Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Material failure”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 289 records · Page 16

Limitations of Hydrogen Detection After 150 Years of Research on Hydrogen Embrittlement

Hydrogen's significance in contemporary society lies in its remarkable energy density, yet its integration into the worldwide energy grid presents a substantial challenge. Exposing materials to hydrogen environments leads to degradation of mechanical properties, damage, and failure. While the current approach for assessing hydrogen's impact on materials involves mainly multiscale modeling and mechanical testing, there exists a significant deficiency in detecting the intricate interactions between hydrogen and materials at the nanoatomic scales and under in situ conditions. This perspective review highlights the experimental endeavors aimed at bridging this gap, pointing toward the imminent need for new experimental techniques that can detect and map hydrogen in materials’ microstructures and their site‐specific dependencies.

Tunes, Matheus A.↗

Physics of Failure Analysis of Nuclear Fusion Divertor Monoblock: An Analytical Approach

Original - A slide package that summarizes research progress of 2025 summer high school internship. To be presented at an internal group presentation to all the high school interns and mentors within C200, plus potential more interested audience from INL. Revision - Based on the original LRS-approved slide package, an updated slide package and a poster were prepared with slight changes (e.g., adjusting the layout of slides and reproducing some plots for better clarity) for the interns' final showcase on August 13. The showcase will be public-facing (i.e., not limited to INL attendees).

99 - GENERAL AND MISCELLANEOUS↗

Dynamic response of 17-4 stainless steel as a function of manufacturing method and heat treatment

We present a series of plate-impact experiments on 17-4 stainless steel to study the effect of manufacturing method and heat treatment on the Hugoniot elastic limit (HEL), Hugoniot, phase transformation stress, and spallation strength. Two traditional manufacturing methods were considered, wrought processing and casting, as well as two additive manufacturing methods, laser powder-bed fusion (LPBF) and wire-fed electron beam (EBAM). For both LPBF and EBAM 17-4 stainless steel variants, two billets were printed, enabling the application of two unique heat treatments. The HEL stress depended heavily on the thermal history, with the HEL increasing after the formation of Cu-rich precipitates via heat treatment. The Hugoniot response both below and above the phase transition was unaffected by the manufacturing method or heat treatment. The phase transition stress depended heavily on the thermal history, with its variation being attributed to the presence of various microstructural features. This is supported by a marked increase in the phase transition stress after precipitation hardening. These results suggest that the notion of the phase transition stress being dictated by bulk composition is an oversimplification and the stress fields generated by the meso-scale structure are a dominant force. The spallation strength was lower in the cast material compared to all other 17-4 stainless steel variants due to the presence of brittle δ-ferrite inclusions. Additionally, a drop in the tensile strain-rate was observed in the spallation response above the phase transition stress, which was hypothesized to stem from the kinetics of the reversion to the low-pressure phase during spall.

Compressive stress↗

Chemo-Mechanics of α-V 2 O 5 During Lithiation and Implications for Rechargeable Battery Cathodes

Chemo-mechanical degradation of layered oxide electrodes is strongly influenced by crystallographic anisotropy, local stress evolution, and ion insertion, yet the intrinsic mechanical response of layered materials remains incompletely understood. Indeed, most prior studies have focused on polycrystalline materials but single crystals enable direct observation of coupling between anisotropic ion diffusion and mechanical response. This study aims to determine how crystallographic anisotropy and lithiation affect deformation, fracture, and mechanical properties in single-crystal V 2 O 5 , and compares this behavior with polycrystalline counterparts. Polycrystalline V 2 O 5 thin films and single-crystal α-V 2 O 5 were studied using nanoindentation, scanning electron microscopy, focused ion beam cross-sectioning, and Raman spectroscopy. Single crystals were tested in pristine and chemically lithiated states, including experiments in which crystals were first plastically deformed via nanoindentation and subsequently lithiated. Polycrystalline films exhibited significantly higher hardness and elastic modulus than single crystals. Single crystals indented normal to the exposed (001) basal plane exhibited pronounced anisotropic deformation, including directional slip, crystallographically-guided cracking, anisotropic crack propagation, interlayer separation, and shear localization. Lithiation caused substantial softening, reduced hardness and modulus, and suppressed displacement bursts during nanoindentation, while previously indented regions showed crack formation and growth upon lithiation. Mechanical behavior of α-V 2 O 5 is strongly governed by crystallographic anisotropy and further altered by lithiation, with pre-existing deformation serving as a strong driver of fracture during ion insertion. These findings illuminate the coupling among ion insertion, deformation, and fracture in layered oxides and provide a basis for understanding and mitigating mechanical failure in electrochemical energy-storage materials.

