An Artificial Protective Coating toward Dendrite-Free Lithium-Metal Anodes for Lithium–Sulfur Batteries
Not provided.
SEARCH · Engineering Papers
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Not provided.
Alkali metals are regarded as the most promising candidates for advanced anode for the next-generation batteries due to their high specific capacity, low electrochemical potential, and lightweight. However, critical problems of the alkali metal anodes, especially dendrite formation and interface stabilization, remain challenging to overcome. The solid electrolyte interphase (SEI) is a key factor affecting Li and Na deposition behavior and electrochemical performances. Herein, a facile and universal approach is successfully developed to fabricate ionic conductive interfaces for Li and Na metal anodes by modified atomic layer deposition (ALD). In this process, the Li metal (or Na metal) plays the role of Li (or Na) source without any additional Li (or Na) precursor during ALD. Moreover, the key questions about the influence of ALD deposition temperature on the compositions and structure of the coatings are addressed. The optimized ionic conductive coatings have significantly improved the electrochemical performances. In addition, the electrochemical phase-field model is performed to prove that the ionic conductive coating is very effective in promoting uniform electrodeposition. Further, this approach is universal and can be potentially applied to other different metal anodes. At the same time, it can be extended to other types of coatings or other deposition techniques.
Silicon-anode lithium-ion batteries (LIBs) suffer from limited cycle life and poor calendar life, constraining their large-scale commercialization. Integrating additives into electrolytes is a simple and cost-effective strategy to improve these aspects. The effects of lithium-free boron-based additives on cycling and calendar performance of high-loading Si-anode LIBs remain largely unexplored. In this work, the influence of five Li-free borate additives, each with distinct molecular structures and elemental compositions, is systematically investigated. All additives enhance cycle life to varying extents. Notably, the addition of 1 v/v% tri(2,2,2-trifluoroethyl) borate to the baseline electrolyte nearly doubles the cycle life at 50% state of health. This enhancement is attributed to three key factors. Specifically, borate additives 1) improve electrochemical activity, 2) act as anion receptors that interact with [PF6]- anions and carbonate solvents to reduce electrolyte decomposition, and 3) promote the formation of a stable and polymeric solid electrolyte interphase layer. Furthermore, these additives exhibited negligible impact in mitigating leakage current during a 180 h voltage-hold calendar-aging test, indicating their limited effect in calendar life. These findings provide insight into the role of Li-free borate additives in improving cycle life while addressing the knowledge gap regarding their influence on calendar aging.
Abstract Lithium dendrite growth is one of the most challenging problems affecting the safety performance of lithium‐ion batteries (LIBs). It causes low Coulombic efficiency as well as safety hazards for LIBs. Understanding the evolution process of Li‐dendrite growth at the nanoscale is critical for solving this problem. Herein, an in situ electrochemical atomic force microscopy (EC‐AFM) investigation of the initial Li deposition in ethylene carbonate (EC)‐based and fluoroethylene carbonate (FEC)‐based electrolytes on graphite anodes is reported. These results show that the solid electrolyte interphase (SEI) formed from the FEC‐based electrolyte can suppress Li‐dendrite growth. The FEC‐based electrolyte induces formation of LiF‐rich SEI films, which are harder and denser than those formed in an EC‐based electrolyte. Due to its better mechanical properties and larger resistance, the SEI layer formed from the FEC‐based electrolyte is sufficient to prevent reduction of Li + ions and deposition of Li + ions on the anode surface. These results demonstrate that EC‐AFM is a powerful in situ technique for the study of lithium‐dendrite growth.
Sodium metal batteries (SMBs) hold great promise for the development of high-energy, sustainable energy storage solutions, but their practical deployment is hampered by unstable solid electrolyte interphases, uncontrollable sodium dendrite growth, and low Coulombic efficiency (CE) during repeated Na plating/stripping cycles. To address these challenges, we introduce an organic interlayer, containing perylenetetracarboxylic dianhydride sodium salt (Na4PT), on the surface of Cu current collector. This interlayer forms a sodiophilic organic interphase that lowers the nucleation barriers for sodium deposition and guides the formation of the interphase through polar carbonyl/carboxylate sites and a π-conjugated organic framework. A dendrite-free sodium metal anode is achieved using Na4PT coated Cu current collector. Under capacity-limited Na plating/stripping, Na||Na4PT@Cu half-cells deliver reversible capacities of 500 and 1,000 mAh g−1 at 0.1 and 1 A g−1 for 500 cycles with average CE above 99%. Post-cycling scanning electron microscopy and X-ray photoelectron spectroscopy measurements confirm that Na4PT@Cu promotes compact and uniform Na deposits and supports the formation of a stable interphase with reduced parasitic decomposition, directly correlating interfacial chemistry/morphology with high plating/stripping reversibility. These results highlight organic carboxylate coating as a practical interface engineering strategy for dendrite-free SMBs.
