Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “zirconia: partially stabilized”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Ball-on-ring test validation for equibiaxial flexural strength testing of engineered ceramics

The validation of a ball-on-ring, equibiaxial flexural strength method to obtain the transverse rupture strength (TRS) of right cylindrical ceramic specimens was performed in this study. Validation of the test method was achieved using commercially available engineered high purity alumina disks and finite element (FE) model analysis. The validated fixture was then used to obtain the TRS and Weibull statistical analysis of MgO-partially stabilized zirconia (MSZ) and Y 2 O 3 -partially stabilized zirconia (YSZ) ceramic disks. TRS data for alumina, MSZ, and YSZ agreed with the TRS values reported in the literature. A statistically relevant number of samples (N > 30) for each material were tested to allow for a Weibull statistical analysis. Weibull parameters for these materials were within the expected values for engineered ceramics. The characteristic strength for alumina, MSZ, and YSZ were determined to be 289, 786, and 814 MPa, respectively. The Weibull modulus was determined between 10 and 25 for each material, which is typical of engineered ceramics. In addition, FE model results were in close agreement with experimental fracture values for the three ceramic materials tested in this study.

36 MATERIALS SCIENCE↗

Impact damage of narrow silicon carbide (SiC) ceramics with and without environmental barrier coatings (EBCs) by various foreign object debris (FOD) simulants

The leading and trailing edges of turbine airfoils are highly susceptible to impact by foreign object debris (FOD) entrained in the gas stream of turbine engines. In this study, a narrow specimen geometry is implemented to study the FOD impact behavior of low curvature airfoil edges. Silicon carbide (SiC) ceramic specimens with and without an environmental barrier coating (EBC) are used as target materials. The EBC consists of an air plasma sprayed mullite topcoat (~ 166 µm) and silicon bond coat (~ 58 µm). Spherical (∅ 1.5 mm) FOD simulants of silicon nitride (Si3N4), partially stabilized zirconia (PSZ), and steel are used as impactors. Additionally, a modified gas gun is used to generate impact damage at normal incidence and velocities ranging between 300 to 400 m/s. In situ phase contrast X-ray radiographs, which render 2D representations of the internal transient damage, are captured during the impact experiments. Impactor hardness and toughness are found to primarily influence damage in the coating. Relative to wide specimens, the narrow specimens experience a greater level of cracking and this is postulated to result from reduced self-confinement. Irrespective of specimen geometry and impactor material type, limited cracking (i.e. enhanced shielding) is observed for the coated condition.

36 MATERIALS SCIENCE↗

In situ characterization of foreign object damage (FOD) in environmental-barrier-coated silicon carbide (SiC) ceramic

Environmental barrier coatings (EBCs) protect advanced ceramics and ceramic matrix composites (CMCs) from oxidation and corrosion in gas turbine engine environments. Foreign object damage (FOD), where debris impact the protective coatings, is a critical hazard which limits the turbine durability. Despite previous efforts to understand FOD in EBCs, a detailed understanding of the fundamental transient damage mechanisms is still lacking. In the current work, the real-time FOD behavior of a Mullite / Silicon EBC was visualized via a dynamic synchrotron X-ray source in phase contrast imaging (PCI) configuration. Prior to the in situ FOD experiments, the microstructure and composition of the coating were respectively characterized using a scanning electron microscope (SEM) and X-ray diffraction (XRD). The variation in the properties of the debris was modeled by ~ 1.5 mm diameter Partially Stabilized Zirconia (PSZ) and Silicon Nitride (Si 3 N 4 ) spheres. A modified light-gas gun setup, synchronized with the X-ray beam, was used to propel the projectiles at velocities ranging between 300 and 355 m·s -1 . Coated samples were impacted under a fully backed support configuration and at normal incidence. Coating penetration and delamination, as well as projectile deformation at the bond coat resulted for FOD by PSZ spheres. Comparatively, projectile fracture, with subsequent rebound of fragments, as well as complete coating penetration and delamination at the substrate interface occurred for FOD by Si 3 N 4 spheres. It should be noted that only cone cracking was observed for FOD by PSZ spheres while back surface cracking was present for both projectile types. Qualitative understanding of the driving forces for the observed damage mechanisms were provided.

