Steam Oxidation Testing in the Severe Accident Test Station

Since 2011, Oak Ridge National Laboratory (ORNL) has been conducting high temperature steam oxidation testing of candidate alloys for accident tolerant fuel (ATF) cladding. These concepts are designed to enhance safety margins in light water reactors (LWR) during severe accident scenarios. In the US ATF community, the Severe Accident Test Station (SATS) has been evaluating candidate materials (including coatings) since 2012. Compared to the current UO 2 /Zr-based alloy fuel system, alternative cladding materials need to offer slower oxidation kinetics and a smaller enthalpy of oxidation in order to significantly reduce the rate of heat and hydrogen generation in the core during a coolant-limited severe accident. The steam oxidation behavior of candidate materials is a key metric in the evaluation of ATF concepts and also an important input into models. However, prior modeling work of FeCrAl cladding has used incomplete information on the physical properties of FeCrAl. Also, the steam oxidation data being collected at 1200°-1700°C is unique as no prior work has considered steam oxidation of alloys at such high temperatures. In some cases, the results have been difficult to interpret and more fundamental information is needed such as the stability of alumina in flowing steam at 1400°-1500°C. This report summarizes recent work to measure the steam oxidation kinetics of candidate alloys, the evaporation rate of alumina in steam and the development of integral data on FeCrAl compared to conventional Zr-based cladding.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Synthesis and characterization of (Ga 1-x Zn x )(N 1-x O x ) nanocrystals with a wide range of compositions

We describe the synthesis and characterization of wurtzite (Ga 1-x Zn x )(N 1-x O x ) nanocrystals with a wide range of compositions and a focus on properties relevant for solar fuel generation. (Ga 1-x Zn x )(N 1-x O x ), a solid solution of GaN and ZnO, is an intriguing material because it exhibits composition-dependent visible absorption even though the parent semiconductors absorb in the UV. When functionalized with co-catalysts, (Ga 1-x Zn x )(N 1-x O x ) is also capable of water splitting under visible irradiation. Here, we examine the synthesis of (Ga 1-x Zn x )(N 1-x O x ) nanocrystals to understand how they form by nitridation of ZnO and ZnGa 2 O 4 nanocrystalline precursors. We find that the ZnO precursor is critical for the formation of crystalline (Ga 1-x Zn x )(N 1-x O x ) at 650 °C, consistent with a mechanism in which wurtzite (Ga 1-x Zn x )(N 1-x O x ) nucleates topotactically on wurtzite ZnO at an interface with ZnGa 2 O 4 . Using this information, we expand the range of compositions from previously reported 0.30 ≤ x ≤ 0.87 to include the low-x and high-x ends of the range. The resulting compositions, 0.06 ≤ x ≤ 0.98, constitute the widest range of (Ga 1-x Zn x )(N 1-x O x ) compositions obtained by one synthetic method. We then examine how the band gap depends on sample composition and find a minimum of 2.25 eV at x = 0.87, corresponding to a maximum possible solar-to-H 2 power conversion efficiency of 12%. Finally, we examine the photoelectrochemical (PEC) oxidation behavior of thick films of (Ga 1-x Zn x )(N 1-x O x ) nanocrystals with x = 0.40, 0.52, and 0.87 under visible illumination. (Ga 1-x Zn x )(N 1-x O x ) nanocrystals with x = 0.40 exhibit solar PEC oxidation activity that, while too low for practical applications, is higher than that of bulk (Ga 1-x Zn x )(N 1-x O x ) of the same composition. The highest photocurrents are observed at x = 0.52, even though x = 0.87 absorbs more visible light, illustrating that the observed photocurrents are a result of an interplay of multiple parameters which remain to be elucidated. This set of characterizations provides information useful for future studies of composition-dependent PEC properties of nanoscale (Ga 1-x Zn x )(N 1-x O x ).

