Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “ENCAPSULATION”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 91 records · Page 5

Hybrid Encapsulated Ionic Liquids for Post-Combustion Carbon Dioxide (CO 2 ) Capture

It is increasingly clear that carbon dioxide (CO 2 ) capture and sequestration (CCS) must play a critical role in curbing worldwide CO 2 emissions to the atmosphere. Previously, we have developed ionic liquids (ILs) and phase change ionic liquids (PCILs) for post-combustion CO 2 capture. In this project, we synthesized and tested 19 ILs and PCILs and chose one of each for further development. The IL selected for further development was triethyl(octyl)phosphonium 2-cyanopyrrolide ([P 2228 ][2CNPyr]), which has the same anion but a different cation, than used in our previous work. The new cation imparts a lower viscosity than the prior cation. The PCIL selected for further development was tetraethylphosphonium benzimidazolide ([P 2222 ][BnIm]), which was developed in an Advanced Research Projects Agency-Energy (ARPA-E) project. Although we made numerous other candidates, none were better than this original PCIL. Here we showed that the CO 2 absorption by the IL and the PCIL was completely reversible, even when water was present. We determined and quantified the additional chemistry, involving the formation of bicarbonate, when water is present. The IL and PCIL were encapsulated in silicone shells using a microfluidic device. Compatibility between the IL/PCIL and the polymer, viscosity, and surface tension issues, getting sufficiently high IL/PCIL loading and leakage (likely from insufficient cross-linking), were serious challenges. Small quantities (~ 1 g) of microcapsules with good integrity of both the IL and the PCIL were produced. The CO 2 uptake by these capsules was the same as for the free IL and PCIL and the capacity of the capsules decreased only slightly even after five absorption and desorption cycles. As expected, the IL and PCIL (and subsequently the encapsulated IL and PCIL) reacted readily with SO 2 and NO, so, like aqueous amine absorbents, the CO 2 capture unit would have to be located downstream of the flue gas desulfurization and other gas treatment units. Large samples (~70 g and 100 g) of encapsulated PCIL were produced in a parallel microfluidic device and in an in-air device. These capsules were tested in a Laboratory Scale Unit (LSU) to demonstrate uptake capacity in a fluidized bed. We also used the LSU to determine recyclability and mass transfer coefficients. Unfortunately, equivalent experiments with the IL were not possible due to difficulties with producing large samples of the encapsulated IL. This IL encapsulation “scale-up” problem was not solved during the course of this project. Nonetheless, using the PCIL microcapsules we demonstrated that, as expected, the mass transfer is internally controlled. In concert with a new rate-based model of the fluidized bed, we determined that the productivity is increased by a factor of 4.75 in the microcapsule fluidized bed absorber compared to a conventional liquid-gas packed bed absorber. The initial technoeconomic model shows that the capital cost for the microcapsule IL continuous fluidized bed process is similar to that of an aqueous amine process (specifically, the Econamine FG Plus technology). However, the stripping heat requirements are about 35% less for the model IL microcapsule case compared to the monoethanolamine (MEA) case. Thus, encapsulated ILs/PCILs in a continuous fluidized bed absorber for post-combustion CO 2 capture are a significant improvement over the free IL/PCIL case and represent a major reduction in the parasitic energy requirements compared to aqueous amine process.

20 FOSSIL-FUELED POWER PLANTS↗

Degradation in Photovoltaic Encapsulant Transmittance: Results of the Second PVQAT TG5 Artificial Weathering Study

