At least 19 records

Understanding the effect of minor alloying elements on helium bubble formation in ferritic-martensitic steels

Ferritic-martensitic steels are promising structural materials for advanced nuclear reactors. To minimize long-term radioactivity, reduced-activation ferritic-martensitic steels have been developed by substituting high-activation elements like Ni and Mo with low-activation elements such as W. However, the impact of these alloying modifications on helium bubble formation, which plays a key role in material swelling, remains unclear. Here, in this study, we compared helium bubble formation in ferritic-martensitic steel T91 and reduced-activation ferritic-martensitic steel F82H. Both materials were irradiated with sequential 100 keV, 150 keV, and 200 keV helium ions to a dose of 0.5 dpa and a helium concentration of 9,000 appm at 500°C. The helium bubbles in F82H exhibited a larger average size and a lower density than those in T91, suggesting differences in minor alloying elements may influence the bubble growth. Here, to investigate the effects of these alloying elements, we characterized radiation-induced segregation near bubbles and grain boundaries. Prominent Ni-Mn-Si enriched clusters were found near bubbles in T91, while only Mn-Si enriched clusters were found near bubbles in F82H. In addition, the obvious Cr enrichment near grain boundaries was absent around bubbles in both steels. The different segregation trends among elements revealed the variations in element diffusion mechanisms and the different sink biases between bubbles and grain boundaries. Cr enrichment near grain boundaries is mostly driven by interstitial-mediated diffusion. However, since bubble growth relies on net vacancy flux, vacancy-mediated diffusion plays a dominant role in controlling element segregation near bubbles. Therefore, Cr enrichment was not found near bubbles. Because of preferential vacancy-drag diffusion for Ni, Si and Mn, these elements were enriched near bubbles. Due to the strong binding energies of vacancies with these solute atoms, the vacancy diffusivity can be reduced near these solutes. Therefore, the more prominent Ni-Si-Mn clustered near helium bubbles in T91 lead to stronger suppression of helium bubble growth compared to F82H.

36 MATERIALS SCIENCE↗

Creep-Resistant Ferritic-Martensitic Steels for Power Plant Applications

Creep-resistant ferritic-martensitic steels are essential materials used in power plants for electricity generation. The efficiency and emissions of the plant are closely related to the operating temperature. Materials used in the hottest sections are one of the main limiting factor for plant operation at 650 °C. This review describes the recent development of creep-resistant ferritic-martensitic steels from a large dataset of in-house research. The findings are tied to available literature for discussion. A first steel, CPJ-7, was developed with an operating temperature approaching 650 °C, and a refined design, JMP, showed the potential to operate at 650 °C. Approximately fifty different ingots, each weighing ~ 7 kg, were vacuum induction melted and processed. Overall, wrought and cast versions of CPJ-7 present superior creep properties when compared to wrought and cast versions of COST alloys for steam turbine and P91/92 for boiler applications. The prolonged creep life was attributed to slowing down the process of the destabilization of the MX and M 23 C 6 precipitates at 650 °C. The cast version of CPJ-7 also revealed superior mechanical performance, above commercially available cast 9% Cr martensitic steel or derivatives. Following the work on CPJ-7, the JMP steels were designed with higher Co for increased solid solution strengthening, Si for oxidation resistance and increased W for matrix strength and stability. The JMP steels showed increases in creep life compared to CPJ-7 between 118 and 150% at 650 °C for testing at various stresses between 138 and 207 MPa. On a Larson–Miller plot, the performance of the JMP steels surpasses that of state-of-the-art MARBN steel. The influence of various elements within the composition of the alloys on the microstructure and mechanical properties is discussed. This review presents approximately 420,000 h of in-house creep testing, the equivalent of almost 50 years of cumulative creep tests.

