Carrier Diffusion Lengths in Continuously Grown and Etched-and-Regrown GaN Pin Diodes

Advanced GaN power devices are promising for many applications in high power electronics but performance limitations due to material quality in etched-and-regrown junctions prevent their widespread use. Carrier diffusion length is a critical parameter that not only determines device performance but is also a diagnostic of material quality. Here we present the use of electron-beam induced current to measure carrier diffusion lengths in continuously grown and etched-and-regrown GaN pin diodes as models for interfaces in more complex devices. Variations in the quality of the etched-and-regrown junctions are observed and shown to be due to the degradation of the n-type material. Finally, we observe an etched-and-regrown junction with properties comparable to a continuously grown junction.

42 ENGINEERING↗

Surface chemistry of InP ridge structures etched in Cl{sub 2}-based plasma analyzed with angular XPS

Two x-ray photoelectron spectroscopy configurations are proposed to analyze the surface chemistry of micron-scale InP ridge structures etched in chlorine-based inductively coupled plasma (ICP). Either a classical or a grazing configuration allows to retrieve information about the surface chemistry of the bottom surface and sidewalls of the etched features. The procedure is used to study the stoichiometry of the etched surface as a function of ridge aspect ratio for Cl{sub 2}/Ar and Cl{sub 2}/H{sub 2} plasma chemistries. The results show that the bottom surface and the etched sidewalls are P-rich, and indicate that the P-enrichment mechanism is rather chemically driven. Results also evidence that adding H{sub 2} to Cl{sub 2} does not necessarily leads to a more balanced surface stoichiometry. This is in contrast with recent experimental results obtained with the HBr ICP chemistry for which fairly stoichiometric surfaces have been obtained.

36 MATERIALS SCIENCE↗

Plasma-assisted atomic layer etching of single-crystal diamond

Applications of near-surface nitrogen-vacancy (NV) centers in diamond are often limited by surface defects created during processing. Understanding and controlling plasma-induced surface damage is important for preserving the optical and spin properties of diamond NV centers. We report molecular dynamics simulations of a novel form of plasma-aided atomic layer etching of diamond. In this proposed scheme, the initial surface modification step consists of Ar + ion bombardment. This creates an amorphous layer at the surface, the thickness of which is controlled by the ion energy. Amorphization is known to help smooth the surface, at least locally, and would also serve to sputter clean an initially contaminated surface. A second step impacts the amorphous carbon layer with O + between about 1 and 5 eV. Simulations show that this energy range will remove the amorphous carbon but will not etch the underlying diamond. Though this energy range is not trivial to achieve in a conventional low-temperature plasma, potential methods for creating these low-energy O + ions are discussed. In addition to a-C etching, the O + impacts are predicted to remove any isolated (100) diamond terraces by selectively attacking the edges of the terraces. The proposed atomic layer etching (ALE) approach reverses the conventional ALE sequence in which the surface modification step is usually chemical modification (oxidation in this case), followed by a removal step using Ar + impacts. This plasma ALE procedure is predicted to create a diamond surface that is atomically flat and defect free.

Draney, J. S. [Princeton University, NJ (United St↗

Using Graphene Liquid Cell Transmission Electron Microscopy to Study in Situ Nanocrystal Etching

Graphene liquid cell electron microscopy provides the ability to observe nanoscale chemical transformations and dynamics as the reactions are occurring in liquid environments. This manuscript describes the process for making graphene liquid cells through the example of graphene liquid cell transmission electron microscopy (TEM) experiments of gold nanocrystal etching. The protocol for making graphene liquid cells involves coating gold, holey-carbon TEM grids with chemical vapor deposition graphene and then using those graphene-coated grids to encapsulate liquid between two graphene surfaces. These pockets of liquid, with the nanomaterial of interest, are imaged in the electron microscope to see the dynamics of the nanoscale process, in this case the oxidative etching of gold nanorods. By controlling the electron beam dose rate, which modulates the etching species in the liquid cell, the underlying mechanisms of how atoms are removed from nanocrystals to form different facets and shapes can be better understood. Graphene liquid cell TEM has the advantages of high spatial resolution, compatibility with traditional TEM holders, and low start-up costs for research groups. Current limitations include delicate sample preparation, lack of flow capability, and reliance on electron beam-generated radiolysis products to induce reactions. With further development and control, graphene liquid cell may become a ubiquitous technique in nanomaterials and biology, and is already being used to study mechanisms governing growth, etching, and self-assembly processes of nanomaterials in liquid on the single particle level.