The optical degradation of encapsulants from ultraviolet (UV) radiation has historically resulted in a significant loss in performance throughout the life of a photovoltaic (PV) module. IEC test methods have recently been developed to screen for PV encapsulants prone to loss in optical performance. The present study was performed to benchmark polymeric packaging materials relative to IEC 62788-1-4 (covering the measurement of optical transmittance) and IEC 62788-1-7 (on the durability of transmittance), provide feedback toward improvement of the methods, and develop insight regarding optical degradation. Contemporary materials were examined, including: poly(ethylene-co-vinyl acetate) (EVA), thermoplastic polyolefin (TPO), polyolefin elastomer (POE), and polyvinyl butyral (PVB) encapsulants; a poly(ethene-co-tetrafluoroethene)/poly(ethylene terephthalate) (ETFE/PET) transparent backsheet; and a polystyrene (PS) working reference material. The use of silica-, specialty-, and rolled-glass was also compared in laminated coupons. Specimen size was separately examined from 2.5 cm to 12.5 cm. Weathering was performed with a xenon source, using IEC TS 62788-7-2 methods A2, A3, A4, and A5 (chamber temperature of 55 Degrees C, 65 Degrees C, 75 Degrees C, or 85 Degrees C), respectively. Characterizations were made using a UV-VIS-NIR spectrophotometer (transmittance and reflectance, with and without an integrating sphere), a UV-VIS fluorescence spectrophotometer, a camera, and an optical microscope. Performance was analyzed, including solar weighted transmittance, yellowness index, UV cut-off wavelength, and haze (scattering). Separate Arrhenius analyses were performed to assess retention of transmittance and changes in yellowness index. The activation energy for both characteristics was found to range from 15 kJ?mol-1-80 kJ/mol-1, with an average of 48 kJ/mol-1, similar to the average of 45 kJ/mol-1 identified in the previous international PV Quality Assurance Task Force (PVQAT) Task Group 5 (TG5) study of more traditional encapsulants. The separate degradation modes of discoloration and scattering were distinguished in the encapsulants using a comprehensive spectral characterization. Based on these results, the IEC 62788-1-7 pass/fail criteria of 5% change in transmittance was confirmed to identify a known bad encapsulant.

durability↗

Thermal behaviors of ethylene vinyl acetate encapsulants in fielded silicon photovoltaic modules

Aging of silicon photovoltaic (PV) module packaging is one of the greatest limiters of PV module service lifetimes. Module characterization typically focuses on power degradation metrics, which do not convey the complexities of often simultaneous degradation mechanisms. In this work, PV modules with pristine references and known fielding histories were investigated by non-destructive and destructive methods. Modules from Canadian Solar, Mission Solar, and Hanwha Q-Cells were fielded for up to three years; select modules were removed from fielding each year for coring to allow for characterization of the encapsulant. Modules are commonly encapsulated with two protective layers of partially-crystalline ethylene vinyl acetate (EVA) polymer that must undergo a crosslinking reaction to achieve desired properties. The extent of crystallinity of the encapsulants as studied by differential scanning calorimetry showed differences between manufacturers and over time. Some encapsulants showed different magnitudes of crystal sizes which changed after fielding; encapsulants with the monodisperse crystal sizes did not change with fielding. This is due to differences in thermal history. In conclusion, these results have implications for stress development during module aging, since EVA crystal melting and crosslinking reactions can result in encapsulant density changes.

36 MATERIALS SCIENCE↗

A blueprint for biomolecular condensation driven by bacterial microcompartment encapsulation peptides

Bacterial microcompartments are protein organelles with diverse metabolic capabilities. Their functional diversity is determined by an enzymatic core that is sequestered within a structurally conserved protein shell architecture. Segregation of protein cargo into the bacterial microcompartment is enabled by encapsulation peptides, which are short helical domains fused to core proteins through a disordered linker. Here, we investigate how encapsulation peptides drive multicomponent cargo assembly into biomolecular condensates. In vitro experiments supported by molecular dynamics simulations demonstrate the importance of both conserved hydrophobic packing and electrostatic interactions in stabilizing trimeric encapsulation peptide bundles. Topological rearrangements of encapsulation peptide domains can drive programmable liquid- or gel-like partitioning in vitro and in vivo. This partitioning is found to be encapsulation peptide-specific, modular, and can co-assemble at least three fluorescent reporters. In summary, we describe the molecular features necessary to drive biomolecular condensation using a widespread peptide tag. This work can serve as a blueprint for implementing encapsulation peptide biotechnology across diverse applications.

59 BASIC BIOLOGICAL SCIENCES↗

Sol-Generating Chemical Vapor into Liquid (SG-CViL) deposition – a facile method for encapsulation of diverse cell types in silica matrices