36 MATERIALS SCIENCE↗

Development of Novel Ferritic-Martensitic Steels with Superior Creep Properties for Power Plant Applications

A creep resistant martensitic steel, CPJ-7, was developed with an operating temperature approaching 650°C. Subsequently, another creep resistant martensitic steel, JMP, was designed with the potential to operate at, or slightly above, 650°C. This report describes the development of these alloys from early iterations of CPJ steels to the final CPJ-7 formulation as well as the more heat resistant JMP steel formulation. The design originated from computational modeling for phase stability and precipitate strengthening using fifteen constituent elements. Approximately forty heats of CPJ and ten of JMP, each weighing ~7 kg, were vacuum induction melted. A computationally optimized heat treatment schedule was developed to homogenize the ingots prior to hot forging and rolling prior to final normalization and tempering. Overall, wrought and cast versions of CPJ-7 present superior creep properties when compared to wrought and cast versions of COST alloys for steam turbine and wrought and cast versions of P91/92 for boiler applications. For instance, the Larson Miller Parameter curve for CPJ-7 at 650°C almost coincides with that of COST E at 620°C. The prolonged creep life was attributed to slowing down the process of the destabilization of the MX and M 23 C 6 precipitates at 650°C. On the other hand, the cast version of CPJ-7 also revealed superior mechanical performance, well above commercially available cast 9% Cr martensitic steel or derivatives, especially for creep life at 650°C. The casting process employed slow cooling to simulate the conditions of a thick wall full-size steam turbine casing but utilized a separate homogenization step prior to final normalization and tempering. To advance the development of CPJ-7 for commercial applications, a process was used to scale up the production of the alloy using vacuum induction melting (VIM) and electroslag remelting (ESR), which underlined the importance of melt processing control of intentionally designed minor and trace elements in these advanced alloys. Following the work on CPJ-7, the JMP steels were designed with higher Co for increased solid solution strengthening, Si for oxidation resistance and increased W (with low Mo content) for matrix strength and stability as well as solid solution strengthening. The JMP steels showed increases in creep life compared to CPJ-7 between 118 to 150% at 650°C for testing at various stresses between 138 MPa and 207 MPa. On a Larson-Miller plot, the performance of the JMP steels surpasses that of state-of-the-art MARBN and other MARBN-type steels. The influence of various elements within the composition of the alloys on the microstructure and mechanical properties are discussed. This report presents approximately 420,000 h of in-house creep testing, the equivalent of almost 50 years of cumulative creep tests.

36 MATERIALS SCIENCE↗

The microstructure effects on irradiation response of ferritic – martensitic steels

Microstructural optimization to achieve greater mechanical strength has been one of the focuses in ferritic–martensitic steels development. However, these optimized microstructures’ effects on the radiation response are not well known. In this work, two ferritic–martensitic steels (9Cr-NbMo and 9Cr-Ta) underwent neutron irradiation in the High Flux Isotope Reactor, and their room-temperature post-irradiation tensile properties and microstructure evolutions were investigated and compared. These two steels exhibit similar pre-irradiation tensile behavior, and their yield strengths are higher than that of other ferritic–martensitic steels by about 200–250 MPa. Microstructural characterization on pre-irradiated materials reveals a smaller grain size in 9Cr-Ta (2.8 ± 0.3 μm in 9Cr-Ta versus 4.3 ± 0.5 μm in 9Cr-NbMo) but higher dislocation density and precipitate density in 9Cr-NbMo. As is common for ferritic–martensitic steels at low irradiation temperatures (less than about 0.45T m ), irradiation-induced hardening at 400 °C was observed for both alloys. Irradiation at 490 °C causes the two alloys to exhibit different tensile behavior: 9Cr-Ta softens by 208 MPa in yield stress, whereas 9Cr-NbMo maintains strength. Additionally, microstructural characterizations were performed, including precipitate growth, dislocation, and defect formation. Using the barrier hardening model for microstructure–property correlation, the softening in irradiated 9Cr-Ta is primarily attributed to the significant dislocation recovery, while the strength lost from the slight dislocation recovery in 9Cr-NbMo was compensated by the additional strength from the irradiation-induced cavities. The microstructure effect (primarily precipitate, dislocation and boundary) on the radiation response is discussed herein.

