Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “weld speed”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 37 records · Page 2

Towards High-Speed friction stir welding of 25 mm Thick AA2139-T8: tool innovation and process development

Joining thick plates (≥ 12 mm) of aluminum (Al) alloys is challenging due to high tool forces, uneven material flow, and non-uniform heat distribution through the material’s thickness. Recent advancements in tool design and welding parameters for friction stir welding (FSW) in thick plates butt joining have encountered a developmental plateau, highlighting the need for innovative approaches to overcome existing limitations. Here, this study focuses on the systematic development of single-pass and double-pass FSW processes for high-strength aluminum alloy AA2139-T8, to improve joint efficiency and enable high-speed welding capabilities. Experimental evidence is presented for a novel tool design with opposing pin threads, enabling high-speed (178 mm/min) single-pass friction stir butt welding of 25 mm thick AA2139-T8. A series of FSW trials was conducted both in air and with a trailing water spray, using steel backing plates (BPs) to investigate the impact of quenching and cooling rates on process response and joint performance. A joint efficiency of 83% was attained using the novel tool features and effectively controlling process forces and thermal boundary conditions.

AA2139-T8↗

Study of gas tungsten arc welding procedures for tantalum alloy T-111 (Ta-8 W-2Hf) plate

Methods of eliminating or reducing underbread cracking in multipass GTA welds in thick T-111 plate were studied. Single V butt welds prepared using experimental filler metal compositions and standard weld procedures resulted in only moderate success in reducing underbread cracking. Subsequent procedural changes incorporating manual welding, slower weld speeds, and three or fewer fill passes resulted in crack-free single V welds only when the filler metal was free of hafnium. The double V joint design with successive fill passes on opposite sides of the joint produced excellent welds. The quality of each weld was determined metallographically since the cracking, when present, was very slight and undetectable using standard NDT techniques. Tensile and bend tests were performed on selected weldments. The inherent filler metal strength and the joint geometry determined the strength of the weldment. Hardness and electron beam microprobe traverses were made on selected specimens with the result that significant filler metal-base metal dilution as well as hafnium segregation was detected. A tentative explanation of T-111 plate underbread cracking is presented based on the intrinsic effects of hafnium in the weldment.

Gold, R. E.↗

Real time computer controlled weld skate

A real time, adaptive control, automatic welding system was developed. This system utilizes the general case geometrical relationships between a weldment and a weld skate to precisely maintain constant weld speed and torch angle along a contoured workplace. The system is compatible with the gas tungsten arc weld process or can be adapted to other weld processes. Heli-arc cutting and machine tool routing operations are possible applications.

Wall, W. A., Jr.↗

Three Sheet Al alloy assembly for automotive application

An update on joint characterization of three sheet friction stir lap welds (FSLW) in three aluminum alloys (7xxx, 5xxx, and 6xxx) for automotive assembly application is presented. Welding speed of 0.3-2.9m/min was used with pin length >5mm with the aim to reduce upturn hooking on the retreating side and avoid wormhole defect on the advancing side. Joints were also made in to enable T peel and U peel testing. Stitch welds were used to understand effects of weld length and ramp length on T peel performance. Hat sections were joined for 3-point bending and axial crush testing and tested with promising results. Several key issues that require further investigations are identified including flash management near the trim edge, weld quality with limited clamping, tool failures at speeds greater than 0.5m/min, and propensity of incipient melting for 7xxx stack-up.

Upadhyay, Piyush↗

Tracing Material Flow Paths in Friction Stir Welds

Heat and mechanical work are coupled in the friction stir welding process. The process variables are RPM, translational weld speed, and downward plunge force. The strain-temperature history of a metal element at each point on the cross-section of the weld is determined by the process variables plus the individual flow path taken by the particular filament of metal flowing around the tool and ending on flat point. The strain-temperature history determines the properties of a metal element on the weld cross-section. The strain-temperature history is carefully controlled in metal processes where direct control is feasible. Indirect estimates of the flow paths and the strain-temperature histories of filaments comprising friction stir welds can be made from a model, if the model is good enough. This paper describes marker studies of flow path geometries for various process parameters. Observed geometries are compared with geometries estimated from models.

