Dielectric Spectroscopy Cable NDE for Unequal Aging Over Different Lengths

Abstract

This Pacific Northwest National Laboratory milestone report assesses the effect of unequal aging over different lengths of cable on dielectric spectroscopy (DS) bulk impedance measurements from the cable end. DS measurements can indicate the remaining useful life of cables; however, most benchmark tests are based on accelerated aging of the entire cable. If only a portion of the cable is exposed to a harsh environment (as is frequently the case), the DS measurement will indicate a significantly less-aged cable than if the entire cable were exposed to a uniform environmental stress. The DS measurement is primarily related to the intrinsic insulation material relative permittivity—typically between 1.5 and 3.0. Insulation aging increases permittivity and, correspondingly, the cable’s overall capacitance measured from the cable end. To judge the health of the overall cable system, operators are primarily interested in the condition of the most severely aged section since that is where a failure is most likely to occur. This can be expressed as the dimensionless relative permittivity of the severely aged section divided by the permittivity of a pristine cable. This relative permittivity is an intrinsic material parameter independent of cable length and can serve as a quantitative indication of the insulation condition. If the relative percentages of cable exposed to a harsh and benign environment are known, the DS measurement of the entire cable length, including both pristine and aged sections, can be compensated to predict the relative permittivity (relative to pristine permittivity) of the most severly aged segment. A test was performed on three 50 ft (16 m) cables with 10%, 50%, and 90% of the cable inside a thermal aging oven. Predictably, the aging effect on the DS response was greatest in the 90% sample, followed by the 50% sample, and then the 10% sample. The more interesting result is the ratio of the aged insulation permittivity to the pristine insulation permittivity. Based on prior work, an end-of-life cable has a value of approximately 1.35. If the relative percentages of pristine and severely aged cable lengths are known, and the total cable-length capacitance of the initial pristine cable and the combined pristine plus aged cable are known, the relative aged permittivity (ratio of aged section permittivity / pristine section permittivity) can be estimated. The relative cable lengths exposed to a harsh environment may be known or estimated based on plant layout drawings or cable reflectometry tests that can locate the oven entry and exit points. The compensation was verified using a lumped-parameter model to predict the aged-segment permittivity e2/e1, where e2 is the aged-segment permittivity and e1 is the pristine-segment permittivity. For all three percentages of aged cable lengths, the ratio was quite similar, as would be expected since all cable segments were exposed to the same aging environment. This ratio of aged permittivity to pristine permittivity can be compared to other damage indicating tests, including elongation at break, to assess cable condition.

Explore related subjects

Keep this discovery

BibTeXRIS

Glass, Samuel W., Elen, Muthu (ORCID:0000000261927091), Fifield, Jacob. 2026-08-28. Dielectric Spectroscopy Cable NDE for Unequal Aging Over Different Lengths. https://doi.org/10.2172/3684099

Cite the original work for its findings. Save a collection to share your selection of sources.

Discover connections

Connections use source metadata and explicit phrase matches, not verified experimental comparisons.

KEEP EXPLORING

Related reports

Monitoring Depolymerization in Mesopores Using Dynamic Properties of Polymeric Melt Accessed via Dielectric Spectroscopy

Traditional design principles for heterogeneous catalysis guide the use of catalytic particles with mesosized (∼2–50 nm) pores to increase the number of surface-active sites by way of an increased surface area. However, the entry of long-chain polymers into such pores may be significantly limited by the size and entanglement of polymers in the melt state, thereby decreasing the number of accessible sites. Assessment of catalyst performance from traditional reactor-based studies averages over intrapore reaction events as well as reactions on the surface of a particle, resulting in an inability to distinguish between differences in site accessibility and activity. Techniques that assess the intrapore performance can inform the design of future heterogeneous catalysts for polymer upcycling. In this work, we demonstrate the use of broadband dielectric spectroscopy to monitor depolymerization of a polymer melt within mesopores via changes in the segmental relaxation time scale of amorphous polymer chains. In particular, we highlight the use of an anodic aluminum oxide (AAO) membrane as a readily available model for catalyst pores with a well-characterized pore morphology. The decrease in the segmental relaxation (α-relaxation) time of the melt with increasing chain scission emerges as a measure of the extent of polymer deconstruction inside mesopores. To demonstrate the utility of this technique, we demonstrate the decomposition of two commercial poly(propylene carbonate) polymers with different decomposition rates within mesopores. As the polymers depolymerize, their segmental relaxation time decreases as the molecular weight decreases (as predicted by the Fox–Flory equation). The BDS-measured change in segmental relaxation time mirrors the expected trend based on change in molecular weight measured by size exclusion chromatography.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH

Strategies for Fabricating Molybdenum Structures Using Laser Powder Bed Fusion

Advances in manufacturing techniques are viewed as enabling technologies for development of high performance nuclear fuel forms that couple high uranium density with improvements to key properties such as thermal conductivity unattainable through conventional fabrication routes. Additive manufacturing (AM) enables the fabrication of complex fuel geometries that are difficult or impossible to achieve using conventional manufacturing methods. Melting-based AM processes, such as laser powder bed fusion (LPBF), provide high geometric resolution (>200 µm depending on the feature) across a variety of metal alloys, including those suitable for high-temperature fuel cladding applications, such as Nb, W, and Mo. Molybdenum is particularly attractive due to its high thermal conductivity, low thermal expansion, and excellent mechanical stability at elevated temperatures. However, its high melting temperature and brittle nature at low temperatures pose significant challenges during LPBF processing. Rapid solidification inherent to LPBF induces high residual stresses, often leading to post-solidification cracking, which limits the manufacturability of Mo components via this method.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS