Under the microscope: Reduced activation ferritic martensitic steel Eurofer-97 following ion-Irradiation and high-temperature high-pressure water exposure

Here, this study is designed to characterise the microstructural behaviour of Eurofer-97 steel under ion irradiation and subsequent exposure to high-temperature high-pressure (HTHP) water. Eurofer-97, a ferritic-martensitic steel, has been developed to withstand the conditions of fusion reactors in the locations in contact with coolant with an elevated level of neutron flux, such as the breeder-wall blanket. The material has been studied after self-ion irradiation (using Fe ions) simulating the microstructural effects of neutron irradiation limited to the subsurface layer. The corrosion properties of the Eurofer-97 steel were studied by exposure to HTHP water up to 331 °C. Advanced microstructural characterisation using scanning, transmission electron and focused ion beam microscopy was performed on the as-received microstructure and after ion irradiation. This was then characterised after exposure for 240 h in high-temperature water. Eurofer-97 had a dense, columnar Cr-rich inner oxide, followed by a Fe-rich outer oxide layer. In the irradiated condition the grain structure and oxide itself was less ordered. No appreciable difference in oxide thickness was identified between the irradiated and unirradiated specimens after this short exposure time.

36 MATERIALS SCIENCE↗

Effect of post-weld heat treatment on microstructure and mechanical properties of rotary inertia friction welded dissimilar 422-4140 martensitic steel piston joints

The study investigated how post‐weld heat treatment (PWHT) temperature affects the microstructure and localized deformation/fracture during bend testing of rotary inertia friction welds (RIFW) between AISI 422 stainless steel and AISI 4140 steel. RIFW produced a fully martensitic interface with approximately 550 HV hardness in both the thermo-mechanically affected (TMAZ) and heat‐affected zones (HAZ). Due to differences in temper resistance, the 4140 TMAZ/HAZ softened progressively under PWHT temperatures from 525 °C to 700 °C, while the 422 TMAZ unexpectedly maintained about 550 HV up to 600 °C before significantly softening at temperatures ≥625 °C. This asymmetric softening generated steep hardness gradients across the interface at temperatures ≤600 °C. Furthermore, carbon migration across the interface was minimal up to 600 °C, moderate at 625 °C, and by 700 °C produced a carbide‐rich eutectoid layer in the 422 TMAZ alongside a carbon‐depleted soft ferrite layer in the 4140 TMAZ. Strain during bending was PWHT‐dependent, concentrating on the 4140 side; in as-welded joints, the high hardness led to deformation and crack initiation in the base metals, whereas in PWHT samples, cracking initiated in the softened 4140 TMAZ near the interface. The intermediate PWHT temperature of 625 °C offered the best balance of limited carbon diffusion across the interface, relatively low peak weld hardness and minimized hardness gradients across the interface, more homogenous deformation, and good bend test performance.

4140 low-alloy steel↗

Creep Resistant Martensitic Steels for Operation at High-Temperatures in Power Generation Applications

Increasing the temperature capabilities of ferritic/martensitic 9-12% Cr steels can help in increasing the operating temperature of land-based turbines and minimize the use of expensive high-temperature alloys in the hot section. A creep resistant martensitic steel, JMP, was developed with the potential to operate at or above 650°C. The design of the alloys originated from computational modeling for phase stability and precipitate strengthening using fifteen constituent elements. Cobalt was used for increased solid solution strengthening, Si for oxidation resistance and different W and Mo concentrations for matrix strength and stability. The JMP steels showed increases in creep life compared to MARBN/SAVE12AD at 650°C for testing at various stresses between 138 MPa and 207 MPa. On a Larson-Miller plot, the performance of the JMP steels surpasses that of state-of-the-art MARBN steel. Approximately 21 years of cumulative creep data are reported for the JMP steels which encompasses various compositions. The relationships between composition-microstructure-creep properties are discussed including characterization of microstructures after >20,000 hours in creep.

