CuCr 2 O 4 particle growth and evolution across sol–gel routes and calcination profiles

CuCr 2 O 4 spinel is a candidate coating material for central receivers in concentrating solar power to protect structural alloys against high temperature oxidation and related degradation. Coating performance and microstructure of dip-coated and sintered coatings is dictated by the initial particle size of the CuCr 2 O 4 and sintering temperature, but can be compromised by particle agglomeration. Here in this study, sub-micron particles were synthesised through the Pechini and modified Pechini sol–gel methods. Phase composition was confirmed via X-ray diffraction. Particle growth during calcination of the nanoparticles at different temperatures (650°C, 750°C, 850°C) and times (between 1 and 24 h) was measured via laser diffraction and scanning electron microscopy. The modified Pechini method displayed evidence of smaller particle sizes and greater agglomeration. The kinetics of particle growth observed are consistent with a diffusion limited inhibited grain growth model.

36 MATERIALS SCIENCE↗

Cometary grain scattering versus wavelength, or 'What color is comet dust'?

Optical and near-infrared observations of comets are combined in a systematic study of the wavelength dependence of the scattering from cometary grains. The normalized rate of change of the reflectivity of cometary grains with respect to the wavelength of observations decreases as the wavelength increases. The observed wavelength dependence of the reflectivity gradient is consistent with an origin by scattering from micron-sized or larger, slightly absorbing spheres. The optically important comet grains are about an order of magnitude larger than the optically important interstellar grains. This size difference is a probable result of grain growth in the cloud from which the comets condensed. Grain properties differ so widely among the comets that any phase angle or heliocentric distance dependences of the continuum color are hidden.

Jewitt, David↗

Effect of Long-Term 1093 K Exposure to Air or Vacuum on the Structure of Several Wrought Superalloys

Long-term 1093 K heat treatments of three commercial superalloy sheet materials were undertaken in air -IAI and vacuum. With either exposure, significant precipitation of second phases occurred in the Co-base Haynes(R) Alloy 188 (HA 188) and the Ni-base Haynes(R) Alloy 230 (HA 230); however, much less precipitation was found in the exposed Ni-base alloy Inconel(R) 617 (IN 617). Although some grain growth occurred in HA 198, no changes in the grain size of either HA 230 or IN 617 were observed after 22,500 h at temperature. Oxidation during air heat treatments led to weight gain due to the formation of chromia + spinel scales and surface-connected grain boundary pits/oxides in all three superalloys. Both the weight gain and depth of intergranular attack were dependent on the square root of time, which is indicative of diffusion-controlled phenomena. Because many alloy samples had neighbors in close proximity, most vacuum heat treated specimens did not suffer significant loss of volatile elements. However, some exposed samples were subjected to unrestricted vacuum heat treatments, allowing estimates of volatilization to be made. Based on the data for HA 188, the weight loss during 1093 K vacuum exposure was diffusion controlled once the inhibiting effects of surface films on the as-received alloys were broken down.

J.D. Whittenberger↗

Microstructure refinement of hot deformed Dy-free NdFeB magnets through a novel cold sintering approach by pressure-assisted spark plasma sintering

Anisotropic fine-grained Dy-free NdFeB high-performance magnets were produced using a novel cold sintering approach by pressure-assisted spark plasma sintering (SPS). The NdFeB nanocrystalline ribbon powders were subjected to cold sintering below 450 °C using pressure-assisted SPS, followed by hot deformation at 710 °C and 810 °C via SPS. Results indicate that cold sintering below 450 °C effectively restricts grain growth in the NdFeB magnets, yielding sub-100 nm scale grains across both fine-grained regions and most coarse-grained regions. The refined grain structure achieved through cold sintering allows for a lower hot deformation temperature as compared with the magnet by conventional sintering, as finer grains allow easier deformation and grain sliding/rotation. This process produces a highly fine-grained and anisotropic microstructure to achieve high magnetic performance (i.e., high intrinsic coercivity, remanence, and maximum energy product) in the magnets. The cold sintering (at 350 °C) and lower hot deformation temperatures required (e.g., 710 °C) help control grain coarsening and limit grain size that is commensurate with the size of a single magnetic domain of the Nd 2 Fe 14 B magnetic matrix phase, resulting in high intrinsic coercivity (H ci =11.4 kOe). Furthermore, the reduced hot deformation temperature mitigates the formation of coarse grain bands, leading to improved magnetic properties, specifically an increased remanence (B r = 14.3 kGs) and a high maximum energy product ((BH) max = 48 MGOe). In conclusion, cold sintered hot deformed NdFeB magnet also shows good thermal stability with reversible temperature coefficient α(B r )= -0.097 %/K and α(H ci )= -0.616 %/K at elevated temperatures up to 400 K.

