Intermediate-Term Thermal Aging Effect Evaluation for Grade 92 and 316L at The LWR Relevant Temperature

Life extension of the existing nuclear reactors imposes accumulated damages, such as higher fluences and longer period of corrosion, to structural materials, which would result in significant challenges to the traditional reactor materials such as type 304 and 316 stainless steels. Advanced alloys with superior radiation resistance will increase safety margins, design flexibility, and economics for not only the life extension of the existing fleet but also new builds with advanced reactor designs. The Electric Power Research Institute (EPRI) teamed up with Department of Energy (DOE) on the Advanced Radiation Resistant Materials (ARRM) program, aiming to develop and test degradation resistant alloys from current commercial alloy specifications by 2021 to a new advanced alloy with superior degradation resistance in light water reactor (LWR)-relevant environments by 2024. Based on a comprehensive microstructure and property screening performed in Phase-1 of the ARRM program, a total of five alloys, together with 316L and X-750 as references, were down-selected for Phase-2 neutron irradiation studies. Because thermal aging could exert a synergistic effect on neutron irradiation due to the low neutron damage rate on the order of 10 –7 displacements per atom per second (dpa/s), Grade 92 (one of the five down-selected alloys) and two heats of 316L were selected in this task to study the effect of aging at 350°C for 12.5–12.7 kh on microstructure and mechanical properties. The aging time is approximately corresponding to 5 dpa neutron irradiation, which can be served as a reference for the 5-dpa-irradiated samples of the alloys to help understand the independent neutron damage influence on microstructure and mechanical properties. Optical microscopy and scanning electron microscopy were used for microstructural characterization. Hardness, tensile, Charpy impact toughness, and fracture toughness in the ductile regime of the aged samples were examined. The aging of Grade 92 led to the formation of many Laves phase in sizes of ~100–200 nm and resulted in some reduction in hardness and yield/ultimate tensile strength with some increases in uniform and total plastic elongations, which may have helped the enhancement of Charpy impact toughness, e.g., ~4 J increase in upper-shelf energy and 20.5°C reduction in ductile-brittle transition temperature compared with the unaged condition. The fracture toughness of the aged Grade 92 showed decent toughness of ~303 MPa√m (K Jq ) with ~87 tearing modulus at 22°C, which reduced to ~241 MPa√m (~20% reduction) with ~75 tearing modulus at 300°C. The two heats of 316L are differentiated by their amounts of δ-ferrite, i.e., ~1 vol% in heat T1103 and ~4 vol% in heat N5B8. The two heats of 316L were subjected to 15% cold work (CW) as this condition is often used in nuclear reactors to help trapping radiation-induced defects and thus postpone the steady state swelling stage. The aging did not result in any noticeable microstructure changes, except for possible segregations at grain boundaries that need to be further investigated. The aging resulted in slight reduction in hardness of 316L-T1103 and slight increase in hardness of 316L-N5B8, which is consistent with their tensile testing results. The 15%CW might have introduced some inhomogeneity, resulting in large standard deviations in hardness, which were reduced after the aging. The aged 316L followed the same trend as the unaged condition for the strength and elongation results from the tensile testing. Minimum elongations appeared within ~300–600°C, above which the elongations seem to increase. Unlike the negligible or minor changes in microstructure, hardness and tensile results of the two heats of 316L, their fracture toughness showed noticeable difference. The aged 316L-T1103 showed good toughness of ~350 MPa√m with ~80 tearing modulus at 22°C, which reduced to ~271 MPa√m (~23% reduction) with ~83 tearing modulus at 300°C. In contrast, the aged 316L-N5B8 showed lower toughness of ~244 MPa√m with ~53 tearing modulus at 22°C, which reduced to ~180 MPa√m (~26% reduction) with ~31 tearing modulus at 300°C. The preliminary results indicate that the presence of high volume of δ-ferrite would noticeable impair fracture toughness although it may not influence hardness and tensile properties.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Using Artificial Microstructures to Understand Microstructure Property Relationship-Toughening Mechanisms in Metallic Glass (Final Report)