Detrois, Martin↗

Primary and Low-Strain Creep Models for 9Cr Tempered Martensitic Steels Including the Effects of Irradiation Softening and High-Helium Re-Hardening

Primary and low-strain creep represents a very important integrity challenge to large, complex structures, like fusion reactors. Here, we develop a predictive empirical primary creep model for 9Cr tempered martensitic steels (TMS), relating the applied stress (σ) to strain (ε), time (t) and temperature (T). The most accurate model is based on the applied σ normalized by the steel’s T-dependent ultimate tensile stress (σo), σ/σo(T). The model, fit to 17 heats of 9Cr TMS, yielded a σ root mean square error (RMSE) of ≈±11 MPa. Notably, the model also provides robust predictions for all the other TMS, when calibrated only by the fusion candidate Eurofer97 database. The model was extended to explore two possible effects of neutron irradiation, which produces both displacements per atom (dpa) and helium (He in atomic parts per million, appm) damage. These effects, which have not been previously considered, include: (a) softening, as a function of dpa, at T > ≈400–450 °C, in low-He fission environments (<1 He/dpa); and (b) subsequent re-hardening in high-He (≥10 He/dpa) fusion first-wall environments. The irradiation effect models predict (a) accelerated primary creep due to irradiation softening; and (b) fully arrested creep due to high-He re-hardening.

Alam, Md Ershadul (ORCID:0000000345968026)↗

Deuterium trapping mechanisms in reduced activation ferritic martensitic steels and their correlation with mechanical strengthening

Development of high-strength materials often involves introduction of additional strengthening microstructures that also serve as tritium trapping sites. Such additions in fusion material development could degrade the fuel efficiency in fusion reactors and raise radiological concerns. The contribution of individual microstructure features in hydrogen trapping must be evaluated to ensure fuel efficiency and radiological safety. This study explores the mechanistic origins of deuterium trapping in reduced-activation ferritic–martensitic steels and its correlation to mechanical strengthening. A series of model alloys and engineering steels were fabricated and subjected to different heat treatments to control deuterium trapping site density. Deuterium retention was evaluated using D 2 gas charging and thermal desorption spectroscopy, focusing on the role of grain boundary, dislocation, M 23 C 6 precipitates, and TiC precipitates. Multiscale microstructure characterization and synchrotron X-ray diffraction were performed to characterize microstructure, which was correlated to the deuterium retention property. Results show that TiC precipitates exhibit the highest deuterium trapping capacity, followed by M 23 C 6 precipitates. Dislocation and grain boundary demonstrate the lowest and similar efficiencies. Furthermore, the relationship of trapping quantity and mechanical strengthening of these microstructure features was quantified, demonstrating that TiC precipitates offer highest deuterium trapping per unit of mechanical strengthening.

Retention↗

Radiation induced amorphization of carbides in additively manufactured and conventional ferritic-martensitic steels: In-situ experiments on extraction replicas

In-situ irradiations using 1 MeV Kr 2+ ions in a transmission electron microscope were performed on extraction replica samples containing M 23 C 6 carbides and MX carbonitrides from two ferritic-martensitic (FM) steels: (i) 9%Cr-1%W-TaV based Eurofer97 and (ii) 9%Cr-1%Mo-VNb (all in wt.%) based additively manufactured (AM) Grade91 steel. The irradiations were performed between 100 and 773 K up to a maximum dose of ~2.4 displacements per atom (dpa). The M 23 C 6 carbides are highly susceptible to radiation induced amorphization (RIA), while the MX type nanoprecipitates are highly amorphization resistant across the entire irradiation temperature range. Between 100 and 423 K, RIA of M 23 C 6 carbides occurs very rapidly with critical amorphization doses ranging between ~0.35 and 0.9 dpa, increasing to higher doses at 573 K. Complete amorphization of the M 23 C 6 carbides up to doses of ~2.4 dpa is not possible at 773 K under the present irradiation conditions. The critical amorphization dose of M 23 C 6 carbides increases nearly exponentially with irradiation temperature. The critical temperature for the crystalline-to-amorphous phase transformation (T c→a ) of M 23 C 6 carbides irradiated as replica samples, i.e. without the surrounding metal matrix, was estimated to be ~812 K. Comparing the present results with neutron irradiation data on bulk samples reveals a decrease in the critical amorphization dose for M 23 C 6 and an increase of T c→a , highlighting the effect of dose rate on the amorphization behavior that is qualitatively consistent with literature on other non-metals. Changes in the minor chemistry of M 23 C 6 , such as presence or absence of W, V, Nb, Mo, seems to have little effect on the amorphization behavior. Here, in-situ irradiations on extraction replica samples provide a novel pathway to explore radiation tolerance of nanoprecipitates in nuclear structural materials