Sanders, Johnny↗

Influence of Processing Parameters on the Flow Path in Friction Stir Welding

Friction stir welding (FSW) is a solid phase welding process that unites thermal and mechanical aspects to produce a high quality joint. The process variables are rpm, translational weld speed, and downward plunge force. The strain-temperature history of a metal element at each point on the cross-section of the weld is determined by the individual flow path taken by the particular filament of metal flowing around the tool as influenced by the process variables. The resulting properties of the weld are determined by the strain-temperature history. Thus to control FSW properties, improved understanding of the processing parameters on the metal flow path is necessary.

Schneider, J. A.↗

Study of Radiographic Linear Indications and Subsequent Microstructural Features in Gas Tungsten Arc Welds of Inconel 718

This study presents examples and considerations for differentiating linear radiographic indications produced by gas tungsten arc welds in a 0.05-in-thick sheet of Inconel 718. A series of welds with different structural features, including the enigma indications and other defect indications such as lack of fusion and penetration, were produced, radiographed, and examined metallographically. The enigma indications were produced by a large columnar grain running along the center of the weld nugget occurring when the weld speed was reduced sufficiently below nominal. Examples of respective indications, including the effect of changing the x-ray source location, are presented as an aid to differentiation. Enigma, nominal, and hot-weld specimens were tensile tested to demonstrate the harmlessness of the enigma indication. Statistical analysis showed that there is no difference between the strengths of these three weld conditions.

Walley, J. L.↗

The Evolution of Friction Stir Welding Theory at Marshall Space Flight Center

From 1995 to the present the friction stir welding (FSW) process has been under study at Marshall Space Flight Center (MSFC). This is an account of the progressive emergence of a set of conceptual tools beginning with the discovery of the shear surface, wiping metal transfer, and the invention of a kinematic model and making possible a treatment of both metallurgical structure formation and process dynamics in friction stir welding from a unified point of view. It is generally observed that the bulk of the deformation of weld metal around the FSW pin takes place in a very narrow, almost discontinuous zone with high deformation rates characteristic of metal cutting. By 1999 it was realized that this zone could be treated as a shear surface like that in simple metal cutting models. At the shear surface the seam is drawn out and compressed and pressure and flow conditions determine whether or not a sound weld is produced. The discovery of the shear surface was followed by the synthesis of a simple 3- flow kinematic model of the FSW process. Relative to the tool the flow components are: (1) an approaching translational flow at weld speed V, (2) a rotating cylindrical plug flow with the angular velocity of the tool , and (3) a relatively slow ring vortex flow (like a smoke ring) encircling the tool and driven by shoulder scrolls and pin threads. The rotating plug flow picks up an element of weld metal, rotates it around with the tool, and deposits it behind the tool ( wiping metal transfer ); it forms plan section loops in tracers cut through by the tool. Radially inward flow from the ring vortex component retains metal longer in the rotating plug and outward flow expels metal earlier; this interaction forms the looping weld seam trace and the tongue and groove bimetallic weld contour. The radial components of the translational and ring vortex flows introduce parent metal intrusions into the small grained nugget material close to the tool shoulder; if this feature is pronounced, nugget collapse may result. Certain weld features, in particular internal banding seen in transverse section as onion rings and associated surface ridges called tool marks , have long implied an oscillation flow component, but have only recently been attributed in the literature to tool eccentricity. Rotating plug shape, typically a hollow cylinder flared at the end where it sticks to the shoulder, varies as pressure distribution on the tool determines where sticking occurs. Simplified power input estimates balanced against heat loss estimates give reasonable temperature estimates, explain why the power requirement changes hardly at all over a wide range of RPM s, and yield isotherms that seem to fall along boundaries of parameter windows of operation.