36 MATERIALS SCIENCE↗

Development of High Temperature (>700°C) molten Salt Pump Technology for Gen3 Solar Power Tower Systems

Generation 3 Concentrating Solar Power (CSP) Systems require thermal energy storage that can efficiently receive solar heat and deliver it to a working fluid at temperatures greater than 700°C. For liquid systems, the thermal transfer fluid must be phase stable over large temperature ranges. High temperature molten salts meet this criteria, but are difficult liquids to handle. The high heat and salt content can be very corrosive to several different materials that are wetted by the liquid salt. For power tower collectors, the molten salt must be pumped under high pressure to the top of the collector tower. These pumps have impellers and shafts as part of their rotating elements, and under load, require bearings to control shaft movement while rotating. These high temperature pumps require submerged bearings, and thus bearing materials that can withstand the temperature and molten salt contact over long periods of time. This is essential for keeping pump maintenance costs low, and downtime to a minimum. Long running bearing materials is an enabling technology for integrated liquid systems in Generation 3 CSP Systems. Keeping costs low and systems reliable are critical for the broad adoption of Gen 3 CSP Systems. Hayward Tyler, Inc (HTI) proposed development of journal bearing materials for use in vertical pumps designed for pumping high temperature molten salt on both the hot and cold sides of the solar power tower. To complete this objective, HTI utilized the testing capabilities of Oak Ridge National Laboratory (ORNL) and High Temperature System Design (HTSD). Materials would first be selected for static corrosion testing, then downselected for tribological testing. Successful tribologically tested materials would then be downselected for use in additional test regimes. Ten samples were selected for static corrosion testing. Three passed the static testing regime. Two of these materials were downselected for ball material in tribological testing against three metallic alloys: Sintered Y2O3 Partially Stabilized Zirconia YTZP and Silicon Nitride, Grade 147-31N. HTI also proposed collecting data from a thorough bearing test regime using a test rig designed and built as part of this project, and also a conceptual design for a high temperature molten salt vertical pump. HTI withdrew from the project prior to completion of this work and this report reflects only the work completed prior to withdrawal. The completed work produced two papers, one manuscript submitted for publication, and one paper published in the journal Solar Energy Materials and Solar Cells. The papers are: “Tribological behavior of ceramic-alloy bearing contacts in molten salt lubrication for concentrating solar power” and “Material Selection and Corrosion Studies Of Candidate Bearing Materials For Use In Molten Chloride Salt."

14 SOLAR ENERGY↗

Examining Graphite Degradation in Molten Salt Environments: A Chemical, Physical, and Material Analysis

Molten-salt reactors (MSRs) are Generation IV nuclear reactors that use liquid salt as a coolant and/or fuel. In several MSR designs, graphite serves as a moderator and/or reflector. However, due to limited experimental data and operational experience, our understanding of graphite behavior in molten salt environments remains incomplete. This report aims to identify the degradation mechanisms of nuclear graphite in MSRs, detail the mechanisms of each factor, and provide an initial assessment of their impact on the structural integrity of graphite components. This assessment is based on an extensive literature review and insights from subject matter experts. Furthermore, given the limited data, a modeling strategy using existing Grizzly software is proposed for a more thorough analysis where appropriate. Additionally, it presents mitigation strategies where applicable. The report covers physical degradation mechanisms such as infiltration, erosion, and abrasion, as well as chemical degradation mechanisms including fluorination, intercalation, corrosion, and oxidation. Molten salt can infiltrate the porous structure of graphite, leading to several detrimental effects. Entrapment of fissile products within the graphite pores can cause radiation damage and could pose challenges in the handling and disposal of contaminated components. The differential thermal expansion between the infiltrated salt and graphite, along with internal stress from pressurized molten salt and volumetric heating, can compromise the structural integrity of graphite. To mitigate these effects, employing ultra-fine graphite grades and applying sealants and coatings are effective strategies. A computational model based on coupled solid mechanics and heat transfer phenomena could be used to predict the internal stresses using Grizzly software. In pebble-bed MSRs, graphite fuel pebbles can cause abrasion against reactor components due to friction and wear. The severity of wear is influenced by various factors such as temperature, environment, and the presence of lubricants. Tribological studies reveal that higher temperatures and molten salt environments, such as FLiBe, significantly reduce wear rates compared to dry conditions. Additionally, the chemical composition of the salt can further optimize graphite's tribological performance. Long-term wear effects can be modeled by incorporating surface defects into the geometry and predict stresses under thermal and radiation effects using Grizzly software. Chemical degradation of graphite in a molten salt environment can occur through fluorination and intercalation. Fluorination can occur via replacement of hydrogen or oxygen atoms, or at the active sites, but does not cause structural degradation. Intercalation, on the other hand, can lead to exfoliation, where layers of graphite separate and peel away, damaging the graphite. Protective coatings can enhance graphite's resistance to intercalation. Graphite generally exhibits good chemical stability in molten salt environments, though it can corrode under specific conditions, particularly in the presence of impurities or oxidants. Studies have shown that protective coatings, such as plasma-sprayed partially stabilized zirconia (PSZ), can effectively prevent such degradation. Corrosion behavior varies significantly with different graphite grades and coating applications, underscoring the need for detailed studies on uncoated and coated graphite to understand and mitigate corrosion mechanisms in MSRs. Research indicates that the presence of oxidants and impurities can accelerate graphite degradation in molten salts, making it essential to explore acceptable impurity limits. Oxidation is another critical degradation mechanism, leading to weight loss and structural damage due to the formation of CO and CO 2 from the reaction of carbon atoms with oxygen. This process creates new porosity and compromises graphite's integrity. While extensive research on graphite oxidation has been conducted for gas-cooled reactors, studies specific to MSRs are limited. Findings from the coal industry suggest that molten alkali metal salts can significantly accelerate graphite oxidation, a hypothesis worth exploring for fluoride salts in MSRs. Understanding oxidation behavior in MSRs is vital for developing protective measures. The analysis of post-irradiated graphite from the MSRE experiment demonstrated exceptional chemical compatibility with molten fluoride salt, suggesting that the extent of chemical attack on graphite largely depends on the salt's infiltration capability. Therefore, the use of ultra-fine grade graphite could help mitigate chemical degradation effects. Existing oxidation modeling capabilities in Grizzly, which use reaction-diffusion equations to model graphite-air interactions, could be adapted to simulate the chemical degradation effects of graphite in molten salt environments.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Development of High Temperature (>700°C) Molten Salt Pump Technology for Generation 3 Solar Power Tower Systems