In nature, cells perform a variety of complex functions such as sensing, catalysis, and energy conversion which hold great potential for biotechnological device construction. However, cellular sensitivity to ex vivo environments necessitates development of bio–nano interfaces which allow integration of cells into devices and maintain their desired functionality. In order to develop such an interface, the use of a novel Sol-Generating Chemical Vapor into Liquid (SG-CViL) deposition process for whole cell encapsulation in silica was explored. In SG-CViL, the high vapor pressure of tetramethyl orthosilicate (TMOS) is utilized to deliver silica into an aqueous medium, creating a silica sol. Cells are then mixed with the resulting silica sol, facilitating encapsulation of cells in silica while minimizing cell contact with the cytotoxic products of silica generating reactions (i.e. methanol), and reduce exposure of cells to compressive stresses induced from silica condensation reactions. Using SG-CVIL, Saccharomyces cerevisiae (S. cerevisiae) engineered with an inducible beta galactosidase system were encapsulated in silica solids and remained both viable and responsive 29 days post encapsulation. By tuning SG-CViL parameters, thin layer silica deposition on mammalian HeLa and U87 human cancer cells was also achieved. Thus, the ability to encapsulate various cell types in either a multi cell (S. cerevisiae) or a thin layer (HeLa and U87 cells) fashion shows the promise of SG-CViL as an encapsulation strategy for generating cell–silica constructs with diverse functions for incorporation into devices for sensing, bioelectronics, biocatalysis, and biofuel applications.

36 MATERIALS SCIENCE↗

Microbead Encapsulation for Protection of Electronic Components

Here, this study investigates the application of microbeads as an innovative encapsulation technique to protect electronic components from harsh mechanical strain. Traditional encapsulation methods using hard epoxy provide substantial mechanical support but create thermal expansion mismatch issues, potentially leading to electronic component failure. We explore the use of finely powdered microbeads to achieve protective structures combining stiffness and energy absorption. The research focuses on key variables, including microbead size, microbead roughness, compaction of microbeads, and circuit board mounting in the encapsulation, all of which influence the encapsulation’s effectiveness. Experimental setups and testing protocols were developed to assess the performance of various microbead materials under different impact conditions. Results demonstrate that microbead encapsulation significantly reduces strain on circuit boards, minimizing the risk of damage during mechanical shocks. However, challenges remain, such as optimizing microbead characteristics and modeling their behavior within large-scale circuit board assemblies. Despite these challenges, the findings suggest that microbead encapsulation offers a promising alternative to conventional methods, enhancing the durability and reliability of electronic components in high-stress environments.

42 ENGINEERING↗

Fabricating Fe nanocrystals via encapsulation at the graphite surface

In this paper, the authors describe the conditions under which Fe forms encapsulated nanocrystals beneath the surface of graphite, and they characterize these islands (graphite + Fe) thoroughly. The authors use the experimental techniques of scanning tunneling microscopy (STM) plus x-ray photoelectron spectroscopy (XPS) and the computational technique of density functional theory (DFT). Necessary conditions for encapsulation are preexisting ion-induced defects in the graphite substrate and elevated deposition temperature of 875–900 K. Evidence of encapsulation consists of atomically resolved STM images of a carbon lattice, both on top of the islands and on the sloping sides. The nature of the images indicates that this carbon lattice corresponds to a graphene blanket consisting of more than one graphene sheet that drapes continuously from the top of the island to the graphite substrate. The formation of iron carbide is not observed based on XPS. Shapes of the island footprints are consistent with metallic Fe, predominantly in the hcp or fcc form, though larger islands tend toward bcc. Island structures with hexagonally close-packed lateral hcp or fcc planes are stabilized by their excellent lattice match with the graphite substrate. Evolution of island density with prolonged deposition time provides evidence of coarsening, perhaps via Smoluchowski ripening. The encapsulated Fe clusters are stable in air at room temperature, protected by smaller Fe clusters that decorate defect sites and block permeation of gases. DFT shows that two configurations of Fe are more stable within the gallery than adsorbed on top of the surface: a single atom of Fe and a film (slab) of metallic Fe. Comparison with other metals shows that encapsulated Fe is similar to Cu but dissimilar to Ru or Dy, leading the authors to conclude that carbon dissolution in the metal does not play a role in encapsulation.

36 MATERIALS SCIENCE↗

Final Scientific/Technical Report (DOE F 241.3) Next-Generation LED Package Architectures Enabled by Thermally Conductive Transparent Encapsulants

The objective of this program is to generate novel LED package designs that would provide 30% improvement in lumen/$ output. This was to be achieved by improving thermal management in encapsulants/ phosphors to reduce their temperatures. Currently, the heat that is generated during down conversion of blue light to longer wavelengths by the phosphors dispersed in the encapsulant does not have optimum thermal pathways for dissipation due to poor thermal conductivity of the encapsulant material. Additionally, high temperature in the encapsulant during operation is one of the primary failure modes in LED luminaires resulting in much shorter than expected life. The thermal issues manifest in color instability (yellowing, browning), cracking and hot spots in the encapsulant leading to failures. This work explored boron nitride (hBN) as thermal fillers in encapsulants to improve thermal conductivity while minimally impacting optical properties. Various approaches to Boron Nitride (BN) were evaluated and over 380 samples were generated to down select appropriate BN morphologies. We developed a range or BN materials for enabling thermal properties while attempting to minimally impact to optical properties.