Cold Sintering↗

Hot Hydrogen Exposure of U x Zr 1-x C y Nuclear Fuel: The Effect of Additional Carbon

Nuclear thermal propulsion (NTP) using hydrogen as propellant in a solid-state fission reactor to reach temperatures of up to 3000K can achieve significantly higher specific impulse than chemical propulsion. A promising fuel that is again considered for NTP is U x Zr 1-x C y . To reduce the overall mass loss as well as the uranium fuel loss, a range of experiments using additional carbon in hot hydrogen (2600 K, 6 SLPM flow rate) were performed for up to 5-6 h. Both a CH 4 addition (0.1 and 0.2 vol%) in the hydrogen stream and the use of sacrificial graphite pieces upstream of the samples were tested, with sample compositions from 5 at% UC to 30 at% UC. The results showed a strong reduction of mass loss, up to a factor of 3, as well as a reduction of surface uranium losses in the presence of additional carbon in the atmosphere. Even with additional carbon in the atmosphere, material with 30 at% UC was not stable, but material with 20 at% UC was stable for up to 6h. The sample surfaces showed texturing after processing, possibly by grain growth on the surface. This led to a separation into grains with high uranium content close to the (100)-orientation, and with low uranium content in grains close to the (111)-orientation.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Colossal Grains for a New Structural Paradigm in Thin-Film Photovoltaics

II-VI based thin-film photovoltaics (PV) have experienced substantial commercial success on a foundation of fast large-scale deposition and processing. This type of processing, regardless of material type, nearly always results in small grain (nm to several um diameters) polycrystalline material that, if not for effective grain boundary (GB) and defect passivation, would severely limit PV performance. In the case of CdTe based PV technology, the nearly ubiquitous CdCl2 treatment is used, in part, to passivate the polycrystalline p-type absorber even though Cl is known to (and used to) compensate p-type II-VI materials. Given that VOC is still the most limited performance metric and it can only be improved through higher p-type absorber concentrations, CdCl2 treatments may be holding the technology back. In this talk, we will discuss results related to a process by which small grain CdSeTe material is rapidly transformed into very large grain material (100-1000um diameters, Fig. 1a). This explosive recrystallization, which we have termed colossal grain growth (CGG), occurs by a Cl free process with thin films (<10um) deposited using the same fast deposition techniques the industry has relied on for more than a decade. Our modeling suggests that GB recombination becomes significantly less important at these grain sizes and thus may eliminate the need for a CdCl2 treatment. This result is complimented by previous results of epitaxial growth at high rates on single crystal seed layers. Thin CdSeTe CGG seed layers can be used for rapid epitaxy of CdTe to complete a standard device stack (Fig.1b). This is an optimistic view and the current limitations and challenges related to this process and these materials will also be discussed, including alloy and substrate roughness sensitivity, intragrain material quality, and complex defect chemistry. These challenges are not insignificant but overcoming them may enable a new structural paradigm for thin-film PV.

CdTe↗

Nanotwin stability in alloyed copper under ambient and cryo-temperature dependent deformation states

Nanometer size grains, solid solution strengthening, low temperatures, and a high density of nanotwins can provide significant strengthening to a material. Nevertheless, under loading the microstructure may evolve altering the effect of grain size, twin density, etc. on this strengthening. In some cases, these effects can be coupled as in detwinning, which is a mechanism for cryogenic grain growth. Here, in this work, a series of copper nanotwinned columnar grains are solid solution alloyed with aluminum and subject to ambient and cryogenic (–196 °C) environments during mechanical indentation, with the influence of alloying on the detwinning evolution studied. Under indentation, at a lower aluminum solute content (2 at.%), the columnar grains bent corresponding to a loss of twins. At a higher aluminum solute content (8 at.%), the grains shear and retain the nanotwins. Atomistic-scale simulations reveal an increase in the incoherent twin boundary velocity with decreasing temperature, but this boundary velocity is reduced with increasing alloy solute content. The coupling of solid solution strengthening and nanotwin stabilization is then used to explain the microstructural stability as a function of indentation at different temperature conditions.

