Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Ferritic steels”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 325 records · Page 18

Postweld Heat Treatment on Toughness of Electric- Resistance Welded X70 Steel

In this report the effect of postweld heat treatment (PWHT) on Charpy V-notch impact toughness of a highfrequency electric-resistance welded (HF-ERW) grade X70 pipeline steel is investigated. PWHT thermal cycles are simulated using the Gleeble on the as-welded specimens. Microstructure, along with crystallographic texture and microhardness, is characterized in specimens that are impact tested at –5°C (23°F), –30°C (–22°F), and –45°C (–49°F). The impact toughness values show a wide scatter band and decrease with the increasing peak temperature of the PWHT. For higher peak temperatures, the microstructure of the heat-affected zone (HAZ) gradually changed from equiaxed ferrite to bainitic ferrite. Furthermore, the prior austenite grain size (PAGS) increases with the increasing peak temperature. The density of high-angle grain boundaries decreases, and the fraction of cleavage planes {100} parallel to the impact fracture plane increases for higher peak temperatures of the PWHT

36 MATERIALS SCIENCE↗

Through-Thickness Microstructure Characterization in a Centrifugally Cast Austenitic Stainless Steel Nuclear Reactor Primary Loop Pipe Using Time-of-Flight Neutron Diffraction

The US code of Federal Regulations mandates regular inspection of centrifugally cast austenitic stainless steel pipe, commonly used in primary cooling loops in light-water nuclear power plants. These pipes typically have a wall thickness of ~8 cm. Unfortunately, inspection using conventional ultrasonic techniques is not reliable as the microstructure strongly attenuates ultrasonic waves. Work is ongoing to simulate the behavior of acoustic waves in this microstructure and ultimately develop an acoustic inspection method for reactor inspections. In order to account for elastic anisotropy in the material, the texture in the steel was measured as a function of radial distance though the pipe wall. Experiments were conducted on two 10 × 12.7 × 80 mm radial sections of a cast pipe using neutron diffraction scans of 2 mm slices using the HIPPO time-of-flight neutron diffractometer at the Los Alamos Neutron Science Center (LANSCE, Los Alamos, NM, USA). Strong textures dominated by a small number of austenite grains with their (100) direction aligned in the radial direction of the pipe were observed. ODF analysis indicated that up to 70% of the probed volume was occupied by just three single-grain orientations, consistent with grain sizes of almost 1 cm. Texture and phase fraction of both ferrite and austenite phases were measured along the length of the samples. These results will inform the development of a more robust diagnostic tool for regular inspection of this material.

42 ENGINEERING↗

Effect of Microstructural Bands on the Localized Corrosion of Laser Surface-melted 316L Stainless Steel

The localized corrosion of laser surface melted (LSM) 316L stainless steel is investigated by a combination of potentiodynamic anodic polarization in 0.1M HCl and microscopic investigation of the initiation and propagation of localized corrosion. The pitting potential of LSM 316L is significantly lower than the pitting potential of wrought 316L. The LSM microstructure is highly banded as a consequence of the high laser power density and high linear energy density. The bands are composed of zones of changing modes of solidification, cycling between very narrow regions of primary austenite solidification and very wide regions of primary ferrite solidification. Pits initiate in the outer edge of each band where the mode of solidification is primary austenite plane front solidification and primary austenite cellular solidification. The primary austenite regions have low chromium concentration (and possibly low molybdenum concentration), which explains their susceptibility to pitting corrosion. The ferrite is enriched in chromium, which explains the absence of pitting in the primary ferrite regions. The presence of the low chromium regions of primary austenite solidification explains the lower pitting resistance of LSM 316L relative to wrought 316L. The influence of banding on localized corrosion is applicable to other rapidly solidified processes such as additive manufacturing.