36 MATERIALS SCIENCE↗

A fusion relevant data-driven engineering void swelling model for 9Cr tempered martensitic steels

The UCSB database on cavity evolution in 9-12Cr tempered martensitic steels (TMS), includes the results for both dual heavy and helium ion (DII), and High Flux Isotope Reactor (HFIR) in situ helium injection (ISHI) neutron irradiations at 500°C. These results were combined with literature single ion and fission neutron irradiation data to derive a model for the void volume fraction, f v , as a function of displacements per atom (dpa) and transmutant helium concentrations in atomic parts per million (appm). The scientific foundation for the paper is described in a companion paper entitled “Cavity Evolution and Void Swelling in Dual Ion Irradiated Tempered Martensitic Steels”. Here, in this study, we show that f v (dpa, He/dpa) is described by the incubation dose, dpa i , for the onset of void growth, and the post-incubation growth rate, f v ’(%/dpa). Both dpa i and f v ’ decrease with increasing He/dpa at > ~ 5. The dpa i is also lower for the ISHI neutron irradiations at the same He/dpa. Single heavy ion and fission reactor neutron irradiations, with low He/dpa ratios, have a much larger dpa i . Based on a combined analysis of DII, single ion, ISHI and fission neutron data, we further show that the post-incubation f v data analyzed here have a common empirical curve shape, with f v ’ reaching up to ~ 0.2%/dpa at very high dpa. We also show that f v ’ can be predicted based on a physical model of defect partitioning between evolving sinks. At 500°C and fusion relevant He/dpa ≈ 10, the best-fit model predicts nominal swelling, S = f v /(1-f v ), of ~ 1.1, 4.9 and 16% at 50, 100 and 200 dpa, respectively. The physically motivated, data-driven model includes estimated uncertainties for both dpa i and f v ’.

36 MATERIALS SCIENCE↗

Evaluation of High-Temperature Martensitic Steels for Heavy-Duty Diesel Piston Applications

Five different commercially available high-temperature martensitic steels were evaluated for use in a heavy-duty diesel engine piston application and compared to existing piston alloys 4140 and microalloyed steel 38MnSiVS5 (MAS). Finite element analyses (FEA) were performed to predict the temperature and stress distributions for severe engine operating conditions of interest, and thus aid in the selection of the candidate steels. Complementary material testing was conducted to evaluate the properties relevant to the material performance in a piston. The elevated temperature strength, strength evolution during thermal aging, and thermal property data were used as inputs into the FEA piston models. Additionally, the long-term oxidation performance was assessed relative to the predicted maximum operating temperature for each material using coupon samples in a controlled-atmosphere cyclic-oxidation test rig. A current commercial steel piston alloy, quenched and tempered martensitic steel 4140, was tested in a single-cylinder research engine for a baseline oxidation and mechanical performance assessment using an abbreviated (50h) durability test plan. The predicted suitability of a candidate piston material in an engine is primarily based on its elevated temperature strength, oxidation resistance, and the complex influence of thermal conductivity, the latter of which is substantially lower for the candidate materials considered in this research relative to the traditional alloys. Although the lower thermal conductivity causes the candidate alloys to operate in higher temperature ranges under identical engine operating conditions and piston geometries, increasing the likelihood of partially or completely negating their strength and oxidation resistance advantages relative to 4140 and MAS steels, this evaluation indicates that several of the candidate piston alloys are predicted to enable improved oxidation resistance under more severe engine operating conditions relative to the current piston materials. However, further evaluation is required to determine if the elevated temperature fatigue strength and durability of these alloys are suitable for more severe engine conditions.