36 MATERIALS SCIENCE↗

Improved bond coatings for use with thermal barrier coatings

The potential for improving the durability of thermal barrier coatings (TBC's) being developed for coal derived fuel fired gas turbines was studied. Furnace oxidation behavior of plasma deposited bond coatings was improved by increasing the thickness from 0.010 cm to 0.015 cm and by depositing the coatings at 20 kW with argon 3.5 vol % hydrogen arc gas rather than at 11 kW with argon. The most oxidation resistant plasma deposited bond coatings were Ni-14, 1Cr-13.4Al-0.10Zr, Ni-14.3Cr-14.4Al.0.16Y, and Ni-15.8Cr-12.8Al-0.36Y on B-1900 + Hf and Ni-30.9Cr-11.1Al-0.48Y on MAR-M-509. The oxidation resistant bond coatings improved TBC life when the coatings were deposited on the specimens supported on a nail bed fixture during coating.

Gedwill, M. A.↗

Oxidation of biogenic U(IV) mediated by iron-bearing clay minerals, iron-reducing bacteria, and organic ligands

Bioreduction of hexavalent uranium (U(VI)) to tetravalent uranium (U(IV)) by dissimilatory metal-reducing bacteria (DMRB) is considered an effective strategy for uranium immobilization in contaminated environments. However, U(IV) can be reoxidized to U(VI) under fluctuating redox conditions and remobilized. This work investigates the oxidation behavior of biogenic U(IV) in the presence of bioreduced iron-bearing clay minerals (rNAu-2), iron-reducing bacteria (Shewanella putrefaciens CN32), and organic ligands (ethylenediaminetetraacetic acid (EDTA) and citrate). Results demonstrate that the presence of CN32 significantly inhibits U(IV) oxidation. rNAu-2 exerted a context-dependent influence on U(IV) oxidation: its effect was masked by bicarbonate-promoted U(VI) mobilization in the absence of active CN32, but became detectable when CN32-mediated microbial protection slowed U(IV) oxidation. EDTA and citrate markedly accelerate U(IV) oxidation via formation of soluble U(IV)-ligand complexes, changing U(IV) redox potentials, and by promoting clay mineral dissolution that enhances Fe(II)/Fe(III) redox cycling. Collectively, our findings constrain the roles that clay minerals, iron-reducing bacteria, and organic ligands play in governing U(IV) stability, emphasizing the need to account for these factors in developing robust bioremediation strategies.

38 RADIATION CHEMISTRY, RADIOCHEMISTRY, AND NUCLEA↗

Oxidation kinetics of SPS-densified U 3 Si 2 fuels—Microstructure impact

Here, U 3 Si 2 is a potential candidate for accident tolerant fuels because of its high uranium density and excellent thermal conductivity in comparison to UO 2 . However, U 3 Si 2 suffers from oxidation, steam corrosion, and subsequent disintegration/pulverization. The detailed investigation of kinetics that incorporates fundamental treatment of oxidation of U 3 Si 2 is scarcely reported, and the oxidation mechanisms have not been fully elucidated. In this paper, the oxidation behavior of microcrystalline (mc - ) and nanocrystalline (nc - ) U 3 Si 2 have been systematically investigated using a thermogravimetric analysis (TGA) apparatus through a series of isothermal and non-isothermal kinetic studies. The isothermal kinetic study with a model-fitting approach indicates oxidation activation energy of 85 kJ/mol for dense mc - U 3 Si 2 and 96.4 kJ/mol for nc - U 3 Si 2 pellets, while the isoconversional approach leads to an activation energy in the range of 70–85 kJ/mol for mc - U 3 Si 2 and 75–86 kJ/mol for nc - U 3 Si 2 with three most common model-free methods, including Kissinger–Akahira–Sunose, Flynn–Wall–Ozawa, and Friedman methods. The derivation of oxidation activation energies using both isothermal and isoconversional methods highlights the approach to evaluate the oxidation resistance of nuclear materials using TGA quantitatively and makes it possible to compare among various nuclear fuels.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Elucidating the impact of stress states on grain boundary passivation in Ni-5Cr using the Rhines pack method