Nunes, Arthur C.↗

Laser Beam Welding for in-Space Joining Demonstrated Under Vacuum on the Ground and By Parabolic Flight Experiments

High energy density electron beam welding enabled the first and, to date, only American weld performed in space during the M551 experiment on Skylab in 1973. Though welding is critical to 90% of durable goods manufacturing in America, there is not yet regular and reliable application of welding processes to the In-space Servicing, Assembly, and Manufacturing (ISAM) sector. Fundamental studies are needed to develop basic capabilities and to enhance fundamental process knowledge, which will support follow-on efforts to mature in-space welding for use in commercial, defense, and other aerospace applications. The current work seeks to build on past flights and improve understanding and quantification of materials joining in space conditions using laser beam welding (LBW). LBW offers several advantages over the electron beam welding of Skylab, amongst others: reduced electromagnetic interference, less exposure of operators to ionizing radiation, and flexible delivery through optical fibers supporting unique workpieces and joints. Since there is no orbital laboratory to mature laser beam welding for space, the current effort addresses maturation of laser beam welding through parabolic flights augmented with data collection to enable numerical modeling efforts that capture the physical effects of the space environment. This team has retrofitted an LBW experimental apparatus that can simulate the vacuum and, during a parabolic flight, the reduced gravity & microgravity conditions of in-space welding. A team of Capstone students modified the setup, originally developed by NASA Langley Research Center for electron beam free-form fabrication, to replace its electron gun with a 1 kW, 1070 nm Yb fiber laser. The apparatus was further instrumented with temperature sensing and high-speed welding cameras to monitor and record changes in the thermal state of the workpiece, the melt pool, the laser penetration level, and the development and orientation of spatter & plumes. The system will operate autonomously, demonstrating its utility to uncrewed missions. During upcoming parabolic flight campaigns expected summer 2024, this LBW equipment will weld common aerospace alloys of aluminum, stainless steel, and titanium under conditions representative of the space environment. This data will guide future computational modeling efforts of laser welding in space and help to qualify in-space welding as a viable ISAM technique.

laser beam welding↗

Friction stir welding of thick 7175 aluminium alloy plates for deepwater riser applications

To substantially reduce the cost of extracting petroleum from ultra-deepwater sources, manufacturing risers from 7175 aluminium (Al) alloys rather than steels is being considered. Friction stir welding (FSW), a solid-phase joining technique, is widely applied to 7XXX Al alloys because its mechanical properties are retained within the nugget zone. And, the primary technical objective of the current study is the development of high-strength, corrosion-resistant weldments that connect 7175 Al riser flanges and pipes. However, as the welding thickness increases, the welding speed can be greatly impeded, which lowers the manufacturing efficiency and weakens the mechanical properties in the heat affected zone (next to the nugget). Therefore, obtaining high-performance thick plate 7175 Al alloy joints via FSW is challenging. To overcome this dilemma, the current work optimises the tool design and welding parameters for achieving high-performance joints between 25.4 mm thick 7175 Al alloy plates in butt joint configuration.

Wang, Tianhao↗

Characterization of fusion welded ceramics in the SiC-ZrB 2 -ZrC system

Various SiC-ZrB 2 -ZrC ceramics were joined by fusion welding to determine the maximum silicon carbide content that could be joined. Commercial powders were hot pressed, machined, and preheated to 1450 °C before joining with a tungsten inert gas welding torch at 160–200 A. Resulting welds were cross-sectioned and analyzed to determine which compositions were weldable and to characterize microstructural evolution in welded samples. As compositions approached the ternary eutectic, the welds had smaller SiC grains and exhibited better weldability. Penetration depth of welds was controlled by a combination of current input and welding speed. Here, the ternary eutectic in the system was found at 36.9 ± 1.3 vol% SiC, 42.7 ± 1.5 vol% ZrB 2 , and 20.4 ± 1.9 vol% ZrC and its melting temperature was 2330 ± 23 °C. A ternary phase diagram for the SiC-ZrB 2 -ZrC was constructed and proposed via microstructural analysis of arc melted pellets on binary joins between each binary eutectic and the ternary eutectic in the system.

