Remote Density Measurements of Molten Salts via Neutron Radiography

With an increased interest in the use of molten salts in both nuclear and non-nuclear systems, measuring important thermophysical properties of specific salt mixtures becomes critical in understanding salt performance and behavior. One of the more basic and significant thermophysical properties of a given salt system is density as a function of temperature. With this in mind, this work aims to present and layout a novel approach to measuring densities of molten salt systems using neutron radiography. This work was performed on Flight Path 5 at the Los Alamos Neutron Science Center at Los Alamos National Laboratory. In order to benchmark this initial work, three salt mixtures were measured, NaCl, LiCl (58.2 mol%) + KCl (41.8 mol%), and MgCl2 (32 mol%) + KCl (68 mol%). Resulting densities as a function of temperature for each sample from this work were then compared to previous works employing traditional techniques. Results from this work match well with previous literature values for all salt mixtures measured, establishing that neutron radiography is a viable technique to measure density as a function of temperature in molten salt systems. Finally, advantages of using neutron radiography over other methods are discussed and future work in improving this technique is covered.

Long, Alexander M. (ORCID:0000000343009454)↗

Atomic Diffusivities of Yttrium, Titanium and Oxygen Calculated by Ab Initio Molecular Dynamics in Molten 316L Oxide-Dispersion-Strengthened Steel Fabricated via Additive Manufacturing

Oxide-dispersion-strengthened (ODS) steels have long been viewed as a prime solution for harsh environments. However, conventional manufacturing of ODS steels limits the final product geometry, is difficult to scale up to large components, and is expensive due to multiple highly involved, solid-state processing steps required. Additive manufacturing (AM) can directly incorporate dispersion elements (e.g., Y, Ti and O) during component fabrication, thus bypassing the need for an ODS steel supply chain, the scale-up challenges of powder processing routes, the buoyancy challenges associated with casting ODS steels, and the joining issues for net-shape component fabrication. In the AM process, the diffusion of the dispersion elements in the molten steel plays a key role in the precipitation of the oxide particles, thereby influencing the microstructure, thermal stability and high-temperature mechanical properties of the resulting ODS steels. In this work, the atomic diffusivities of Y, Ti, and O in molten 316L stainless steel (SS) as functions of temperature are determined by ab initio molecular dynamics simulations. The latest Vienna Ab initio Simulation Package (VASP) package that incorporates an on-the-fly machine learning force field for accelerated computation is used. At a constant temperature, the time-dependent coordinates of the target atoms in the molten 316L SS were analyzed in the form of mean square displacement in order to obtain diffusivity. The values of the diffusivity at multiple temperatures are then fitted to the Arrhenius form to determine the activation energy and the pre-exponential factor. Given the challenges in experimental measurement of atomic diffusivity at such high temperatures and correspondingly the lack of experimental data, this study provides important physical parameters for future modeling of the oxide precipitation kinetics during AM process.

Chemistry↗

Assessment of Galvanic Corrosion in Molten Salts

Molten salts are an excellent choice for thermal energy storage materials in concentrated solar power (CSP) plants, yet some salts can cause corrosion of containment alloys that damage plants and increase maintenance costs. Corrosion rates have been characterized for many salt/alloy combinations. However, corrosion rates at junctions of dissimilar alloys in molten salts are relatively poorly characterized. At such junctions, which are common in CSP plants, it is possible that galvanic interactions or other mechanisms could increase corrosion above the industry standard of 20 µm/year. Preliminary reports measured corrosion at dissimilar alloy junctions with a variety of methods, but the results are not uniform. Additionally, some reports have shown that corrosion rates are higher for single alloys than for the same alloys when paired in a galvanic couple, suggesting complex corrosion mechanisms. Here we present a discussion on measuring galvanic corrosion in molten salts that accounts for differences in results between methods and explores the possibility of other mechanisms of corrosion in the system.