Anisotropy↗

Detection of Defects in Additively Manufactured Metallic Materials with Machine Learning of Pulsed Thermography Images

Additive manufacturing (AM) is an emerging method for cost-efficient fabrication of nuclear reactor parts. AM of metallic structures for nuclear energy applications is currently based on laser powder bed fusion (LPBF) process, which can introduce internal material flaws, such as pores and anisotropy. Integrity of AM structures needs to be evaluated nondestructively because material flaws could lead to premature failures due to exposure to high temperature, radiation and corrosive environment in a nuclear reactor. Quality control (QC) requires nondestructive evaluation (NDE) of actual AM structures. Pulsed thermography is a potentially promising QC technique because it is scalable to arbitrary structure size. However, detection sensitivity of this method is limited by noises. We investigate separation of signal from noise in thermography images using several machine learning (ML) methods, including new spatio-temporal blind source separation (STBSS) and spatio-temporal sparse dictionary learning (STSDL) methods. Performance of the ML methods is benchmarked using thermography data obtained from imaging stainless steel 316L and Inconel 718 specimens produced LPBF method with imprinted calibrated porosity defects. The ML methods are ranked by F-score and execution runtime. The ML methods with higher accuracy require longer run time. However, this runtime is sufficiently short to perform QC within a realistic time frame.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Development of Thermal Tomography Imaging System for In-Service Nondestructive Evaluation of Additively Manufactured Components

Additive manufacturing (AM) is an emerging method for cost-efficient fabrication of nuclear reactor parts. AM of metallic structures for nuclear energy applications is currently based on laser powder bed fusion (LPBF) process, which can introduce internal material flaws, such as pores and anisotropy. Integrity of AM structures needs to be evaluated nondestructively because material flaws could lead to premature failures due to exposure to high temperature, radiation and corrosive environment in a nuclear reactor. Thermal tomography (TT) provides a capability for non-destructive evaluation of sub-surface defects in arbitrary size structures. We investigate TT of AM stainless steel 316L specimen with imprinted internal porosity defects using relatively low-cost, small form factor infrared (IR) camera based on uncooled micro bolometer detector. Sparse coding related K-means singular value decomposition (SVD) machine learning, image processing algorithms are developed to improve quality of TT images through removal of Additive white Gaussian noise without blurring the images. Following initial qualification of an AM component for deployment in a nuclear reactor, a compact TT can also be used for in-service nondestructive evaluation (NDE). With capability to perform in-service NDE of the AM component lifecycle, TT data can be used for development of a component digital twin. MIT research reactor (MITR) has been identified as a representative environment to perform investigation of feasibility of in-service NDE during shutdown. Preliminary study of radiation level in the MITR viewport, with geometric parameters potentially compatible with compact TT system, has been conducted.

36 MATERIALS SCIENCE↗

Infusible thermoplastic resin based sandwich structures for wind blade applications and the influence of scrim on facesheet to core interface debonding

Infusible thermoplastic Elium® family of resins from Arkema have garnered much attention in recent years as a possible replacement for thermoset resins in laminate and sandwich composite manufacturing for wind blade applications due to its ease of recyclability and the ability to utilize existing manufacturing processes without imposing complicated variations. However, physical and mechanical properties of the proposed Elium® based thermoplastic composites must be comparable to existing epoxy (thermoset) based composites using manufacturing processes relevant for large wind turbine blades. A 13-meter-long demonstration blade was manufactured for that purpose and sandwich samples were obtained from that project for a detailed study. This paper details three-point flexural properties of unidirectional E-glass fiber reinforced acrylic and epoxy based sandwich panels with identical balsa wood core materials. In addition, to evaluate the relative merit considering debond failure mode, the interfacial critical strain energy release rate, predominantly in mode-1, was compared via single cantilever beam testing. In sandwich composites constructed with balsa wood core material, resin uptake by the balsa core is traditionally impeded via the insertion of a scrim material at the facesheet to core interface. Results revealed that inclusion of scrim mesh layer at the facesheet to core interface reduced flexural properties and strain energy release rates in panels infused with acrylic resin but did not significantly reduce these properties in epoxy infused facesheets.

