Tuning Composition and Activity of Cobalt Titanium Oxide Catalysts for the Oxygen Evolution Reaction
Not Available
SEARCH · Engineering Papers
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Not Available
We develop a new approach for modeling titanium carbide derived-carbon (TiC-CDC) systems with residual titanium by the generation of modified atomistic structures based on a silicon carbide derived-carbon (SiC-CDC) model and the application of weighted combinations of these structures. In our approach, the original SiC-CDC structure is modified by (i) removing carbon, (ii) adding carbon and (iii) adding titanium. The new atomic scale carbide-derived carbon (CDC) structures are investigated using classical molecular dynamics simulations, and their pure CO 2 adsorption isotherms are calculated using grand canonical Monte Carlo simulations. The system of TiC-CDC with residual titanium is modeled as weighted combinations of pure carbon CDC structures, CDC structures with titanium and a TiC crystalline structure. Our modeling is able to produce both structural properties and adsorption isotherms in accordance with experimental data. The fraction of different models in the systems successfully reflects the structural differences in various experimental TiC-CDC samples. The modeling also suggests that in partially etched TiC-CDC systems, the titanium that may be accessible to CO 2 gas at the transitional interface may provide significant interaction sites for CO 2 and may lead to more efficient overall gas adsorption.
An experimental study was undertaken to investigate the mechanical response of four hybrid titanium composite laminate (HTCL) systems, each prepared using a graphite fiber reinforced thermoplastic polyimide as the adhesive in a unidirectional prepreg. Two of the four HTCL systems were fabricated with the titanium Ti-15-3 alloy, while the other two systems were fabricated with the titanium Timetal Beta-21S alloy. Each HTCL system consisted of either three plies or four plies of the titanium alloy. Systems with only three plies of titanium had plies measuring 10 mils thick, whereas systems consisting of four plies of titanium had plies measuring 5 mils thick. The improvement in mechanical properties achieved by comparing the uniaxial tensile results of static strength at room temperature. Results included stress-strain curves, ultimate strength, strain-to-failure, initial modulus of the HTCL's, and the description of the observed modes of failure.
The surface chemistry for TiO{sub 2} atomic layer deposition (ALD) typically utilizes water or other oxidants that can oxidize underlying substrates such as magnetic disks or semiconductors. To avoid this oxidation, waterless or oxidant-free surface chemistry can be used that involves titanium halides and titanium alkoxides. In this study, waterless TiO{sub 2} ALD was accomplished using titanium tetrachloride (TiCl{sub 4}) and titanium tetraisopropoxide (TTIP). In situ transmission Fourier transform infrared (FTIR) studies were employed to study the surface species and the reactions during waterless TiO{sub 2} ALD. At low temperatures between 125 and 225 °C, the FTIR absorbance spectra revealed that the isopropoxide species remained on the surface after TTIP exposures. The TiCl{sub 4} exposures then removed the isopropoxide species and deposited additional titanium species. At high temperatures between 250 and 300 °C, the isopropoxide species were converted to hydroxyl species by β-hydride elimination. The observation of propene gaseous reaction product by quadrupole mass spectrometry (QMS) confirmed the β-hydride elimination reaction pathway. The TiCl{sub 4} exposures then easily reacted with the hydroxyl species. QMS studies also observed the 2-chloropropane and HCl gaseous reaction products and monitored the self-limiting nature of the TTIP reaction. Additional studies examined the waterless TiO{sub 2} ALD growth at low and high temperature. Quartz crystal microbalance measurements observed growth rates of ∼3 ng/cm{sup 2} at a low temperature of 150 °C. Much higher growth rates of ∼15 ng/cm{sup 2} were measured at a higher temperature of 250 °C under similar reaction conditions. X-ray reflectivity analysis measured a growth rate of 0.55 ± 0.05 Å/cycle at 250 °C. X-ray photoelectron depth-profile studies showed that the TiO{sub 2} films contained low Cl concentrations <1 at. %. This waterless TiO{sub 2} ALD process using TiCl{sub 4} and TTIP should be valuable to prevent substrate oxidation during TiO{sub 2} ALD on oxygen-sensitive substrates.
ABSTRACT Physical and chemical properties of graphene-metal interfaces have been largely examined with the objective of producing nanostructured carbon-based electronic devices. Although electronic properties are key to such devices, appropriate structural, thermal and mechanical properties are important for device performance as well. One of the most studied is the graphene-titanium (G-Ti) interface. Titanium is a low density, high strength versatile metal that can form alloys with desirable properties for applications ranging from aerospace to medicine. Small clusters and thin films of titanium deposited on graphene have also been examined. However, while some experiments show that thin films of titanium on graphene can be removed without damaging graphene hexagonal structure, others reported the formation of titanium-carbide (TiC) at G-Ti interfaces. In a previous work [ACS Appl. Mater. Interfaces, 2017, 9 (38), pp 33288-33297], we have shown that pristine G-Ti interfaces are resilient to large thermal fluctuations even when G-Ti structures lie on curved or kinked substrates. Here, using classical molecular dynamics with the third-generation Charge Optimized Many Body (COMB3) potential, we show that di-interstitial defective G-Ti structures on a copper substrate with a relatively large curvature kink, present signs of TiC formation. This result might help explain the different experimental results mentioned above.