Massimi, Scott Edward (ORCID:0000000244008093)↗

Design of a Continuous Electrochemical Purification Reactor for Corrosion Mitigation in Molten Chloride Salt Systems

The utility of molten chloride salts in concentrating solar power (CSP) is dependent on the ability to maintain low corrosive impurities. Without proper purification, the corrosion rates of containment alloys exceed the industry standard of corrosion—under 20 μm/year. An extensive body of literature focuses on the initial purification stage of molten chloride salts. However, occurrences such as maintenance, leaks, and so forth expose the salt to the atmosphere and reintroduce impurities. Therefore, it is critical to develop a purification strategy that can control impurity levels during CSP plant operation. Here we present the design and fabrication of a purification vessel to continuously remove impurities out of flowing molten salt.

Witteman, Liam↗

Experimental Operation of a Prototype 750C Advanced Chloride Molten Salt Bellows Valve

To achieve DOE 2030 SunShot targets that reduce the cost of liquid-based solar by an additional 40% to 70% beyond 2018 costs, a more reliable, highly manufacturable flow valve, capable of achieving operational temperatures of >700°C is required [1]. This paper investigates the development of an innovative high-temperature chloride molten salt valve, with operation up to 750°C. This valve is intended to be employed within Gen 3 CSP liquid-based thermal energy storage (TES) systems as well as Gen 4 modular salt reactor (MSR) technologies. This work details the general design and flow testing of a bellows-seal flow control valve (FCV). This design includes an integrated closed-loop thermal control system to ensure robust design for freeze-thaw cycles. The self-contained thermal management STM system, is unique in the salt valve industry since it is an integrated solution to provide a consistent, repeatable alternative to typical heat tracing. Additionally, the design includes the employment of a novel heat pipe valve stem to facilitate enhanced passive thermal management into the valve assembly. This valve stem heat pipe is designed to facilitate natural circulation within the bonnet to ensure robust operation, during both nominal and transient thermal operation. The valve body and trim will be designed using SS316H, consistent with Flowserve Corporation’s existing product base and is code qualified but will utilize clad material for materials corrosion, manufacturing cost reduction and compatibility to ensure design flexibility. A test campaign was performed in this investigation utilizing a novel 750°C ternary chloride (20%NaCl/40%MgCl2/40%KCl by mol. wt. %) molten salt flow loop. A discussion about the design and installation of the valves within this test bed is provided for this investigation. Valve test results from this study assessed Cv curves as well as multiple actuator cycles, under varying thermodynamic and operational mode conditions, which would be characteristic within a commercial molten salt facility. The results indicate nominal operation for the baseline design, though improved performance and reliability is expected with the full designed FCV.

Armijo, Kenneth (ORCID:0000000346832147)↗

Molten salt environment creep testing extensometry system

Disclosed herein are systems, devices and methods for creep testing selected materials within a high-temperature molten salt environment. Exemplary creep testing systems include a load train for holding a test specimen under a load within a heated inert gas vessel. An extensometry system can be included to measure elongation of the test specimen while under load. The extensometry system can include fixed members and axially translating member that move along with the elongation of the test specimen, and the system can include a sensor to measure the relative axial motion between such components to measure elongation of the test specimen over time. The test specimen can include a cylindrical gage portion having an internal void filled with a molten salt during creep testing to simulate the corrosive effect of the molten salt on the specimen material during testing.

Ren, Wenlin↗

Multielectrode sensor for concentration and depth measurements in molten salt

A multi electrode sensor that provides in-situ, real time measurements for molten salts and other process fluids such as real-time concentration and salt level measurements for nuclear systems such as molten salt reactors, nuclear reprocessing facilities utilizing molten salts and concentrated solar power systems. The sensor has multiple electrodes with unique lengths which are connected to a potentiostat. Measurements are taken when the electrodes are immersed in the process fluid.

