Frequency dependent deformation reversibility during cyclic loading
Not Available
Engineering topics
Publications and source records attributed to Li, Nan.
Not Available
We report that Si/Ge core/shell nanowire heterostructures have been expected to provide high energy and power densities for lithium ion battery anodes due to the large capacity of Si and the high electrical and ionic conductivities of Ge. Although the battery anode performances of Si/Ge core/shell nanowire heterostructures have been characterized, the degradation of Si/Ge core/shell nanowire heterostructures has not been thoroughly investigated. Here we report the compositional and structural changes of the Si/Ge core/shell nanowire heterostructure over cycling of lithiation and delithiation at different charging rates. The Si/Ge core/shell nanowire heterostructure holds the core and shell structure at a charging rate of 0.8 A g -1 up to 50 cycles. On the other hand, compositional intermixing and loss of Si occur at a charging rate of 20 A g -1 within 50 cycles. Lastly, the operation condition-dependent degradation provides a new aspect of materials research for the development of high performance lithium ion battery anodes with a long cycle life.
Here, we present a methodology for developing ultra-thin and strong formvar-based membranes with controlled morphologies. Formvar is a thin hydrophilic and oleophilic polymer inert to most chemicals and resistant to radiation. The formvar-based membranes are viable materials as support structures in micro- and macro-scale systems depending on thinness and porosity control. Tunable sub-micron thick porous membranes with 20%–65% porosity were synthesized by controlling the ratios of formvar, glycerol, and chloroform. This synthesis process does not require complex separation or handling methods and allows for the production of strong, thin, and porous formvar-based membranes. An expansive array of these membrane characterizations including chemical compatibility, mechanical responses, wettability, as well as the mathematical simulations as a function of porosity has been presented. The wide range of chemical compatibility allows for membrane applications in various environments, where other polymers would not be suitable. Our formvar-based membranes were found to have an elastic modulus of 7.8 GPa, a surface free energy of 50 mN m -1 and an average thickness of 125 nm. Stochastic model simulations indicate that formvar with the porosity of ~50% is the optimal membrane formulation, allowing the most material transfer across the membrane while also withstanding the highest simulated pressure loadings before tearing. Development of novel, resilient and versatile membranes with controlled porosity offers a wide range of exciting applications in the fields of nanoscience, microfluidics, and MEMS.
The microstructures and mechanical behavior of high-temperature co-sputtered Cu/Mo nanocomposites were investigated and compared with Cu/Mo multilayers. The co-sputtered nanocomposites present hierarchical architectures with bicontinuous intertwined Cu/Mo phases, the feature size of which can be tuned from 35 to 3 nm by changing the deposition parameters. After indentation, shear bands were found in the multilayers but not in the hierarchical nanocomposites. In situ nanocompression tests in Transmission electron microscopy showed that the hierarchical nanocomposite containing fine-length-scale intertwined Cu/Mo phases has very high strength. Finally, the hierarchical structure is proposed to play an important role in suppressing shear band formation.
Highlights: • Fam20c deficiency decreases the proliferation, mobility and mineralization of mouse immortalized dental mesenchymal cells. • Fam20c deficiency decreases the tooth mineralization, as well as the gene expression on dental mesenchymal differentiation. • Canonical and non-canonical BMP signaling pathways are declined in the mouse Fam20c-deficient dental mesenchyaml cell line. FAM20C mutations compromise the mineralization of skeleton and tooth in both human and mouse. Putatively, the mineralization disorder is attributed to the elevated fibroblast growth factor 23 (FGF23), which reduced the serum phosphorus by suppressing the reabsorption of phosphorus in kidney. Besides the regulation on systemic phosphorus homeostasis, FAM20C was also implicated to regulate cell behaviors and gene expression through a cell-autonomous manner. To identify the primary effects of Fam20c on dental mesenchymal cells, mouse Fam20c-deficient dental mesenchymal cells were generated by removing the floxed alleles from the immortalized mouse Fam20c{sup f/f} dental mesenchymal cells with Cre-expressing lentivirus. The removal of Fam20c exerted no impact on cell morphology, but suppressed the proliferation and mobility of the dental mesenchymal cells. Fam20c deficiency also significantly reduced the expression of Osterix, Runx2, type I Collagen a 1 (Col1a1), Alkaline phosphatase (Alpl) and the members of the small integrin-binding ligand, N-linked glycoprotein (SIBLING) family, but increased Fgf23 expression. Consistently, the in vitro mineralization of Fam20c-deficient dental mesenchymal cells was severely disabled. However, supplements of the non-collagenous proteins from wild type rat dentin failed to rescue the compromised mineralization, suggesting that the roles of FAM20C in tooth mineralization are more than phosphorylating local matrices and regulating systemic phosphorus metabolism. Moreover, the down-regulated BMP signaling pathways in the Fam20c deficient dental mesenchymal cells revealed that the kinase activity of FAM20C might be required to maintain BMP signaling. In summary, our study discloses that Fam20c indeed regulates cell behaviors and cell signaling pathway in a cell-autonomous manner.