The flash technique was used to measure the thermal diffusivity and specific heat of titanium potassium perchlorate (TKP) ignition powder (33wt% Ti - 67wt% KP) with Ventron sup- plied titanium particles, TKP ignition powder (33wt% Ti - 67wt% KP) with ATK supplied titanium particles, TKP output powder (41wt% Ti - 59wt% KP), and titanium subhydride potassium perchlorate (THKP) (33wt% TiH 1.65 - 67wt% KP) at 25°C. The influence of density and temperature on the thermal diffusivity and specific heat of TKP with Ventron supplied titanium particles was also investigated. Lastly, the thermal diffusivity and specific heats of 9013 glass, 7052 glass, SB-14 glass, and C-4000 Muscovite mica are presented as a function of temperature up to 300° C.
Thin metallic foils of antimony and titanium have been investigated in an attempt to develop an EUV filter with a bandpass from 350 to 550 A. A composite filter has been developed composed of antimony sandwiched between two titanium foils. The transmissions of sample composite foils and of pure titanium foils from 130 to 1216 A are presented. The absorption coefficients of anatimony and titanium and the effect of titanium oxide on the transmission are derived. The composite filter has been found to be quite stable and mechanically rugged. Among other uses, the filter shows substantial promise for EUV astronomy.
Accurate modeling of powder densification has been an area of active research for more than 60 years. The earliest efforts were focused on linearization of the data because computers were not readily available to assist with curve-fitting methods. In this work, eight different titanium powders (three different sizes of sponge fines<150 {micro}m,<75 {micro}m, and<45 {micro}m; two different sizes of a hydride-dehydride [HDH]<75 {micro}m and<45 {micro}m; an atomized powder; a commercially pure [CP] Ti powder from International Titanium Powder [ITP]; and a Ti 6 4 alloy powder) were cold pressed in a single-acting die instrumented to collect stress and deformation data during compaction. From these data, the density of each compact was calculated and then plotted as a function of pressure. The results show that densification of all the powders, regardless of particle size, shape, or chemistry, can be modeled accurately as the sum of an initial density plus the sum of a rearrangement term and a work-hardening term. These last two terms are found to be a function of applied pressure and take the form of an exponential rise.
Traditionally, titanium alloys with satisfactory mechanical properties can only be produced via energy-intensive and costly wrought processes, while titanium alloys produced using low-cost powder metallurgy methods consistently result in inferior mechanical properties, especially low fatigue strength. Herein, we demonstrate a new microstructural engineering approach for producing low-cost titanium alloys with exceptional fatigue strength via the hydrogen sintering and phase transformation (HSPT) process. The high fatigue strength presented in this work is achieved by creating wroughtlike microstructures without resorting to wrought processing. This is accomplished by generating an ultrafine-grained as-sintered microstructure through hydrogen-enabled phase transformations, facilitating the subsequent creation of fatigue-resistant microstructures via simple heat treatments. Finally, the exceptional strength, ductility, and fatigue performance reported in this paper are a breakthrough in the field of low-cost titanium processing.
This article presents and interprets a series of experiments performed to measure the velocity of four inert low-density porous materials that were accelerated by an ablated thin-film titanium metal, created by vaporizing a 250-nm-thick layer of titanium with a high-energy, Q-switched, pulsed, and 1.054 {mu}m neodymium-glass laser. Inert powder materials were chosen to match, among other characteristics, the morphology of energetic materials under consideration for use in detonator applications. The observed behavior occurs near the thin-film titanium ablation layer, through complex physical mechanisms, including laser absorption in the metal layer, ablation and formation of confined plasma that is a blackbody absorber of the remaining photon energy, and vaporization of the remaining titanium metal. One-dimensional hydrodynamic modeling provided a basis of comparison with the measured velocities. We found, as predicted in wave-propagation-code modeling, that an Asay foil can indicate total momentum of the driven material that is mechanically softer (lower in shock impedance) than the foil. The key conclusion is that the specific impulse delivered by the laser transfers a corresponding momentum to soft, organic power columns that are readily compacted. Impulse from the laser is less efficient in transferring momentum to hard inorganic particles that are less readily compacted.
Not Available
Experiments were conducted to determine the friction and wear characteristics of aluminum bronzes and copper-tin, titanium-tin, and copper-silver alloys sliding against a titanium-6% aluminum-4% vanadium alloy (Ti-6Al-4V). Hemispherically tipped riders of aluminum bronze and the titanium and copper alloys were run against Ti-6Al-4V disks in air at 430 C. The sliding velocity was 13 cm/sec, and the load was 250 g. Results revealed that high tin content titanium and copper alloys underwent significantly less wear and galling than commonly used aluminum bronzes. Also friction force was less erratic than with the aluminum bronzes.
Presentation describes research to understand failure mechanisms under shock loading as part of a broader effort to reduce the costs of materials science testing through use of additive manufactured materials.