Hoyt, Nathaniel C.↗

Safeguards Material Control And Accountancy Considerations For Molten Salt Reactors

Molten salt reactors are a class of nuclear reactor designs with features and operational characteristics that vary significantly. Variations in design features include the physical, chemical, and isotopic composition of fresh and irradiated fuel, neutron energy spectrums, breeding ratios, and the design’s plans for chemical processing. Specific designs within these variations affect the material control and accountancy approaches implemented by both domestic and international nuclear safeguards. This paper identifies safeguards-relevant design features for molten salt reactors and describes how each feature might influence both domestic and international nuclear safeguards implementation. Additionally, this paper describes two potential general categories of material control and accountancy approaches that may be appropriate for molten salt reactors: a black box material-balance approach with measurements on the feed and waste streams combined with robust containment and surveillance on the nuclear material within the reactor or an approach that aims to quantify the nuclear material throughout the reactor (i.e., a process monitoring approach). This paper describes the benefits and challenges of these approaches to meet technical safeguards objectives and identifies gaps in current technologies.

Hogue, Karen↗

Corrosion evaluation of metal foams in eutectic molten salts for high temperature latent heat energy storage application

High-temperature Thermal Energy Storage (TES) has drawn great attention as a technology that can increase the role and profitability of micro nuclear reactors in the decentralized clean energy market. Various research needs have been proposed by Idaho National Laboratory (INL) in "the Integrated Energy Systems: 2020 Roadmap" with the goal of utilizing the high temperature of 550 degrees or more generated in the 4th generation reactor to industrial purposes from the standpoint of integrated energy systems [1]. With the recent development of the 4th generation nuclear power plant, including micro nuclear reactor, there is a great deal of interest in researching how to efficiently couple a heat source to an industrial process through thermal processing. Texas A&M University (TAMU) and INL are currently collaborating to develop a novel latent heat storage design called HITB (Heat pipe-Integrated Thermal Battery). As part of the small-scale experimental demonstration research for HITB, a study for storage medium selection was conducted at TAMU. Eutectic salts have attracted interest as high-temperature heat storage medium for HITB. Especially, chloride molten salts and fluoride molten salts are considered promising candidates due to their high melting temperature, thermal stability, and high latent heat of fusion. Since eutectic salts have poor thermal conductivity in general, it is critical to distribute materials with high thermal conductivity evenly to facilitate the charging and discharging of heat. In this study, metal foam was considered in the HITB system to overcome the poor heat transfer characteristics of eutectic salts. In order to improve heat transfer, it is necessary to study materials with high thermal conductivity, corrosion resistant to molten salts, such as fins, extended surfaces, particles, microcapsulation, or foam structure. Porous structure of copper or aluminum can increase heat transfer area, form a thermal transfer network, and increase the effective thermal conductivity of thermal storage medium [2]. Since the melting temperature is required to be at least 450? in the current HITB design, various eutectic salts are being considered. FLiNaK and FLiBe, which are famous for fluoride salts, are good candidates, but due to the sharp rise in the price of LiF recently, they are excluded for economic reasons to be applied to large-capacity thermal energy storage. On the other hand, chloride salts are very cheap and easy to obtain, have a high melting temperature, and have a high latent heat of fusion, so they are recently in the spotlight as a phase change material. However, because of the hygroscopic nature of chloride salts, HCl gas due to impurity is easy to be released and is particularly vulnerable to corrosion. Chloride eutectic salts have been tested and suggested for metal alloys that are particularly resistant to corrosion, such as SS304, SS316, Hastelloy, Inconel 625, Incoloy 800H, which has low thermal conductivity, and is very expensive [3-6]. Porous materials with high thermal conductivity such as copper and aluminum have been tested for stability in fluids such as paraffin or water as metal foam or metal fin structures, but high temperature corrosion tests were not performed on various eutectic salts yet. Therefore, this study investigated the high temperature corrosion characteristics of metal alloys, such as C10100 foam, C10100 plate, 6101 alloy foam, and SS316 plate, while immersed in the candidate eutectic salts. A total of 20 tests for SS316 coupons and 10 tests for C10100 coupons were performed to ensure the repeatability of the present measurements. Since it is difficult to completely remove the salt inside metal foam due to the complex inner structure of the metal foam, only the surface condition was observed with a microscopy and scanning electron microscopy (SEM) image, except for measuring the corrosion rate and average mass loss.