Metallic glasses are a new class of structural materials which exhibit exciting mechanical properties including high strength and elasticity. In terms of fracture toughness, the material class of metallic glasses spans a wide range; Some metallic glasses are extremely brittle and exhibit near ideal brittle behavior whereas others can be exceptional tough with values comparable to the toughest metals out there. Such large range of observed fracture toughness within the material class of metallic glasses is surprising as they have seemingly a very similar atomic structure. Therefore, we developed “artificial microstructures” which allows to decouple the various contribution of sample geometry, imperfection and structure. Specifically, we decouple variations in the alloys’ chemical composition and the atomic structure and quantified the resulting fracture toughness. Atomic structure of a metallic glass can be modified by the fictive temperature. The fictive temperature of a glass is the temperature at which the liquid metallic glass falls out of equilibrium upon colling and forms a glass. Upon further cooling the structure is maintained only thermal oscillations decrease due to a lower absolute temperature. We found that the effect of fictive temperature (same chemistry, different structural stages of the glass) is comparable to the variations of fracture toughness when the chemistry is varied. Hence, it appears that the subtle differences in the glass structure are responsible for the large range of fracture toughness’s observed. Our results reveal that fracture toughness within the material class of metallic glasses varies significantly and we found some example alloys with exceptional high resistance to fracture and others that are almost ideally brittle. Significant influences on the fracture toughness have the structure of the glass, its chemistry, and some imperfections in the structure.

36 MATERIALS SCIENCE↗

Kink bands promote exceptional fracture resistance in a NbTaTiHf refractory medium-entropy alloy

Single-phase body-centered cubic (bcc) refractory medium- or high-entropy alloys can retain compressive strength at elevated temperatures but suffer from extremely low tensile ductility and fracture toughness. We examined the strength and fracture toughness of a bcc refractory alloy, NbTaTiHf, from 77 to 1473 kelvin. This alloy’s behavior differed from that of comparable systems by having fracture toughness over 253 MPa·m 1/2 , which we attribute to a dynamic competition between screw and edge dislocations in controlling the plasticity at a crack tip. Whereas the glide and intersection of screw and mixed dislocations promotes strain hardening controlling uniform deformation, the coordinated slip of <111> edge dislocations with {110} and {112} glide planes prolongs nonuniform strain through formation of kink bands. These bands suppress strain hardening by reorienting microscale bands of the crystal along directions of higher resolved shear stress and continually nucleate to accommodate localized strain and distribute damage away from a crack tip.

36 MATERIALS SCIENCE↗

Role of water in fracture of modified silicate glasses

Decarbonizing the glass industry requires alternative melting technology, as current industrial melting practices rely heavily on fossil fuels. Hydrogen has been proposed as an alternative to carbon-based fuels, but the ensuing consequences on the mechanical behavior of the glass remain to be clarified. A critical distinction between hydrogen and carbon-based fuels is the increased generation of water during combustion, which raises the equilibrium solubility of water in the melt and alters the behavior of the resulting glass. A series of five silicate glasses with 80% silica and variable [Na 2 O]/([H 2 O] + [Na 2 O]) ratios were simulated using molecular dynamics to elucidate the effects of water on fracture. Several fracture toughness calculation methods were used in combination with atomistic fracture simulations to examine the effects of hydroxyl content on fracture behavior. Here, this study reveals that the crack propagation pathway is a key metric to understanding fracture toughness. Notably, the fracture propagation path favors hydrogen sites over sodium sites, offering a possible explanation of the experimentally observed effects of water on fracture properties.

36 MATERIALS SCIENCE↗

Effect of Composition on Mechanical Properties and Conductivity of the Dual-Ion Conductor Na 1+ x Mn x /2 Zr 2– x /2 (PO 4 ) 3 for Solid-State Batteries

Here we report the dependence of mechanical properties and ionic conductivity of the Na 1+ x Mn x /2 Zr 2– x /2 (PO 4 ) 3 (designated as NMZP) ionic conductor on its composition (with x = 0.5, 1.0, 1.5, and 2.0). Local mechanics was studied by instrumented nanoindentation, and the properties of interest included the elastic modulus, hardness, and fracture toughness. Overall, the material becomes more compliant and soft with the increase in the Na content. The elastic modulus reduces from 120 to 80 GPa, and nanoindentation hardness reduces from 7.8 to 4.2 GPa when x changes from 0.5 to 2.0. The relationship with fracture toughness ( K C ) is highly nonlinear: fracture toughness first decreases and then increases with the increase in the sodium content, reaching a maximum value of 0.89 MPa × m 1/2 at x = 2.0. Such a relationship was found to correlate with the formation of a glassy phase in NMZP at intermediate Na concentration. The maximum ionic conductivity coincides with the maximum fracture toughness in this material.