36 MATERIALS SCIENCE↗

Effect of thermal treatments on electrochemical behavior of binder jetted 17-4 PH stainless steel

Binder jetted 17–4 PH stainless steel was post-processed to relate heat treatment, microstructure, and corrosion in 3.5 wt% NaCl. Specimens were sintered at 1380 or 1400 °C, solution-annealed at 1055 °C for 1 h, and aged at 482 °C for 1 h. Here, as-sintered parts showed α′-martensitic matrix with a δ-ferrite network and Cu-rich precipitates in ferrite; inclusions (MnS, NbC) promoted localized attack. solutionizing redistributed elements and reduced ferrite, while aging generated coherent Cu nano-precipitates. Corrosion resistance was highly sensitive to post-processing in which aged specimens exhibited the lowest corrosion current density and formed a thicker, stable Cr 2 O 3 -rich passive film, whereas sintered specimens degraded most. Pitting potential depended on sintering temperature and microstructure, with 1400 °C sintering yielding more positive pitting potentials and the best overall performance after aging. Although the 1400-solutionized condition showed a relatively noble pitting response versus 1380-solutionized, it displayed unstable corrosion kinetics attributed to an imperfect passive film linked to higher NbC density. XPS depth profiles corroborated these trends, showing thicker, more continuous Cr 2 O 3 in aged states and discontinuous/thinning oxides in less resistant conditions. Practically, high-temperature sintering (∼1400 °C) followed by solutionizing and aging is recommended, with further gains expected from reducing NbC/MnS populations and porosity via powder and process control.

36 MATERIALS SCIENCE↗

Probing the fatigue enhancement in a thermally aged cast duplex stainless steel by in situ neutron diffraction

After long-term thermal aging at 400 °C for 3000 h and 10,000 h, a cast duplex stainless steel exhibits promoted fatigue performance, including enhanced three-stage cyclic hardening and prolonged fatigue life. Utilizing in situ neutron diffraction, the phase-specific stresses are resolved, and their evolutions over entire fatigue cycling reveal the underlying mechanisms of the fatigue enhancement. It is found that the ferrite phase bears a much higher stress than the austenite matrix under both as-received and aged conditions. The enhanced cyclic hardening in Stage I is attributed to the strengthening of both phases due to thermal aging, while the enhancement in Stage III results from the martensitic transformation induced strengthening. The fatigue life is prolonged thanks to the cyclic hardening and the delay of martensitic transformation in the austenite phase after thermal aging.

Yu, Dunji↗

Transient Microstructure Evolutions and Local Properties of Dual-Phase 980 MPa Grade Steel Via Friction Stir Spot Processing

Friction stir processing is a novel solid-state process to modify microstructures and their properties by intense, localized plastic deformation. However, little research has been reported for microstructure evolutions of advanced high-strength steels during the process. The present work focuses on the study of transient microstructure changes and local mechanical properties for friction stir spot processed dual-phase (DP) 980 MPa grade steel (DP980) under different peak temperatures. A pinless silicon nitride ceramic tool was used to produce relatively simple material deformation and flow near the tool. Friction stir spot processed steel samples were characterized by optical and electron microscopies. Furthermore, Vickers microhardness and nano-indentation measurements were used to study local mechanical properties for correlation with microstructures. A swallow layer of refined grains (<0.6 µm) was obtained with a low peak temperature (under 400 °C), whereas higher peak temperatures (>Ac 1 ) led to a change in grain size with different microstructures (fine-grained DP or martensite). Electron back-scattered diffraction characterizations revealed a large deformation in the as-received microstructures (mixture of ferrite and tempered martensite) induced by friction stir spot processing, leading to recrystallization and grain refinement around the stirred zone. Also, nano-indentation measurements showed a higher hardness than the hardness of the as-received DP980. Friction stir processing with different process conditions effectively changed microstructures and local mechanical properties.

36 MATERIALS SCIENCE↗

In-situ investigation of strengthening and strain hardening mechanisms of Cu-added medium-Mn steels by synchrotron-based high-energy X-ray diffraction