Bearings are required for long-shafted pumps historically used in concentrating solar thermal power applications. For molten chloride salts, bearings for such service conditions are not commercially available, nor has a design been demonstrated to work. Therefore, a project was sponsored by the Department of Energy’s Solar Energy Technologies Office for the development and demonstration of a submerged bearing for use in chloride salt pumps. This project’s tasks covered the tribological testing of candidate materials and the design, fabrication, testing, and post-test analysis of full-scale salt-compatible bearings. This work expands upon previous work. The effects of potential particulate in the salt were investigated through tribological bench testing. Through 11 tests, the MgO particulate size and concentration in a molten chloride salt were varied, and the effects on friction, wear rate, and wear characteristics were recorded. Novel journal bearings for chloride salt service were designed and fabricated based on these results. The bearings were of a relevant scale (i.e., for a 1.5 in. pump shaft) to demonstrate the technology with respect to further scale-up. The bearings were made of Haynes 244 and Yttria Partially Stabilized Zirconia. A custom bearing test rig, salt tanks, and associated infrastructure (e.g., heaters, tanks, transfer lines, gas flow control) were designed, procured, and installed. A few issues were encountered in the system fabrication process, resulting in delay of the project schedule. The system was successfully fabricated and assembled. Heating, cover gas, and pump motor systems were integrated into the control logic. This progress of the bearing test system represents a significant step forward towards demonstrating this promising technology. Nevertheless, the project ended before testing of the full-scale bearings could be performed.

14 SOLAR ENERGY↗

Survey of the mechanical and physical behaviors of yttria-stabilized zirconia from multiple dental laboratories

Background: When selecting zirconia for a dental restoration, laboratory prescriptions often refer to high strength and high translucency. In this survey, zirconia specimens were ordered from various dental laboratories for posterior (high strength) and anterior (high translucency) clinical indications. The specimens were then tested and evaluated for their mechanical and physical behaviors. Methods: In a double-blinded manner, 9 laboratories provided 32 specimens from 17 different zirconia blanks, which were tested in the American Dental Association laboratory. Flexural strength tests were performed on standard specimens, and fracture surfaces were examined using both optical and scanning electron microscopy. Chemical composition, Vickers hardness, and absolute transmittance measurements were also performed. Results: A large scatter in the strength values was observed. The zirconia intended for posterior applications displayed strengths (SD) from 195 through 783 MPa (490 [183] MPa), which overlapped greatly with the strengths (SD) of the zirconia intended for anterior applications, 320 through 768 MPa (581 [136] MPa). However, when the strength values were recalculated on the basis of yttria content, the strengths (SD) were 584 (158) MPa for 3 mol% yttria and 373 (104) MPa for 5 mol% yttria. Conclusions: When a prescription was given to dental laboratories to request zirconia on the basis of clinical requirements, there was a large scatter and no consistency in the resulting strength values partly because of mixed use of 3 mol% and 5 mol% yttria zirconia. The 3 mol% materials had much higher strength when the strength values were grouped according to yttria content. Strength was also highly dependent on processing and finishing at the dental laboratories.