25 ENERGY STORAGE↗

Electrochemical Characterization of Molten Salt Chemistry During Atmospheric Ingressions

This report describes the salt chemistry and sedimentation studies that were completed in FY23 as part of the Pyrochemical Fuel Cycles – ANL project. The primary objective of these activities was to employ electrochemical methods in order to quantify and gain insights into the reaction mechanisms associated with the interaction of O2 and moisture impurities with the molten chloride salts used for the pyrochemical processing of nuclear materials. If not monitored and controlled, the ingression of these atmospheric impurities can lead to changes in the salt redox conditions and initiate the formation of oxide particles, potentially resulting in operational and safeguards challenges. By elucidating the mechanisms underlying the formation of oxide particles, we can effectively monitor the conditions of the salt and design systems to mitigate the influence of atmospheric O2 and H2O. To achieve these goals, we designed a test system that allowed for precisely controlled gas ingressions into the molten salt vessel. This system included on-line monitoring provided by electrochemical probes that enable near real-time measurements of the salt conditions throughout the course of the experiment. Using this system, we systematically varied experimental conditions, including O2/Ar flow rates and O2 concentrations, to comprehensively understand their impact on solid particle formation. We also used a particle size and shape analyzer to characterize the particles that were generated. Tests in FY23 concentrated on the formation of CeO2 particles, but we also prepared a separate apparatus targeting UO2 particles for use in FY24. We additionally conducted extensive modeling activities in support of this work. This included multiphysics simulations of the gas ingressions along with the development of a machine learning workflow to enable accelerated molecular dynamics modeling of the molten salt chemistry of LiCl-KCl-UCl3. The combination of experimental and modeling tools has allowed us to begin to get a more complete understanding of the reactions that occur when atmospheric ingressions occur in pyroprocessing systems.

Guo, Jicheng↗

Addressing Failures in Molten Salt Thermal Energy Storage Tank for Central Receiver Concentrating Solar Power Plants

The thermal energy storage (TES) system is a critical component in concentrated solar power (CSP) plants that increases the plant's capacity factor and economic competitiveness by reducing the levelized cost of energy (LCOE) while simultaneously increasing the value of the delivered energy. Failures including molten-salt leaks and diverse localized cracking after several months to a few years of operation have been reported in hot tanks for CSP plants operating around the world. A model of a molten salt thermal energy storage tank was developed and validated to analyze the impact of different tank design features on the temperature and stress distributions as a function of typical plant operation conditions. Design features included the floor plate thicknesses, friction coefficients between the tank floor and the foundation, and the sparger ring location. Maximum stresses in the tank floor frequently surpassed the yield point of the material during operation, leading to a detriment of the tank's lifetime. Recommendations on design features to improve the reliability of new molten salt tanks for CSP plants are provided.

concentrating solar power↗

Methods, materials systems, and devices for inhibiting infiltration and penetration of molten salts into solid materials

Methods, materials systems, and devices for inhibiting the infiltration and penetration of molten salts into solid materials, including porous materials at temperatures above the solidus temperature of the molten salt. The methods, materials systems, and devices utilize a non-wetted solid that is introduced into pores having entrances at an exterior surface of a porous solid material adapted to contact the molten salt.

Sandhage, Kenneth Henry↗

Initial steady-state core simulation capability or thermal and pool-type molten salt reactors, coupling reactor physics, thermal-hydraulics, and evolving chemistry