36 MATERIALS SCIENCE↗

Adaptive control for weld skate

Modified weld state is more mechanically stabel and welding speed error is reduced. Constant torch-tip travel rate is maintained even with curbed work surfaces.

Ives, R. E.↗

Electron-beam welder circle generator

Generator rotates electron beam and performs other convenient functions during welding process. Device eliminates time-consuming techniques relying heavily on operator's skill. Welding speed is varied with frequency selector, and amplitudes of x- and y-axes are varied by adjusting phase shift. Both high and low-range adjustments are available, and each axis can be separately controlled. Crosshair is provided for set-up and beam alinements.

Burley, R. K.↗

Residual stresses in welded plates

The purpose of this project was to develop a simple model which could be used to study residual stress. The mechanism that results in residual stresses in the welding process starts with the deposition of molten weld metal which heats the immediately adjacent material. After solidification of weld material, normal thermal shrinkage is resisted by the adjacent, cooler material. When the thermal strain exceeds the elastic strain corresponding to the yield point stress, the stress level is limited by this value, which decreases with increasing temperature. Cooling then causes elastic unloading which is restrained by the adjoining material. Permanent plastic strain occurs, and tension is caused in the region immediately adjacent to the weld material. Compression arises in the metal farther from the weld in order to maintain overall static equilibrium. Subsequent repair welds may add to the level of residual stresses. The level of residual stress is related to the onset of fracture during welding. Thus, it is of great importance to be able to predict the level of residual stresses remaining after a weld procedure, and to determine the factors, such as weld speed, temperature, direction, and number of passes, which may affect the magnitude of remaining residual stress. It was hoped to use traditional analytical modeling techniques so that it would be easier to comprehend the effect of these variables on the resulting stress. This approach was chosen in place of finite element methods so as to facilitate the understanding of the physical processes. The accuracy of the results was checked with some existing experimental studies giving residual stress levels found from x-ray diffraction measurements.

Bernstein, Edward L.↗

Modeling aluminum-lithium alloy welding characteristics

The purpose of this project was to develop a finite element model of the heat-affected zone in the vicinity of a weld line on a plate in order to determine an accurate plastic strain history. The resulting plastic strain increments calculated by the finite element program were then to be used to calculate the measure of damage D. It was hoped to determine the effects of varying welding parameters, such as beam power, efficiency, and weld speed, and the effect of different material properties on the occurrence of microfissuring. The results were to be compared first to the previous analysis of Inconel 718, and then extended to aluminum 2195.

Bernstein, Edward L.↗

Low Speed Control for Automatic Welding

Amplifier module allows rotating positioner of automatic welding machine to operate at speeds below normal range. Low speeds are precisely regulated by a servomechanism as are normal-range speeds. Addition of module to standard welding machine makes it unnecessary to purchase new equipment for low-speed welding.

Iceland, W. E.↗

Impact of Backing Plate and Thermal Boundary Conditions for High-Speed Friction Stir Welding of 25-mm Thick Aluminum Alloy 7175-T79

Here this study demonstrates high-speed (150 mm/min) single pass friction stir butt joining of 25 mm thick aluminum alloy 7175-T79. To understand the impact of quenching and cooling rate on process responses, joint strength, and grain size distributions across the weld thickness, we performed a series of friction stir welding (FSW) trials in air and with a trailing water spray using steel and composite backing plates (BP). Welds made in air and trailing water spray exhibit significantly different hardness distributions across the nugget, heat affected zone (HAZ), and HAZ minimum hardness as evidenced by detailed microhardness mapping. The effect of trailing water spray (TWS) on joint efficiency overshadows the influence of BP composition due to the vastly different contribution to quenching. TWS also resulted in a multifaceted effect on FSW such as lowering processing temperature, increasing X and Z forces while lowering Y force, and narrow heat affecting zone. Finally, digital image correlation (DIC)-based fracture mode analysis and grain size measurements correlate with the hardness distribution.

42 ENGINEERING↗