Engineering Papers⌕ Search

Engineering topics

Roy, Utpal N.

Publications and source records attributed to Roy, Utpal N..

28 records · Page 2

Impact of selenium addition to the cadmium-zinc-telluride matrix for producing high energy resolution X-and gamma-ray detectors

Abstract Both material quality and detector performance have been steadily improving over the past few years for the leading room temperature radiation detector material cadmium-zinc-telluride (CdZnTe). However, although tremendous progress being made, CdZnTe still suffers from high concentrations of performance-limiting defects, such as Te inclusions, networks of sub-grain boundaries and compositional inhomogeneity due to the higher segregation coefficient of Zn. Adding as low as 2% (atomic) Se into CdZnTe matrix was found to successfully mitigate many performance-limiting defects and provide improved compositional homogeneity. Here we report record-high performance of Virtual Frisch Grid (VFG) detector fabricated from as-grown Cd 0.9 Zn 0.1 Te 0.98 Se 0.02 ingot grown by the Traveling Heater Method (THM). Benefiting from superior material quality, we achieved superb energy resolution of 0.77% at 662 keV (as-measured without charge-loss correction algorithms) registered at room temperature. The absence of residual thermal stress in the detector was revealed from white beam X-ray topographic images, which was also confirmed by Infra-Red (IR) transmission imaging under cross polarizers. Furthermore, neither sub-grain boundaries nor their networks were observed from the X-ray topographic image. However, large concentrations of extrinsic impurities were revealed in as-grown materials, suggesting a high likelihood for further reduction in the energy resolution after improved purification of the starting material.

36 MATERIALS SCIENCE↗

Growth of Cd 0.9 Zn 0.1 Te 1-y Se y Single Crystals for Room Temperature Gamma-Ray Detection

Quaternary Cd 0.9 Zn 0.1 Te 1-y Sey (CZTS) single crystals, a novel room-temperature nuclear radiation detector semiconductor material, have been grown using a modified vertical Bridgman method (VBM) and a travelling heater method (THM). The percentage concentration of selenium in the VBM-grown crystal was 3% and that in the THM-grown crystal was 2%. While the THM Frisch collar detector (4.4 × 4.4 × 10.7 mm 3 ) produced a highly resolved pulse height spectra (PHS) with a resolution of ~1.06% for 662-keV gamma rays without any correction, the VBM-grown detector (10 × 10 × 2 mm 3 ) offered a high energy resolution of ~2% after application of a digital biparametric correction. The high-resolution performance of these detectors has been attributed to the addition of Se in the Cd 0.9 Zn 0.1 Te (CZT) matrix. Ab-initio calculations based on density functional theory (DFT) also confirmed that the addition of Se in the CZT matrix helps to reduce the formation of TeCd and the TeZn anti-sites. The VBM-grown crystals were characterized using powder x-ray diffraction (XRD) and energy dispersive x-ray spectroscopy (EDS). While XRD results revealed sharp diffraction peaks confirming the crystalline nature of the grown crystal, the EDS results confirmed the targeted stoichiometry of the elemental composition. The bulk resistivity of the grown crystal was calculated to be ~3 × 10 10 Ω-cm from current-voltage characteristics recorded at room temperature in a planar configuration, ensuring that the grown CZTS crystals have low dark current as required for detector-grade crystals.

42 ENGINEERING↗

Advances in CdZnTeSe for Radiation Detector Applications

Detection of X- and gamma-rays is essential to a wide range of applications from medical imaging to high energy physics, astronomy, and homeland security. Cadmium zinc telluride (CZT) is the most widely used material for room-temperature detector applications and has been fulfilling the requirements for growing detection demands over the last three decades. However, CZT still suffers from the presence of a high density of performance-limiting defects, such as sub-grain boundary networks and Te inclusions. Cadmium zinc telluride selenide (CZTS) is an emerging material with compelling properties that mitigate some of the long-standing issues seen in CZT. This new quaternary is free from sub-grain boundary networks and possesses very few Te inclusions. In addition, the material offers a high degree of compositional homogeneity. The advancement of CZTS has accelerated through investigations of the material properties and virtual Frisch-grid (VFG) detector performance. The excellent material quality with highly reduced performance-limiting defects elevates the importance of CZTS as a potential replacement to CZT at a substantially lower cost.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Optimization of selenium in CdZnTeSe quaternary compound for radiation detector applications

X- and gamma-ray detectors are increasingly becoming essential tool for science and technology in various fields include homeland security, nonproliferation, nuclear security, medical imaging, astrophysics, and high energy physics. Cd 1-x Zn x Te 1-y Se y (CZTS) is emerging as a next-generation compound semiconductor for such applications. CZTS was found to possesses a very low concentration of Te inclusions and free from sub-grain boundary networks. Being a quaternary compound with varying alloy composition, optimization of the composition was performed to determine the minimum amount of selenium required to produce CZTS with reduced defects. The optimized composition was found to be x=0.10 and y=0.02, i.e., Cd 0.9 Zn0.1Te 0.98 Se 0.02 , for excellent material properties as a radiation detector. The resulting material was free from sub-grain boundary networks and with a highly reduced concentration of Te inclusions. The bulk dark resistivity obtained was in the range of 1-3x1010 ohm-cm with the highest achieved mobility-lifetime product of ~6.6x10-3 cm2/V for the optimized CZTS composition. Impurity analyses were performed by the Glow Discharge Mass Spectroscopy (GDMS) technique, and the results showed relatively high impurity concentrations compared to commercial detector-grade CdZnTe. Thus, CZTS has room for further improvement with additional purification of the starting materials.

