Effects of Geometric Discontinuities on Creep Behavior of Alloy 617
Due to the excellent long-term high-temperature performance of Alloy 617, the Alloy has been identified as the primary structural material for the intermediate heat exchanger of the Very High Temperature Reactor (VHTR). Both the base and welded alloy has been qualified to be used up to 950 °C up to 100,000 hours by the American Society of Mechanical Engineer (ASME) Boiler and Pressure Vessel Code (BPVC). The qualification properties of the material were exclusively determined by uniaxial creep tests. The components may, however, experience multiaxial stress conditions in service due to the reactor geometry. This study used notched creep tests to investigate the effect of geometric discontinuities on creep behavior of both the base and welded Alloy 617. The V-notch tests reveal that the geometric discontinuities do not reduce the creep rupture live under high and intermediate stress conditions. The U-notch tests show that a larger radius notch behave in a similar way as a straight gauge section of a uniaxial test. The creep rupture live of the welded alloy was slightly longer than the base metal.