Engineering↗

In-device Battery Failure Analysis

Lithium-ion batteries are indispensable power sources for a wide range of modern electronic devices. However, battery lifespan remains a critical limitation, directly affecting the sustainability and user experience. Conventional battery failure analysis in controlled lab settings may not capture the complex interactions and environmental factors encountered in real-world, in-device operating conditions. Here, this study analyzes the failure of commercial wireless earbud batteries as a model system within their intended usage context. Through multiscale and multimodal characterizations, the degradations from the material level to the device level are correlated, elucidating a failure pattern that is closely tied to the specific device configuration and operating conditions. The findings indicate that the ultimate failure mode is determined by the interplay of battery materials, cell structural design, and the in-device microenvironment, such as temperature gradients and their fluctuations. This holistic, in-device perspective on environmental influences provides critical insights for battery integration design, enhancing the reliability of modern electronics.

36 MATERIALS SCIENCE↗

A novel method may reveal bulk metallic glass compressive ductility trends in high data rate nanoindentation

Recent methods allow novel amorphous alloy compositions to be rapidly manufactured at small scale; however, obtaining materials properties such as compressive ductility from these smaller specimens has remained a challenge. Here, we suggest a potential high-throughput nanoindentation method that may be able to rapidly characterize the relative compressive ductility between these alloys based on their serration characteristics. The properties of emergent serrations, when interpreted in a simple micromechanical stress relaxation model, may order these materials by their compressive plastic strain to failure. These results are consistent with the ordering obtained from compressed specimens as well as with model simulations, suggesting that this model may be broadly useful for interpreting compressive ductility from nanoindentation serrations. After it is validated on more materials, this new method will match the rapid pace of amorphous alloy development, thus allowing metallic glass properties to be fine-tuned for each application prior to scale prototyping.

36 MATERIALS SCIENCE↗

Additively Manufactured Carbon Fiber and Fused Deposition Modeling PLA Interlaminar Shear Testing Report

This test report summarizes the torsional test setup, procedure, and results for interlaminar shear (ILS) failure of additively manufactured carbon fiber (CFAM) material developed at LLNL. In addition, the report also includes testing of fused deposition modeled (FDM) polylactic acid (PLA), including ILS test standard D7078 and the same torsional test mentioned above. The test hopes to characterize ILS properties of CFAM, however substantial further testing and improvements still need to be done to induce a proper failure mode. This testing was performed by Sundi Win as part of her summer internship project in Kinetic Technologies.

36 MATERIALS SCIENCE↗

Micro-mechanical investigation of the thermo-mechanical properties of micro-architectured tungsten coatings

The thermo-mechanical response of micro-architectured tungsten coatings is characterized in the temperature range of 293 to 673 K using both in situ micro-compression experiments inside a scanning electron microscope (SEM) as well as image-based crystal plasticity finite element method (CPFEM) simulations. The experiments were conducted on micropillar-like specimens that were focus ion beam milled into the coatings, while the simulations were conducted on columnar-grained micropillar simulation cells constructed based on the statistics of the coating’s microstructure. The experimental results show that the stress–strain response and deformation mode exhibit a strong temperature-dependence. At room temperature, catastrophic failure is observed shortly after yield and is manifested in the form of intergranular fracture and buckling of individual columnar grains. With increasing temperature, this catastrophic failure is gradually suppressed and the material exhibits a steadier strain hardening response at 693 K. The CPFEM simulations are also shown to be in good agreement with the experimental results, and these simulations indicate that the material response is strongly influenced by the local crystallographic anisotropy and microstructure inhomogeneity. Furthermore, the simulations capture the underlying mechanisms that control the temperature-dependent transition in deformation mode. The current results highlight that the micro-architectured microstructure offers a great combination of excellent mechanical strength and structural integrity at elevated temperatures, which is of importance for high temperature applications.