36 MATERIALS SCIENCE↗

Mapping of inhomogeneous quasi-3D electrostatic field in electro-optic materials

Abstract This paper describes a new method for direct measurement and evaluation of the inhomogeneous electrostatic vector field with translational symmetry in electro-optic materials exhibiting the Pockels effect. It is based on the evaluation of maximum transmittance of low intensity light passing through a sample under a voltage bias. Here, the sample is located between rotating crossed polarizers, and camera images are obtained at each point to determine the electric field. The evaluation procedure is demonstrated using data acquired on a CdZnTeSe quasi-hemispheric semiconductor gamma-ray detector. In addition to CdTe-related compounds, the method can be used for various other materials showing $$\overline{4}3m$$ 4 ¯ 3 m symmetry such as GaAs, CdTe, GaP, 3C-SiC, and ZnS. Furthermore, it can be generalized to other crystalline materials showing the Pockels effect. The method can be used to probe the space charge and the electric field in several kinds of electronic components and devices, as well as provide useful data on the role of defects, contact configurations and other surface and bulk inhomogeneities in the material that can affect the distribution of the internal electric field.

36 MATERIALS SCIENCE↗

Study of CdZnTeSe Gamma-Ray Detector under Various Bias Voltages

Cadmium zinc telluride selenide (CdZnTeSe) is a new semiconductor material for gamma-ray detection and spectroscopy applications at room temperature. It has very high crystal quality compared to similar materials such as cadmium telluride and cadmium zinc telluride. The consistency of peak position in radiation detection devices is important to practical applications. In this paper, we have characterized a CdZnTeSe planar detector for bias voltages in the range of -20 V to -200 V and amplifier shaping time of 2, 3 and 6 μs. The peak position of the 59.6-keV gamma line of 241 Am becomes more stable as the absolute value of the applied voltage increases. The best energy resolution of 8.5% was obtained for the 59.6-keV gamma peak at -160 V bias voltage and 3-μs shaping time. The energy resolution was relatively stable in the -120 V to -200 V range for a 6-μs shaping time. Future work will be focused on the study of the peak position and energy resolution over time.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

X-ray topographic study of Bridgman-grown CdZnTeSe

We have characterized the structural quality of Cd 0.9 Zn 0.1 Te 0.93 Se 0.07 ingot grown by the vertical Bridgman growth technique. The structural quality of Cd 0.9 Zn 0.1 Te 0.93 Se 0.07 ingot along the length was investigated via X-ray topography in the reflection mode using a white beam synchrotron radiation source. The X-ray topography data revealed the presence of very few sub grain boundaries and no sub-grain boundary network for the CdZnTeSe samples used in this study.

36 MATERIALS SCIENCE↗

Radiation detector

Technologies are described for semiconductor radiation detectors. The semiconductor radiation detectors may comprise a semiconductor material. The semiconductor material may include a first surface and a second surface. The first surface may be opposite from the second surface. The semiconductor material may include at least one metal component. The semiconductor material may be effective to absorb radiation and induce a current pulse in response thereto. The semiconductor radiation detector may comprise an electrode contact. The electrode contact may include a metal doped oxide deposited on the first surface of the semiconductor material. The metal doped oxide may include the metal component element of the semiconductor material.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Characterization of large-volume Frisch grid detector fabricated from as-grown CdZnTeSe

CdZnTe (CZT) has been under continuous development as a room-temperature radiation detector for the past 2-3 decades. Due to its intrinsic defects, such as a high concentration sub-grain boundary network, it has been very challenging to consistently produce high-quality CZT detectors with high yield, particularly for detector volumes exceeding a few cm 3 . In this paper, we report characterization of a relatively large-volume Frisch-grid detector (dimensions: 11x10.8x19.4 mm 3 ) fabricated from a new material Cd 0.9 Zn 0.1 Te 0.985 Se 0.015 . Furthermore, the detector was fabricated from an as-grown ingot with a two-inch diameter grown by the Traveling Heater Method (THM). The detector sample was evaluated by infrared (IR) transmission microscopy to study the presence of Te inclusions. X-ray topography using a synchrotron light source was deployed to measure the presence of sub-grain boundaries and their networks. Finally, the detector performance was measured for an optimized Frisch-grid length to extract the best energy resolution at room temperature.

36 MATERIALS SCIENCE↗