Engineering Papers⌕ Search

Engineering topics

Colvin, Dylan

Publications and source records attributed to Colvin, Dylan.

Susceptibility to polarization type potential induced degradation in commercial bifacial p-PERC PV modules

Potential induced degradation (PID) is a reliability issue affecting photovoltaic (PV) modules, mainly when PV strings operate under high voltages in hot/humid conditions. Polarization-type PID (PID-p) has been known to decrease module performance quickly. PID-p can be reduced or recovered under the light in some cases, but this effect, as expected, would be less pronounced on the rear side of bifacial PV modules receiving lower irradiance. As bifacial PV modules are projected to dominate the PV market within the next 10 years, it is crucial to understand the PID-p issue in bifacial modules better. In this study, we performed indoor PID testing to induce PID-p on 14 commercial bifacial p-PERC modules with three different module constructions from three manufacturers. Here, four rounds (+ve and –ve polarities for front and rear sides) of PID testing are done at 25°C, 54% relative humidity (RH) for 168 h using the aluminum foil method. Each module side (front cell side and back cell side) is tested individually under both negative and positive voltage bias. The results show that the highest degradation of 32% in maximum power (Pmax) at standard test conditions (1000 W/m 2 ) and 51% at low irradiance (200 W/m 2 ) has been observed in some cases. Recovery under sunlight is also done, and outcomes show a near-complete recovery in Pmax. This study presents an extensive experimental methodology and a detailed analysis to systematically and simultaneously/sequentially evaluate multiple construction types of bifacial modules to the PID-p susceptibility and recovery.

14 SOLAR ENERGY↗

Review of Potential–Induced Degradation in Bifacial Photovoltaic Modules

Bifacial modules are increasingly deployed in the field and are expected to represent half of the market share within 10 years. Their rear structure differs from monofacial modules to allow additional light absorption. However, it brings new reliability challenges to address. In particular, the risk of potential-induced degradation (PID) is increased as both module sides are impacted. Different PID processes have been identified in the literature: shunting type (PID-s), polarization type (PID-p), Na penetration type, and corrosion type (PID-c). Their occurrence depends on the photovoltaic system configuration as well as the module's materials. Apart from PID-s, PID processes are not well understood and extensive research is needed to elucidate the PID scenario and underlying mechanisms. Herein, current knowledge about PID processes and their impact on the main bifacial modules in the market are gathered with the aim to guide future research. Bifacial module technologies and leakage current paths leading to PID are described. Indoor and outdoor PID testing methods are detailed. For each bifacial module technology, the PID processes are investigated with their indicators, mechanism and recovery process. Furthermore, PID-impacting factors and limitation solutions are finally reported and a state of the art on PID modeling is presented.

14 SOLAR ENERGY↗

Silicon Heterojunction Field Performance

The market share of silicon heterojunction (SHJ) modules are expected to increase in the following years. The presentation discusses field performance of SHJ and compares it to other high-efficiency modules. In-depth materials characterization is used to understand the origins of degradation in these type of modules.

ENGINEERING,SOLAR ENERGY↗

Spatially resolved characterization of optical and recombination losses for different industrial silicon solar cell architectures

In this work, spatially resolved characterization methods are used to identify loss mechanisms for common p -type silicon solar cell architectures, including multicrystalline aluminum back surface field (Al-BSF), monocrystalline Al-BSF, monocrystalline passivated emitter and rear cells (PERC), and bifacial monocrystalline PERC. The characterization methods used in this work include suns-V OC , photoluminescence imaging, and spatially resolved external quantum efficiency and reflectance measurements. The optical and recombination losses are driven by the material properties, cell processing conditions, and device architecture. These losses are quantified and categorized in terms of underlying mechanisms (e.g., front reflectance, escape reflectance, front recombination, and parasitic optical absorption and recombination in the bulk and rear). The ability to create images of these loss parameters can be used to gain more insight into the materials and manufacturing processes used to produce solar cells, and examples are given in this work to illustrate how these images can help reveal the origin of defects.

14 SOLAR ENERGY↗