36 MATERIALS SCIENCE↗

Influence of implantation temperature and He implantation-induced defects on morphological evolution of co-deposited Cu-Mo nanocomposites

Here, we investigate the effect of high-temperature helium (He) implantation on microstructural evolution in physical-vapor-co-deposited nanocomposite thin films of copper (Cu) and molybdenum (Mo). The microstructure morphologies of He-implanted and He-free domains are characterized using transmission electron microscopy and statistical analysis. High implantation temperatures (500°C and 750°C) lead to coarsening of Cu and Mo domains and their eventual reorientation. The microstructure evolution in He-implanted and He-free domains is comparable, indicating that implantation-induced defects do not accelerate the coarsening of the nanocomposite as compared to annealing alone. This observation contrasts with previously reported effects of implantation-induced defects on single-phase nanocrystalline metals, which include enhancement of grain growth by increasing self-diffusivity or its inhibition by pinning of grain boundaries.

36 MATERIALS SCIENCE↗

Imaging CdCl 2 defect passivation and formation in polycrystalline CdTe films by cathodoluminescence

Polycrystalline thin-film solar cells are attractive for low-cost photovoltaics, but their efficiencies are hindered by material quality issues. State-of-the-art CdTe solar cells use CdCl 2 annealing treatments whose effects are still being discovered at a fundamental level. Here, a series of CdTe samples with different annealing temperatures is investigated with high-resolution hyperspectral cathodoluminescence mapping measured at both room temperature and low temperature on the same microscopic areas. A statistical analysis over a large number of grains is combined with a local analysis at grain boundaries. The results elucidate the dynamic interplay between grain boundary and intragrain defect passivation and formation, in the midst of grain growth. The CdCl 2 annealing initially contributes to an increase of the grain size and the passivation of both grain boundaries and grain interiors, increasing the overall luminescence and diffusion length. For higher annealing temperatures, a further increase of grain size is counterbalanced by the rise of bulk defects. The results illustrate the tradeoffs that lead to an optimal annealing temperature, as well as new methods for understanding defect passivation and creation in thin film solar cells.

14 SOLAR ENERGY↗

Reduced thermal conductivity due to scattering centers in p-type SiGe alloys

Spark erosion was used to produce ultra-fine particles of SiGe thermoelectric material and boron nitride, an inert phonon-scattering material. A homogeneous powder was made by mixing the two powders. The mixture was hot pressed to produce a thermoelectric material with uniformity dispersed, ultra-fine, inert, phonon-scattering centers. It is shown that, in samples with inert boron nitride or silicon nitride, thermal conductivity of a SiGe alloy can be reduced by about 25 percent while maintaining the electrical properties of the samples. Annealing of all the samples at 1525 K caused grain growth to over a micron, eliminating the detrimental effect attributable to small grains. Only in the sample with boron nitride the thermal conductivity did remain well below that for standard p-type SiGe (about 25 percent), while the electrical resistivity and Seebeck coefficient were very close to the values for standard p-type 80/20 SiGe.

Beaty, John S.↗

Euhedral metallic-Fe-Ni grains in extraterrestrial samples

Metallic Fe-Ni is rare in terrestrial rocks, being largely restricted to serpentinized peridotites and volcanic rocks that assimilated carbonaceous material. In contrast, metallic Fe-Ni is nearly ubiquitous among extraterrestrial samples (i.e., meteorites, lunar rocks, and interplanetary dust particles). Anhedral grains are common. For example, in eucrites and lunar basalts, most of the metallic Fe-Ni occurs interstitially between silicate grains and thus tends to have irregular morphologies. In many porphyritic chondrules, metallic Fe-Ni and troilite form rounded blebs in the mesostasis because their precursors were immiscible droplets. In metamorphosed ordinary chondrites, metallic Fe-Ni and troilite form coarse anhedral grains. Some of the metallic Fe-Ni and troilite grains has also been mobilized and injected into fractures in adjacent silicate grains where local shock-reheating temperatures reached the Fe-FeS eutectic (988 C). In interplanetary dust particles metallic Fe-Ni most commonly occurs along with sulfide as spheroids and fragments. Euhedral metallic Fe-Ni grains are extremely rare. Several conditions must be met before such grains can form: (1) grain growth must occur at free surfaces, restricting euhedral metallic Fe-Ni grains to systems that are igneous or undergoing vapor-deposition; (2) the metal (+/-) sulfide assemblage must have an appropriate bulk composition so that taenite is the liquidus phase in igneous systems or the stable condensate phase in vapor-deposition systems; and (3) metallic Fe-Ni grains must remain underformed during subsequent compaction, thermal metamorphism, and shock. Because of these restrictions, the occurrence of euhedral metallic Fe-Ni grains in an object can potentially provide important petrogenetic information. Despite its rarity, euhedral metallic Fe-Ni occurs in a wide variety of extraterrestrial materials. Some of these materials formed in the solar nebula; others formed on parent body surfaces by meteoroid impacts.