The oxidation behavior of a Ni–5Cr (at.%) alloy was evaluated at 420 ° C using the Rhines pack method and simultaneous tensile and compressive stress states via a miniature four-point bending fixture. At this moderate temperature, grain boundaries dominate mass transport and the resulting oxidation response. Oxidation produced approximately 1μ⁢m-wide protective Cr 2 O 3 films capping some grain boundaries and penetrative, intergranular Cr-rich oxides at other grain boundaries. Externally applied tensile and compressive stress during oxidation increased the prevalence of Cr 2 O 3 cap formation compared to no applied stress, with tensile stress resulting in more Cr 2 O 3 caps than compressive stress. The observed oxide cap morphology was similar across all test conditions. Regions under compressive stress showed an order of magnitude greater Cr depletion depth along the grain boundary. Chromium nitrides (CrN), likely from N contamination of the Rhines pack cell, were observed both at the oxide–metal interface and intergranularly within the alloy. Collectively these results demonstrate that applied stress promotes localized protective oxide cap formation over grain boundaries, with compressive stress additionally promoting deeper Cr depletion. Furthermore the experimental approach helped separate out the effects of stress on local oxide formation and grain boundary passivation.

4 point bend↗

Oxidation of ZrB2-SiC

In this paper the oxidation behavior of ZrB2-20 vol% SiC is examined. Samples were exposed in stagnant air in a zirconia furnace (Deltech, Inc.) at temperatures of 1327, 1627, and 1927 C for ten ten-minute cycles. Samples were removed from the furnace after one, five, and ten cycles. Oxidized material was characterized by mass change when possible, x-ray diffraction (XRD), scanning electron microscopy (SEM), and energy dispersive spectroscopy (EDS). Oxidation kinetics, oxide scale development, and matrix recession were monitored as a function of time and temperature. Oxidation and recession rates of ZrB2 - 20 vol% SiC were adequately modeled by parabolic kinetics. Oxidation rates of this material are rapid, allowing only very short-term application in air or other high oxygen partial pressure environments.

Opila, Elizabeth J.↗

Development of Oxidation Protection Coatings for Gamma Titanium Aluminide Alloys

Metallic material systems play a key role in meeting the stringent weight and durability requirements for reusable launch vehicle (RLV) airframe hot structures. Gamma titanium aluminides (gamma-TiAl) have been identified as high-payoff materials for high-temperature applications. The low density and good elevated temperature mechanical properties of gamma-TiAl alloys make them attractive candidates for durable lightweight hot structure and thermal protection systems at temperatures as high as 871 C. However, oxidation significantly degrades gamma-TiAl alloys under the high-temperature service conditions associated with the RLV operating environment. This paper discusses ongoing efforts at NASA Langley Research Center to develop durable ultrathin coatings for protecting gamma-TiAl alloys from high-temperature oxidation environments. In addition to offering oxidation protection, these multifunctional coatings are being engineered to provide thermal control features to help minimize heat input into the hot structures. This paper describes the coating development effort and discusses the effects of long-term high-temperature exposures on the microstructure of coated and uncoated gamma-TiAl alloys. The alloy of primary consideration was the Plansee alloy gamma-Met, but limited studies of the newer alloy gamma-Met-PX were also included. The oxidation behavior of the uncoated materials was evaluated over the temperature range of 704 C to 871 C. Sol-gel-based coatings were applied to the gamma-TiAl samples by dipping and spraying, and the performance evaluated at 871 C. Results showed that the coatings improve the oxidation resistance, but that further development is necessary.

Wallace, T. A.↗

Initial Assessment of Environmental Effects on SiC/SiC Composites in Helium-Cooled Nuclear Systems

