Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “lithium anode”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 271 records · Page 15

Synthesis of hierarchical graphene coated porous Si anode for lithium-ion batteries

The ultra-high capacity and widespread availability of Si materials have resulted in them being the focus of extensive studies to replace the graphite anode. However, the main barriers preventing the Si anodes from large-scale applications are their huge volume change and severe interface reactions in the lithiation/delithiation process, which pulverizes its structure and subsequently deteriorates its cycle life. Here, micrometer-scale porous Si coated with graphene coating (mpSi@G) has been synthesized by using SiO 2 nanoparticles and novel coal-derived humic acid as feedstocks through a magnesiothermic reduction, followed by spray drying and calcination techniques. SEM, Raman, and X-ray absorption analysis demonstrate that the hierarchical graphene shell and micrometer-sized porous Si structure effectively release the Si anode's mechanical stress upon lithiation to achieve good structural stability. Here, the synthesized mpSi@G anode delivers a high initial lithiation capacity of 2974.9 mAh g –1 at 0.1 A g –1 with an initial coulombic efficiency of 70.2 %. Furthermore, the conductive hierarchical graphene network, along with the tight contacts of porous-Si and the graphene shell, contribute to a high capacity of 1109.5 mAh g –1 at a high current density of 5.0 A g –1 , showing excellent rate capability.

25 ENERGY STORAGE↗

Cryogenic EM Across Length Scales for Li Metal Anode Batteries

An interfacial understanding is necessary for developing strategies to commercialize high-energy density rechargeable lithium metal anode batteries, as currently, the lithium anode/electrolyte interface is unstable with prolonged cycling. We have used several strategies to improve the cycling performance of lithium metal anodes, including reducing the parasitic reactions between lithium metal and the electrolyte, and improving the electrodeposited lithium metal morphology. These strategies have generated unconclusive electrochemical data, that has required the need for nanoscale interfacial characterization of these solid-liquid interfaces. Our team has used the cryogenic transfer workflow developed by Leica in collaboration with cryo-SEM/FIB tools by Thermo Fisher Scientific to cross-section lithium metal anodes and intact coin cell batteries to observe the interfacial structures, lithium morphology, and failure mechanisms relative to changes in electrode contract pressure and electrolyte chemistry. Cross-sectional SEM images and EDS maps of the lithium metal anodes have provided a better understanding of the electrodeposited lithium morphology, quantity of 'dead' lithium metal, and quantity of solid electrolyte interphase material that has formed alongside the lithium metal. In understanding lithium metal battery failure at the system level, we used a cryogenic stage in a laser plasma FIB to cross-section through the coin cell's cap for imaging/mapping the entire battery stack under cryogenic conditions. The tools, methods, and results of these studies will be detailed in this presentation.

characterization↗

Effect of Fluoroethylene Carbonate Additives on the Initial Formation of the Solid Electrolyte Interphase on an Oxygen-Functionalized Graphitic Anode in Lithium-Ion Batteries

The formation of a solid electrolyte interphase (SEI) at the electrode/electrolyte interface substantially affects the stability and lifetime of lithium-ion batteries (LIBs). One of the methods to improve the lifetime of LIBs is by the inclusion of additive molecules to stabilize the SEI. To understand the effect of additive molecules on the initial stage of SEI formation, in this work we compare the decomposition and oligomerization reactions of a fluoroethylene carbonate (FEC) additive on a range of oxygen-functionalized graphitic anodes to those of an ethylene carbonate (EC) organic electrolyte. A series of density functional theory (DFT) calculations augmented by ab initio molecular dynamics (AIMD) simulations reveal that EC decomposition on an oxygen-functionalized graphitic ($11\bar{2}0$) edge facet through a nucleophilic attack on an ethylene carbon site (C E ) of an EC molecule (S2 mechanism) is spontaneous during the initial charging process of LIBs. However, decomposition of EC through a nucleophilic attack on a carbonyl carbon (C C ) site (S1 mechanism) results in alkoxide species regeneration that is responsible for continual oligomerization along the graphitic surface. In contrast, FEC prefers to decompose through an S1 pathway, which does not promote alkoxide regeneration. Including FEC as an additive is thus able to suppress alkoxide regeneration and results in a smaller and thinner SEI layer that is more flexible toward lithium intercalation during the charging/discharging process. In addition, we find that the presence of different oxygen functional groups at the surface of graphite dictates the oligomerization products and the LiF formation mechanism in the SEI.

25 ENERGY STORAGE↗

Operating High-Energy Lithium-Metal Pouch Cells with Reduced Stack Pressure Through a Rational Lithium-Host Design

Transitioning from a liquid electrolyte to an inorganic solid electrolyte offers a potential pathway to enable highly reversible lithium-metal anodes. However, the solid-electrolyte-protected lithium-metal anode suffers from poor interfacial ionic contacts and requires an impractically high stack pressure (>1.0 MPa) to maintain the interfacial contacts. It is demonstrated here that combining a hollow silver/carbon fiber scaffold and an inorganic/organic composite electrolyte enables a highly reversible lithium-metal anode. Since the high surface area of the electrode provides intimate contact and the hollow structure of the electrode relieves the lithium plating-induced stress, the electrode/electrolyte interface remains stable during cycling even under mild stack pressure. This unconventional structural design is validated in practical pouch cells assembled with the 3D lithium host containing a onefold excess of lithium and a high-nickel cathode. At a mild stack pressure of 320 kPa, the pouch cell displays 83% capacity retention for 200 cycles. This work illustrates that combining a hollow electrode architecture and a robust solid electrolyte offers a practical pathway toward rechargeable lithium-metal anodes.