25 ENERGY STORAGE↗

Determination of Constraint-Independent Crack Tip Opening Angle for Stable Crack Growth in High-Strength Ductile Steels

The crack tip opening angle (CTOA) is one of fracture toughness parameters that has been used for decades in describing large stable crack growth in thin-walled aerospace structures under the low-constraint conditions. Recently, the pipeline industry has developed a growing interest in using the CTOA parameter to serve as the minimum required fracture toughness to arrest dynamic crack propagation in modern gas transmission pipelines made of high-strength ductile steel. To meet this industrial need, the CTOA test standard ASTM E3039 was therefore developed for measuring the constant critical CTOA. ASTM E3039 recommends a drop weight tearing test (DWTT) specimen with a shallow crack for standard CTOA testing, but its CTOA may depend on the low constraint condition of the DWTT specimen at the crack tip. Verifying the constraint independence of the DWTT-measured CTOA thus becomes indispensable for applying CTOA toughness to the running fracture control in the pipeline design. For this purpose, the present paper evaluates critical CTOA values in a set of fracture toughness tests on single-edge notched bend (SENB) specimens with shallow and deep cracks, based on four CTOA estimation models. Among these, the Ln(P)-LLD linear fit model is similar to that recommended by ASTM E3039 for CTOA calculation. Fracture test data for X80 pipeline steel and HY80 structural steel were considered in the CTOA evaluation. The results showed that the four CTOA models were able to determine a constraint independent CTOA value for stable crack growth in the SENB specimens. As a result, a single, reliable, constant CTOA value could be determined regardless of the specimen geometry or the crack-tip constraint conditions. Therefore, the CTOA measured using ASTM E3039 is constraint-independent and transferable to use in cases of actual cracks propagating in gas transmission pipelines.

36 MATERIALS SCIENCE↗

LDRD 22A1059-068FP Tailoring the Properties of Multi-Phase Materials Through the Use of Correlative Microscopy and Machine Learning - Poster

High strength alloys with good ductility, hardness, and toughness are needed to meet stringent design requirements for extreme environments. One complication in this pursuit is the evidence that metals rarely exhibit both high strength and good fracture toughness as the underlying mechanisms work in opposition. An exception to this behavior is found in multiphase alloys that form complex microstructures of mixed phases with variable grain sizes and shapes that provide increased fracture toughness by the arrangement of their constituent elements. We propose to explore this phenomenon using state-of-the-art machine learning (ML) techniques in a new and novel manner to identify and correlate the critical microstructural features in a Titanium-10Vanadium-2Iron-3Aluminum (Ti-10V-2Fe-3Al) alloy that is reported to exhibit high strength and fracture toughness. Additionally, we will employ multiple, complementary characterization techniques such as optical microscopy, electron backscatter diffraction (EBSD), energy dispersive spectroscopy (EDS) and scanning electron microscopy to provide multi-layer, quantitative ground truth measures of the microstructures. This data will be used to train a Convolutional Neural Network (CNN) in a semi-supervised environment to identify key microstructural features such as ? platelet dimensions and locations and ?/? phase boundaries and correlate those features with the strength and toughness. Here the ? and ? nomenclature refers to hexagonal close pack (hcp) and body center cubic (bcc) crystal structures, respectively. Previous work has focused on popular alloys and typically used one characterization technique. This research is focused on a promising titanium alloy, uses multiple complimentary characterization tools to provide precise microstructural information and correlates to improved fracture toughness. The resulting ML tool can be trained for additional microstructural features, different alloy(s), and or target mechanical properties.