36 MATERIALS SCIENCE↗

Investigation on gate oxide reliability under gate bias screening for commercial SiC planar and trench MOSFETs

This paper evaluates the impact of the fast high gate-voltage screening technique on gate oxide reliability of commercial 1.2 kV 4H-SiC power metal-oxide-semiconductor field-effect transistors (MOSFETs) with planar and trench gate structures. The measurements are conducted on packaged devices with the intent that the results will be applicable to wafer-level screening. The threshold voltage (V th ) of SiC MOSFETs is measured before and after various screening treatments and recovery process. In addition, constant-voltage time-dependent dielectric breakdown (TDDB) measurements are performed on SiC MOSFETs to obtain the intrinsic lifetime of gate oxide. The objective of this study is to determine the optimal screening conditions and improve screening efficiency without degradation of gate oxide reliability, such as V th shift and reduced oxide intrinsic lifetime. Due to the differences in the gate oxidation process and structural design of SiC planar and trench MOSFETs, the two types of devices exhibit different oxide reliability in the screening process. The recommended screening conditions obtained in this paper reveal that SiC trench MOSFETs can accept higher screening voltages compared to SiC planar MOSFETs. Hence, it can be concluded that more efficient screening techniques can be adopted for SiC MOSFETs with thicker gate oxide to meet the requirements of industrial applications.

36 MATERIALS SCIENCE↗

Predicting Thermochemical Equilibria with Interacting Defects: Sr 1 − x Ce x Mn O 3 − δ Alloys for Water Splitting

Solar thermochemical hydrogen is one of the few potential routes towards direct fuel production from renewable energy sources, but the thermodynamic boundary conditions for efficient and economic energy conversion are challenging. Success or failure of a given oxide working material depends on the subtle balance between enthalpy and entropy contributions in the redox processes. Developing a mechanistic understanding of the behavior of materials on the basis of atomistic models and first-principles calculations is an important part of advancing the technology. One challenge is to quantitatively predict thermochemical equilibria at high concentrations when the redox-active defects start to interact with each other, thereby impeding the formation of additional defects. This problem is of more general importance to applications that rely on high levels of off-stoichiometry or doping, including, for example, batteries, thermoelectrics, and ceramic fuel cells. To account for such repulsive defect interactions, we introduce a statistical mechanics approach, defining an expression for the free energy of defect interaction based on limited sampling of defect configurations in density functional theory supercell calculations. The parameterization of this energy contribution as a function of defect concentration and temperature allows on-the-fly simulation of thermochemical equilibria. The approach consistently incorporates finite temperature effects by including the leading contributions to the temperature-dependent free energy for the case at hand, i.e., the ideal gas and configurational enthalpies and entropies. We demonstrate the capability and utility of the approach by simulating the water splitting redox processes for Sr 1 − x Ce x Mn O 3 − δ alloys. Published by the American Physical Society 2024

08 HYDROGEN↗

Novel Tube Design for Superheater Heat Exchanger Enabled Via Additive Manufacturing

Superheater tubes are critical boiler components that operate at relatively higher temperatures and pressure. Amongst the primary concerns for these tubes is the deposition of ash particles on the tube surface, leading to the reduced thickness of the tube due to material corrosion, consequently causing early creep failure of the component. In this research, a novel tube design has been proposed which resembles a teardrop or ogive shape to reduce the drag and concurrently improve the creep life of the superheater tubes. To administer the practicality of novel tubes, metal additive manufacturing (AM), for instance, laser-powder bed fusion (L-PBF), has been proposed. These unconventional designs were assessed and compared with the baseline circular tube design for mechanical design requirements (hoop stress and creep life) and the particle and flue gas flow characteristics around the differently shaped tubes. A thermomechanical finite element (FE) analysis was performed for hoop stress calculations. This study also emphasizes on effect of circumferential thermal variation on hoop stress distribution in tubes. Therefore, a detailed two-dimensional (2D) thermal simulation has been performed to report the circumferential thermal variation on the tube. A computational fluid dynamics (CFD) analysis coupled with particle tracing was performed for gas flow visualization and particle tracing around the proposed shapes and baseline circular-shaped tube design. The Schlieren optic setup was built and leveraged for qualitative validation of the proposed design. The complete design methodology established in the paper shows teardrop-shaped tubes better in terms of drag and creep life in contrast to the circular-shaped tube.