36 MATERIALS SCIENCE↗

Use of Sirtl etch for silicon-slice evaluation.

An investigation was conducted to explore the possibility of using Sirtl etch as a nondestructive evaluation step for categorizing silicon wafers before device fabrication is begun. It is known that chromium is deposited as a residue during the chemical reaction associated with etching silicon in Sirtl etch. There has been concern that the use of Sirtl etch could result in the diffusion of chromium into the silicon slice during subsequent high-temperature processing steps. The investigation revealed, however, that residual chromium resides only on the surface of the slice and can easily be removed.

Porter, W. A.↗

Etching and Growth of GaAs

In-place process for etching and growth of gallium arsenide calls for presaturation of etch and growth melts by arsenic source crystal. Procedure allows precise control of thickness of etch and newly grown layer on substrate. Etching and deposition setup is expected to simplify processing and improve characteristics of gallium arsenide lasers, high-frequency amplifiers, and advanced integrated circuits.

Seabaugh, A. C.↗

Controlled in situ etch-back

A controlled in situ etch-back technique is disclosed in which an etch melt and a growth melt are first saturated by a source-seed crystal and thereafter etch-back of a substrate takes place by the slightly undersaturated etch melt, followed by LPE growth of a layer by the growth melt, which is slightly supersaturated.

Mattauch, R. J.↗

Anisotropic etching of Al by a directed Cl2 flux

A new Al etching technique is described that uses an ion beam from a Kaufman ion source and a directed Cl2 flux. The ion beam is used primarily to remove the native oxide and to allow the Cl2 to spontaneously react with the Al film forming volatile Al2Cl6. By controlling both the flux equivalent pressure of Cl2 and the ion beam current, this etching technique makes possible the anisotropic etching of Al with etch rates from 100 nm/min to nearly 10 microns/min with a high degree of selectivity.

Efremow, N. N.↗

Chemical etching and organometallic chemical vapor deposition on varied geometries of GaAs

Results of micron-spaced geometries produced by wet chemical etching and subsequent OMCVD growth on various GaAs surfaces are presented. The polar lattice increases the complexity of the process. The slow-etch planes defined by anisotropic etching are not always the same as the growth facets produced during MOCVD deposition, especially for deposition on higher-order planes produced by the hex groove etching.

Bailey, Sheila G.↗

Metal etching composition

The present invention is directed to a chemical etching composition for etching metals or metallic alloys. The composition includes a solution of hydrochloric acid, phosphoric acid, ethylene glycol, and an oxidizing agent. The etching composition is particularly useful for etching metal surfaces in preparation for subsequent fluorescent penetrant inspection.

Otousa, Joseph E.↗

Visible luminescence from silicon wafers subjected to stain etches

Etching of Si in a variety of solutions is known to cause staining. These stain layers consist of porous material similar to that produced by anodic etching of Si in HF solutions. In this work, photoluminescence peaked in the red from stain-etched Si wafers of different dopant types, concentrations, and orientations produced in solutions of HF:HNO3:H2O was observed. Luminescence is also observed in stain films produced in solutions of NaNO2 in HF, but not in stain films produced in solutions of CrO3 in HF. The luminescence spectra are similar to those reported recently for porous Si films produced by anodic etching in HF solutions. However, stain films are much easier to produce, requiring no special equipment.

Fathauer, R. W.↗

Anodic etching of p-type cubic silicon carbide

p-Type cubic silicon carbide was anodically etched using an electrolyte of HF:HCl:H2O. The etching depth was determined versus time with a fixed current density of 96.4 mA/sq cm. It was found that the etching was very smooth and very uniform. An etch rate of 22.7 nm/s was obtained in a 1:1:50 HF:HCl:H2O electrolyte.

Harris, G. L.↗

Multilayer Badges Indicate Depths Of Ion Sputter Etches

Multilayer badges devised to provide rapid, in-place indications of ion sputter etch rates. Badges conceived for use in estimating ion erosion of molybdenum electrodes used in inert-gas ion thrustors. Concept adapted to measure ion erosion in industrial sputter etching processes used for manufacturing of magnetic, electronic, and optical devices. Badge etched when bombarded by energetic ions. Badge layers exposed using mask. Contrast between layers facilitates counting of layers to determine etch depth.

