Foundation Model (MFM), like ChatGPT and Gemini, have emerged as powerful tools for their exceptional natural language processing capabilities and their emerging potential in image analysis. This paper investigates the application of MFMs for photovoltaic (PV) fault detection through image analysis, focusing on ChatGPT 4.0 and Gemini 1.5 Pro. Three types of PV images and the corresponding common PV faults are detected: bird droppings using visible images, cell cracks via electroluminescence (EL) images, and hotspots using infrared (IR) images. Among the two models, Gemini 1.5 Pro demonstrated superior performance, achieving near-perfect results with an average F1 score of 0.97, consistently outperforming ChatGPT 4.0 in accuracy and reliability. Unlike traditional machine learning (ML) models, MFMs can operate in a zero shot manner that does not require additional training by the user, and the input images are not limited by size, angle, scope, or PV technology. The strong adaptability and user-friendliness make MFM a promising tool for analyzing PV images and advancing health monitoring for PV modules.

Li, Baojie↗

The NEXT-100 Detector

The NEXT collaboration is dedicated to the study of double beta decays of 136 Xe using a high-pressure gas electroluminescent time projection chamber. This advanced technology combines exceptional energy resolution (≤ 1% FWHM at the Q ββ value of the neutrinoless double beta decay) and powerful topological event discrimination. Building on the achievements of the NEXT-White detector, the NEXT-100 detector started taking data at the Laboratorio Subterráneo de Canfranc (LSC) in May of 2024. Designed to operate with xenon gas at 13.5 bar, NEXT-100 consists of a time projection chamber where the energy and the spatial pattern of the ionising particles in the detector are precisely retrieved using two sensor planes (one with photo-multiplier tubes and the other with silicon photo-multipliers). The detector has been operating at stable conditions using argon and xenon gases at ~4 bar and drift fields of 74 V cm –1 and 118 V cm –1 , respectively. Alpha decays from the 222 Rn chain have been used to test and monitor the stability of the detector, showing a constant electron lifetime in the drift volume. In this paper, in addition to reporting the results of the commissioning run, we provide a detailed description of the NEXT-100 detector, describe its assembly, and present the current estimation of the radiopurity budget.

Adams, C. [Argonne National Laboratory; NVIDIA] (O↗

First results of the NEXT-100 detector using $^{83m}$Kr decays

The NEXT collaboration is investigating the double beta decay of $ ^{136}\mathrm Xe$ using high-pressure gas electroluminescent time projection chambers, which provide excellent energy resolution together with a robust topological signature. Operating at the Laboratorio Subterráneo de Canfranc (LSC) and building on the success of the NEXT-White detector, the NEXT-100 apparatus began commissioning in May 2024 and started operation with xenon at a pressure of 4 bar in October 2024. We report here the first results obtained with NEXT-100 using low-energy calibration data from $^{83\text {m}}\textrm{Kr}$ decays, which allow mapping of the detector response in the active volume and monitoring of its stability over time. After homogenizing the light response, we achieve an energy resolution of 4.37% FWHM at 41.5 keV for $^{83\text {m}}\textrm{Kr}$ point-like energy deposits contained in a radius of 425 mm. In a fiducial region representing the operating conditions of NEXT-100 at 10 bar we obtain an improved energy resolution of 4.16% FWHM. These results are in good agreement with that obtained in NEXT-White, and an $E^{-1/2}$ extrapolation to $Q_{\beta \beta }$ yields an energy resolution close to 0.5% FWHM, well below the 1% FWHM design target.

Martínez-Lema, G. [Donostia Intl. Phys. Ctr., San ↗

Performance Assessment of Photovoltaic Panels Using Impedance Spectroscopy

The goal of this project was to develop a technique for measuring internal characteristics of a PV module using light modulation under a fixed voltage bias while measuring the resulting alternating current. This technique, light-intensity modulated impedance spectroscopy (LIMIS), has the promise of detecting early signs of panel aging and degradation that could be used for example by solar farm operators to have early warnings to repair or replace panels to maintain reliability of the overall PV array. LIMIS would be complementary with the previously developed electrochemical impedance spectroscopy (EIS), which uses an alternating voltage applied electrically to a solar cell with a similar alternating current measurement. EIS has mostly been developed for individual PV cells rather than whole modules. The project was intended to assess what different information could be revealed by LIMIS, which may in some cases be more scalable to larger modules and potentially more practical to apply in field measurements without needing to electrically disconnect PV modules. We began with small 10 W PV modules and built a testbed capable of oscillating the light intensity with frequencies up to 50 kHz. In parallel, we built a large testbed for testing large 250 W PV modules. Meanwhile, we developed procedures for established measurement techniques: current–voltage (I–V), EIS, and electroluminescence (EL) imaging, where panels are subjected to forward bias while their infrared emission is recorded using a camera modified to be sensitive to IR wavelengths. In addition, we developed protocols for accelerated aging of PV modules in two ways. Thermal cycling from –40°C to +90°C simulates the diurnal temperature cycles on a rooftop. Mechanical stress by dropping a 227 g ball from a height of 1 m simulates damage such as that due to hail impacts.

14 SOLAR ENERGY↗

Diagnosis of PV Cell Antireflective Coating Degradation Resulting from Hot-Humid, High Voltage Potential Aging

Corrosion of the antireflective coating on a photovoltaic cell ("ARc corrosion") has previously been observed in studies using hot-humid test conditions with external high-voltage (HV) bias. This study primarily focuses on known vulnerable, legacy aluminum back surface field (Al-BSF) cells in mini-modules (MiMos) put through comparative stepped stress tests. Each cell type had MiMos at +1500 V, -1500 V, or unbiased ("Voc") potential, which were sequentially subjected to test conditions of 60deg C/60% relative humidity (RH) for 96 h, as in International Electrotechnical Commission (IEC) Technical Specification 62804-1; 70 deg C/70% RH for 200 h; and 85 deg C/85% RH for 200 h. Characterizations at each step included visual camera and electroluminescence (EL) imaging, colorimetry, and current-voltage (I-V) curve tracing. Final characterizations included: Suns-Voc; spatial mapping of external quantum efficiency (EQE); high-resolution photoluminescence (PL), EL, and dark lock-in thermography (DLIT) imaging. Forensics were performed on extracted cores, including scanning electron microscopy (SEM) with energy-dispersive X-ray spectroscopy (EDS), X-ray photoelectron spectroscopy (XPS), and scanning Auger microscopy (SAM). Forensics were also conducted on MiMos from previous studies that underwent stepped HV aging and separate outdoor aged full-sized modules. ARc corrosion was specifically seen for the glass/encapsulant/cell side of the +1500V (HV+) stressed MiMos and modules. Appearance, color, and reflectance were the most distinguishing characteristics relative to glass corrosion, gridline-corrosion and -delamination as well as other concurrent degradation modes. SEM/EDS and SAM identified conversion of silicon nitride to hydrated silica, hydrous silica, or hydrated amorphous silica, which preferentially occurred at the edges and tips of the pyramidal textured cell surface.