This report presents the development and validation of an initial steady-state multiphysics capability for molten salt reactors (MSRs) under the Nuclear Energy Advanced Modeling and Simulation (NEAMS) program in Fiscal Year 2025. The framework integrates neutronics, thermal-hydraulics, species transport, and thermochemistry to capture the coupled dynamics of liquid-fueled systems. Implementation and testing were performed on two representative designs: the Molten Salt Reactor Experiment (MSRE), a thermal-spectrum, channeled-flow reactor, and the Lotus Molten Salt Reactor (L-MSR), a fast-spectrum, pool-type reactor. The modeling suite employs Griffin for reactor physics and depletion, Pronghorn and SAM for thermal-hydraulics, Thermochimica for chemistry, and Saline for thermophysical properties, with benchmarking and validation carried out against historical MSRE data, experimental flow-loop measurements, and reference depletion calculations from Monte Carlo codes. The framework demonstrated the ability to reproduce key reactor behaviors including temperature feedback, reactivity losses, delayed neutron precursor transport, xenon poisoning, and redox potential evolution. The results confirm the feasibility and accuracy of the coupled models in predicting steady-state and selected transient MSR behaviors. This latter ones are used in this report as a proxy indicating that the steady-state models from which the transient starts are accurate. For MSRE, validation showed good agreement with pump start-up and natural circulation tests, while for the L-MSR, benchmarking confirmed hydraulic calibration and consistency of neutronics–thermal coupling. The tools also provided new insights into species transport, noble metal deposition, and salt solidification dynamics. On the Xenon transport front, the code is validated against the steady state Xenon poisoining measurement and showed good agreement with the experimental value. Identified areas for future work include advanced void transport modeling, three-dimensional simulations, improved alloy corrosion models, and tighter integration with high-fidelity Monte Carlo codes. These developments provide a foundation for high-fidelity MSR simulations that can support reactor design optimization, safety assessments, and long-term operational strategies.

42 - ENGINEERING↗

Electrochemical recovery of Gd into liquid Bi in molten LiCl-KCl-GdCl 3

The electrochemical recovery of Gd into liquid Bi electrodes was investigated in molten LiCl-KCl-GdCl 3 electrolyte at 773–973 K using constant currents of 10–150 mA cm −2 . High round-trip coulombic efficiency (>97 %) was demonstrated for deposition and removal of Gd into and from liquid Bi at all temperatures, confirming chemically reversible electrode reactions towards high recovery yield of Gd using liquid Bi. Furthermore, the overpotential associated with deposition of Gd into the liquid Bi electrode gradually increased with current density and decreased with temperature. At the lowest temperature of 773 K, a steep increase in overpotential was evident at high current densities due to slower mass transport and low solubility of Gd in liquid Bi (0.5 at.% Gd). Based on the impedance spectra of Bi electrodes at 773–973 K, the exchange current density was estimated to be 110–220 mA cm −2 , indicating facile charge transfer at the liquid electrode-electrolyte interface. Post-mortem characterization of Bi cathodes after electrolysis at 873 K indicated the formation of a solid GdBi(s) compound layer at the Bi electrode surface. Chemical analysis of Bi cathodes at various deposited Gd compositions resulted in Faradaic efficiencies of ∼75–84 %, promising a high recovery yield of Gd from molten salts using a strongly-interacting liquid Bi electrode.

36 - MATERIALS SCIENCE↗

Ab initio molecular dynamics (AIMD) simulations of NaCl, UCl 3 molten salts

Ab initio molecular dynamics (AIMD) simulations are used to calculate select thermophysical and thermodynamic properties of NaCl, UCl and NaCl-UCl 3 molten salts. Following established approaches, the AIMD simulations include a model for Van der Waals interactions. The Langreth & Lundqvist (vDW-DF2), DFT-D3, and density-dependent energy correction (DFT-dDsC) dispersion models are first tested for molten NaCl in order to assess their accuracy for density and heat capacity predictions across a range of temperatures. Based on the NaCl results, the vdW-DF2 and DFT-dDsC methods are extended to the UCl 3 system and compared to available experimental data. Next, mixtures of NaCl-UCl 3 are investigated and analyzed with respect to the deviation from ideal solution behavior. For the DFT-dDsC simulations, density deviates by up to 2% from an ideal mixture, with the maximum occurring close to the eutectic composition. The mixing energy also deviates from an ideal solution and exhibits a minimum of about -0.074 to eV per formula unit, again close to the eutectic composition. Finally, the compressibility and species diffusivity of the pure and mixed salt systems are calculated. The diffusivities are slightly reduced in the mixed compared to the pure systems and the compressibilities loosely follow a linear correlation as a function of the UCl 3 composition. The trends observed for mixing properties are rationalized by correlating them to the coordination chemistry, which emphasizes the importance of maintaining the extended network formed by U and Cl ions as the NaCl concentration increases. The concentration at which breakdown of the extended network occurs, roughly coincides with the minimum of both the mixing energy and the deviation from ideal solution behavior for density.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Continuous Purification of Molten Chloride Salt: Electrochemical Behavior of MgOHCl Reduction

