High-Mobility Transparent Conducting Oxides for Compact Epsilon-Near-Zero Silicon Integrated Optical Modulators.
Abstract not provided.
SEARCH · Engineering Papers
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Abstract not provided.
Not Available
Explore the source record for details and available documents.
NREL and MEMC Electronic Materials are interested in developing a robust technique for monitoring material quality of mc-Si and mono-Si wafers -- a technique that can provide relevant data to accurately predict the performance of solar cells fabricated on them. Previous work, performed under two TSAs between NREL and MEMC, has established that dislocation clusters are the dominant performance-limiting factor in MEMC mc-Si solar cells. The work under this CRADA will go further in verifying these results on a larger data set, evaluate possibilities of faster method(s) for mapping dislocations in wafers/ingots, understanding dislocation generation during ingot casting, and helping MEMC to have an internal capability for basic characterization that will provide feedback needed for more accurate crystallization simulations. NREL has already developed dislocation mapping technique and developed a basic electronic model (called Network Model) that uses spatial distribution of dislocations to predict the cell performance. In this CRADA work, we will use these techniques to: (i) establish dislocation, grain size, and grain orientation distributions of the entire ingots (through appropriate DOE) and compare these with theoretical models developed by MEMC, (ii) determine concentrations of some relevant impurities in selected wafers, (iii) evaluate potential of using photoluminescence for dislocation mapping and identification of recombination centers, (iv) evaluate use of diode array analysis as a detailed characterization tool, and (v) establish dislocation mapping as a wafer-quality monitoring tool for commercial mc-Si production.
Abstract not provided.
Abstract not provided.
Explore the source record for details and available documents.
Explore the source record for details and available documents.
Abstract not provided.
Al interconnections discontinuities at integrated circuit contact windows observed by scanning electron microscope, noting catastrophic failure and Si presence
Ten SiC materials and five Si3N4 materials were exposed in a Mach 1-gas-velocity burner simulating a gas-turbine engine environment. All materials studied are commercially available. Cyclic tests up to 100 hours' duration were conducted at specimen temperatures of 1200 C. A specimen geometry was used that develops thermal stresses during thermal cycling in a manner similar to blades and vanes of a gas turbine engine. Materials were compared on a basis of weight change, dimensional reductions, metallography, fluorescent-penetrant inspection, X-ray diffraction analyses, failure mode, and general appearance. One hot-pressed SiC, one reaction-sintered SiC, and three hot-pressed Si3N4 materials survived the program goal of 100 one-hour cycles of exposures. Of the materials that failed to meet the program goal, thermal fatigue was identified as the exclusive failure mode.
Wafer-like crystals suitable for making solar cells are formed by pouring molten Si containing suitable dopants into a mold of the desired shape and allowing it to solidify in a temperature gradient, whereby the large surface of the melt in contact with the mold is kept at less than 200 D and the free surface is kept at a temperature of 200-1000 D higher, but below the melting point of Si. The mold can also be made in the form of a slit, whereby the 2 sides of the mold are kept at different temperatures. A mold was milled in the surface of a cylindrical graphite block 200 mm in diameter. The granite block was induction heated and the bottom of the mold was cooled by means of a water-cooled Cu plate, so that the surface of the mold in contact with one of the largest surfaces of the melt was held at approximately 800 D. The free surface of the melt was subjected to thermal radiation from a graphite plate located 2 mm from the surface and heated to 1500 D. The Si crystal formed after slow cooling to room temperature had a columnar structure and was cut with a diamond saw into wafers approximately 500 mm thick. Solar cells prepared from these wafers had efficiencies of 10 to 11%.
Explore the source record for details and available documents.
The presence of copper promotes a more rapid approach to the steady stete operating condition and results in a more consistent reactor effluent composition. The average kinetic and equilibrium yield are unchanged. Incoloy has been identified as the preferred choice of material of construction for the hydrogenation reactor although certain metallurgical changes were noted in samples exposed to the H2/HCl atmosphere at 500 C which indicate the need for more testing.
Development of inside diameter slicing technology to significantly increase the number of useable slices per inch of crystal over industry practice is discussed. The required reduction of both blade and slice thickness is to be accomplished by a combination of three key elements of slicing technology: (1) ingot rotation with minimum exposed blade area; (2) dynamic cutting edge control; and (3) the use of prefabricated insert blades. Design modifications on a slicing saw with microprocessor controls and hardware fabrication to complete this conversion were initiated. Several runs were conducted on the engineering saw incorporating the method of ingot rotation. Ingots with diameters up to six inches were sliced successfully on a production saw.
The results of the free space reactor experimental work are summarized. Overall, the objectives were achieved and the unit can be confidently scaled to the EPSDU size based on the experimental work and supporting theoretical analyses. The piping and instrumentation of the fluidized bed reactor was completed.
Modifications to a 16 inch STC automated saw included: a programmable feed system; a crystal rotating system; and a STC dynatrack blade boring and control system. By controlling the plating operation and by grinding the cutting edge, 16 inch I.D. blades were produced with a cutting edge thickness of .22 mm. Crystal rotation mechanism was used to slice 100 mm diameter crystals with a 16 inch blade down to a thickness of .20 mm. Cutting rates with crystal rotation were generally slower than with standard plunge I.D. slicing techniques. Using programmed feeds and programmed rotation, maximum cutting rates were from 0.3 to 1.0 inches per minute.