Not Available
Material degradation due to precipitation of implanted helium (He) is a key concern in nuclear energy. Decades of research have mapped out the fate of He precipitates in metals, from nucleation and growth of equiaxed bubbles and voids to formation and bursting of surface blisters. By contrast, we show that He precipitates confined within nanoscale metal layers depart from their classical growth trajectories: They self-organize into elongated channels. These channels form via templated nucleation of He precipitates along layer surfaces followed by their growth and spontaneous coalescence into stable precipitate lines. The total line length and connectivity increases with the amount of implanted He, indicating that these channels ultimately interconnect into percolating “vascular” networks. In conclusion, vascularized metal composites promise a transformative solution to He-induced damage by enabling in operando outgassing of He and other impurities while maintaining material integrity.
In this study, recent experimental and modeling studies in nanolayered metal/ceramic composites are reviewed, with focus on the mechanical behaviors of metal/nitrides interfaces. The experimental and modeling studies of the slip systems in bulk TiN are reviewed first. Then, the experimental studies of interfaces, including co-deformation mechanism by micropillar compression tests, in situ TEM straining tests for the dynamic process of the co-deformation, thickness-dependent fracture behavior, and interrelationship among the interfacial bonding, microstructure, and mechanical response, are reviewed for the specific material systems of Al/TiN and Cu/TiN multilayers at nanoscale. The modeling studies reviewed cover first-principles density functional theory-based modeling, atomistic molecular dynamics simulations, and mesoscale modeling of nanolayered composites using discrete dislocation dynamics. The phase transformation between zinc-blende and wurtzite AlN phases in Al/AlN multilayers at nanoscale is also reviewed. Finally, a summary and perspective of possible research directions and challenges are given.
In recent years, high entropy alloys (HEAs), composed of four or more metallic elements mixed in equal or near equal atomic percent, have attracted significant attention due to their excellent mechanical properties and good corrosion resistance. They show significant promise as candidates for high temperature fission and fusion structural applications. However, the conventional synthesis methods are unlikely to present an industrially suitable route for the production and use of HEAs. Recognizing rapidly evolving additive manufacturing (AM) techniques, the goal of this proposal is to optimize the AM process to fabricate HEAs with predesigned chemical compositions and phase morphologies for nuclear components. For this project, two HEAs FeCrNiMn and FeCrNiMnAl have been successfully synthesized. Correlated mechanical response has been systematically characterized under a variety of laser processing and ion irradiations. Both high entropy alloys are found to present comparable swelling and extraordinary irradiation tolerance (limited voids and stabilized phase structure under high irradiation dose). In addition, the microstructure and radiation-induced hardening can be tailored by laser processing under additive manufacturing. And we have assembled at LANL a unique database of HEAs containing a total of 674 compositions with Phase Stability information. Based on this, the machine learning and Artificial Intelligence capability now are established to predict the microstructure of casted HEAs by given chemical compositions. This unique integration will lead to an optimal AM recipe for fabricating radiation tolerant HEAs. The development of both modeling models and experimental capability will also benefit other programs at LANL.
Mathematical models suggest that the strain along the film formed by parallel passes of a nanoindentation probe in contact with the film can be either homogenous or heterogeneous, depending on contact pressure and spacing between passes. Here, in this study, a 1 µm copper thin film was worn with a cono-spherical diamond probe with normal loads ranging from 25 to 800 µN and wear box edge lengths of 40, 60, and 80 µm. The nanoindenter counterface was rastered across the surface to mimic dry sliding wear. To determine potential strain field changes, 10-step quasi-static indents (200–2000 µN) were performed using nanoindentation inside the wear boxes created at various loads to determine if a strain field alteration could be observed in changes in hardness of the copper thin film. It was shown that there was a softening effect in the hardness for normal loads < 400 µN used during nanowear compared to the as-deposited copper. Normal loads ≥ 400 µN had a similar or higher hardness than the as-deposited copper. This is believed to have occurred due to a relaxation in the residual stresses created during deposition in the copper thin films at lower loads, which caused a decrease in hardness. Conversely, at the higher loads, increased deformation leads to an increase in hardness. Lastly, all of the wear boxes displayed a higher estimated strain hardening exponent than the as-deposited material.