Rechargeable lithium-ion batteries are the most popular devices for energy storage but still a lot of research needs to be done to improve their cycling and storage capacity. Silicon has been proposed as an anode material because of its large theoretical capacity of ~3600 mAh/g. Therefore, focus is needed on the lithiation process of silicon anodes where it is known that the anode increases its volume more than 300%, producing cracking and other damages. In this study, we performed molecular dynamics atomistic simulations to study the swelling, alloying, and amorphization of a silicon nanocrystal anode in a full nanobattery model during the first charging cycle. A dissolved salt of lithium hexafluorophosphate in ethylene carbonate was chosen as the electrolyte solution and lithium cobalt oxide as cathode. External electric fields are applied to emulate the charging, causing the migration of the Li-ions from the cathode to the anode, by drifting through the electrolyte solution, thus converting pristine Si gradually into Li 14 Si 5 when fully lithiated. When the electric field is applied to the nanobattery, the temperature never exceeds 360 K due to a temperature control imposed resembling a cooling mechanism. The volume of the anode increases with the amorphization of the silicon as the external field is applied by creating a layer of LiSi alloy between the electrolyte and the silicon nanocrystal and then, at the arrival of more Li-ions changing to an alloy, where the drift velocity of Li-ions is greater than the velocity in the initial nanocrystal structure. Charge neutrality is maintained by concerted complementary reduction-oxidation reactions at the anode and cathode, respectively. Also, the nanobattery model developed here can be used to study charge mobility, current density, conductance and resistivity, among several other properties of several candidate materials for rechargeable batteries and constitutes the initial point for further studies on the formation of the solid electrolyte interphase in the anode.
As the demand for higher-performance batteries has increased, so has the body of research on theoretical high-capacity anode materials. However, the research has been hindered because the high-capacity anode material properties and interactions are not well understood, largely due to the difficulty of observing cycling in situ. Using electrochemical scanning transmission electron microscopy (ec-STEM), we report the real-time observation and electrochemical analysis of pristine tin (Sn) and titanium dioxide-coated Sn (TiO 2 @Sn) electrodes during lithiation/delithiation. As expected, we observed a volume expansion of the pristine Sn electrodes during lithiation, but we further observed that the expansion was followed by Sn detachment from the current collector. Remarkably, although the TiO 2 @Sn electrodes also exhibited similar volume expansion during lithiation, they showed no evidence of Sn detachment. We found that the TiO 2 surface layer acted as an electrochemically activated artificial solid-electrolyte interphase that serves to conduct Li ions. As a physical coating, it mechanically prevented Sn detachment following volume changes during cycling, providing significant degradation resistance and 80% Coulombic efficiency for a complete lithiation/delithiation cycle. Interestingly, upon delithiation, TiO 2 @Sn electrode displayed a self-healing mechanism of small pore formation in the Sn particle followed by agglomeration into several larger pores as delithiation continued.
Deviation between thermodynamic and experimental voltages is one of the key issues in Li-ion conversion-type electrode materials; the factor that affects this phenomenon has not been understood well in spite of its importance. In this work, we combine first principles calculations and electrochemical experiments with characterization tools to probe the conversion reaction voltage of transition metal difluorides MF2 (M = Fe, Ni, and Cu). We find that the conversion reaction voltage is heavily dependent on the size of the metal nanoparticles generated. The surface energy of metal nanoparticles appears to penalize the reaction energy, which results in a lower voltage compared to the thermodynamic voltage of a bulk-phase reaction. Furthermore, we develop a reversible CuF2 electrode coated with NiO. Electron energy loss spectroscopy (EELS) elemental maps demonstrate that the lithiation process mostly occurs in the area of high NiO content. This suggests that NiO can be considered a suitable artificial solid electrolyte interphase that prevents direct contact between Cu nanoparticles and the electrolyte. Thus, it alleviates Cu dissolution into the electrolyte and improves the reversibility of CuF2.