36 MATERIALS SCIENCE↗

Solvation-protection-enabled high-voltage electrolyte for lithium metal batteries

To facilitate the practical application of lithium metal batteries (LMBs), stable interfaces between the electrolyte and the lithium metal must be achieved. Herein, we introduce a solvation protection strategy for designing a functional electrolyte for high-voltage LMBs. Fluoroethylene carbonate (FEC) was introduced as a solvation protection solvent for the difluoroethylene carbonate (DFEC)/trifluoroethyl methyl carbonate (FEMC) electrolyte system to enable the cycling of lithium metal anode. The addition of FEC alters the structures of lithium complexes in solution because of its relatively high solvating power. Through the precise control of the solvation number (> 1) of fluorinated cyclic carbonate (i.e., FEC:DFEC > critical ratio), lithium complexes with Li + solvated solely by FEMC, which decompose on the lithium surface to form detrimental by-products, can be effectively eliminated. Here, the new ternary FEC/DFEC/FEMC system not only maintains the beneficial effect of DFEC in forming a robust solid-electrolyte interphase on the lithium anode, but also confers outstanding anodic stability provided by FEMC, while eliminating detrimental FEMC decomposition through the solvation protection effect of FEC. Clearly, this ternary system outperforms the FEC/FEMC and DFEC/FEMC binary systems in facilitating the stable cycling of LMBs.

25 ENERGY STORAGE↗

Using the Principals of Electrochemistry to Understand and Overcome the Complicated Degradation Mechanisms of Silicon Anodes in Lithium-Ion Batteries [Slides]

Battery technology is the most significant problem facing widespread market adoption of battery electric vehicles (BEVs). The low energy density of state-of-the-art lithium-ion electrode materials leaves BEV owners and prospective buyers with lower ranges than a comparable internal combustion engine (ICE) vehicle, and vulnerable to a nascent fast charging network. Silicon has the potential to increase the anode energy density by nearly ten times compared to the incumbent material (graphite) and make BEVs a more competitive transportation option. However, lithiated silicon is extremely reactive towards components of the electrolyte and forms a heterogeneous, complicated, and dynamic solid at its surface known as the solid electrolyte interphase (SEI). Ideally, the SEI would passivate the silicon surface, but continuous chemical degradation persists even when the battery is not operating. This reactivity reduces silicon anode lifetimes well below the necessary standards for BEVs. The NREL-led Silicon Consortium Project is dedicated to understanding and solving these mechanisms of degradation. Here, I will discuss an electrochemical method that provides deep insights into the silicon interface during battery operation. I will link these observations to fundamental electrochemical principals and how they translate into actionable strategies that extend the lifetime of silicon anodes.

25 ENERGY STORAGE↗

Computation-guided discovery of coating materials to stabilize the interface between lithium garnet solid electrolyte and high-energy cathodes for all-solid-state lithium batteries

All-solid-state batteries with a lithium metal anode, enabled by lithium garnet solid electrolytes such as Li 7 La 3 Zr 2 O 12 (LLZO), are a promising next-generation energy-storage technology. The further development of all-solid-state battery requires the integration of high-energy cathodes such as LiNi 1-x-y Mn x Co y O 2 (NMC) with the garnet solid electrolyte with stable and low-resistance interfaces, which requires a coating layer to stabilize the interface during high-temperature sintering and electrochemical cycling. In order to guide the future development of interfacial coatings, we perform high-throughput thermodynamic analyses based on first-principles computation to investigate the stability of LLZO garnet and high-energy NMC cathodes with a wide range of materials chemistries. Here our study reveals the factors governing the materials stability with LLZO garnet and NMC cathodes, and identifies the mechanisms of good coating layers stable with LLZO and NMC. In addition to classifying known coating layers, our study provides detailed guiding charts and multiple new materials systems as promising coatings for stabilizing LLZO—NMC interfaces to enable high-energy-density garnet-based all-solid-state batteries. Our demonstrated computation scheme and high-throughput analyses are generally applicable to investigate and screen coating materials for stabilizing interfaces in energy-related applications.

25 ENERGY STORAGE↗

Crack-Free Silicon Monoxide as Anodes for Lithium-Ion Batteries

The volume expansion of Si and SiO particles was investigated using a single-particle battery assembled with a focused ion beam and scanning electron microscopy (FIB-SEM) system. Single Si and SiO particles were galvanostatically charged and discharged as in real batteries. Microstructural changes of the particles were monitored in situ using FIB-SEM from two different angles. The results revealed that the volume expansion of micrometer size particle SiO was not only much smaller than that of Si, but it also kept its original shape with no sign of cracks. Additionally, this isotropic mechanical property of a SiO particle can be attributed to its microstructure: nanosized Si domains mixed with SiO 2 domains. The nanosized Si domains can mitigate the anisotropic swelling caused by the orientation-dependent lithium-ion insertion; the surrounding SiO 2 domains can act as a buffer to further constrain the localized anisotropic swelling.