A novel Cu-added medium-Mn steel with a chemical composition of Fe–0.27C–9.1Mn–1.86Al–3.3Cu (wt.%) was designed and subjected to intercritical annealing (IA) temperature range from 620 °C to 680 °C for 1 h. The ultimate tensile strength (UTS) increases and the yielding strength (YS) decreases with the IA temperature increasing. The YS of 824 MPa, UTS of 1222 MPa, total elongation (TE) of 55%, and product of strength and elongation (PSE) of 67.2 GPa·% are achieved after IA at 660 °C. Transmission electron microscopy confirmed that Cu-rich nanoparticles precipitate in the ferrite. The in-situ high-energy X-ray diffraction (HE-XRD) experiments show that at the beginning of plastic deformation, both austenite and ferrite bear the applied load. The load is mainly undertaken by martensite with effective transformation-induced plasticity (TRIP) effect triggered. The YS of ferrite is significantly higher than that of austenite. The individual contribution of solid solution strengthening, grain refinement strengthening, dislocation strengthening, and precipitation strengthening in ferrite and austenite is analyzed. The discrepancy between the YS of ferrite and austenite is mainly attributed to the precipitation strengthening due to the Cu-rich nanoparticles precipitation. The moderate mechanical stability and the collaboration of TRIP and twinning-induced plasticity (TWIP) effects of austenite contributed to the enhanced strain hardening capability and resulted in large ductility.

36 MATERIALS SCIENCE↗

Austenite Formation and Manganese Partitioning during Double Soaking of an Ultralow Carbon Medium‐Manganese Steel

Double soaking (DS) is a thermal processing route intended to produce austenite–martensite microstructures in steels containing austenite‐stabilizing additions and consists of intercritical annealing (primary soaking), followed by heating and brief isothermal holding at an increased temperature (secondary soaking), and quenching. Herein, experimental dilatometry during DS of a medium‐manganese (Mn) steel with nominally 7 wt% Mn and an ultralow residual carbon concentration, in combination with phase‐field simulations of austenite formation during secondary soaking, is presented. The feasibility of maintaining heterogeneous Mn distributions during DS is demonstrated and insight is provided on the effects of the secondary soaking temperature and prior Mn distribution on the ferrite‐to‐austenite phase transformation during the secondary soaking portion of the DS treatment.

36 MATERIALS SCIENCE↗

High-efficiency, air-stable manganese–iron oxide nanoparticle-pigmented solar selective absorber coatings toward concentrating solar power systems operating at 750 °C

Solar selective absorber coating with long-term thermal stability at high temperatures ≥750 °C in air is an important component to reduce the levelized cost of energy (LCOE) of concentrating solar power (CSP) systems toward 50% power efficiency and dispatchable solar electricity. Conventionally, solar spectral selectivity requires multilayer-interference coatings implemented by stringently controlled vacuum deposition, and these coatings degrade significantly at >700 °C in air. Herein, we established a quantitative design approach and demonstrated a proof-of-concept air-stable, manganese–iron oxide nanoparticle (NP)-pigmented solar selective coatings with a high solar absorptance of ~93%, a relatively low thermal emittance of ~52%, and an optical-to-thermal energy conversion efficiency >89% under 1,000× solar concentration at 750 °C toward Generation 3 CSP systems. These coatings demonstrate spectral selectivity using cost-effective spray coating approach, a notable improvement over conventional vacuum-deposited, multilayer solar selective coatings for low-cost, high-efficiency solar thermal receivers. In contrast to the thermal degradation of spectrally non-selective benchmark Pyromark 2500 coatings at 750 °C in air, the solar absorptance of the MnFe 2 O 4 -pigmented coatings on stainless steel 310 (SS 310) substrates is increased to ~92.9% and the optical-to-thermal energy conversion efficiency is improved to 89.7% after serving at 750 °C in air for 700 h. X-ray diffraction results reveal that this improvement is due to the transformation of MnFe 2 O 4 NPs into more thermodynamically stable, non-stoichiometric manganese-rich manganese ferrite and iron-rich manganese–iron oxide phases after 500 h aging at 750 °C. For >1,000 h-endurance testing at 750 °C in air and the subsequent 19 day-night thermal cycling between 750 °C (12 h/cycle) and 25 °C (12 h/cycle) on SS 310 substrates, the thermal degradation is mainly due to the CrO x microflake formation from SS 310 substrates rather than the coatings, which can be suppressed by preoxidizing the surface of SS 310. With lower emittance matrix material and further optimization of pigment NP stoichiometry, concentration, and coating thickness, it is promising to achieve an optimized thermal efficiency ≥92.5% with long-term thermal stability at 750 °C for Generation 3 CSP systems.