This study investigates the impacts of applying different thermal gradient patterns to cylindrical lithium-ion cells in a module on cell dynamics (temperatures, current flows, state of charge), module performance (evolution of resistance, capacity, and energy versus cycle number), and module lifetime. The thermal gradients were generated using cooling plates (CPs) with three different flow-field designs, namely, straight, perpendicular, and U-turn. The study uses computational fluid dynamics (CFD), the pseudo-two-dimensional (P2D) battery model, capacity loss and increased impedance due to the growth of a solid-electrolyte-interphase, and the electric current distribution from module terminals to cells that depends on the series-parallel electrical connections among the cells. The impact of the thermal gradient (resulting from the CP designs) on the variability in resistance, current, state of charge, and voltage among the cells was analyzed and linked to differences in the module's performance. Applying a thermal gradient to parallel-connected strings of series-connected cells led to variation in the current through each parallel string and an imbalance in the voltage of series-connected cells. Module performance is poorer when the thermal gradient causes a voltage imbalance than when it causes a current imbalance. Module performance becomes the worst when both current variation and voltage imbalance happen together. For instance, the module's lifetime (estimated as reaching 80% of its initial capacity) varied by 5% to 17.5%, depending on the magnitude and pattern of the imposed thermal gradient. As the relative orientation between thermal gradients and cells' electrical connectivity influences the module's performance, appropriate consideration should be given to the choice of the CP, especially if large thermal gradients are allowed.
Behind-the-meter storage (BTMS) systems - a viable method to minimize potential risk of blackout events and stabilize the grid - require a different type of cost-effective energy storage with excellent safety, ultra-long (>20 years) cycle life and reasonable energy density compared that of electric vehicles. To increase the energy density and reduce the cost of a long-term cyclable lithium-titanate-based cell, it is required to employ a critical-material-free high voltage cathode and an electrolyte with good electrochemical and transport properties. In this report the long-term electrochemical performance and behaviors of selected critical-material-free Li 4 Ti 5 O 12 (LTO)//LiNi 0.9 Mn 0.1 O 2 (LNMO) full cells for BTMS applications are evaluated and analyzed in the optimized voltage range of 1.4-2.7 V at 45 degrees C with different fluorinated carbonate-based electrolytes. The fluoroethylene carbonate (FEC)-based electrolyte cell shows the highest capacity retention of 57.9% and Coulombic efficiency (CE) of 99.96% after 1000 cycles, potentially attributed to a dense, homogenous and less resistive LiF-rich solid-electrolyte interphase (SEI) layer formed on the surface of LTO that may mitigate electrolyte decomposition and maintain relatively low cell impedance during cycling. The 3,3,3-fluoroethylmethyl carbonate (F-EMC)-based electrolyte cell, however, presents the worst performance with lower capacity and a sharp decrease of CE, due to unstable and non-uniform SEI formation and continuous oxidative electrolyte decomposition. This mechanistic understanding of cell aging behaviors and failure mechanisms with detailed analysis of surface chemistry and electrode morphology can guide design of new electrode chemistries and electrolyte formulations for the development of BTMS batteries.
Silicon carbon (Si/C) materials are promising anode candidates for high performance lithium ion batteries (LIBs). However, serious volume expansion and solid electrolyte interface formation limited their actual capacity during lithiation and delithiation. In the present study, an innovative and low-cost synthetic approach was developed for synthesizing carbon-rich silicon-containing polymer-derived ceramics from poly(dimethylsilyene)diacetylenes (PDSDA) and its feasibility to be used as anodes was demonstrated. The attained PDCs@800 °C exhibited a high specific capacity upto 883 mAhg -1 at 400 mAg -1 , with >99% coulombic efficiency (CE), and 90% capacity retention even after 500 cycles, setting a new record for PDCanode materials in LIBs. The high specific capacity was attributed to the incessant Si/C network which delivered consistent conductance and a stable solid electrolyte interphase (SEI). Here, this study opens the door to explore and apply well-designed ceramic materials derived from tailored polymers as high performance anodes for lithium ion batteries.
Recycling processes for lithium-ion batteries typically overlook graphite because of its lower market value relative to that of transition-metal-containing cathode materials. However, graphite recovered from cycled lithium-ion batteries holds additional engineered value associated with the solid-electrolyte interphase (SEI). The SEI contributes critical electronic passivation of the graphite surface but becomes highly resistive with extended cycling, yielding poor cell performance. In this work, we apply tailored solvent treatment to end-of-life (EOL) graphite anodes to selectively remove adverse SEI components while retaining beneficially passivating species. We evaluate a series of polar protic solvents to achieve targeted removal of SEI components and control selectivity through rational variation in solvent properties. The physiochemical properties of treatment solvents correlate with both the retained SEI composition and the corresponding electrochemical performance of solvent-treated “upcycled” graphite anodes. Within the initial set of solvents evaluated, top-performing candidates show capacity and Coulombic efficiency nearly equivalent to those of an analogous pristine anode, as well as promising electrochemical performance enhancement with regard to irreversible capacity-loss metrics. This study establishes critical design principles for an optimized anode upcycling method that enhances the value of recycled graphite by retaining and upgrading the SEI.