36 MATERIALS SCIENCE↗

Characteristics and mechanisms of hydrogen-induced quasi-cleavage fracture of lath martensitic steel

Here this study presents an in-depth characterization of the microstructures, crystallographic orientations, and dislocation characteristics beneath hydrogen-induced quasi-cleavage fracture features of an as-quenched, lath martensitic (α') 22MnB5 steel. The fracture surfaces of gaseous hydrogen-embrittled martensitic specimens were analyzed by a combination of multiple analytical tools: scanning electron microscopy (SEM), electron backscatter diffraction (EBSD), transmission electron microscopy (TEM), and transmission Kikuchi diffraction (TKD). The dominant fracture mode in the hydrogen-affected zones was quasi-cleavage fracture, which involved significant plasticity, evidenced by plastic zones near tear ridges and a high density of dislocations beneath the quasi-cleavage facets. The martensite constituent sizes, variant orientations, and boundaries influenced the quasi-cleavage surface morphologies. Fractography revealed the occurrence of {100} α' -type cleavage across martensitic laths, developing relatively “flat” quasi-cleavage surfaces, in addition to {110} α' -type cracking likely along lath and block boundaries, and fracture along non-cleavage planes. The likelihood of the formation of the relatively “flat” quasi-cleavage surfaces increased with increasing martensitic constituent sizes. Substantial dislocation bands formed on intersecting {112} α' slip planes within a martensite block below the hydrogen-induced cleavage fractures on {100} α' planes. River markings on the quasi-cleavage surfaces were found to originate from the complex, hierarchical lath martensitic microstructure. Steps and ridges on the quasi-cleavage facets generally linked with the various martensitic boundaries, suggesting that they were produced as a result of crack deviations at those boundaries. The fracture paths and martensite quasi-cleavage mechanisms are discussed in the context of the role of hydrogen and Cottrell cleavage model.

36 MATERIALS SCIENCE↗

Microstructures and mechanical properties of a modified 9Cr ferritic-martensitic steel in the as-built condition after additive manufacturing

A newly developed nano-structured high-Mn 9Cr ferritic-martensitic (FM) steel designed for additive manufacturing (Additive-manufactured Nanostructured Alloy, ANA) was fabricated via the direct energy deposition method. The as-printed ANA2 showed tensile properties (strength and elongation) and Charpy impact toughness (upper-shelf energy and ductile-brittle transition temperature) comparable to oxide-dispersion-strengthened (ODS) Eurofer and PM2000. Compared with wrought P91, the as-built ANA2 showed significantly higher yield strength but inferior Charpy impact toughness and ductility. Microstructural characterization revealed uniformly distributed sub-micron pores, an extremely high dislocation density, and a high density of ultrafine nano-structured precipitates in the matrix. The microstructures indicated the dislocations as the dominant strengthening element and the ultrafine precipitates as the primary contribution to estimated irradiation sink density. This work demonstrates the ability to exploit the unique consolidation properties of additive manufacturing to fabricate steels which marry the benefits of both ODS alloys and conventionally processed FM steels.