3 mol% yttria-tetragonal zirconia polycrystal (3Y-↗

3D Ferroelectric Phase Field Simulations of Polycrystalline Multi‐Phase Hafnia and Zirconia Based Ultra‐Thin Films

Abstract HfO 2 – and ZrO 2 –based ferroelectric thin films have emerged as promising candidates for the gate oxides of next‐generation electronic devices. Recent work has experimentally demonstrated that a tetragonal/orthorhombic (t/o‐) phase mixture with partially in‐plane polarization can lead to negative capacitance (NC) stabilization. However, there is a discrepancy between experiments and the theoretical understanding of domain formation and domain wall motion in these multi‐phase, polycrystalline materials. Furthermore, the effect of anisotropic domain wall coupling on NC has not been studied so far. Here, 3D phase field simulations of HfO 2 – and ZrO 2 –based mixed‐phase ultra‐thin films on silicon are applied to understand the necessary and beneficial conditions for NC stabilization. It is found that smaller ferroelectric grains and a larger angle of the polar axis with respect to the out‐of‐plane direction enhances the NC effect. Furthermore, it is shown that theoretically predicted negative domain wall coupling even along only one axis prevents NC stabilization. Therefore, it is concluded that topological domain walls play a critical role in experimentally observed NC phenomena in HfO 2 – and ZrO 2 –based ferroelectrics.

30 DIRECT ENERGY CONVERSION↗

Locally developed electronic conduction in a yttria stabilized zirconia (YSZ) electrolyte for durable solid oxide fuel cells

In the present work, anode supported solid oxide fuel cells (SOFCs) based on a YSZ single layer electrolyte with locally developed electronic conduction near the anode side is fabricated to improve the cell durability under negative voltage conditions. A ceria added Ni/YSZ anode functional layer is utilized and co-sintered with the YSZ electrolyte at 1460 °C. Cerium ions are diffused into a limited region of the YSZ layer (~6 μm), establishing a ceria doped YSZ region. We successfully demonstrate that this YSZ single layer cell can operate stably for ~100 h without anode/electrolyte interface delamination, even under a negative voltage. The embedded probe technique and theoretical calculation reveal that the internal oxygen partial pressure (near the anode) is substantially reduced (stabilized) by means of local electronic conduction of ceria doped YSZ. Thus, we propose an SOFC electrolyte design comprising a YSZ single layer with a ceria added anode functional layer (locally formed ceria doped YSZ in the electrolyte) as a protection method against fuel cell stack degradation caused by negative voltage operation.

25 ENERGY STORAGE↗

On the role of the zirconia/ceria interface in the degradation of solid oxide electrolysis cells

Gd-doped Ceria (GDC) barrier layers are widely used in solid oxide electrolysis cells to prevent reactions between the Y-stabilized Zirconia (YSZ) electrolyte and oxygen electrode. In some cases, electrolysis operation causes fracture near the GDC/YSZ interface. Here, we explain this effect using a numerical calculation, showing that a peak oxygen pressure is observed near the GDC/YSZ interface during electrolysis operation. Moreover, GDC/YSZ interdiffusion and possible zirconate phase formation occurring during electrode firing yield a low oxygen ion conductivity region that introduces a much higher peak oxygen partial pressure at the interdiffusion layer/YSZ interface, thereby exacerbating degradation. The results indicate that the peak pressure can be reduced and, thereby, damage can be mitigated by altering processing in order to minimize interdiffusion, decreasing the GDC layer thickness, and reducing oxygen electrode polarization resistance or altering electrolyte transport properties, e.g., changing the Gd doping level of GDC to increase the oxygen vacancy diffusivity.