36 MATERIALS SCIENCE↗

Preparation, mechanical properties, and toughening mechanisms of SiCw/SiCp‐reinforced zirconia‐toughened alumina ceramics

ABSTRACT Zirconia‐toughened alumina (ZTA) ceramics with high mechanical properties were sintered by hot‐pressing method using SiC particles (SiCp) and SiC whiskers (SiCw) as the reinforcing agents simultaneously. The influences of sintering temperature, SiCp, and SiCw contents on the microstructure and mechanical properties of ZTA ceramics were investigated. It was found that both SiCp and SiCw could contribute to grain refinement significantly and promote the mechanical properties of the ceramics. However, the excess addition of SiCp or SiCw led to the formation of pores with large sizes and degraded the mechanical properties instead. When 13 wt% SiCp was introduced, the maximum flexural strength of 1180.0 MPa and fracture toughness of 15.9 MPa·m 1/2 were obtained, whereas the maximum flexural strength of 1314.0 MPa and fracture toughness of 14.7 MPa·m 1/2 were achieved at 20 wt% SiCw. Interestingly, the simultaneous addition of SiCp and SiCw could further improve the mechanical properties, and the highest flexural strength of 1334.0 MPa and fracture toughness of 16.0 MPa·m 1/2 were achieved at a SiCw/SiCp ratio of 16/4. The reinforcement mechanisms in the ceramics mainly included the phase transformation toughening of ZrO 2 , the crack deflection and bridging of SiCp and SiCw, and the pull‐out of SiCw.

Liu, Longyang↗

J-integral measured from experimental torque load versus torque-ends rotation angle obtained from a spiral notch torsion test

In this work, Spiral Notch Torsion Test (SNTT) was developed to measure the intrinsic fracture toughness of structural materials using small specimens. The SNTT system operates by applying pure torsion to cylindrical specimens with a notch line that spirals around the specimen at a 45° pitch. 3-D finite-element analysis has been used to estimate the fracture toughness obtained from SNTT test specimen with 3-D non-coplanar crack front. Furthermore, here a newly developed SNTT protocol to estimate J-integral directly from the experimental torque load versus torque-ends rotation angle trend curve without the aid of 3-D finite element analyses is presented and its applicability is illustrated by applying it for the evaluation of fracture toughness of SS304/308 weldment. The estimated JQ’ for the SS304/308 weld is 144.2 kJ/m2, which is consistent with that obtained from CT specimen.

36 MATERIALS SCIENCE↗

Thermomechanical Processing for Improved Mechanical Properties of HT9 Steels

Thermomechanical processing (TMP) of ferritic–martensitic (FM) steels, such as HT9 (Fe–12Cr–1MoWV) steels, involves normalizing, quenching, and tempering to create a microstructure of fine ferritic/martensitic laths with carbide precipitates. HT9 steels are used in fast reactor core components due to their high-temperature strength and resistance to irradiation damage. However, traditional TMP methods for these steels often result in performance limitations under irradiation, including embrittlement at low temperatures (<~430 °C), insufficient strength and toughness at higher temperatures (>500 °C), and void swelling after high-dose irradiation (>200 dpa). This research aimed to enhance both fracture toughness and strength at high temperatures by creating a quenched and tempered martensitic structure with ultrafine laths and precipitates through rapid quenching and unconventional tempering. Mechanical testing revealed significant variations in strength and fracture toughness depending on the processing route, particularly the tempering conditions. Tailored TMP approaches, combining rapid quenching with limited tempering, elevated strength to levels comparable to nano-oxide strengthened ferritic alloys while preserving fracture toughness. For optimal properties in high-Cr steels for future reactor applications, this study recommends a modified tempering treatment, i.e., post-quench annealing at 500 °C or 600 °C for 1 h, possibly followed by a brief tempering at a slightly higher temperature.