36 MATERIALS SCIENCE↗

Effects of niobium and tantalum on the microstructure and strength of ferritic-martensitic steels

Herein, detailed investigations of two ferritic-martensitic steels, i.e., Nb- and Ta-steel, indicate that the higher Nb diffusivity and the lower nucleation driving force of Nb-carbide promote preferential nucleation of Nb-carbides at grain boundaries and thus a higher boundary occupancy than Ta-carbides, which favored greater creep resistance of Nb-steel than that of Ta-steel despite their similar yield strength.

36 MATERIALS SCIENCE↗

ORNL Post-irradiation Examination (LAMDA) Final Report on Characterization of Irradiated Grade 92 Ferritic-Martensitic Steels

Irradiation effects on ferritic-martensitic steel Grade 92 were investigated in this project. Samples from two heats of Grade 92, i.e., G92-2b and NF616, were selected, which were irradiated in the High Flux Isotope Reactor (HFIR) and the Advanced Test Reactor (ATR), respectively. Samples from two heats of ferriticmartensitic steel T91, irradiated in the ATR, were also selected as references for the Grade 92 samples. The selected G92-2b samples were irradiated to 0.5–14.7 displacements per atom (dpa) at two temperature regimes: 400–497 °C and 683–720°C. The selection of the high irradiation temperatures up to ~720°C is to test the performance at such upper bound temperatures, which would provide insights for the upper bound applicable temperature for Grade 92. The selected NF616 and T91 samples were irradiated to 3–8.2 dpa at 292–448°C. Except for T91 heat2 samples in 3-mm diameter discs, all the other selected samples are of type SS-J2 miniature tensile specimens. Two Nuclear Science User Facilities (NSUF), i.e., the Irradiated Materials Examination and Testing (IMET) hot cell facility and the Low Activation Materials Design and Analysis (LAMDA) facility, were used in the Post-Irradiation Examination (PIE) activities for the selected samples, which include: Tensile tests at room temperature (IMET); Fractography of the tensile fracture surfaces (LAMDA: scanning electron microscopy and energy; dispersive spectroscopy); Vickers hardness measurements (LAMDA); and Microstructural characterization (LAMDA: electron backscatter diffraction, focused-ion beam, and transmission electron microscopy).

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Creep of MARBN-type 9Cr martensitic steel in gaseous CO 2 environment

Here, with an interest in moving from steam to supercritical CO 2 as the working fluid in advanced energy systems, it is important to study the mechanical response of structural alloys to CO 2 -containing environments. MARBN-type 9Cr martensitic steel was originally developed for application in boilers for supercritical and ultra-supercritical power plants where the steam temperature reaches 650 °C. In this research, a MARBN-type 9Cr martensitic steel designed and manufactured at NETL was creep tested in a gaseous CO 2 environment (i.e., 0.1 MPa at 650 °C), and the results are directly compared to creep tests conducted in air. It was found that environmentally-assisted cracking facilitated by carbide formation beneath the growing oxide accelerated failure in gaseous CO 2 . This work indicates that creep-oxidation interactions in advanced martensitic steels represent an important consideration for materials selection in supercritical CO 2 power cycles. Furthermore, this work confirms that more oxidation-resistant alloys will be required for the highest temperature portions of these systems.

36 MATERIALS SCIENCE↗

Benchmarking a 9Cr-2WVTa Reduced Activation Ferritic Martensitic Steel Fabricated via Additive Manufacturing

