Performance of PTFE-lined composite journal bearings
(Previously announced in STAR as N82-17263)
Engineering topics
Publications and source records attributed to Sliney, H. E..
(Previously announced in STAR as N82-17263)
(Previously announced in STAR as N81-20275)
Plain cylindrical journal bearings consisting of aramid fiber reinforced epoxy outer shells and glass fiber reinforced PTFE lubricating liners were evaluated. All materials in these bearings are electrically nonconductive; thus eliminating the problem of galvanic corrosion sometimes encountered with metal bearings installed in dissimilar metal mountings. Friction and wear characteristics were determined for loads, temperatures, and oscillating conditions that are typical of current airframe bearing applications. Friction and wear characteristics were found to be compatible with most airframe bearing requirements from -23 C to 121 C. Contamination with MIL H-5606 hydraulic fluid increased wear of the PTFE liners at 121 C, but did not affect the structural integrity of the aramid/epoxy composite.
The need for high temperature tribological coatings and self-lubricating materials in advanced technology is discussed. A qualitative model for the mechanism of solid lubrication is proposed. The model is based upon microscopic observations of the dynamics of third-body solids in lubricated contacts. In this model, the rheology of plastic flow is suggested as a more general criterion for predicting the lubricating potential of a solid material than, for example, a specific crystal structure. Some examples of layer-lattice and nonlayer-lattice solids that lubricate by virtue of their extreme plasticity, film coherence, and adhesion to the lubricated metal are described. Circumstantial evidence for the model is presented for low shear-strength solids at room temperature and for solids such as calcium fluoride that become lubricative only when their brittle-to-ductile transition temperature is exceeded. Some materials considerations in the selection of hard-coat materials for wear control are also presented.
A Hertzian contact is lubricated with dispersed graphite in mineral oils under boundary lubrication conditions. The contacts are optically observed under pure rolling, combined rolling and sliding, and pure sliding conditions. The contact is formed with a steel ball on the flat surface of a glass disk. Under pure rolling and combined rolling and sliding conditions, it is found that, for low speeds, a graphite film can form which will separate the contacting surfaces. In contrast, under pure sliding conditions, graphite accumulates at the inlet and sweeps around the contact, but very little of graphite passes through the contact. The accumulated graphite appears to act as a barrier which reduces the supply of oil available to the contact for boundary lubrication. Friction data show no clear short-term beneficial or detrimental effect caused by addition of graphite to the base oil. However, during pure sliding, more abrasion occurs on the polished balls lubricated with the dispersion than on those lubricated with the base oil alone.
A Hertzian contact was lubricated with dispersed graphite in mineral oils under boundary lubrication conditions. The contact was optically observed under pure rolling, combined rolling and sliding, and pure sliding conditions. The contact was formed with a steel ball on the flat surface of a glass disk. Photomicrographs are presented which show the distribution of the graphite in and around the contact. Friction and surface damage are also shown for conditions when the base oils are used alone and when graphite is added to the base oils. Under pure rolling and combined rolling and sliding conditions, it is found that, for low speeds, a graphite film can form which will separate the contacting surfaces. Under pure sliding conditions, graphite accumulates at the inlet and sweeps around the contact, but very little of the graphite passes through the contact. The accumulated graphite appears to act as a barrier which reduces the supply of oil available to the contact for boundary lubrication. Friction data show no clear short term beneficial or detrimental effect caused by addition of graphite to the base oil. However, during pure sliding, more abrasion occurs on the polished balls lubricated with the dispersion than on those lubricated with the base oil alone. All observations were for the special case of a highly-polished ball on a glass surface and may not be applicable to other geometries and materials, or to rougher surfaces.
A Hertzian contact consisting of a steel ball in contact with a glass disk is lubricated with MoS2 dispersions and observed by optical microscopy at various slide/roll conditions. In general the behavior of MoS2 and graphite are similar. That is, the solids tend to enter the contact and form a film on the contacting surfaces whenever a rolling component of motion is used, but solid particles seldom enter the contact during pure sliding. The MoS2 has more pronounced plastic flow behavior than graphite. However, the polished steel ball is more readily scratched by MoS2 than by graphite. Under the conditions of these studies, lower friction and wear are observed with pure oil rather than with the dispersions. However under other conditions (such as different contact geometry or rougher surfaces) the solid lubricant dispersions might be beneficial.
The mechanical properties of two types of self lubricating composites (polymer matrix composites and inorganic composites) are discussed. Specific emphasis is given to the applicability of these composites in the aerospace industry.
A composite material is described which will provide low friction surfaces for materials in rolling or sliding contact and is self lubricating and oxidation resistant up to and in excess of about 930 C. The composite is comprised of a metal component which lends strength and elasticity to the structure, a fluoride salt component which provides lubrication and, lastly, a glass component which not only provides oxidation protection to the metal but may also enhance the lubrication qualities of the composite.