Carbothermic selective reduction of titanium concentrate ore for the preparation of titanium oxycarbide was presented and SiO{sub 2} was found to be partly reduced during the process. The equilibrium relationship between Si dissolved in metallic Fe and SiO{sub 2} existed in corresponding slag was analyzed thermodynamically, and then revealed by a series of designed equilibration experiments. The results are in accordance with the calculated values obtained from thermodynamic analysis and have well explained the phenomenon that part of SiO{sub 2} is reduced during selective reduction processing of titanium concentrate ore.
Purpose: The aim of this study was to characterize the levels of artifacts and distortions of titanium applicators on 3.0-Tesla magnetic resonance imaging (MRI). Methods and Materials: Fletcher-Suit-Delclos-style tandem and ovoids (T and O) and tandem and ring applicator (T and R) were examined. The quality assurance (QA) phantoms for each applicator were designed and filled with copper sulphate solution (1.5 g/l). The artifacts were quantified with the registration of corresponding computed tomography (CT) images. A favorable MR sequence was searched in terms of artifacts. Using the sequence, the artifacts were determined. The geometric distortions induced by the applicators were quantified through each registration of CT and MRI without applicators. The artifacts of T and O were also evaluated on in vivo MRI datasets of 5 patients. Results: T1-weighted MRI with 1-mm slice thickness was found as a favorable MR sequence. Applying the sequence, the artifacts at the tandem tip of T and O and T and R were determined as 1.5 {+-} 0.5 mm in a superior direction in phantom studies. In the ovoids of T and O, we found artifacts less than 1.5 {+-} 0.5 mm. The artifacts of a T and O tandem in vivo were found as less than 2.6 {+-} 1.3 mm on T1-weighted MRI, whereas less than 6.9 {+-} 3.4 mm on T2-weighted MRI. No more than 1.2 {+-} 0.6 mm (3.0 {+-} 1.5 mm) of distortions, due to a titanium applicator, were measured on T1-weighted MRI (T2-). Conclusion: In 3.0-Tesla MRI, we found the artifact widths at the tip of tandem were less than 1.5 {+-} 0.5 mm for both T and O and T and R when using T1-weighted MRI in phantom studies. However, exclusive 3.0-Tesla MRI-guided brachytherapy planning with a titanium applicator should be cautiously implemented.
Under sufficient stresses, such as during dynamic loading, titanium experiences a phase transformation from hcp alpha phase to hexagonal omega phase. Omega phase is often retained in the microstructure after unloading, and has a strong influence on subsequent mechanical properties. Simulations suggest there are multiple pathways and underlying mechanisms for this transformation. Due to the incredibly short timescales involved, experimental measurements for model validation have been difficult. However, new capabilities at the Advanced Photon Source have enabled diffraction measurements during plate impact experiments to study the evolution of titanium during transformation. These high-rate data allow us to probe the mechanism and kinetics of phase transformations in new ways. Recent results will be presented and compared to post-mortem characterization of soft-recovered shocked specimens. Comparisons are then made with previous tests where material was shock-loaded and soft recovered for microstructural analysis. Together these techniques create a consistent picture of material behavior during the shock-induced α–ω phase transformation in titanium.
Heterogeneous strain was analyzed in polycrystalline, commercial-purity titanium using many experimental techniques that provide information about microstructure, dislocation arrangement, grain orientation, orientation gradients, surface topography, and local strain gradients. The recrystallized microstructure with 50-200 {micro}m grains was extensively characterized before and after deformation using 4-point bending to strains between 2% and 15%. Extremely heterogeneous deformation occurred along some grain boundaries, leading to orientation gradients exceeding 10{sup o} over 10-20 {micro}m. Patches of highly characterized micro-structure were modeled using crystal plasticity finite element (CPFE) analysis to simulate the deformation to evaluate the ability of the CPFE model to capture local deformation processes. Damage nucleation events were identified that are associated with twin interactions with grain boundaries. Progress toward identifying fracture initiation criteria based upon slip and twin interactions with grain boundaries is illustrated with related CPFE simulations of deformation in a TiAl alloy.
Titanium and Ti-8Al-1Mo-1V alloy were nitrided with an ion-beam source of nitrogen or argon and nitrogen at a total pressure of 2 x 10 to the minus 4th power to 10 x 10 to the minus 4th power torr. The treated surface was characterized by surface profilometry, X-ray diffractometry, Auger electron spectroscopy and microhardness measurements. The tetragonal Ti2N phase formed in pure titanium and Ti-8Al-1Mo-1V alloy with traces of AlN in the alloy. Two opposite processes competed during the ion-beam-nitriding process: (1) formation of nitrides in the surface layer and (2) sputtering of the nitrided layers by the ion beam. The highest surface hardnesses, about 500 kg/sq mm in titanium and 800 kg/sq mm in Ti-8Al-1Mo-1V, were obtained by ion nitriding with an ion beam of pure nitrogen at 4.2 x 10 to the minus 4th power torr at a beam voltage of 1000 V.