Nanostructure templating using low temperature atomic layer deposition

Abstract

Methods are described for making nanostructures that are mechanically, chemically and thermally stable at desired elevated temperatures, from nanostructure templates having a stability temperature that is less than the desired elevated temperature. The methods comprise depositing by atomic layer deposition (ALD) structural layers that are stable at the desired elevated temperatures, onto a template employing a graded temperature deposition scheme. At least one structural layer is deposited at an initial temperature that is less than or equal to the stability temperature of the template, and subsequent depositions made at incrementally increased deposition temperatures until the desired elevated temperature stability is achieved. Nanostructure templates include three dimensional (3D) polymeric templates having features on the order of 100 nm fabricated by proximity field nanopatterning (PnP) methods.

Explore related subjects

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

Grubbs, Robert K, Bogart, Gregory R, Rogers, John A. 2011-12-20. Nanostructure templating using low temperature atomic layer deposition. https://www.osti.gov/biblio/1034170

Cite the original work for its findings. Save a collection to share your selection of sources.

KEEP EXPLORING

Related reports

Gold Quantum Rods: Modulation of Singlet and Triplet Exciton Populations by the Rod Length

Abstract Gold quantum rods (QRs) of Au60, Au78, Au96, and Au114 (protected by thiolate ligands) exhibit exclusive fluorescence, which is different from the shorter Au42 QR with dual emission (fluorescence + phosphorescence). Herein, we report the excitation wavelength-dependent near-infrared-II photoluminescence (PL) and exciton dynamics of this series of QRs. Interestingly, the fluorescence quantum yield (QY) of the QRs is much higher (2–10×) when the lowest singlet excited state (S1) is excited compared to the excitation of high-lying states (Sn). A metastable intermediate singlet state (denoted S′) is identified by transient absorption spectroscopy when Sn is excited, and this S′ state leads to fast “skybridge” intersystem crossing (ISC), which contributes primarily (>60%) to the total triplet population. With increasing aspect ratio (AR) of QRs (from 6.3 to 18.7), nonradiative processes accelerate, leading to fast decay of the S1 state (hence, less QY) and of the T1 state (barely phosphorescent). A detailed energy flow mechanism is determined for the QRs after photoexcitation, which offers a design principle for manipulation of exciton dynamics toward potential utilization of higher excited states in applications.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Demonstration of gold nanorod systems for enhanced total efficiency: Experimental and numerical analysis

This study investigates the photothermal performance of gold nanorods engineered to exhibit longitudinal plasmon resonances at 695 nm, 780 nm, and 970 nm. The work combines synthesis, structural characterization, extinction measurements, numerical modeling, and controlled temperature experiments to quantify how nanorod geometry, resonance tuning, concentration, and chamber shape jointly influence heat generation. Transmission electron microscopy confirms that increasing nanorod aspect ratio systematically shifts the longitudinal plasmon peak toward the near-infrared region. Extinction measurements show strong agreement with theoretical predictions, validating the numerical model across two independent datasets. Three chamber geometries were tested under laser excitation at 640 nm, 808 nm, and 980 nm: an ascending stepped base, a flat base, and a descending stepped base. Without nanorods, the ascending geometry produced the highest efficiency due to enhanced natural convection. After introducing gold nanorods, all geometries exhibited substantial thermal enhancement, with total efficiencies exceeding 20%. The strongest improvement was obtained for nanorods resonant at 780 nm with a mass concentration of 4.6 mg/mL implemented on the descending stepped-base geometry. This performance resulted from the combined effect of spectral overlapping with the 808 nm laser, the highest nanorod concentration, and localized heat accumulation that intensified buoyancy-driven flow. The findings demonstrate that total efficiency is governed by a synergistic interplay between optical resonance, nanoparticle concentration, and macroscopic chamber design, revealing the system-level coupling between nanoscale plasmonic absorption and macroscale heat-transfer phenomena. The results provide a validated framework for tuning nanoscale plasmonic absorbers and optimizing thermal systems for applications requiring efficient light-to-heat conversion.

77 NANOSCIENCE AND NANOTECHNOLOGY↗