36 MATERIALS SCIENCE↗

Mechanical testing of PH13-8Mo H950 Steel for Xue-Wierzbicki Fracture Criterion Determination at 20° C and -40° C

Mechanical testing was conducted to collect the data needed to build a Xue-Wierzbicki (XW) fracture model for PH13-8 Mo H950 stainless steel (PH 13-8 SS). This model is intended for use in structural analysis of this material between room temperature and -40° C. Tests were performed on four different specimen geometries such that a range of stress states were characterized at room temperature and -40° C. Tensile tests on R5 tensile specimens were also performed to assess material anisotropy. Fracture toughness test were also conducted. The fracture toughness of this material at -40° C was 68% of the room-temperature value. Material strength generally increased with decreasing temperature while the opposite trend was observed for ductility. These trends were most pronounced for specimens with the largest stress triaxialities.

36 MATERIALS SCIENCE↗

Effects of secondary void-initiating particles on the steady-state crack growth resistance of high-strength steel

In this investigation, we focus on the dependence of stable crack growth resistance, as measured by the short-rod fracture toughness test, on secondary void-initiating particles such as AlN and Ti-based grain-refining precipitates in a variety of high-strength steels with tempered martensitic microstructures. The model developed by Ritchie and Thompson is modified to illustrate the significant amounts of toughening that can result from the refinement of secondary particles. Analysis of the data suggests that material strength is a predominant factor in increasing the short-rod fracture toughness relative to linear-elastic measures of initiation fracture toughness, but the extent of toughening is limited by the size and number density of secondary particles in the microstructure. The variation in estimates of secondary microvoid initiation and growth strains with precipitate size reinforce the notion that primary fracture at non-metallic inclusions and secondary fracture at smaller particles occur as sequential processes with a degree of concurrence that is dependent on the state of precipitation in both particle dispersions. Toughening in this connection is maximized by increases in microvoid growth strain that result from decreases in the size and areal number density of secondary void-initiating particles. Finally, the occurrence of transient instabilities during crack extension in short-rod specimens is explained with a phenomenological model that relates crack growth stability to natural variations in the dispersion of secondary void-initiating particles in the microstructure.

42 ENGINEERING↗

Reactive flash sintering and characterization of bulk high entropy nitrides

Over the past decade, numerous high-entropy ceramics have been synthesized, often displaying attractive properties. However, the study on facile preparation of bulk high entropy nitrides (HEN) are limited, despite its broad potential applications. This research demonstrates for the first time rapid fabrication (within ∼6 min) of bulk high-entropy nitrides, especially (Al 0.17 Nb 0.17 Ta 0.17 Ti 0.32 Zr 0.17 )N, from binary nitride powder mixtures using a highly efficient reactive flash sintering (RFS) technique. X-ray diffraction (XRD) shows the HENs from RFS are near single-phase solid solutions with a rock salt crystal structure, while in situ synchrotron study carried out during RFS captured in real time the formation of HEN, which was preserved upon cooling, suggesting thermodynamic stability of the HEN phase, even up to extreme pressure (∼35.6 GPa). Microscopic analyses using SEM, STEM, and EDS reveal decent uniformity for HEN with no obvious segregation of elements, even to submicron scale. Some properties of the obtained bulk HENs are consistent with expectations. For example, their hardness and bulk modulus are close to estimates based on rule-of-mixture (ROM) values from the constituent binary nitrides. Meanwhile, some other measured properties seem to show surprises. For example, the fracture toughness for the HENs (e.g., 7.81 ± 1.40 MPa•m 1/2 or higher) turns out to be more than double of the expected ROM estimates. The significantly improved fracture toughness is attributed to the observed nano-layered structure of the HENs, despite the HEN’s cubic crystal structure and high hardness. In addition, the oxidation resistance shows improvement up till ∼800°C, possibly due to Ta doping that suppress oxygen vacancy formation in the oxide shell, while the 5-metal HEN of (Al 0.17 Nb 0.17 Ta 0.17 Ti 0.32 Zr 0.17 )N displays superconductivity (T c of ∼5–7 K from magnetism and resistivity measurements, slightly lower than ROM estimate), despite insulating property of starting AlN. Furthermore, future study combining experimental investigation using larger samples to confirm the observed increase in fracture toughness and oxidation resistance, theoretical modeling at different length scale, and more detailed structural/chemical characterization, especially at the atomic scale, are all needed to fully understand the inter-relationships between composition, processing, structure, and novel properties for these HENs and the development of related new materials for different applications.

Flash sintering↗