Rubin, Alan E.↗

High temperature stabilization of ultrafine grain tungsten alloys through synergistic compositional complexities

Thermally-stabilized fine-grained microstructures in tungsten provide a pathway to harnessing enhanced properties such as a reduced ductile-to-brittle transition temperature and improved strength while mitigating the adverse effects of grain growth and recrystallization. Here, in this study, we employ a material design strategy that relies on grain boundary segregation in the nanocrystalline state driven by alloy thermodynamics balanced with impurity scavenging through in situ formation of kinetically-stabilizing metal carbides. A W-Ti-Cr alloy is designed through lattice Monte Carlo methods and subsequently synthesized in a single-phase nanocrystalline state, which upon annealing, evolves into an ultrafine grained microstructure containing chromium grain boundary segregation collectively with a dispersed TiX (X=C,O) phase through the reaction of titanium with carbon and oxygen impurities. In situ synchrotron X-ray diffraction experiments demonstrate that increased Ti promotes stabilization across a larger temperature range but with diminishing returns above 10 at.% Ti. Long-term stability was confirmed through the retention of the ultrafine grained microstructure for a total of 8 days (192 h) at 1300 °C without grain/carbide growth and/or recrystallization. Our results demonstrate that, through strategic tailoring of composition and microstructure, one can harness the benefits of both thermodynamic and kinetic stabilization mechanisms, opening pathways for future alloy formulations that expand the window of stability.

36 MATERIALS SCIENCE↗

Nanostructured Oxide-Dispersion-Strengthened CoCrFeMnNi High-Entropy Alloys with High Thermal Stability

A nanostructured oxide-dispersion-strengthened (ODS) CoCrFeMnNi high-entropy alloy (HEA) is synthesized by a powder metallurgy process. The thermal stability, including the grain size and crystal structure of the HEA matrix and oxide dispersions, is carefully investigated by X-ray diffraction (XRD) and electron microscopy characterizations after annealing at 900 °C. The limited grain growth may be attributed to Zener pinning of yttria dispersions that impede the grain boundary mobility and diffusivity. The high hardness is caused by both the fine grain size and yttria dispersions, which are also retained after annealing at 900 °C. In this study, it is implied that the combination of ODS and HEA concepts may provide a new design strategy for the development of thermally stable nanostructured alloys for extreme environments.

36 MATERIALS SCIENCE↗

Microstructural Transitions during Powder Metallurgical Processing of Solute Stabilized Nanostructured Tungsten Alloys

Exploiting grain boundary engineering in the design of alloys for extreme environments provides a promising pathway for enhancing performance relative to coarse-grained counterparts. Due to its attractive properties as a plasma facing material for fusion devices, tungsten presents an opportunity to exploit this approach in addressing the significant materials challenges imposed by the fusion environment. Here, we employ a ternary alloy design approach for stabilizing W against recrystallization and grain growth while simultaneously enhancing its manufacturability through powder metallurgical processing. Mechanical alloying and grain refinement in W-10 at.% Ti-(10,20) at.% Cr alloys are accomplished through high-energy ball milling with transitions in the microstructure mapped as a function of milling time. We demonstrate the multi-modal nature of the resulting nanocrystalline grain structure and its stability up to 1300 °C with the coarser grain size population correlated to transitions in crystallographic texture that result from the preferred slip systems in BCC W. Field-assisted sintering is employed to consolidate the alloy powders into bulk samples, which, due to the deliberately designed compositional features, are shown to retain ultrafine grain structures despite the presence of minor carbides formed during sintering due to carbon impurities in the ball-milled powders.

