Nanoindentation mapping defects filtration for heterogeneous materials using generative adversarial networks

Abstract

Advanced composite materials with multiple phases and heterogeneous microstructure necessitate spatial mapping characterization of elastic modulus to develop constitutive relations and overall mechanical response. Such modulus mapping can be obtained using the nanoindentation technique, where the indenter tip raster over the selected microstructure region. Typically, a surface preparation procedure is done in the specimens to ensure proper contact between the indenter tip and sample surface. However, a near-perfect surface finish is unachievable in heterogeneous materials, primarily with ceramic reinforcements, due to the differential material removal rate during polishing. Thus, the nanoindenter records localized erroneous measurements due to differences in surface roughness and corresponding force response. This study establishes a novel deep learning-based strategy to rectify incorrect experimental spatial measurements acquire during nanoindentation modulus mapping. Here, the integrated bicubic interpolation and generative adversarial networks (GANs) model was trained using 14 ceramic and 18 metallic data sets, each comprising 65,536 measurements. The developed algorithm was validated against experimental measurements on four unknown specimens. The standard deviation in measured elastic modulus reduces by ~50% in ceramics and ~72% in metallic samples. This computational framework proposes a novel approach to reducing uncertainty in materials’ properties using state-of-the-art computer vision techniques.

Explore related subjects

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

Bianco, Giuseppe, Paul, Tanaji, Nisar, Ambreen, Hamrani, Abderrachid, Boesl, Benjamin, Agarwal, Arvind. 2022-07-09. Nanoindentation mapping defects filtration for heterogeneous materials using generative adversarial networks. https://doi.org/10.1016/j.matchar.2022.112107

Cite the original work for its findings. Save a collection to share your selection of sources.

KEEP EXPLORING

Related reports

Cyclic moisture reactivation of calcium sorbents for long duration thermochemical energy storage

The transition to a flexible and reliable energy infrastructure, using electro-thermal energy generation technologies such as geothermal, concentrated solar power, and nuclear, usually demands simultaneous advancement of thermal energy storage (TES) to support on-demand electricity generation and industrial applications while mitigating the inherent intermittency of renewable energy sources and power outages from direct energy generation. Among TES technologies, thermochemical energy storage (TCES) based on calcium looping emerges as a compelling high-power energy storage candidate due to its high reaction enthalpy, compatibility with elevated operating temperatures, and abundance of low-cost materials. However, the long-term durability of calcium-based sorbents for TCES is hindered by surface sintering and particle aggregation, leading to performance degradation over repeated thermal cycles. This study explores a moisture hydration-based strategy to regenerate a degraded calcium sorbent and mitigate performance degradation for long duration TCES. The addition of moisture transforms calcium oxide into calcium hydroxide and produces intercalation water layers, associated with a regenerated surface area and reduced calcium oxide crystallite size. Both these effects are beneficial in restoring the sorbents' reactivity for carbonization. Additionally, an optimized hydration-assisted reactivation protocol balances the recovered energy storage capacity with heating penalty required for moisture removal from hydrated samples, resulting in an enhanced energy storage capacity up to 176% compared to benchmark sorbents that undergo cycling without reactivation after 60 cycles. In conclusion, these results highlight the potential of hydration-assisted reactivation to enhance the long-term performance of TCES, providing an effective pathway to advancing electro-thermal storage technologies.

36 MATERIALS SCIENCE↗