Engineering Papers⌕ Search

Engineering topics

Feit, M D

Publications and source records attributed to Feit, M D.

25 records · Page 2

Modeling Wet Chemical Etching of Surface Flaws on Fused Silica

Fluoride-based wet chemical etching of fused silica optical components is useful to open up surface fractures for diagnostic purposes, to create surface topology, and as a possible mitigation technique to remove damaged material. To optimize the usefulness of etching , it is important to understand how the morphology of etched features changes as a function of the amount of material removed. In this study, we present two geometric etch models that describe the surface topology evolution as a function of the amount etched. The first model, referred to as the finite-difference etch model, represents the surface as an array of points in space where at each time-step the points move normal to the local surface. The second model, referred to as the surface area-volume model, more globally describes the surface evolution relating the volume of material removed to the exposed surface area. These etch models predict growth and coalescence of surface fractures such as those observed on scratches and ground surfaces. For typical surface fractures, simulations show that the transverse growth of the cracks at long etch times scales with the square root of etch time or the net material removed in agreement with experiment. The finite-difference etch model has also been applied to more complex structures such as the etching of a CO{sub 2} laser-mitigated laser damage site. The results indicate that etching has little effect on the initial morphology of this site implying little change in downstream scatter and modulation characteristics upon exposure to subsequent high fluence laser light. In the second part of the study, the geometric etch model is expanded to include fluid dynamics and mass transport. This later model serves as a foundation for understanding related processes such as the possibility of redeposition of etch reaction products during the etching, rinsing or drying processes.

42 ENGINEERING↗

Material removal and surface figure during pad polishing of fused silica

The material removal and surface figure after ceria pad polishing of fused silica glass have been measured and analyzed as a function of kinematics, loading conditions, and polishing time. Also, the friction at the workpiece/lap interface, the slope of the workpiece relative to the lap plane, and lap viscoelastic properties have been measured and correlated to material removal. The results show that the relative velocity between the workpiece & lap (determined by the kinematics) and the pressure distribution determine the spatial and temporal material removal and hence the final surface figure of the workpiece. In the case where the applied loading and relative velocity distribution over the workpiece are spatially uniform, a significant non-uniform spatial material removal from the workpiece surface is observed. This is due to a non-uniform pressure distribution resulting from: (1) a moment caused by a pivot point and interface friction forces; (2) viscoelastic relaxation of the polyurethane lap; and (3) a physical workpiece/lap interface mismatch. Both the kinematics and these contributions to the pressure distribution are quantitatively described, and then combined to form a spatial and temporal Preston model & code for material removal (called Surface Figure or SurF{copyright}). The surface figure simulations are consistent with the experiment for a wide variety of polishing conditions. This study is an important step towards deterministic full-aperture polishing, which would allow optical glass fabrication to be performed in a more repeatable, less iterative, and hence more economical manner.

42 ENGINEERING↗

Using shaped pulses to probe energy deposition during laser-induced damage of SiO2 surfaces

Laser-induced damage initiation in silica has been shown to follow a power-law behavior with respect to pulse-length. Models based on thermal diffusion physics can successfully predict this scaling and the effect of pulse shape for pulses between about 3ns and 10ns. In this work we use sophisticated new measurement techniques and novel pulse shape experiments to test the limits of this scaling. We show that simple pulse length scaling fails for pulses below about 3ns. Furthermore, double pulse initiation experiments suggest that energy absorbed by the first pulse is lost on time scales much shorter than would be predicted for thermal diffusion. This time scale for energy loss can be strongly modulated by maintaining a small but non-zero intensity between the pulses. By producing damage with various pulse shapes and pulse trains it is demonstrated that the properties of any hypothetical thermal absorber become highly constrained.

42 ENGINEERING↗

Laser Damage Growth in Fused Silica with Simultaneous 351 nm and 1053 nm irradiation

Laser-induced growth of optical damage often determines the useful lifetime of an optic in a high power laser system. We have extended our previous work on growth of laser damage in fused silica with simultaneous 351 nm and 1053 nm laser irradiation by measuring the threshold for growth with various ratios of 351 nm and 1053 nm fluence. Previously we reported that when growth occurs, the growth rate is determined by the total fluence. We now find that the threshold for growth is dependent on both the magnitude of the 351 nm fluence as well as the ratio of the 351 nm fluence to the 1053 nm fluence. Furthermore, the data suggests that under certain conditions the 1053 nm fluence does not contribute to the growth.