Beattie, J. R.↗

Method for anisotropic etching in the manufacture of semiconductor devices

Hydrocarbon polymer coatings used in microelectronic manufacturing processes are anisotropically etched by hyperthermal atomic oxygen beams (translational energies of 0.2 to 20 eV, preferably 1 to 10 eV). Etching with hyperthermal oxygen atom species obtains highly anisotropic etching with sharp boundaries between etched and mask protected areas.

Koontz, Steven L.↗

Etching in Chlorine Discharges Using an Integrated Feature Evolution-Plasma Model

Etching of semiconductor materials is reliant on plasma properties. Quantities such as ion and neutral fluxes, both in magnitude and in direction, are often determined by reactor geometry (height, radius, position of the coils, etc.) In order to obtain accurate etching profiles, one must also model the plasma as a whole to obtain local fluxes and distributions. We have developed a set of three models that simulates C12 plasmas for etching of silicon, ion and neutral trajectories in the plasma, and feature profile evolution. We have found that the location of the peak in the ion densities in the reactor plays a major role in determining etching uniformity across the wafer. For a stove top coil inductively coupled plasma (ICP), the ion density is peaked at the top of the reactor. This leads to nearly uniform neutral and ion fluxes across the wafer. A side coil configuration causes the ion density to peak near the sidewalls. Ion fluxes are thus greater toward the wall's and decrease toward the center. In addition, the ions bombard the wafer at a slight angle. This angle is sufficient to cause slanted profiles, which is highly undesirable.

Hwang, Helen H.↗

Etch Profile Simulation Using Level Set Methods

Etching and deposition of materials are critical steps in semiconductor processing for device manufacturing. Both etching and deposition may have isotropic and anisotropic components, due to directional sputtering and redeposition of materials, for example. Previous attempts at modeling profile evolution have used so-called "string theory" to simulate the moving solid-gas interface between the semiconductor and the plasma. One complication of this method is that extensive de-looping schemes are required at the profile corners. We will present a 2D profile evolution simulation using level set theory to model the surface. (1) By embedding the location of the interface in a field variable, the need for de-looping schemes is eliminated and profile corners are more accurately modeled. This level set profile evolution model will calculate both isotropic and anisotropic etch and deposition rates of a substrate in low pressure (10s mTorr) plasmas, considering the incident ion energy angular distribution functions and neutral fluxes. We will present etching profiles of Si substrates in Ar/Cl2 discharges for various incident ion energies and trench geometries.

Hwang, Helen H.↗

Reactive Ion Etching in a VHF Parallel Plate Reactor

VHF (very high frequency) capacitive plasma reactors may allow development of new RIE (reactive ion etching) systems with high etch rates, excellent uniformity and anisotropy and low damage. High ion and radical fluxes can be obtained by raising the RF (radio frequency) frequency which increases plasma density dramatically at a fixed voltage. The effects of variation in frequency (25-120 MHz), pressure (10-250 mTorr), and flow rate (1-100 sccm) in a CF4 discharge have been investigated. The RF current versus voltage characteristics and spatially resolved optical emission are used as diagnostics. Experiments on etch rates, etch uniformity and anisotropy in silicon, silicon dioxide and silicon nitride will be discussed. Results of fluid model simulations are used to interpret the experimental data.

Dahi, H.↗

Etching of Silicon in HBr Plasmas for High Aspect Ratio Features

Etching in semiconductor processing typically involves using halides because of the relatively fast rates. Bromine containing plasmas can generate high aspect ratio trenches, desirable for DRAM and MEMS applications, with relatively straight sidewalk We present scanning electron microscope images for silicon-etched trenches in a HBr plasma. Using a feature profile simulation, we show that the removal yield parameter, or number of neutrals removed per incident ion due to all processes (sputtering, spontaneous desorption, etc.), dictates the profile shape. We find that the profile becomes pinched off when the removal yield is a constant, with a maximum aspect ratio (AR) of about 5 to 1 (depth to height). When the removal yield decreases with increasing ion angle, the etch rate increases at the comers and the trench bottom broadens. The profiles have ARs of over 9:1 for yields that vary with ion angle. To match the experimentally observed etched time of 250 s for an AR of 9:1 with a trench width of 0.135 microns, we find that the neutral flux must be 3.336 x 10(exp 17)sq cm/s.

Hwang, Helen H.↗