Physics↗

Support Effect and Surface Reconstruction in In 2 O 3 / m- ZrO 2 Catalyzed CO 2 Hydrogenation

Here, we investigate the chemical and structural dynamics at the interface of In 2 O 3 /m-ZrO 2 and their consequences on the CO 2 hydrogenation reaction (CO 2 HR) under reaction conditions. While acting to enrich CO 2 , monoclinic zirconia (m-ZrO 2 ) was also found to serve as a chemical and structural modifier of In 2 O 3 that directly governs the outcome of the CO 2 HR. These modifying effects include the following: (1) Under reaction conditions (above 623 K), partially reduced In 2 O 3 , i.e., InO x (0 < x < 1.5), was found to migrate in and out of the subsurface of m-ZrO 2 in a semireversible manner, where m-ZrO 2 accommodates and stabilizes InO x by serving as a reservoir. The decreased concentration of surface InO x under elevated temperatures coincides with significantly decreased selectivity toward methanol and a sharp increase of the reverse water–gas shift reaction. The reconstruction-induced variation of InO x concentration appears to be one of the most important factors contributing to the altered catalytic performance of CO 2 HR at different reaction conditions. (2) The strong interactions and reactions between m-ZrO 2 and In 2 O 3 result in the activation of a pool of In–O bonds at the In 2 O 3 /m-ZrO 2 interface to form oxygen vacancies. On the other hand, the high dispersity of In 2 O 3 nanostructures onto m-ZrO 2 prevents their over-reduction under catalytically relevant conditions (up to 673 K), when bare In 2 O 3 is unavoidably reduced into the metallic phase (In 0 ). The relationship between the extent of reduction of In 2 O 3 and catalytic performance (CO 2 conversion, CH 3 OH selectivity, or yield of CH 3 OH) suggests the presence of an optimum coverage of surface InO x and oxygen vacancies under reaction conditions. The conventional model that links catalytic performance solely to the coverage of oxygen vacancies appears invalid in the present case. In situ analysis also allows the observation of surface reaction intermediates and their interconversions, including the reduction of CO 3 * into formate, a precursor for the formation of methanol and CO. The combinative ex situ and in situ study sheds light on the reaction mechanism of the CO 2 HR on In 2 O 3 /m-ZrO 2 -based catalysts. Our findings on the large-scale surface reconstructions, support effect, and the reaction mechanism of In 2 O 3 /m-ZrO 2 for CO 2 HR may apply to other related metal oxide catalyzed CO 2 reduction reactions.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Electronic and reactivity changes in epitaxially grown Ce 1-x Zr x O 2-δ (111) thin films

Ceria composite catalysts have long been used for ketonization reactions, which is a valuable chemistry for the upgrading of biomass-derived carboxylates. To better understand the interaction of zirconia with ceria in the context of ketonization, thin epitaxial films of ceria-zirconia mixed metal oxide Ce 1-x Zr x O 2-δ (x = 0-1) were grown on a Pt(111) substrate in ultrahigh vacuum conditions and studied with X-ray photoelectron spectroscopy (XPS). Core level and valence band XPS results suggest a strong interaction between ceria and zirconia cations, possibly due to increased filling of unoccupied 4f 0 orbitals of ceria from neighboring Zr cations in the lattice structure. This leads to a partial reduction of ceria from Ce 4+ to Ce 3+ , with Zr remaining predominantly in the 4+ oxidation state. Ketonization of acetic acid was studied using temperature programmed desorption (TPD) and high-resolution electron energy loss spectroscopy (HREELS). These results found ketonization over mixed Ce-Zr composite oxides exhibited lower activation energies than for pure CeO 2 and ZrO 2 , with Ce 0.38 Zr 0.62 O 2-δ exhibiting the highest yield of acetone among the studied surfaces. In conclusion, these results suggest the high activity of Ce-Zr catalysts appears to be a result of oxygen vacancy formation, stabilized by electron donation from Zr cations.