14 SOLAR ENERGY↗

Two-step deformation-induced martensitic transformation in additively manufactured High-Si stainless steel

Deformation-induced phase transformation in the additively manufactured (AM) Fe–18Cr–8Ni-5.5Si (in wt.%) alloy was analyzed using the in-situ electron backscattered diffraction (EBSD) record during uniaxial tensile testing in a scanning electron microscope (SEM). Analysis of EBSD data was focused to investigate phase transformation behavior during deformation with consideration of mechanical interactions among phases and grains in the ultrafine AM microstructure. The initial EBSD phase map illustrated that the as-built microstructure was a duplex structure consisting of major austenite (γ) and minor ferrite phases, some of which showed non-traditional orientation relationship since the rapid solidification in the AM process has produced non-equilibrium state in phase formation. In the deformed as-built AM alloy, the two-step martensitic transformation (γ→ε→α´) was identified as the main deformation-induced transformation mechanism. Martensitic transformation steps were found to be associated with glides of Shockley partial dislocations on closed packed (111) planes under the influence of atomic disturbance in the γ and ε phases, respectively. Using the closed-packed plane pole figures and unit cell orientations, their evolutions and mechanisms accompanying with the transformation were analyzed. Finally, the results indicate that one variant of ε-martensite forms from their parent γ phase, while two variants of α´ form from their parent ε phase.

36 MATERIALS SCIENCE↗

Phase stability and mechanical properties of wire + arc additively manufactured H13 tool steel at elevated temperatures

Wire + arc additive manufacturing (WAAM) is considered an innovative technology that can change the manufacturing landscape in the near future. WAAM offers the benefits of inexpensive initial system setup and a high deposition rate for fabricating medium- and large-sized parts such as die-casting tools. Here, AISI H13 tool steel, a popular die-casting tool metal, is manufactured by cold metal transfer (CMT)-based WAAM and is then comprehensively analyzed for its microstructural and mechanical properties. Location-dependent phase combinations are observed, which could be explained by nonequilibrium thermal cycles that resulted from the layer-by-layer stacking mechanism used in WAAM. In addition, remelting and reheating of the layers reduces welding anomalies (e.g., pores and voids). The metallurgical characteristics of the H13 strongly correlate with the mechanical properties. The combinations of phases at different locations of the additively manufactured part exhibit a periodic microhardness profile. Martensite, Retained Austenite, Ferrite, and Carbide phases are found in combination at different locations of the part based on the part’s temperature distribution during additive deposition. Moreover, the tensile properties at elevated temperatures (23 °C, 300 °C, and 600 °C) are comparable to those from other WAAM and additive manufacturing (AM) processes. The X-ray diffraction results verify that the microstructural stability of the fabricated parts at high temperatures would allow them to be used in high temperatures.

36 MATERIALS SCIENCE↗

Understanding Microstructural Effects on Dynamic Performance Towards the Development of Shock Metamaterials

With the recent advances in additive manufacturing (AM), long-range periodic lattice assemblies are being developed for vibration and shock mitigation components in aerospace and military applications with unique geometric and topological structures. There has been extensive work in understanding the static properties associated with varying topology of these lattice architectures, but there is almost no understanding of microstructural affects in such structures under high-strain rate dynamic loading conditions. Here we report the shock behavior of lattices with varying intrinsic grain structures achieved by post process annealing. High resolution 316L stainless steel lattices were 3D printed by a laser-powder bed fusion machine and characterized by computed tomography. Subsequent annealing resulted in stress-relieved and recrystallized lattices. Overall the lattices had strong cubic texture aligning with the x-, y- and z-directions of the build with a preference outside the build direction (z). The recrystallized sample had more equiaxed polygonal grains and a layer of BCC ferrite at the surface of the structure approximately 1 grain thick. Upon dynamic compression the as-deposited lattice showed steady compaction behavior while the heat-treated lattices exhibit negative velocity behavior indicative of failure. We attribute this to the stiffer BCC ferrite in the annealed lattices becoming damaged and fragmenting during compression.