32 ENERGY CONSERVATION, CONSUMPTION, AND UTILIZATI↗

Photovoltaic module encapsulation design and materials selection, volume 1

Encapsulation material system requirements, material selection criteria, and the status and properties of encapsulation materials and processes available are presented. Technical and economic goals established for photovoltaic modules and encapsulation systems and their status are described. Available encapsulation technology and data are presented to facilitate design and material selection for silicon flat plate photovoltaic modules, using the best materials available and processes optimized for specific power applications and geographic sites. The operational and environmental loads that encapsulation system functional requirements and candidate design concepts and materials that are identified to have the best potential to meet the cost and performance goals for the flat plate solar array project are described. Available data on encapsulant material properties, fabrication processing, and module life and durability characteristics are presented.

Cuddihy, E.↗

Flat-plate solar array project. Volume 7: Module encapsulation

The objective of the Encapsulation Task was to develop, demonstrate, and qualify photovoltaic (PV) module encapsulation systems that would provide 20 year (later decreased to 30 year) life expectancies in terrestrial environments, and which would be compatible with the cost and performance goals of the Flat-Plate Solar Array (FSA) Project. The scope of the Encapsulation Task included the identification, development, and evaluation of material systems and configurations required to support and protect the optically and electrically active solar cell circuit components in the PV module operating environment. Encapsulation material technologies summarized include the development of low cost ultraviolet protection techniques, stable low cost pottants, soiling resistant coatings, electrical isolation criteria, processes for optimum interface bonding, and analytical and experimental tools for evaluating the long term durability and structural adequacy of encapsulated modules. Field testing, accelerated stress testing, and design studies have demonstrated that encapsulation materials, processes, and configurations are available that meet the FSA cost and performance goals.

Cuddihy, E.↗

Monte Carlo Simulation of Nanoparticle Encapsulation in Flames

Two critical challenges facing the application of flames for synthesis of nanopowder materials are: (1) overcoming formation of agglomerates and (2) ensuring that the highly reactive nanopowders that are synthesized in flames can be produced in such a manner that their purity is maintained during subsequent processing. Agglomerates are produced in flames because particle formation occurs in a high temperature and high number density environment. They are undesirable in most advanced applications of powders. For example, agglomerates have a deleterious effect on compaction density, leading to voids when nanopowders are consolidated. Efforts to avoid agglomeration in flames without substantially reducing particle number density and, consequently, production rate, have had limited success. Powder purity must also be maintained during subsequent handling of nanopowders and this poses a significant challenge for any synthesis route because nanopowders, particularly metals and non-oxide ceramic powders, are inherently reactive. Impurities acquired during handling of nanopowders have slowed the advancement of the nanostructured materials industry. One promising approach that has been proposed to address these problems is nano-encapsulation. In this approach, the core particles are encapsulated in a removable material while they are within the flame but before excessive agglomeration has occurred. Condensation can be very rapid so that core particles are trapped within the condensed material and agglomeration is limited. Nano-encapsulation also addresses the handling concerns for post-synthesis processing. Results have shown that when nano-encapsulated powders are exposed to atmosphere the core particles are protected from oxidation and/or hydrolysis. Thus, handling of the powders does not require extreme care. If, for example, at the time of consolidation the encapsulation material is removed by vacuum annealing, the resulting powder remains unagglomerated and free of impurities. In this work, we described a novel aerosol model that has been developed to simulate particle encapsulation in flames. The model will ultimately be coupled to a one-dimensional spherical flame code and compared to results from microgravity flame experiments.