Ceramic matrix composites, in particular SiC/SiC composites, are currently being evaluated for use at high temperatures and high radiation fields in advanced concept reactors, including high-temperature gas cooled reactors (HTGR), very high temperature reactors (VHTR), gas fast reactors (GFR), sodium fast reactors (SFR) and fluoride-cooled high temperature reactors (FHR). SiC/SiC composites have many desirable properties for high temperature nuclear applications, including excellent thermal and mechanical properties and radiation resistance. However, their behavior in contact with the chemical environment in normal operation conditions and in off-normal accident conditions scenarios still needs to be evaluated. This report summarizes the information available in the literature on the chemical reactivity of SiC/SiC composites and of their components in contact with the helium coolant used in HTGR, VHTR and GFR designs. Under normal operating conditions, ultra-high purity helium will have chemically controlled impurities (water, oxygen, carbon dioxide, carbon monoxide, methane, hydrogen) that will create a slightly oxidizing gas environment. Little is known from direct experiments on the reactivity of third generation (nuclear grade) SiC/SiC composites in contact with low concentrations of water or oxygen in inert gas, at high temperature. However, there is ample information regarding the oxidation behavior of SiC/SiC composites in dry and moist air at high temperatures. This information is reviewed first in the next chapters. The emphasis is placed on the improvement in material oxidation, thermal, and mechanical properties during three stages of development of SiC fibers and at least two stages of development of the fiber/matrix interphase. The chemical stability of SiC/SiC composites in contact with oxygen or steam at temperatures that may develop in off-normal reactor conditions supports the conclusion that most advanced composites (also known as nuclear grade SiC/SiC composites) have the chemical resistance that would allow them maintain mechanical properties at temperatures up to 1200 – 1300 °C in the extreme conditions of an air or water ingress accident scenario. Further research is needed to assess the long-term stability of advanced SiC/SiC composites in inert gas (helium) in presence of very low concentrations (traces) of water and oxygen at the temperatures of normal operation of helium-cooled reactors.

ceramic matrix composites↗

Post Quench Ductility Evaluation of Zircaloy-4 and Select Iron Alloys under Design Basis and Extended LOCA Conditions

Oxidation experiments were conducted at 1200 C in flowing steam with tubing specimens of Zircaloy-4, 317, 347 stainless steels, and the commercial FeCrAl alloy APMT. The purpose was to determine the oxidation behavior and post quench ductility of these alloys under postulated loss-of-coolant accident conditions. The parabolic rate constant for Zircaloy-4 tubing samples at 1200 were determined to be k = 2.173 107 g2/cm4/s C, in excellent agreement with the Cathcart-Pawel correlation. The APMT alloy experienced the slowest oxidation rate among all materials examined in this work. The ductility of post quenched samples was evaluated by ring compression tests at 135 C. For Zircaloy-4, the ductile to brittle transition occurs at an equivalent cladding reacted (ECR) of 19.3%. SS-347 was still ductile after being oxidized for 2400 s (CP-ECR 50%), but the maximum load was reduced significantly owing to the metal layer thickness reduction. No ductility decrease was observed for the post-quenched APMT samples oxidized up to four hours.

accident test↗

Thermochemical Compatibility and Oxidation Resistance of Advanced LWR Fuel Cladding

We assessed the thermochemical compatibility of potential replacement cladding materials for zirconium alloys in light water reactors. Considered were FeCrAl steel (similar to Kanthal APMT), Nb-1%Zr (similar to PWC-11), and a hybrid SiC-composite with a metallic barrier layer. The niobium alloy was also seen as requiring an oxidation protective layer, and a diffusion silicide was investigated. Metallic barrier layers for the SiC-composite reviewed included a FeCrAl alloy, Nb-1%Zr, and chromium. Thermochemical calculations were performed to determine oxidation behavior of the materials in steam, and for hybrid SiC-composites possible interactions between the metallic layer and SiC. Additionally, experimental exposures of SiC-alloy reaction couples at 673K, 1073K, and 1273K for 168 h in an inert atmosphere were made and microanalysis performed. Whereas all materials were determined to oxidize under higher oxygen partial pressures in the steam environment, these varied by material with expected protective oxides forming. Finally, the computed and experimental results indicate the formation of liquid phase eutectic in the FeCrAl-SiC system at the higher temperatures.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Toward Optimum Scale and TBC Adhesion on Single Crystal Superalloys