36 MATERIALS SCIENCE↗

Understanding Selectivity in CO2 Hydrogenation to Methanol for MoP Nanoparticle Catalysts Using In Situ Techniques

Molybdenum phosphide (MoP) catalyzes the hydrogenation of CO, CO2, and their mixtures to methanol, and it is investigated as a high-activity catalyst that overcomes deactivation issues (e.g., formate poisoning) faced by conventional transition metal catalysts. MoP as a new catalyst for hydrogenating CO2 to methanol is particularly appealing for the use of CO2 as chemical feedstock. Herein, we use a colloidal synthesis technique that connects the presence of MoP to the formation of methanol from CO2, regardless of the support being used. By conducting a systematic support study, we see that zirconia (ZrO2) has the striking ability to shift the selectivity towards methanol by increasing the rate of methanol conversion by two orders of magnitude compared to other supports, at a CO2 conversion of 1.4% and methanol selectivity of 55.4%. In situ X-ray Absorption Spectroscopy (XAS) and in situ X-ray Diffraction (XRD) indicate that under reaction conditions the catalyst is pure MoP in a partially crystalline phase. Results from Diffuse Reflectance Infrared Fourier Transform Spectroscopy coupled with Temperature Programmed Surface Reaction (DRIFTS-TPSR) point towards a highly reactive monodentate formate intermediate stabilized by the strong interaction of MoP and ZrO2. This study definitively shows that the presence of a MoP phase leads to methanol formation from CO2, regardless of support and that the formate intermediate on MoP governs methanol formation rate.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Ferro-ionic states and domains morphology in Hf x Zr 1–x O 2 nanoparticles

Unique polar properties of nanoscale hafnia-zirconia oxides (Hf x Zr 1–x O 2 ) are of great interest for condensed matter physics, nanophysics, and advanced applications. These properties are connected (at least partially) to the ionic–electronic and electrochemical phenomena at the surface, interfaces, and/or internal grain boundaries. Here, we calculated the phase diagrams, dielectric permittivity, spontaneous polar, and antipolar ordering, as well as the domain structure morphology in Hf x Zr 1–x O 2 nanoparticles covered by ionic–electronic charge originating from surface electrochemical adsorption. We revealed that the ferro-ionic coupling supports the polar long-range order in nanoscale Hf x Zr 1–x O 2 , induces, and/or enlarges the stability region of the labyrinthine domains toward smaller sizes and smaller environmental dielectric constant at low concentrations of the surface ions. The ferro-ionic coupling causes the transition to the single-domain ferro-ionic state at high concentrations of the surface ions. We predict that the labyrinthine domain states, being multiple-degenerated, may significantly affect the emergence of the negative differential capacitance state in the nanograined/nanocrystalline Hf x Zr 1–x O 2 films.

36 MATERIALS SCIENCE↗

Group 4 Metallocenes Supported on Sulfated Zirconium Oxide Catalyze Benzene C–H Borylation

C−H bond functionalization of arenes with boranes continues to be a challenge in catalysis, with late transition and rare earth metals shown to be catalytically active. In this study, group 4 metallocenes grafted onto acidic sulfated zirconia (SZO) are demonstrated to catalyze arene borylation with pinacolborane (HBpin). Catalysis studies at partial HBpin conversions (59−68%) using Cp 2 M(Me)/SZO (M = Ti, Zr, or Hf; Cp = cyclopentadienyl) catalysts reveal that Zr exhibits greater selectivity and activity than Ti and Hf. At 0.16 mol % of Zr, Cp 2 ZrMe/SZO achieves 332 turnovers at high HBpin conversion (86%), making this catalyst comparably active to previously reported Ir and Rh C−H borylation catalysts. At 160 °C, a maximum chemoselectivity of 82% for PhBpin was observed at 24% HBpin conversion. The superior activity of ionic Cp 2 ZrMe/SZO compared to neutral Cp 2 ZrMe/SiO 2 demonstrates the borylation mechanism relies on the highly electrophilic, coordinatively unsaturated cationic sites stabilized by the weakly coordinating sulfated support. Furthermore, both catalysts significantly outperform their molecular analogues, Cp 2 ZrMe 2 and [Cp 2 ZrMe][B(C 6 F 5 ) 4 ], suggesting that the support enhances catalytic performance by stabilizing the active species.

Aromatic compounds↗

Unlocking liquid chemisorption in solid matrices: immobilized deep eutectic solvent-ZIF-8 composites for next-generation CO 2 capture