36 MATERIALS SCIENCE↗

A novel design of transitional layer structure between reduced activation ferritic martensitic steels and tungsten for plasma facing materials

Plasma-facing components (PFCs) are among the most critical gaps for fusion energy to establish technical and economic feasibility. Tungsten as a first wall/blanket material in PFCs requires to be integrating with reduced activation ferritic martensitic (RAFM) steels as a structural component. Currently, major drawbacks are the requirement of brazing, the formation of a brittle interface, and a large difference between the coefficients of thermal expansion of tungsten and steel. Here, a novel transitional multilayer structure was designed and investigated to join tungsten and RAFM steels using three interlayers. The composition of each interlayer was selected based on computational thermodynamics and diffusion kinetics to ensure a body-centered cubic (bcc) single-phase structure and prevent the formation of a brittle intermetallic phase region in the temperature range of 600–1150 °C. Although the transitional layer structure was designed for additive manufacturing, spark plasma sintering (SPS) as proof of concept was used to bond the individual layers. Interfaces were investigated using scanning and transmission electron microscopy methods but no layered intermetallic phase was observed. Nanoindentation maps across the interface suggest major hardness differences at the interface between tungsten and the vanadium interlayer, as well as the interface between RAFM steel and the FeCrAl interlayer.

36 MATERIALS SCIENCE↗

How Austenitic Is a Martensitic Steel Produced by Laser Powder Bed Fusion? A Cautionary Tale

Accurate phase fraction analysis is an essential element of the microstructural characterization of alloys and often serves as a basis to quantify effects such as heat treatment or mechanical deformation. Additive manufacturing (AM) of metals, due to the intrinsic nonequilibrium solidification and spatial variability, creates additional challenges for the proper quantification of phase fraction. Such challenges are exacerbated when the alloy itself is prone to deformation-induced phase transformation. Using commonly available in-house X-ray diffraction (XRD) and electron backscatter diffraction (EBSD) and less commonly used synchrotron-based high-energy X-ray diffraction, we characterized nitrogen-atomized 17-4 precipitation-hardening martensitic stainless steel, a class of AM alloy that has received broad attention within the AM research community. On the same build, our measurements recovered the entire range of reported values on the austenite phase fractions of as-built AM 17-4 in literature, from ≈100% martensite to ≈100% austenite. Aided by Calphad simulation, our experimental findings established that our as-built AM 17-4 is almost fully austenitic and that in-house XRD and EBSD measurements are subject to significant uncertainties created by the specimen’s surface finish. Hence, measurements made using these techniques must be understood in their correct context. Our results carry significant implications, not only to AM 17-4 but also to AM alloys that are susceptible to deformation-induced structure transformation and suggest that characterizations with less accessible but bulk sensitive techniques such as synchrotron-based high energy X-ray diffraction or neutron diffraction may be required for proper understanding of these materials.

17-4 steel↗

Effect of stress on Laves phase precipitation in creep ruptured Grade 92 ferritic martensitic steel characterized by a novel accessible method

At high temperature conditions relevant to fossil and nuclear energy plants, Laves phase (Fe 2 X, X=Mo, W) precipitation is observed in common ferritic martensitic (FM) structural steels, with various reported effects on creep behavior. Despite being valuable metrics to correlate with mechanical properties and other precipitate phases, the volume fraction and number density of Laves phase precipitates has been difficult to quantify accurately using common techniques such as transmission electron microscopy (TEM) due to the relatively large size (∼0.25 μm) and low number density (∼10 11 cm −3 ) of Laves precipitates. Here, to address this characterization challenge, we developed and demonstrated a high-throughput and widely accessible method to quantify the volume fraction and number density of the Laves phase based on scanning electron microscope (SEM) images with a backscattered electron signal and the information depth (ID) of backscattered electrons. We applied this new technique in creep ruptured Grade 92 FM steel to study the effect of Laves phase on creep properties and determine the influence of stress on Laves phase precipitation. The quantitative accuracy of the SEM-based volume fraction and number density values was verified using synchrotron high energy X-ray diffraction and serial sectioning tomography. Stress did not significantly affect the Laves phase size or volume fraction during creep testing at 550 – 650°C and stress levels of 90 – 260 MPa (vs. unstressed conditions). Conversely, a moderate but statistically significant stress-enhanced increase in Laves phase number density, corresponding to an increase in nucleation rate, occurred during creep exposure above 110 MPa.