Single crystal superalloys exhibit excellent cyclic oxidation resistance if their sulfur content is reduced from typical impurity levels of approximately 5 ppmw to below 0.5 ppmw. Excellent alumina scale adhesion was documented for PWA 1480 and PWA 1484 without yttrium additions. Hydrogen annealing produced effective desulfurization of PWA 1480 to less than 0.2 ppmw and was also used to achieve controlled intermediate levels. The direct relationship between cyclic oxidation behavior and sulfur content was shown. An adhesion criterion was proposed based on the total amount of sulfur available for interfacial segregation, e.g., less than or equal to 0.2 ppmw S will maximize adhesion for a 1 mm thick sample. PWA 1484, melt desulfurized to 0.3 ppmw S, also exhibited excellent cyclic oxidation resistance and encouraging TBC lives (10 mils of 8YSZ, plasma sprayed without a bond coat) in 1100 C cyclic oxidation tests.

Smialek, James L.↗

In Situ Optical Absorption Studies of Point Defect Kinetics and Thermodynamics in Oxide Thin Films

The authors discuss the use of in situ optical absorption to probe point defect equilibria and kinetics in oxides, with particular attention to thin films and high-temperature measurements evaluating changes in oxygen content. The introduction notes the effect of point defects on oxide behavior, including differences in thin films versus bulk materials, and describes methods to evaluate point defect equilibria and kinetics; advantages of optical absorption among these methods are highlighted. Section 2 provides an overview of how optical absorption and point defect concentrations are related, including various possible structural and electronic origins of defect-mediated absorption changes corresponding to oxygen content changes. Section 3 traces the development of historical understanding of optical absorption in nonstoichiometric oxides and emergence of thin film applications and measurement approaches that resulted. Section 4 details the procedure for determining surface exchange coefficients from optical transmission relaxation measurements and provides specific examples of how this approach uniquely has enabled new insights into thin film surface exchange behavior with and without current collectors. Section 5 provides examples of optically derived diffusivity measurements and comparisons of bulk and thin film defect equilibria. Section 7 outlines potential opportunities and future developments in this area, and Section 7 concludes the manuscript.

36 MATERIALS SCIENCE↗

Characterization of surface layers formed on DU10Mo ingots after processing steps and high humidity exposure

The design of monolithic U-Mo fuel elements fabricated from low-enriched uranium for use in high-power research reactors requires bonding of the fuel foil to either Al cladding or a Zr barrier layer. Processing of the U-Mo ingot to final foil form has the potential to generate surface layers on the foil that differ from the bulk, metallic U-Mo. The interfacial properties between the U-Mo and Zr or Al cladding layers will then be determined by these surface layers. We use x-ray photoelectron spectroscopy, cross-sectional scanning electron microscopy, and atomic force microscopy to characterize the composition, oxidation state, and morphology of the surface layers that form after hot rolling and cold rolling depleted U–10 wt% Mo alloy (DU10Mo). A thick uranium nitride layer is observed after hot rolling, although its origin is likely from a previous processing step. The surface composition of cold-rolled DU10Mo varied significantly between two foils, with a strongly Mo-depleted surface oxide layer observed on one foil but nominal Mo composition observed on the other. The efficacy of acid etching in HNO 3 is compared to that of electropolishing in H 2 SO 4 to remove the surface layers, and both methods are found to be similarly effective. Both laboratory (low humidity) air exposure and longer rinse times in water are shown to promote the formation of surface oxide layers. Exposure of both acid-etched and electropolished DU10Mo foils to humid air (97% relative humidity) for six weeks results in formation of a thick oxide layer due to corrosion. The oxide layer on the acid-etched foil is thicker and more highly oxidized than the oxide layer that forms on the electropolished foil, and these differences in oxidation behavior are attributed to higher surface roughness on the acid-etched foil. In general, Mo is found to play a role as a sacrificial element, typically exhibiting a larger ratio of Mo 6+ / Mo 4+ than U 6+ / U 4+ . This is unexpected, given the greater thermodynamic driving force to form U oxides than Mo oxides.