Sun, Z.↗

Special Form Testing of Sealed Source Encapsulation for High-Alpha-Activity Actinide Materials

In the United States all transportation of radioactive material is regulated by the U.S. Department of Transportation (DOT). Beginning in 2008 a new type of sealed-source encapsulation package was developed and tested by Oak Ridge National Laboratory (ORNL). These packages contain high-alpha-activity actinides and are regulated and transported in accordance with the requirements for DOT Class 7 hazardous material. The DOT provides specific regulations pertaining to special form encapsulation designs. The special form designation indicates that the encapsulated radioactive contents have a very low probability of dispersion even when subjected to significant structural events. The special form designs have been shown to simplify the delivery, transport, acceptance, and receipt processes. It is intended for these sealed-source encapsulations to be shipped to various facilities making it very advantageous for them to be certified as special form. To this end, DOT Certificates of Competent Authority (CoCAs) have been sought for the design suitable for containing high-alpha-activity actinide materials. This design consists of the high-alpha-activity material encapsulated within a triangular zirconia canister, referred to as a ZipCan, tile that is then enclosed by a spherical shell. The spherical shell design, with ZipCan tile inside, was tested for compliance with the special form regulations found in 49 CFR 173.469. The spherical enclosure was subjected to 9-m impact, 1 m percussion, and 10-minute thermal tests at the Packaging Evaluation Facility located at the National Transportation Research Center in Knoxville, TN USA and operated by ORNL. Before and after each test, the test units were subjected to a helium leak check and a bubble test. The ZipCan tiles and core were also subjected to the tests required for ISO 2919:2012(E), including a Class IV impact test and heat test and subsequently subjected to helium leakage rate tests [49 CFR 173.469(a)(4)(i)]. The impact-tile test unit contained a nonradioactive surrogate; however, the thermal test unit contained a radioactive source. This paper describes the regulatory special form tests and presents detailed impact and leak test results that demonstrate that the sealed source encapsulation designs satisfy the regulatory tests.

Martinez, Oscar A↗

Field testing of thermoplastic encapsulants in high‐temperature installations

Abstract Recently there has been increased interest in using thermoplastic encapsulant materials in photovoltaic modules, but concerns have been raised about whether these would be mechanically stable at high temperatures in the field. Recently, this has become a significant topic of discussion in the development of IEC 61730 and IEC 61215. We constructed eight pairs of crystalline‐silicon modules and eight pairs of glass/encapsulation/glass thin‐film mock modules using different encapsulant materials, of which only two were formulated to chemically crosslink. One module set was exposed outdoors with thermal insulation on the back side in Mesa, Arizona, in the summer (hot‐dry), and an identical module set was exposed in environmental chambers. High‐precision creep measurements (±20 μ m) and electrical performance measurements indicate that despite many of these polymeric materials operating in the melt or rubbery state during outdoor deployment, no significant creep was seen because of their high viscosity, lower operating temperature at the edges, and/or the formation of chemical crosslinks in many of the encapsulants with age despite the absence of a crosslinking agent. Only an ethylene‐vinyl acetate ( EVA ) encapsulant formulated without a peroxide crosslinking agent crept significantly. In the case of the crystalline‐silicon modules, the physical restraint of the backsheet reduced creep further and was not detectable even for the EVA without peroxide. Because of the propensity of some polymeric materials to crosslink as they age, typical thermoplastic encapsulants would be unlikely to result in creep in the vast majority of installations.

14 SOLAR ENERGY↗

Optical Durability of Contemporary PV Encapsulants Through Artificial UV Weathering

Modern c-Si photovoltaic (PV) cells provide high performance but can be vulnerable to ultraviolet light induced degradation (UV-ID). Encapsulants, if chosen correctly, can mitigate UV-ID of the PV cell. Here, we explore performance and durability of 14 commercial encapsulant materials before, during, and after irradiation with UV-containing light. Materials include contemporary, polymer-based encapsulants with a base polymer of poly (ethylene co-vinyl acetate) (EVA), polyethylene-..alpha..-olefin (POE), or their composite (EPE). Polymers contain additives that induce UV-blocking, UV-transmitting, or UV-downshifting properties. We use test coupons to study degradation in a chamber held at 65 degrees C under a xenon light source for up to 4000 h of exposure, corresponding to a cumulative dose of 11.5 MJ/m2 at 340 nm. We examine optical properties including spectral transmittance, yellowness index and spectral fluorescence, considering changes to both the encapsulant and glass as a function of weathering time. Degradation modes identified include discoloration, changes to UV cutoff wavelength, changes to solar-weighted transmittance, and most notably a change to the UV-managing properties of some additives. We propose the use of solar-weighted transmittance in the 300- to 400-nm range to better track performance changes in the UV region associated with the UV-related additive. This is especially relevant for the emerging class of UV-downshifting additives, as metrics like UV-cutoff can understate the degree of degradation or change in these materials. While most encapsulants show very little change after weathering, some show significant changes that directly impact how much UV light would reach an underlying cell.