Achieving net-zero emissions by 2050 requires scalable and durable CO 2 capture solutions, with direct air capture (DAC) gaining increasing prominence. Deep eutectic solvents (DESs) have emerged as promising candidates due to their strong chemisorptive properties, but their liquid-phase nature limits integration into solid systems. In this study, we introduce a solid–liquid hybrid approach by immobilizing [TEAB][TEPA] 2 , a highly CO 2 -reactive DES, onto various supports via non-covalent immobilization. This strategy induces solid-like behavior while retaining molecular-level reactivity of the DES. Among the supports including ZIF-8, zeolite Y, zirconia, and alumina, the [TEAB][TEPA] 2 @ZIF-8-56% composite demonstrated promising CO 2 uptake capacity of 2.00 mmol g −1 adsorbent at 1 bar, 1.48 at 0.15 bar, 0.96 at 0.01 bar, and 0.59 at 0.4 mbar. Particularly, we can observe that the chemisorption capacity under 400 ppm conditions is successfully introduced into ZIF-8, whereas pristine ZIF-8 showed negligible uptake under these same conditions. Breakthrough experiments confirmed robust capture behavior under humid conditions. The composite exhibited excellent cycling stability over 100 capture-release cycles, supported by thermogravimetric analysis. In situ DRIFTS verified that the chemisorptive nature of the DES remained intact after immobilization. Additional characterization studies, including FTIR, PXRD, N 2 physisorption, and XPS depth profiling, revealed partial DES infiltration and strong interfacial interactions. Comparative results using alumina-based composites underscored the importance of microporosity in stability. Finally, these findings suggest that DES-MOF composites hold promise as carbon capture materials, bridging liquid-phase functionality and solid-state robustness.

Yoo, Yunsung [Northwestern Univ., Evanston, IL (Un↗

Zr 6 O 8 Node-Catalyzed Butene Hydrogenation and Isomerization in the Metal–Organic Framework NU-1000

Zirconium-based metal–organic frameworks (Zr-MOFs) have been increasingly studied over the past two decades as heterogeneous catalysts due to their synthetic tunability, well-defined nature, and chemical stability. In contrast to traditional zirconia-based heterogeneous catalysts, the community has assumed that Zr-MOFs are inert catalyst supports that do not participate directly in hydrocarbon transformations, such as olefin hydrogenation and isomerization. Here, we report that the Zr-MOF NU-1000 is capable of catalyzing olefin hydrogenation and isomerization, without any postsynthetic modifications, under a hydrogen atmosphere. We probe H 2 activation over the nodes of NU-1000 via spectroscopic and computational techniques revealing that H 2 dissociation can occur heterolytically across coordinatively unsaturated Zr sites and proximal hydroxide and μ3-oxo ligands. These results, along with catalytic experiments, suggest that H 2 activation results in node-supported zirconium hydrides capable of the hydrogenation and isomerization of 1-butene. When examining rate dependence on the partial pressure of H 2 , we observe first-order dependence for hydrogenation and half-order dependence for isomerization. Half-order H 2 rate dependence is consistent with a mechanism where both fragments of cleaved H 2 are active for 1-butene isomerization, suggesting that heterolytic cleavage generates acidic protons resulting in parallel, acid-, and hydride-catalyzed isomerization pathways. In conclusion, this work shows that Zr-MOFs have more diverse reactivity than the current literature may suggest and opens possibilities for ways in which Zr-MOFs can be used as heterogeneous catalysts and supports.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

The Detection of Monoclinic Zirconia and Non-Uniform 3D Crystallographic Strain in a Re-Oxidized Ni-YSZ Solid Oxide Fuel Cell Anode

The solid oxide fuel cell (SOFC) anode is often composed of nickel (Ni) and yttria-stabilized zirconia (YSZ). The yttria is added in small quantities (e.g., 8 mol %) to maintain the crystallographic structure throughout the operating temperatures (e.g., room-temperature to >800 °C). The YSZ skeleton provides a constraining structural support that inhibits degradation mechanisms such as Ni agglomeration and thermal expansion miss-match between the anode and electrolyte layers. Within this structure, the Ni is deposited in the oxide form and then reduced during start-up; however, exposure to oxygen (e.g., during gasket failure) readily re-oxidizes the Ni back to NiO, impeding electrochemical performance and introducing complex structural stresses. In this work, we correlate lab-based X-ray computed tomography using zone plate focusing optics, with X-ray synchrotron diffraction computed tomography to explore the crystal structure of a partially re-oxidized Ni/NiO-YSZ electrode. These state-of-the-art techniques expose several novel findings: non-isotropic YSZ lattice distributions; the presence of monoclinic zirconia around the oxidation boundary; and metallic strain complications in the presence of variable yttria content. This work provides evidence that the reduction–oxidation processes may destabilize the YSZ structure, producing monoclinic zirconia and microscopic YSZ strain, which has implications upon the electrode’s mechanical integrity and thus lifetime of the SOFC.

25 ENERGY STORAGE↗