A method for preparing an improved article including a nickel-based superalloy is presented. The method includes heat-treating a workpiece including a nickel-based superalloy at a temperature above the gamma-prime solvus temperature of the nickel-based superalloy and cooling the heat-treated workpiece with a cooling rate less than 50 degrees Fahrenheit/minute from the temperature above the gamma-prime solvus temperature of the nickel-based superalloy so as to obtain a cooled workpiece. The cooled workpiece includes a coprecipitate of a gamma-prime phase and a gamma-double-prime phase, wherein the gamma-prime phase of the coprecipitate has an average particle size less than 250 nanometers. An article having a minimum dimension greater than 6 inches is also presented. The article includes a material having a coprecipitate of a gamma-prime phase and a gamma-double-prime phase, wherein the gamma-prime phase of the coprecipitate has an average particle size less than 250 nanometers.

Explore related subjects

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

Detor, Andrew Joseph, DiDomizio, Richard, Hanlon, Timothy, Shen, Chen, Zhou, Ning. 2020-05-05. Methods for preparing superalloy articles and related articles. https://www.osti.gov/biblio/1650850

Cite the original work for its findings. Save a collection to share your selection of sources.

KEEP EXPLORING

Related reports

Cyclic moisture reactivation of calcium sorbents for long duration thermochemical energy storage

The transition to a flexible and reliable energy infrastructure, using electro-thermal energy generation technologies such as geothermal, concentrated solar power, and nuclear, usually demands simultaneous advancement of thermal energy storage (TES) to support on-demand electricity generation and industrial applications while mitigating the inherent intermittency of renewable energy sources and power outages from direct energy generation. Among TES technologies, thermochemical energy storage (TCES) based on calcium looping emerges as a compelling high-power energy storage candidate due to its high reaction enthalpy, compatibility with elevated operating temperatures, and abundance of low-cost materials. However, the long-term durability of calcium-based sorbents for TCES is hindered by surface sintering and particle aggregation, leading to performance degradation over repeated thermal cycles. This study explores a moisture hydration-based strategy to regenerate a degraded calcium sorbent and mitigate performance degradation for long duration TCES. The addition of moisture transforms calcium oxide into calcium hydroxide and produces intercalation water layers, associated with a regenerated surface area and reduced calcium oxide crystallite size. Both these effects are beneficial in restoring the sorbents' reactivity for carbonization. Additionally, an optimized hydration-assisted reactivation protocol balances the recovered energy storage capacity with heating penalty required for moisture removal from hydrated samples, resulting in an enhanced energy storage capacity up to 176% compared to benchmark sorbents that undergo cycling without reactivation after 60 cycles. In conclusion, these results highlight the potential of hydration-assisted reactivation to enhance the long-term performance of TCES, providing an effective pathway to advancing electro-thermal storage technologies.

36 MATERIALS SCIENCE↗