42 ENGINEERING↗

Scratch Forensics

Scratches on optical components which are formed during fabrication, cleaning, handling and end-use, are widespread and almost always detrimental. The impact of scratches on the end-use of the optic includes increased optical scatter, reduced system performance, and reduced strength. In the case of optics used in high intensity laser applications, prevention of scratches is paramount because they are closely associated with laser damage. Evaluation of the characteristics (dimensions, location on optic, shape, and orientation) of a scratch can serve a powerful tool to identify the cause of the scratch and lead to mitigations to prevent their reoccurrence. It is likely that opticians have used such techniques for hundreds of years. In recent years, by applying techniques of fracture mechanics and tribology, several new semi-quantitative rules-of-thumb have been developed allowing one to estimate the size and shape of the scratch inducing asperity or rogue particle, the load on the particle, the depth of the fractures in the scratch, and properties of material housing the rogue particle. The following discussion reviews some these techniques, which as a whole, we refer to as 'Scratch Forsenics'.

42 ENGINEERING↗

The energy coupling efficiency of multiwavelength laser pulses to damage initiating defects in deuterated KH{sub 2}PO{sub 4} nonlinear crystals

The bulk damage performance of potassium dihydrogen phosphate crystals under simultaneous exposure to 1064, 532, and 355 nm nanosecond-laser pulses is investigated in order to probe the mechanisms governing damage initiation during frequency conversion. The results provide insight into the dependence on laser parameters of the defect-assisted excitation process responsible for coupling of the laser energy into the lattice under exposure to high power laser light. In addition, it is suggested that the damage performance can be directly related to and predicted from the damage behavior of the crystal at each wavelength separately.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

The Effect of HF/NH4F Etching on the Morphology of Surface Fractures on Fused Silica

The effects of HF/NH{sub 4}F, wet chemical etching on the morphology of individual surface fractures (indentations, scratches) and of an ensemble of surface fractures (ground surfaces) on fused silica glass has been characterized. For the individual surface fractures, a series of static or dynamic (sliding) Vickers and Brinnell indenters were used to create radial, lateral, Hertzian cone and trailing indentation fractures on a set of polished fused silica substrates which were subsequently etched. After short etch times, the visibility of both surface and subsurface cracks is significantly enhanced when observed by optical microscopy. This is attributed to the removal of the polishing-induced Bielby layer and the increased width of the cracks following etching allowing for greater optical scatter at the fracture interface. The removal of material during etching was found to be isotropic except in areas where the etchant has difficulty penetrating or in areas that exhibit significant plastic deformation/densification. Isolated fractures continue to etch, but will never be completely removed since the bottom and top of the crack both etch at the same rate. The etching behavior of ensembles of closely spaced cracks, such as those produced during grinding, has also been characterized. This was done using a second set of fused silica samples that were ground using either fixed or loose abrasives. The resulting samples were etched and both the etch rate and the morphology of the surfaces were monitored as a function of time. Etching results in the formation of a series of open cracks or cusps, each corresponding to the individual fractures originally on the surface of the substrate. During extended etching, the individual cusps coalesce with one another, providing a means of reducing the depth of subsurface damage and the peak-to-valley roughness. In addition, the material removal rate of the ground surfaces was found to scale with the surface area of the cracks as a function of etch time. The initial removal rate for the ground surface was typically 3.5 x the bulk etch rate. The evolving morphology of ground surfaces during etching was simulated using an isotropic finite difference model. This model illustrates the importance that the initial distributions of fracture sizes and spatial locations have on the evolution of roughness and the rate at which material is removed during the etching process. The etching of ground surfaces can be used during optical fabrication to convert subsurface damage into surface roughness thereby reducing the time required to produce polished surfaces that are free of subsurface damage.

42 ENGINEERING↗