Al/SiC nanolaminates with equal nominal thicknesses of the Al and SiC layers (10, 25, 50 and 100 nm) were manufactured by magnetron sputtering. The mechanical properties were measured at 25 °C and 100 °C by means of nanoindentation and micropillar compression tests and the deformation mechanisms were analyzed by in situ micropillar compression tests in the transmission electron microscope. In addition, finite element simulations of both tests were carried out to ascertain the role played by the strength of the Al layers and by the elastic constraint of the ceramic layers on the plastic flow of Al in the mechanical response. It was found that the mechanical response was mainly controlled by the constraint during nanoindentation or micropillar compression tests of very thin layered (≈10 nm) laminates, while the influence of the strength of Al layers was not as critical. This behavior was reversed, however, for thick layered laminates (100 nm). Here, these mechanisms point to the different effects of layer thickness during nanoindentation and micropillar compression, at both temperatures, and showed the critical role played by constraint on the mechanical response of nanolaminates made of materials with a very large difference in the elasto-plastic properties.
Iron-chromium-aluminum (FeCrAl) alloys are of interest to the nuclear materials community due to their resistance to high temperature steam oxidation under accident conditions. The present work investigates oxide formation at temperatures relevant to light water reactor cladding operation following extended aging to assess growth kinetics, chemical composition, and microstructure of oxide formation on a commercial FeCrAl alloy, Fe-21wt.%Cr-5wt.%Al-3wt.%Mo (Kanthal APMT). Aging treatments were performed for 100-1000 hours in stagnant air at 300, 400, 500, and 600 °C, respectively. Oxide growth behavior under the investigated conditions follows a logarithmic time dependence. When the oxidization temperature is 400 °C or below, the oxide is amorphous. At 500 °C, isolated crystalline regions start to appear during short period aging time and expand with extended exposures. Crystalline α-Al2O3 oxide film develops at 600 °C and the correlated logarithmic rate constant decreases significantly, indicating enhanced oxidation resistance of the formed oxide film. In addition, Mo segregation at grain boundaries has been observed when the aging temperature exceeds 500 °C. The results of this study can be viewed as an upper bounding result for potential oxide coarsening during reactor operation.
In this paper, we summarize recent work on helium (He) interaction with various heterophase boundaries under high temperature irradiation. We categorize the ion-affected material beneath the He-implanted surface into three regions of depth, based on the He/vacancy ratio. The differing defect structures in these three regions lead to the distinct temperature sensitivity of He-induced microstructure evolution. The effect of He bubbles or voids on material mechanical performance is explored. Finally, overall design guidelines for developing materials where He-induced damage can be mitigated in materials are discussed.
A few dark matter substructures have recently been detected in strong gravitational lenses through their perturbations of highly magnified images. We derive a characteristic scale for lensing perturbations and show that they are significantly larger than the perturber’s Einstein radius. We show that the perturber’s projected mass enclosed within this radius, scaled by the log-slope of the host galaxy’s density profile, can be robustly inferred even if the inferred density profile and tidal radius of the perturber are biased. We demonstrate the validity of our analytic derivation using several gravitational lens simulations where the tidal radii and the inner log-slopes of the density profile of the perturbing subhalo are allowed to vary. By modeling these simulated data, we find that our mass estimator, which we call the effective subhalo lensing mass, is accurate to within about 10% or smaller in each case, whereas the inferred total subhalo mass can potentially be biased by nearly an order of magnitude. We therefore recommend that the effective subhalo lensing mass be reported in future lensing reconstructions, as this will allow for a more accurate comparison with the results of dark matter simulations.
The In-doped SnTe nanowire surface is composed of In 2 O 3 , SnO 2 , Te and TeO 2 which can be readily removed by argon ion sputtering.
Galaxy-scale strong gravitational lensing can not only provide a valuable probe of the dark matter distribution of massive galaxies, but also provide valuable cosmological constraints, either by studying the population of strong lenses or by measuring time delays in lensed quasars. Due to the rarity of galaxy-scale strongly lensed systems, fast and reliable automated lens finding methods will be essential in the era of large surveys such as Large Synoptic Survey Telescope, Euclid and Wide-Field Infrared Survey Telescope. To tackle this challenge, we introduce CMU DeepLens, a new fully automated galaxy-galaxy lens finding method based on deep learning. This supervised machine learning approach does not require any tuning after the training step which only requires realistic image simulations of strongly lensed systems. We train and validate our model on a set of 20 000 LSST-like mock observations including a range of lensed systems of various sizes and signal-to-noise ratios (S/N). We find on our simulated data set that for a rejection rate of non-lenses of 99 per cent, a completeness of 90 per cent can be achieved for lenses with Einstein radii larger than 1.4 arcsec and S/N larger than 20 on individual g-band LSST exposures. Finally, we emphasize the importance of realistically complex simulations for training such machine learning methods by demonstrating that the performance of models of significantly different complexities cannot be distinguished on simpler simulations. We make our code publicly available at https://github.com/McWilliamsCenter/CMUDeepLens.