36 MATERIALS SCIENCE↗

Adding calcium improves lithium ferrite core

Adding calcium increases uniformity of grain growth over a wide range of sintering temperatures and reduces porosity within the grain. Ferrite cores containing calcium have square hysteresis loops and high curie temperatures, making them useful in coincident current memories of digital electronic computers.

Lessoff, H.↗

Sintering of BaCe(sub 0.85)Y(sub 0.15)O(sub 3-delta) with/without SrTiO3 Dopant

The perovskite composition, BaCe(sub 0.85)Y(sub 0.15)O(sub 3-delta), displays excellent protonic conduction at high temperatures making it a desirable candidate for hydrogen separation membranes. This paper reports on the sintering behavior of BaCe(sub 0.85)Y(sub 0.15)O(sub 3-delta) powders doped with SrTiO3. Two methods were used to synthesize BaCe(sub 0.85)Y(sub 0.15)O(sub 3-delta) powders: (1) solid state reaction and (2) wet chemical co-precipitation. Co-precipitated powder crystallized into the perovskite phase at 1000 C for 4 hrs. Complete reaction and crystallization of the perovskite phase by solid state was achieved by calcining at 1200 C for 24 hrs. Solid state synthesis produced a coarser powder with an average particle size of 1.3 microns and surface area of 0.74 sq m/g. Co-precipitation produced a finer powder with a average particle size of 65 nm and surface area of 14.9 sq m/g. Powders were doped with 1, 2, 5, and 10 mole % SrTiO3. Samples were sintered at 1450 C, 1550 C and 1650 C. SrTiO3 enhances sintering, optimal dopant level is different for powders synthesized by solid state and co-precipitation. Both powders exhibit similar grain growth behavior. Dopant levels of 5 and 10 mole % SrTiO3 significantly enhances the grain size.

Dynys, F.↗

Thermal properties of field-assisted-sintered SiCN–Y 2 O 3 composites

Polymer-derived amorphous SiCN has excellent high-temperature stability and properties. To reduce the shrinkage during pyrolysis and to improve the high-temperature oxidation resistance, Y 2 O 3 was added as a filler. In this study, polymer-derived SiCN–Y 2 O 3 composites were fabricated by mixing a polymeric precursor of SiCN with Y 2 O 3 submicron powders in different ratios. The mixtures were cross-linked and pyrolyzed in argon. SiCN–Y 2 O 3 composites were processed using field-assisted sintering technology at 1350°C for 5 min under vacuum. Dense SiCN–Y 2 O 3 composite pellets were successfully made with relative density higher than 98% and homogeneous microstructure. Due to low temperature and short time of the heat-treatment, the grain growth of Y 2 O 3 was substantially inhibited. The Y 2 O 3 grain size was ~1 μm after sintering. The composites’ heat capacity, thermal diffusivity, and thermal expansion coefficients were characterized as a function of temperature. The thermal conductivity of the composites ceramics decreased as the amount of amorphous SiCN increased and the coefficient of thermal expansion (CTE) of the composites increased with Y 2 O 3 content. However, the thermal conductivity and CTE did not follow the rule of mixture. This is likely due to the partial oxidation of SiCN and the resultant impurity phases such as Y 2 SiO 5 , Y 2 Si 2 O 7 , and Y 4.67 (SiO 4 ) 3 O.

36 MATERIALS SCIENCE↗

Grain engineering for efficient near-infrared perovskite light-emitting diodes

Metal halide perovskites show promise for next-generation light-emitting diodes, particularly in the near-infrared range, where they outperform organic and quantum-dot counterparts. However, they still fall short of costly III-V semiconductor devices, which achieve external quantum efficiencies above 30% with high brightness. Among several factors, controlling grain growth and nanoscale morphology is crucial for further enhancing device performance. This study presents a grain engineering methodology that combines solvent engineering and heterostructure construction to improve light outcoupling efficiency and defect passivation. Solvent engineering enables precise control over grain size and distribution, increasing light outcoupling to ~40%. Constructing 2D/3D heterostructures with a conjugated cation reduces defect densities and accelerates radiative recombination. The resulting near-infrared perovskite light-emitting diodes achieve a peak external quantum efficiency of 31.4% and demonstrate a maximum brightness of 929 W sr -1 m -2 . These findings indicate that perovskite light-emitting diodes have potential as cost-effective, high-performance near-infrared light sources for practical applications.