42 ENGINEERING↗

Independence of Environmental and Mechanical Damages on Silicone Adhesive Stored in a Thermo-Oxidative Environment

Abstract Elastomeric polymer materials hold a special place in today’s industrial sectors with respect to structural application needs. Low quality materials are detrimental to industries like aerospace, and automotive engineering. Assessment of the durability of elastomers for structural applications has been of much interest among the literary circles for decades and new materials keep outperforming the existing ones. Polymeric adhesives are one of the most abundantly used materials in these industries. All polymeric materials get damaged when in contact with aggressive environments in presence of high temperature and oxygen. Commonly referred to as thermo-oxidation, this environment exposes the material to heat and oxidation reactions in presence of oxygen. Resultantly, during service life, the damage to the polymer matrix is primarily caused by two factors: mechanical damage and environmental aging. Environmental aging is an irreversible phenomenon caused by changes in the molecular structure while mechanical damage maintains the shape of the polymer matrix, and the deterioration is mostly due to polymer chain mobility. Environmental aging can be caused by a single environmental agent or by a synergized impact of several environmental elements. Increasing temperature is found to be proportional to decreasing tensile strength and toughness of material. The rate and extent of degradation can be accessed by scrutinizing the changes in constitutive behavior of material through mechanical and chemical properties. Accelerated thermal aging is among the most common modes of process related degradation, leading generally to chain scission, and crosslinking phenomena and reduced resistance to fracture stress, and strain. In this experimental study, our goal is to separate the environmental degradation from mechanical damage. A silicone-based adhesive was aged in thermo-oxidative at (0%RH) aging environment. The damage and decay mechanisms have been used to draw a distinction between environmental degradation and mechanical damage. Material characterization included uniaxial tensile test (failure and cyclic) and scanning electron microscopy (SEM) tests on as-received and aged samples. Aging was conducted at three different temperatures (60°C, 80°C and 95°C) and six different exposure durations (1, 3, 10, 30, 90 and 200 days). This work confirms that environmental damage is superposed on top of the mechanical damage, and thus, they are separable. The total mechanical and environmental damage is a synergized effect of all exposure conditions and parameters involved i.e., aging time, temperature, and oxygen. The chemistry and mechanics of the polymer degradation were found to be in good agreement with each other.

Alazhary, Sharif↗

Exploring Failure of Adhesively-Bonded Joints with Different Void Sizes at the Same Void Volume Fraction through A Micro-scale Numerical Modeling

This paper studied the effects of void sizes on the failure behavior of adhesively-bonded materials under global shear via micro-scale computational modeling. The numerical results indicate that large void sizes with increased distances between them at the same void volume fraction can alleviate the reduced joint strength of a weaker adherend-adhesive interface caused by interfacial voids. However, this is not the case for an adherend-adhesive interface with the interfacial tensile strength being sufficiently higher than the adhesive strength, showing the negligible effect on the joint strength due to various void sizes and the amount of interfacial voids. This preliminary investigation provides insightful information for scaling up the void size in the macro-scale computational modeling of joints, and enhances the understanding of the micro-mechanical adhesion in adherend-adhesive interfaces with different levels of bonding.

Qiao, Yao↗

TEAMER: Biofouling Analysis for Wave Energy Piston Design - Load Cell Data

Biofouling and corrosion are a major concern for all ocean-deployed components, especially when mechanical motion is involved. Triton has developed the concept of a biofouling mitigation seal as part of the piston sealing assembly for the Triton Wave Energy Converter (TSI-WEC). This mitigation seal has the purpose of preventing the formation of a biofilm on the inside of the piston cylinder. It is hypothesized that the prevention of a biofilm will reduce the amount of macro-biofouling that can occur in the piston assembly. The mitigation seal can also reduce the wear on the main dynamic seal, helping to maintain smooth operation and water-tightness. The cylinder is made from a thermoset composite epoxy, which is resistant to corrosion. However, no studies have researched the material's performance with biofouling. Triton placed two prototype Power Take-Off (PTO) assemblies in a PNNL biofouling tank, one with a biofouling mitigation seal and one without, allowing for an evaluation of seal effectiveness at the prevention of biofouling. In actual WEC operation, wave action would react against the piston, which would drive the linear actuator and electric generator, providing electrical power. In the test setup, this was reversed; a linear actuator was powered to drive the piston in a consistent motion within the cylinder. There are two assemblies: one has a biofouling mitigation seal, the other (control) does not. The following data encompasses a 4 month test period, with load cells being used to monitor piston friction force. Results from this testing will be used to improve seal design and material selection, mitigating risk of premature failure during open water testing and evaluation. This project is part of the TEAMER RFTS 3 (request for technical support) program.

16 TIDAL AND WAVE POWER↗