The unstable and fragile solid electrolyte interphase (SEI) has restricted the application of Na metal anodes. Despite numerous research efforts being put into understanding its chemical composition and physical properties, direct observation of its formation remains a challenge due to the lack of temporal and spatial resolution. Here, through combined in situ probing techniques, we exhibit two pivotal stages associated with SEI instability during the often -neglected formation process. It is revealed that Na metal that is not uniformly passivated at the initial (passivating) stage will trigger unrestricted electrolyte decomposition and homogeneous components distribution during the subsequent (growing) stage. SEI with homogenously distributed components is found to have higher solubility than that with a layered structure evolved from a compact passivation layer. Furthermore, through demonstrating an SEI dissolution model that is closely related to its formation process and compositional distribution, this work sheds light on an uncharted territory of Na metal batteries.
Cu2Sb thin films prepared by magnetron sputtering are evaluated as an anode material for Na-ion batteries. The starting material is composed of nanocrystallites with the desired tetragonal P4/nmm structure. The study of the reaction mechanism reveals the formation of an amorphous/nanocrystalline phase of composition close to Na3Sb as the final reaction product. The solid electrolyte interphase (SEI) material is mostly composed of carbonates (Na2CO3, NaCO3R). The Cu2Sb anode possesses moderate capacity retention with a reversible storage capacity (250 mAh/g) close to the theoretical value (323 mAh/g), an average reaction potential of around 0.55 V vs. Na/Na+, and a high rate performance (10 C-rate).
The use of blended silicon-graphite (Si-Gr) negative electrodes increases the energy density of lithium-ion cells over those containing only graphite (Gr) electrodes. However, volume changes in the Si particles that occur during cycling causes deterioration of the solid-electrolyte interphase (SEI) layer on the particles resulting in further electrolyte reduction that immobilizes Li+ ions and, therefore, capacity fade. Because the volume changes are not expected to occur during a potentiostatic hold (referred to as calendar-life aging), by comparison of cycle-life and calendar-life aged cells one can expect to assess the role of volume changes in the deterioration of cell performance. To this end, cells with Si-Gr and Gr negative electrodes (and Li 1.03 (Ni 0.5 Co 0.2 Mn 0.3 ) 0.97 O 2 containing positive electrodes) were assembled, tested, and compared using cycle-life and calendar-life aging protocols. As expected, the capacity loss of the cycle-life aged cells was higher than that of the calendar-life aged cells. However, the measurable capacity loss for the calendar-life aged cells indicated continued immobilization of Li + ions. Furthermore, electrolytes extracted from the calendar-life aged cells showed more LiPF 6 hydrolysis products than those extracted from the cycle-life aged cells. In conclusion, we discuss possible mechanistic causes for the observed aging behaviors in this article.
In solid-state lithium (Li)-metal batteries (SSLMBs), sulfide-based Li-ion conductors represent one of the most popular solid electrolytes (SEs). However, the development of sulfide-based SSLMBs is significantly hampered by interfacial issues including large solid-solid contact resistance and serious side reactions at the SE/electrode interface. To address these issues, here, we demonstrated a simple and efficient strategy by using LiCl-rich argyrodite Li 6 PS 5 Cl (Li 6 PS 5 Cl-LiCl) SE and trace amount of propylene carbonate (PC) at the SE/electrode interface to facilitate the formation of stable and robust solid electrolyte interphase (SEI). Additionally, the formed SEI not only serves as a buffer layer to passivate the interfacial reactions and suppress Li dendrite growth, but also acts as a bridge for Li-ion conduction to reduce the contact resistance. As a result, the Li||Li symmetric cell exhibited long-term electrochemical cycling stability over 1000 h at a current density of 0.2 mA cm -2 . Furthermore, the assembled Li||Li 4 Ti 5 O 12 (LTO) batteries delivered a specific capacity of 175 mAh g–1 at 0.2 C, and remained an excellent specific capacity of 116 mAh g –1 after 200 cycles at a high current rate of 1 C. These features indicate a feasible strategy to enhance the interfacial property of high-performance SSLMBs.