DOE OSTI · 1805398
Molten salt environment creep testing extensometry system
Abstract
Disclosed herein are systems, devices and methods for creep testing selected materials within a high-temperature molten salt environment. Exemplary creep testing systems include a load train for holding a test specimen under a load within a heated inert gas vessel. An extensometry system can be included to measure elongation of the test specimen while under load. The extensometry system can include fixed members and axially translating member that move along with the elongation of the test specimen, and the system can include a sensor to measure the relative axial motion between such components to measure elongation of the test specimen over time. The test specimen can include a cylindrical gage portion having an internal void filled with a molten salt during creep testing to simulate the corrosive effect of the molten salt on the specimen material during testing.
Keep this discovery
Explore connections, maps & timelines
Ren, Wenlin. 2021-01-19. Molten salt environment creep testing extensometry system. https://www.osti.gov/biblio/1805398
Cite the original work for its findings. Save a collection to share your selection of sources.