Reduced activation ferritic (RAF) martensitic steels are promising candidates for the first wall of fusion reactors. However, current manufacturing capabilities call for these components to be made by welding wrought plates. This limits design freedom and necessitates the use of post-weld heat treatments (PWHT) in accordance with the boiler and pressure vessel code. Additive manufacturing (AM) can offer a unique solution to solve this challenge by leveraging the layer-wise deposition strategy to come up with temper bead deposition techniques to eliminate post-processing heat treatments (PPHT). However, it is necessary to benchmark the properties of RAF steels fabricated by AM with their wrought counterparts to identify the process-structure-property correlation, which is the goal of this study. The study demonstrates that while tensile properties at room temperature and high temperatures are satisfactory, the as fabricated and samples after PPHT have significant heterogeneity in tensile elongation. This has been attributed to the presence of discontinuities in the build. The as-fabricated samples have an average tensile strength of 1190 + 12 MPa and an average elongation of 15 + 5% at room temperature and 658 ± 20 MPa ultimate tensile strength (UTS) and 14 ± 7% at 600 °C. After the post-weld heat treatment, mechanical properties decrease to around 600–650 MPa and an elongation between 20–25% at room temperature to 300 MPa UTS and 25–28% elongation at 600 °C. The characterization of microstructures at various length scales demonstrates that the as-fabricated structure has a significant fraction of delta ferrite in a lath martensitic matrix. No precipitates could be identified in the as-fabricated structure. PPHT led to a decrease in the area fraction of delta ferrite and precipitation of M 23 C 6 and MX. Detailed characterization clearly demonstrates that the lack of precipitates in the as-fabricated structure could be due to the slow tempering response of the alloy. Finally, the needs to develop new alloys to achieve the objectives stated above are articulated.

36 MATERIALS SCIENCE↗

Cavity evolution and void swelling in dual ion irradiated tempered martensitic steels

Microstructural evolutions in two variants of the F82H 8 wt%Cr tempered martensitic steel under dual (He + plus Fe 3+ ) ion irradiations at 500 °C have been characterized by transmission electron microscopy. Emphasis is on understanding the combined effects of displacements per atom (dpa) and the helium/dpa ratio (He/dpa) on cavity evolution and void swelling (f v ). The dual ion database includes 231 alloy-dpa-He/dpa conditions for irradiations up to ~ 82 dpa and 3700 appm helium. Here, we hypothesize that the large “scatter” observed in the f v data is primarily due to local microstructural variations, especially those that shield regions at shallower depths from the effects of injected interstitial atoms, which would otherwise reduce f v . More generally, our hypothesis is that the highest f v data, at a specified dpa and He/dpa, provides the most appropriate estimate of swelling for fusion neutron irradiation conditions. The dose dependence of f v can be described by an incubation dpa i , marking the onset of significant void growth, and a post-incubation swelling rate, f v ’ = Δf v /Δdpa. Both dpa i and f v ’ decrease with increasing He/dpa. The f v ’ data are quantitatively consistent with a simple model for defect partitioning between evolving bubble, void, and dislocation sinks strengths and biases. Most notably, the model correctly predicts both the incubation dpa i , and the subsequent f v ’, in spite of the fact that they reflect somewhat different physics. Our analysis also suggests that defect recombination is modest at 500 °C. Along with other considerations, this supports the hypothesis that, even at high dpa rates, dual ion irradiations can be used to reasonably emulate void nucleation and growth for a range of fusion-relevant neutron irradiation service conditions. A companion paper incorporates the results of this study in a reduced-order, data-driven void swelling model.

36 MATERIALS SCIENCE↗

Development of creep resistant ferritic-martensitic steels for operation at 650°C

Creep resistant ferritic-martensitic steels capable of operating at 650°C have long been under development for electricity generation. This presentation will showcase the design and development of alloys CPJ-7 and JMP with approximately 420,000 h of in-house creep testing, the equivalent of ~50 years of cumulative creep tests. Approximately fifty different alloy compositions were manufactured as part of an ICME approach. CPJ-7 present superior creep properties compared to COST alloys for steam turbine and P91/92 for boiler applications. The prolonged creep life was attributed to slowing down the destabilization of fine precipitates at 650°C. The JMP steels were designed with higher Co for solid solution strengthening and increased W for matrix strength and stability. The creep life compared to CPJ-7 increased between 118 and 150% at 650°C depending on the stress. On a Larson-Miller plot, the performance of the JMP steels surpasses that of MARBN steel. Composition-microstructure-properties relationships will be discussed.