Creep↗

Austenitic parent grain reconstruction in martensitic steel using deep learning

In this work we develop a deep convolutional architecture to estimate the prior austenite structure from observed martensite electron backscatter diffraction micrographs. A novel data augmentation strategy randomizes the global reference coordinate system which makes it possible to train our model from only four micrographs. The model is much faster than algorithmic approaches and generalizes well when applied to micrographs of a different material. Empirical evidence suggests the efficacy of the model depends on the scale of the microstructure and receptive field of the vision model. Furthermore, this work demonstrates that modern computer vision approaches are well suited for capturing complex spatial-orientation patterns present in orientation imaging micrographs.

36 MATERIALS SCIENCE↗

The Role of Co-injected Helium on Swelling and Cavity Evolution at High Damage Levels in Ferritic-Martensitic Steels

The influence of helium co-injection at rates from 0 to 4 appm He/dpa on swelling in ferritic-martensitic alloys T91 and HT9 was explored. Irradiations with 5.0 MeV Fe++ ions and degraded He++ ions were performed at 445°C up to damage levels of 150 dpa and helium co-injection rates of 0, 0.02, 0.2 and 4 appm He/dpa in T91, and at 460°C to a damage level of 188 dpa and helium co-injection rates of 0, 0.06 and 4 appm He/dpa in HT9. Helium was observed to enhance cavity nucleation at low damage levels, resulting in the maximum swelling at the highest helium co-injection rate. As the damage level was increased, the helium content at which swelling was maximized shifted to lower helium concentrations, ultimately resulting in the highest swelling occurring with zero helium by 150 dpa. Finally, this behavior was due to the helium-stabilized bubble microstructure that increased the cavity sink strength and reduced both cavity growth rate and swelling relative to the helium-free condition.

36 MATERIALS SCIENCE↗

Uncertainty Quantification Framework for Predicting Material Response with Large Number of Parameters: Application to Creep Prediction in Ferritic-Martensitic Steels Using Combined Crystal Plasticity and Grain Boundary Models

This paper presents an uncertainty quantification (UQ) framework for the physics-based model prediction of material response with a large number of parameters. The application problem presented in this work is that of predicting creep in Grade 91 steel at 600°C. The material response is defined with a physically based microstructural model with constitutive equations emulating several observed phenomena in Grade 91 and embodied into an explicit geometry mesoscale finite element model for prior austenite grains and grain boundaries. Creep within the grains and in grain boundaries are represented by crystal plasticity for dislocation motion and a physics-based model for cavity growth and nucleation, respectively. The creep behavior of this material is influenced by several parameters, some of which have a wide range of variation based on experimental data. UQ combined with microstructural modeling can discover the core microstructural causes of experimental variability, leading to improved materials with lower variability in critical long-term material properties. In this study, we investigate the model's uncertainty to identify material properties that may be modified during production to increase creep life and analyze different components of the crystal plasticity model for improvements. For this purpose, a quantity of interest is defined as time to minimum creep rate, which correlates well to the creep failure of the material. A deep neural network model was trained and validated to be used as a surrogate for the finite element model. Then, a variance-based sensitivity analysis is performed on the surrogate model to find the Sobol indices of the input parameters in respect to the output quantity of interest. The Sobol indices are used to reduce the dimensionality of the model. Generalized polynomial chaos expansion is used on the reduced basis models to propagate the uncertainty from the input parameters to the quantity of interest using the deep neural network surrogate model. These results are benchmarked against uncertainty propagation using Monte Carlo simulations. In conclusion, the UQ performed through the reduced basis model captures almost all the uncertainty in the model with significantly fewer simulations, making it possible to perform the UQ directly via simulations with the finite element model rather than surrogate machine-learned models.

36 MATERIALS SCIENCE↗