We present a study on the electrochemical behavior of magnesium hydroxide (MgOH + ) reduction on a tungsten (W) cathode in molten chloride salt (MgCl 2 -KCl-NaCl) across the temperature range of 475 °C–525 °C. MgOH + , which forms within the salt upon exposure to moisture, is a leading cause of corrosion. Corrosion is a major barrier to deployment of chloride salts across a number of applications, including concentrating solar power plants and nuclear power plants. While pre-purification protocols have been developed to ensure MgOH + is removed from molten chloride salts prior to deployment, MgOH + forms in situ during operation of chloride-salt based plants. Thus, methods for continuous purification during plant operation are needed. Continuous electrochemical purification via electrolysis using a Mg anode and W cathode has been proposed, but little has been done to assess scalability. Here, we assess fundamental properties of electrochemical removal of MgOH + to enable future scale up of this method.

14 SOLAR ENERGY↗

Investigation of a U(IV)/U(III) Thermodynamic Reference Electrode for High-Temperature Molten Fluoride Salts

While thermodynamic reference electrodes with known and stable potentials are common in traditional aqueous systems, the high temperature and corrosive environment of a molten fluoride salt makes achieving long term stability with a thermodynamic reference electrode challenging, especially at temperatures of 600°C or higher. In this work, a thermodynamic reference electrode consisting of U(IV)/U(III) in a boron nitride compartment was evaluated for use in FLiBe at temperatures ≥ 600°C. FLiBe used in the study was purified by AlphaTech's proprietary process and characterized by ICP-MS and square wave voltammetry. The free oxide concentration was <2 ppm. Using the purified FLiBe, the U(IV)/U(III) thermodynamic reference electrode was shown to provide a stable, well-defined, and reproducible potential for more than 600+ hours of use in different tests. Moreover, the thermodynamic reference electrode showed a consistent potential with no signs of failure, even after being cooled between tests and then reheated for reuse. Thus, the U(IV)/U(III) reference electrode is suitable for use in rigorous electrochemical studies in molten fluoride salts. As a result, it may be useful as a common standard, facilitating the advancement of nuclear applications such as isotope separation or online monitoring of reactor systems through improved certainty in the measurement of thermodynamic potentials.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Quantitative Voltammetry Measurements of High-Concentration Actinides in Molten Chloride Fuel Salts

Molten chloride mixtures containing high concentrations of UCl 3 (i.e., >70 wt%) are candidates for next-generation molten salt reactor (MSR) fuel salts that enable new plant optimization and fuel cycle strategies. MSR licensing, however, is contingent on the development of effective material control and accounting (MC&A) practices for these salts. To close this gap, we have developed an electroanalytical approach that enables accurate in situ measurements of uranium concentrations in these highly loaded fuel salts. This methodology uses a multielectrode array voltammetry sensor combined with digital simulations that account for non-idealities such as uncompensated resistance effects. The theory-based numerical simulations of voltammetry responses yielded correction factors that are agnostic of electrochemical cell geometry and produced consistent voltammetry peak current results when correcting for varying amounts of ohmic resistance. In doing so, we have demonstrated accurate concentration measurements for UCl 3 in LiCl-KCl-UCl 3 across a range of mass fractions between 55 and 72.3 wt% at 550 °C.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