Detrois, Martin↗

Modeling of Stress and Temperature Effects on Creep of Reduced Activation Ferritic-Martensitic Steel Alloy F82H (Tertiary Creep Modeling of RAFM Steel)

A Bayesian optimization procedure is presented for calibrating a multi-mechanism micromechanical model for creep to experimental data of F82H steel. Reduced activation ferritic martensitic (RAFM) steels based on are the most promising candidates for some fusion reactor structures. Although there are indications that RAFM steel could be viable for fusion applications at temperatures up to 600 °C, the maximum operating temperature will be determined by the creep properties of the structural material and the breeder material compatibility with the structural material. Due to the relative paucity of available creep data on F82H steel compared to other alloys such as Grade 91 steel, micromechanical models are sought for simulating creep based on relevant deformation mechanisms. As a point of departure, this work recalibrates a model form that was previously proposed for Grade 91 steel to match creep curves for F82H steel. Due to the large number of parameters (9) and cost of the nonlinear simulations, an automated approach for tuning the parameters is pursued using a recently developed Bayesian optimization for functional output (BOFO) framework [1]. Incorporating extensions such as batch sequencing and weighted experimental load cases into BOFO, a reasonably small error between experimental and simulated creep curves at two load levels is achieved in a reasonable number of iterations. Validation with an additional creep curve provides confidence in the fitted parameters obtained from the automated calibration procedure to describe the creep behavior of F82H steel at 600 °C. The model is further extended using a temperature dependent scaling law approach to simulate creep response between 550 °C and 650 °C. The efficacy of this extension is compared with the previously used scaling law approach for Grade 91 steel.

36 MATERIALS SCIENCE↗

Carburization and decarburization behavior of Grade 91 ferritic-martensitic steel in liquid sodium environments

Here, this paper presents a study of carbon transfer and its effect on microstructure and tensile properties of Grade 91 (G91) ferritic-martensitic steel exposed to sodium at 550–650 °C. Sodium exposure tests were conducted in Argonne's forced convection sodium loops up to exposure times of ~40,000 h. Thermal aging study of G91 steel was conducted in parallel to isolate the thermal aging effect from the sodium effect. It was found that sodium exposures at 650 °C dissolved M 23 C 6 carbides, eliminated the martensite subgrain structure resulting in excessive grain growth and reduced the tensile strength by >50%, while sodium exposures at 550 and 600 °C had an insignificant effect on its microstructure and tensile properties. These effects were attributed to the carburization/decarburization process of G91 steel in sodium environments. Carbon concentrations in sodium were determined by a foil equilibration method. The estimated carbon concentration was in the range of 0.8–1.2 ppm in the SMT-1 loop and 0.3–0.7 ppm in the SMT-2 loop. Thermodynamic analysis of the carburization – decarburization process was conducted for G91 steels exposed in sodium environments. The carbon activity-concentration relationship for G91 was evaluated by considering four phases in G91, i.e. bcc ferrite, M 23 C 6 , NbC and VC carbides. It was found that the carburization-decarburization process in G91 steel was dictated by M 23 C 6 carbides at high carbon activities, while NbC and VC carbides dominated the process at low carbon activities. The calculated carburization-decarburization boundary showed that G91 would undergo decarburization at 650 °C and carburization at 550 °C in the sodium loop environments, which was consistent with our experimental observations. This experimental and theoretical analysis provided a basis for predicting the effect of carbon transfer on the integrity of reactor components in sodium environments and for the design of new alloys used in sodium-cooled fast reactors.