36 MATERIALS SCIENCE↗

Nondestructive ultrasonic characterization of a triple-weld-bead wire arc additively manufactured ER70S-6 S-curved wall

Understanding build-scale microstructural variation in wire arc additive manufacturing (WAAM) of low-carbon steels is essential for ensuring consistent structure–property relationships throughout large components. Conventional destructive characterization techniques, such as scanning electron microscopy (SEM) and electron backscatter diffraction (EBSD), are time-intensive and limited to localized regions, making comprehensive evaluation of large WAAM structures challenging. In this study, a nondestructive ultrasonic approach was employed to characterize a 252 mm tall ER70S-6 S-curved WAAM wall produced using a triple-bead deposition strategy. Optical and SEM analysis revealed a repeating dual-region microstructure consisting of uniform polygonal ferrite at melt pool centers and heterogeneous ferrite with coarse and fine grains near melt pool boundaries, attributed to cyclic thermal conditions. Longitudinal ultrasonic backscatter imaging was used to evaluate the continuity of this periodicity along the full build height. The ultrasonic response exhibited a consistent repeating pattern that correlated with the observed layer-wise microstructural variation. X-ray computed tomography confirmed the absence of detectable porosity, indicating that ultrasonic contrast is primarily governed by grain morphology. Overall, the results indicate that longitudinal backscatter ultrasound is a promising nondestructive characterization technique for validating microstructural variations along the s-curved WAAM wall, with significant potential for microstructure optimization and process control.

36 MATERIALS SCIENCE↗

Mechanical responses of 316L stainless steel printed by wire arc additive manufacturing with different thermal histories

In this paper, 316L stainless steel walls were printed using single-bead pass and multiple-bead pass wire arc additive manufacturing (WAAM), which represent the internal basket wall and external wall of a spent nuclear fuel (SNF) canister; respectively. Scanning electron microscopy (SEM) microstructure characterization and tensile tests at room temperature (21 °C) and elevated temperature (250 °C) were performed on specimens extracted along the length and height directions of the printed walls. Results showed that grain morphology, grain angles, and retained ferrite are different between the two printed walls, which received different heat input in WAAM. The single-bead pass printed wall exhibited higher yield strength than the multiple-bead pass printed wall because of more retained ferrite and larger portion of random-high angle boundaries (RHAB) grains.

Tang, Wei↗

On residual stress analysis and microstructural evolution for stainless steel type 304 spent nuclear fuel canisters weld joint: Numerical and experimental studies

Chloride-induced stress corrosion cracking (CISCC) in the weldments of austenitic stainless steel canisters is one of the primary safety concerns during the dry storage of used nuclear fuel at Independent Spent Fuel Storage Installations in coastal areas. In order to evaluate the CISCC behavior in the canister, a 3D sequentially coupled thermo-mechanical finite element model was built to simulate the residual stresses induced by two intersecting longitudinal and circumferential multi-pass welds in austenitic stainless steel mockup canister. Weld-induced residual stresses from simulation were in good agreement with the experimental measurement results by deep-hole drilling and contour methods. Through-wall high tensile axial and hoop stresses were observed in both the fusion zone and heat affected zone (HAZ) in the longitudinal and circumferential weld, respectively. On the other hand, the microstructure within the weldments of 304 stainless steel mockup was characterized using optical microscopy, scanning electron microscopy, electron back-scattered diffraction and energy dispersive X-ray spectroscopy methods. A few amount of MnS inclusions in both the base metal and HAZ, and a lot of (Mn,Si) x O y inclusions in the fusion zone were found. Meanwhile, there is some α'-martensite in the base metal, while the martensite was reversed in the HAZ. In the fusion zone, there is a lot of δ-ferrite. The martensite reversion phenomenon was also verified by the combination of Feritscope test and thermal simulation, which could predict a martensite reversion temperature as 400C°. The welding residual stresses and microstructure analysis results could offer the instructive information for the prediction of CISCC behavior of the spent nuclear fuel canisters.