Four different compositions of self-lubricating, plasma-sprayed, composite coatings with calcium fluoride dispersed throughout cobalt alloy-silver matrices were evaluated on a friction and wear apparatus. In addition, coatings of the cobalt alloys alone and of one coating with a nickel alloy-silver matrix were evaluated for comparison. The wear specimens consisted of two, diametrically opposed, flat rub shoes sliding on the coated, cylindrical surface of a rotating disk. Two of the cobalt composite coatings gave a friction coefficient of about 0.25 and low wear at room temperature, 400 and 650 C. Wear rates were lower than those of the cobalt alloys alone or the nickel alloy composite coating. However, oxidation limited the maximum useful temperature of the cobalt composite coating to about 650 C compared to about 900 C for the nickel composite coating.
Self-lubricating graphite-fiber-reinforced polyimide liners for plain bearings raise service temperature from 325 F to 608 F.
Plasma sprayed coatings of pure silver and of composite materials containing silver were investigated as possible self lubricating coatings for titanium alloys in air at 430 C. Pure silver provided low friction but was prone to severe plastic deformation and excessive transfer except in coating thicknesses of 0.02 mm or less. Additions of nichrome, calcium fluoride, and glass to silver were all beneficial in reducing plastic deformation and otherwise improving the coatings. The longest coating wear life, low wear of Ti alloy pins in sliding contact with the coatings, and a steady friction coefficient of 0.19 were obtained with a four component coating of 0.17 mm thickness. The coating composition, in weight percent is 30 nichrome-30 Ag-25 CaF2-15 glass.
Self-lubricating, multicomponent coatings, which lubricate over a wide range of operating conditions, are described. The coatings have been successfully applied by plasma-spraying mixed powders onto superalloy substrates. They have been evaluated in friction and wear experiments, and in sliding contact bearing tests. These coatings are wear resistant by virtue of their self-lubricating characteristics rather than because of extreme hardness; a further benefit is low friction. Experiments with simple pin on disk sliding specimens and oscillating plain cylindrical bearing tests were performed to evaluate the tribological properties of the coatings. It was shown that coatings of nichrome, glass and calcium fluoride are self-lubricating from about 500 to 900 C, but give high friction at the lower temperatures. The addition of silver to the coating composition improved the low temperature bearing properties and resulted in coatings which are self-lubricating from cryogenic temperatures to at least 870 C; they are therefore 'wide temperature spectrum,' self-lubricating compositions.
A method is described for making a composite material which provides low friction surfaces for materials in rolling or sliding contact. The composite material which is self-lubricating and oxidation resistant up to and in excess of about 930 C is comprised of a metal component which lends strength and elasticity to the structure and a fluorine salt component which provides oxidation protection to the metal but may also enhance the lubrication qualities of the composite.
Self-lubricating, multicomponent coatings, which lubricate over a wide range of operating conditions, are described. The coatings were successfully applied by plasma-spraying mixed powders onto superalloy substrates. They were evaluated in friction and wear experiments, and in sliding contact bearing tests. These coatings are wear resistant by virtue of their self lubricating characteristics rather than because of extreme hardness; a further benefit is low friction. Experiments with simple pin on disk sliding specimens and oscillating plain cylindrical bearing tests were performed to evaluate the tribological properties of the coatings. It was shown that coatings of nichrome, glass and calcium fluoride are self-lubricating from about 500 to 900 C, but give high friction at the lower temperatures. The addition of silver to the coating composition improved the low temperature bearing properties and resulted in coatings which are self-lubricating from cryogenic temperatures to at least 870 C; they are therefore, wide temperature spectrum, self-lubricating compositions.
Four different compositions of self-lubricating, plasma-sprayed, composite coatings with calcium fluoride dispersed throughout cobalt alloy-silver matrices were evaluated on a friction and wear apparatus. In addition, coatings of the cobalt alloys alone and one coating with a nickel alloy-silver matrix were evaluated for comparison. The wear specimens consisted of two, diametrically opposed, flat rub shoes sliding on the coated, cylindrical surface of a rotating disk. Two of the cobalt composite coatings gave a friction coefficient of about 0.25 and low wear at room temperature, 400 and 650 C. Wear rates were lower than those of the cobalt alloys alone or the nickel alloy composite coating. However, oxidation limited the maximum useful temperature of the cobalt composite coating to about 650 C compared to about 900 C for the nickel composite coating.
Explore the source record for details and available documents.
A plain spherical bearing design with a ball diameter of 28.6 mm, a race length of 12.7 mm, and a 1.7-mm-thick, molded composite liner was evaluated. The liner material is a self-lubricating composite of graphite-fiber-reinforced polyimide resin (GFRPI). The liner is prepared by transfer molding a mixture of one part chopped graphite fiber and one part partially polymerized resin into the space between the bearing ball and the outer race and then completing the polymerization under heat and pressure. Several liner compositions were evaluated: two types of polyimide, condensation and addition; two types of graphite fiber, low and high modulus; and four powder additives - cadmium oxide, cadmium iodide, graphite fluoride, and molybdenum disulfide. The bearings were oscillated + or - 15 deg at 1 Hz for 20 kilocycles under a radial unit load of 29 MN sq m (4200 psi) in dry air at 25, 200, or 315 C. Both types of fiber and polyimide gave low friction and wear. A simple equation was developed to fit the wear-time data and adequately predicted wear to 100 kilocycles.