14 SOLAR ENERGY↗

Investigations of degradation and encapsulation of plastic scintillator

Studies have revealed that plastic scintillators such as polyvinyl toluene and polystyrene can undergo environmentally related material damage (“fogging”) that adversely affects detection performance under certain conditions and histories. A significant decrease in sensitivity has been seen in some gamma-ray detectors as they age as a result of this damage. Performance degradation due to such damage is characterized by a signal change from the detector, which shifts to lower energy, and ultimately a reduction in the ability to detect gamma radiation. This degradation is due to the permeation of water into the plastic, which can then cause temporary fogging and permanent damage to the material. As an example, a 1-mm thick barrier of high-density polyethylene with an area of 1 m 2 would allow 5 g per year of water transmission at 100% relative humidity. Thus, significant amounts of water can penetrate plastics over time and provide the potential for damage to the plastic. Such damage to plastic scintillator can cause problems for radiation detection applications in uncontrolled environments. Mitigation approaches that have been proposed to prevent damage to plastic scintillator include encapsulation of the plastic scintillator to prevent water intrusion that leads to damage during cold cycles. It is concluded that an encapsulation material with a moisture vapor transmission rate on the order of 10 -4 g∙m -2 ∙d -1 or better is needed for protecting large pieces of plastic scintillator from fogging over years of use. This article presents information on testing of bare and encapsulated plastic scintillator samples and on diagnostic approaches to measure the nature and progression of the fogging condition. It is shown that several encapsulation approaches fail to prevent water intrusion, while a couple methods can successfully encapsulate plastic and prevent water from penetrating the plastic and producing fogging.

36 MATERIALS SCIENCE↗

Reliability Analysis of Field-aged Glass/Glass PV Modules: Influence of Different Encapsulant Types

This paper presents a preliminary reliability analysis of field-aged glass/glass (G/G) PV modules. Several characterization tests were performed on more than 60 modules with two different encapsulant types (EVA and ionomer) exposed in hot-dry Arizona (AZ) climate over 10-35 years. The common degradation mode observed in both encapsulant types was the delamination of encapsulant along with encapsulant browning (EVA only), glass cracking (EVA only), and metallic corrosion over junction box area (ionomer only). The EVA encapsulated G/G modules showed the higher median power degradation rate at 0.91-1.99%/yr whereas modules with ionomer showed the lower at 0.21%/yr.

photovoltaic, failures, field exposed, glass/glass↗

Recent progress in realizing novel one-dimensional polymorphs via nanotube encapsulation

Encapsulation of various materials inside nanotubes has emerged as an effective method in nanotechnology that facilitates the formation of novel one-dimensional (1D) structures and enhances their functionality. Because of the effects of geometrical confinement and electronic interactions with host nanotubes, encapsulated materials often exhibit low-dimensional polymorphic structures that differ from their bulk forms. These polymorphs exhibit unique properties, including altered electrical, optical, and magnetic behaviors, making them promising candidates for applications in electronics, energy storage, spintronics, and quantum devices. This review explores recent advancements in the encapsulation of a wide range of materials such as organic molecules, elemental substances, metal halides, metal chalcogenides, and other complex compounds. In particular, we focus on novel polymorphs formed through the geometrical confinement effect within the nanotubes. The atomic structure, other key properties, and potential applications of these encapsulated materials are discussed, highlighting the impact of nanotube encapsulation on their functionalities.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Encapsulation Materials Tailored to Perovskite Photovoltaics

The work combines NREL as the world leader in perovskite and polymeric materials, and teams them up with The Dow Chemical Company, the world leader in commercial production of PV encapsulation materials. The team will design and evaluate encapsulation materials that are tailored to perovskite photovoltaics. Demonstration of polyolefin-based encapsulants for perovskite PV will be impactful for a number of reasons: 1) There is no clear-cut choice for encapsulation for perovskite PV to date. 2) There is high synthetic control of the material properties for future perovskite module designs. 3) Among the candidate materials, they have the highest barrier properties, 4) Polyolefins are the most prevalent (>20 million metric tons consumed in the US alone) and inexpensive (<1.5 $USD/kg) polymers used worldwide. 5) They are recyclable and may play a role in future of circular PV materials. 6) They are manufactured domestically. The work also highlights careful design of perovskite transport layer materials for surviving vacuum encapsulation.