36 MATERIALS SCIENCE↗

Effect of post-weld heat treatment on microstructure and mechanical properties of rotary inertia friction welded dissimilar 422-4140 martensitic steel piston joints

The study investigated how post‐weld heat treatment (PWHT) temperature affects the microstructure and localized deformation/fracture during bend testing of rotary inertia friction welds (RIFW) between AISI 422 stainless steel and AISI 4140 steel. RIFW produced a fully martensitic interface with approximately 550 HV hardness in both the thermo-mechanically affected (TMAZ) and heat‐affected zones (HAZ). Due to differences in temper resistance, the 4140 TMAZ/HAZ softened progressively under PWHT temperatures from 525 °C to 700 °C, while the 422 TMAZ unexpectedly maintained about 550 HV up to 600 °C before significantly softening at temperatures ≥625 °C. This asymmetric softening generated steep hardness gradients across the interface at temperatures ≤600 °C. Furthermore, carbon migration across the interface was minimal up to 600 °C, moderate at 625 °C, and by 700 °C produced a carbide‐rich eutectoid layer in the 422 TMAZ alongside a carbon‐depleted soft ferrite layer in the 4140 TMAZ. Strain during bending was PWHT‐dependent, concentrating on the 4140 side; in as-welded joints, the high hardness led to deformation and crack initiation in the base metals, whereas in PWHT samples, cracking initiated in the softened 4140 TMAZ near the interface. The intermediate PWHT temperature of 625 °C offered the best balance of limited carbon diffusion across the interface, relatively low peak weld hardness and minimized hardness gradients across the interface, more homogenous deformation, and good bend test performance.

4140 low-alloy steel↗

Neutron Diffraction Residual Stress Characterization of Large-Scale Components by WA-DED

Two large scale 316L stainless steel cylindrical shells were fabricated by wire arc directed energy deposition (WA DED). Residual stresses were measured by neutron diffraction, and the microstructure and mechanical properties of the printed material were characterized. Longitudinal and transverse residual stresses were compressive at the inner diameter, near neutral at mid wall, and tensile at the outer diameter; radial (through thickness) residual stresses were relatively low in magnitude, and peak tensile residual stresses occurred at the outer diameter surface along the longitudinal direction. The printed 316L SS exhibited a heterogeneous microstructure with finely dispersed δ ferrite, and demonstrated high yield and tensile strengths with large elongation and ductile fracture at ambient temperature and at 250 °C. These results indicate that the outer diameter surface and near surface regions—where tensile residual stress is highest—are the most vulnerable to residual stress–sensitive failure modes, such as stress corrosion cracking and fatigue.

36 MATERIALS SCIENCE↗

Bottom-Up Soft Magnetic Composites

In order to meet 2025 goals for enhanced peak power (100 kW), specific power (50 kW/L), and reduced cost (3.3 $/kW) in a motor that can operate at ≥ 20,000 rpm, improved soft magnetic materials must be developed. Better performing soft magnetic materials will also enable electric motors without rare earth elements. In fact, replacement of permanent magnets with soft magnetic materials was highlighted in the Electrical and Electronics Technical Team (EETT) Roadmap as a R&D pathway for meeting 2025 targets. Eddy current losses in conventional soft magnetic materials, such as silicon steel, begin to significantly impact motor efficiency as rotational speed is increased. Soft magnetic composites (SMCs), which combine magnetic particles with an insulating matrix to boost electrical resistivity (ρ) and decrease eddy current losses, even at higher operating frequencies (or rotational speeds), are an attractive solution. Today, SMCs are being fabricated with values of ρ ranging between 10 -3 to 10 -1 μohm∙m, which is significantly higher than 3% silicon steel (~0.5 μohm∙m). The isotropic nature of SMCs is ideally suited for motors with 3D flux paths, such as axial flux motors. Additionally, the manufacturing cost of SMCs is low and they are highly amenable to advanced manufacturing and net-shaping into complex geometries, which further reduces manufacturing costs. There is still significant room for advancement in SMCs, and therefore additional improvements in electrical machine performance. For example, despite the inclusion of a non-magnetic insulating material, the electrical resistivities of SMCs are still far below that of soft ferrites (10 – 10 8 μohm∙m).

36 MATERIALS SCIENCE↗