Kaspar, Tiffany C. (ORCID:0000000328167569)↗

Predicting the Oxidation/Corrosion Performance of Structural Alloys in Supercritical CO 2

This project was the first research to address oxidation of alloys under supercritical CO 2 conditions relevant to a semi-open Allam Cycle system. The levels of impurities expected in the CO 2 for typical operation were determined by thermodynamic and mass balance calculations, and a test rig was assembled and used to run corrosion tests at temperatures from 650 to 750°C in CO 2 at 200 bar for up to 5,000h, with and without impurities. Oxidation rates were measured for seven alloys representing high-strength ferritic steels, standard austenitic steels, and Ni-based alloys with higher-temperature capabilities. The very thin, protective scales formed on the high-temperature alloys provided significant challenges in characterization and thickness measurement. The rates of mass gain and scale thickening were possibly slower when oxidizing impurities were present in the sCO 2 , and the scale morphologies formed on the ferritic and austenitic steels were consistent with expectations, and similar to those formed in high-pressure steam, with some potential influences of C. Some surface hardening (possibly due to carbon uptake) was identified in ferritic steels Grade 91 and VM12, and appeared more severe in commercially-pure CO 2 . Hardening was also observed in austenitic steel TP304H, but that in HR3C appeared anomalous, probably the result of work-hardening from specimen preparation. No hardening was found in Ni-base alloys IN617 and IN740H. An existing EPRI Oxide Exfoliation Model was modified for this application and used to evaluate the potential impact of the scales grown in sCO 2 on service lifetimes in compact heat exchanger designs. Results suggested that reduction in flow area by simple oxide growth as well as by accumulation of exfoliated scale may have a major effect on the design of small-channel heat exchangers. In addition, the specific oxidation behavior of each alloy strongly influences the relationship of channel wall thickness to service lifetime.

20 FOSSIL-FUELED POWER PLANTS↗

High-Temperature Performance of Cast CF8C-Plus Austenitic Stainless Steel

Covers and casings of small to medium size gas turbines can be made from cast austenitic stainless steels, including grades such as CF8C, CF3M, or CF10M. Oak Ridge National Laboratory and Caterpillar have developed a new cast austenitic stainless steel, CF8C-Plus, which is a fully austenitic stainless steel, based on additions of Mn and N to the standard Nb-stabilized CF8C steel grade. The Mn addition improves castability, as well as increases the alloy solubility for N, and both Mn and N synergistically act to boost mechanical properties. CF8C-Plus steel has outstanding creep-resistance at 600-900 C, which compares well with Ni-based superalloys such as alloys X, 625, 617, and 230. CF8C-Plus also has very good fatigue and thermal fatigue resistance. It is used in the as-cast condition, with no additional heat-treatments. While commercial success for CF8C-Plus has been mainly for diesel exhaust components, this steel can also be considered for gas turbine and microturbine casings. The purposes of this paper are to demonstrate some of the mechanical properties, to update the long-term creep-rupture data, and to present new data on the high-temperature oxidation behavior of these materials, particularly in the presence of water vapor.

36 MATERIALS SCIENCE↗

Mechanical behavior of carbon-carbon composites

A general background, test plan, and some results of preliminary examinations of a carbon-carbon composite material are presented with emphasis on mechanical testing and inspection techniques. Experience with testing and evaluation was gained through tests of a low modulus carbon-carbon material, K-Karb C. The properties examined are the density - 1.55 g/cc; four point flexure strength in the warp - 137 MPa (19,800 psi) and the fill - 95.1 MPa (13,800 psi,) directions; and the warp interlaminar shear strength - 14.5 MPa (2100 psi). Radiographic evaluation revealed thickness variations and the thinner areas of the composite were scrapped. The ultrasonic C-scan showed attenuation variations, but these did not correspond to any of the physical and mechanical properties measured. Based on these initial tests and a survey of the literature, a plan has been devised to examine the effect of stress on the oxidation behavior, and the strength degradation of coated carbon-carbon composites. This plan will focus on static fatigue tests in the four point flexure mode in an elevated temperature, oxidizing environment.

Rozak, G. A.↗