36 MATERIALS SCIENCE↗

Effects of helium on irradiation response of reduced-activation ferritic-martensitic steels: Using nickel isotopes to simulate fusion neutron response

Understanding the effects of helium on microstructures and mechanical properties of reduced-activation ferritic-martensitic steels is important to use of these steels in fusion reactor structures. The 9Cr-2WVTa steels were doped with 58Ni and 60Ni isotopes at 2 weight percent to control the rate of transmutation helium generation. The samples were irradiated in the High Flux Isotope Reactor to ~24 displacements per atom at nominal temperatures of 300, 400, and 500°C, producing 228 and 7 atomic parts-per-million helium in the 58 Ni- and 60 Ni-doped samples, respectively. Transmission electron microscopy revealed a variety of precipitates and the radiation-induced dislocation loops and cavities (voids or helium bubbles). Tensile tests of the irradiated samples at the irradiation temperatures showed radiation-induced hardening at 300°C and radiation-induced softening at 400°C. Analysis indicates that the hardening primarily originated from the loops and cavities. The 58 Ni-doped samples had greater strengthening contributions from loops and cavities, leading to higher hardening with lower ductility than the 60 Ni-doped samples. The greater helium production of 58 Ni did not show pronounced reductions in ductility of the samples.

36 MATERIALS SCIENCE↗

Under the microscope: Reduced activation ferritic martensitic steel Eurofer-97 following ion-Irradiation and high-temperature high-pressure water exposure

Here, this study is designed to characterise the microstructural behaviour of Eurofer-97 steel under ion irradiation and subsequent exposure to high-temperature high-pressure (HTHP) water. Eurofer-97, a ferritic-martensitic steel, has been developed to withstand the conditions of fusion reactors in the locations in contact with coolant with an elevated level of neutron flux, such as the breeder-wall blanket. The material has been studied after self-ion irradiation (using Fe ions) simulating the microstructural effects of neutron irradiation limited to the subsurface layer. The corrosion properties of the Eurofer-97 steel were studied by exposure to HTHP water up to 331 °C. Advanced microstructural characterisation using scanning, transmission electron and focused ion beam microscopy was performed on the as-received microstructure and after ion irradiation. This was then characterised after exposure for 240 h in high-temperature water. Eurofer-97 had a dense, columnar Cr-rich inner oxide, followed by a Fe-rich outer oxide layer. In the irradiated condition the grain structure and oxide itself was less ordered. No appreciable difference in oxide thickness was identified between the irradiated and unirradiated specimens after this short exposure time.

36 MATERIALS SCIENCE↗

Effect of post-weld heat treatment on microstructure and mechanical properties of rotary inertia friction welded dissimilar 422-4140 martensitic steel piston joints

The study investigated how post‐weld heat treatment (PWHT) temperature affects the microstructure and localized deformation/fracture during bend testing of rotary inertia friction welds (RIFW) between AISI 422 stainless steel and AISI 4140 steel. RIFW produced a fully martensitic interface with approximately 550 HV hardness in both the thermo-mechanically affected (TMAZ) and heat‐affected zones (HAZ). Due to differences in temper resistance, the 4140 TMAZ/HAZ softened progressively under PWHT temperatures from 525 °C to 700 °C, while the 422 TMAZ unexpectedly maintained about 550 HV up to 600 °C before significantly softening at temperatures ≥625 °C. This asymmetric softening generated steep hardness gradients across the interface at temperatures ≤600 °C. Furthermore, carbon migration across the interface was minimal up to 600 °C, moderate at 625 °C, and by 700 °C produced a carbide‐rich eutectoid layer in the 422 TMAZ alongside a carbon‐depleted soft ferrite layer in the 4140 TMAZ. Strain during bending was PWHT‐dependent, concentrating on the 4140 side; in as-welded joints, the high hardness led to deformation and crack initiation in the base metals, whereas in PWHT samples, cracking initiated in the softened 4140 TMAZ near the interface. The intermediate PWHT temperature of 625 °C offered the best balance of limited carbon diffusion across the interface, relatively low peak weld hardness and minimized hardness gradients across the interface, more homogenous deformation, and good bend test performance.

4140 low-alloy steel↗