Determination of kinetic parameters of six ablation polymers by thermogravimetric analysis
Thermogravimetric analysis of ablating polymers to determine kinetic parameters describing mass loss due to thermal degradation
SEARCH · Engineering Papers
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Thermogravimetric analysis of ablating polymers to determine kinetic parameters describing mass loss due to thermal degradation
Thermogravimetric analysis (TGA) is widely employed in the thermal characterization of non-metallic materials, yielding valuable information on decomposition characteristics of a sample over a wide temperature range. However, a potential wealth of chemical information is lost during the process, with the evolving gases generated during thermal decomposition escaping through the exhaust line. Fourier Transform-Infrared spectroscopy (FT-IR) is a powerful analytical technique for determining many chemical constituents while in any material state, in this application, the gas phase. By linking these two techniques, evolving gases generated during the TGA process are directed into an appropriately equipped infrared spectrometer for chemical speciation. Consequently, both thermal decomposition and chemical characterization of a material may be obtained in a single sample run. In practice, a heated transfer line is employed to connect the two instruments while a purge gas stream directs the evolving gases into the FT-IR, The purge gas can be either high purity air or an inert gas such as nitrogen to allow oxidative and pyrolytic processes to be examined, respectively. The FT-IR data is collected real-time, allowing continuous monitoring of chemical compositional changes over the course of thermal decomposition. Using this coupled technique, an array of diverse materials has been examined, including composites, plastics, rubber, fiberglass epoxy resins, polycarbonates, silicones, lubricants and fluorocarbon materials. The benefit of combining these two methodologies is of particular importance in the aerospace community, where newly developing materials have little available data with which to refer. By providing both thermal and chemical data simultaneously, a more definitive and comprehensive characterization of the material is possible. Additionally, this procedure has been found to be a viable screening technique for certain materials, with the generated data useful in the selection of other appropriate analytical procedures for further material characterization.
Thermogravimetric analysis (TGA) is widely employed in the thermal characterization of non-metallic materials, yielding valuable information on decomposition characteristics of a sample over a wide temperature range. However, a potential wealth of chemical information is lost during the process, with the evolving gases generated during thermal decomposition escaping through the exhaust line. Fourier Transform-Infrared spectroscopy (FT-IR) is a powerful analytical technique for determining many chemical constituents while in any material state, in this application, the gas phase. By linking these two techniques, evolving gases generated during the TGA process are directed into an appropriately equipped infrared spectrometer for chemical speciation. Consequently, both thermal decomposition and chemical characterization of a material may be obtained in a single sample run. In practice, a heated transfer line is employed to connect the two instruments while a purge gas stream directs the evolving gases into the FT-IR. The purge gas can be either high purity air or an inert gas such as nitrogen to allow oxidative and pyrolytic processes to be examined, respectively. The FT-IR data is collected realtime, allowing continuous monitoring of chemical compositional changes over the course of thermal decomposition. Using this coupled technique, an array of diverse materials has been examined, including composites, plastics, rubber, fiberglass epoxy resins, polycarbonates, silicones, lubricants and fluorocarbon materials. The benefit of combining these two methodologies is of particular importance in the aerospace community, where newly developing materials have little available data with which to refer. By providing both thermal and chemical data simultaneously, a more definitive and comprehensive characterization of the material is possible. Additionally, this procedure has been found to be a viable screening technique for certain materials, with the generated data useful in the selection of other appropriate analytical procedures for further material characterization.
Polymeric materials thermal degradation kinetic parameters using combined mass spectrometric and thermogravimetric analysis /MS-TGA/
Differential scanning calorimetry and thermogravimetric analysis combination for thermochemical kinetic measurements, matching analytical and experimental curves for data accuracy
An improved protocol for thermogravimetric analysis (TGA) of samples of single-wall carbon nanotube (SWCNT) material has been developed to increase the degree of consistency among results so that meaningful comparisons can be made among different samples. This improved TGA protocol is suitable for incorporation into the protocol for characterization of carbon nanotube material. In most cases, TGA of carbon nanotube materials is performed in gas mixtures that contain oxygen at various concentrations. The improved protocol is summarized.
Thermogravimetric analysis of silicon carbide-silicon nitride fibers was carried out at ambient to 1000 C in air. The weight loss over this temperature range was negligible. In addition, the oxidative stability at high temperature for a short period of time was determined. Fibers heated at 1000 C in air for fifteen minutes showed negligible weight loss (i.e., less than 1 percent).
Thermogravimetric analysis data are presented on the unmeltable polycarbosilazane precursor of silicon carbide-silicon nitride fibers, over the room temperature-1000 C range in a nitrogen atmosphere, in order to establish the weight loss at various temperatures during the precursor's pyrolysis to the fiber material. The fibers obtained by this method are excellent candidates for use in applications where the oxidation of carbon fibers (above 400 C) renders them unsuitable.
The resin content, and by extension the fiber volume, of carbon fiber/cyanate ester composite laminates are measured using thermogravimetric analysis (TGA). Conventional measurement involves acid digestion of the laminate to determine resin content. The mean difference between techniques is 0.03%. In addition to eliminating the hazards and environmental impact of standard acid digestion, the TGA technique allows quantification of errors associated with fiber volume measurements, e.g. incomplete resin removal or fiber degradation. An additional benefit of the TGA technique is a reduction in sample size requirements, allowing the examination of fiber volume changes in complex shapes.
Thermal degradation of polymeric materials analyzed by combined mass spectrometric and thermogravimetric technique
High performance polymeric materials are finding increased use in aerospace applications. Proposed high speed aircraft will require materials to withstand high temperatures in an oxidative atmosphere for long periods of time. It is essential that accurate estimates be made of the performance of these materials at the given conditions of temperature and time. Temperatures of 350 F (177 C) and times of 60,000 to 100,000 hours are anticipated. In order to survey a large number of high performance polymeric materials on a reasonable time scale, some form of accelerated testing must be performed. A knowledge of the rate of a process can be used to predict the lifetime of that process. Thermogravimetric analysis (TGA) has frequently been used to determine kinetic information for degradation reactions in polymeric materials. Flynn and Wall studied a number of methods for using TGA experiments to determine kinetic information in polymer reactions. Kinetic parameters, such as the apparent activation energy and the frequency factor, can be determined in such experiments. Recently, researchers at the McDonnell Douglas Research Laboratory suggested that a graph of the logarithm of the frequency factor against the apparent activation energy can be used to predict long-term thermo-oxidative stability for polymeric materials. Such a graph has been called a kinetic map. In this study, thermogravimetric analyses were performed in air to study the thermo-oxidative degradation of several high performance polymers and to plot their kinetic parameters on a kinetic map.
Conjugated polyenes, and polyesters containing phthalocyanine in their backbone, were synthesized. These polymers were characterized by chemical analysis, thermogravimetric analysis, spectral analysis, and X-ray diffraction studies for crystallinity, as well as for their film-forming capability and gas/polymer interactions. Most of the polymers were relatively insensitive to water vapor up to 50 percent relative humidity, but the polyester/phthalocyanine (iron) polymer was relatively insensitive up to 100 percent RH. On the other hand, poly(p-dimethylaminophenylacetylene) was too conductive at 100 percent RH. Of the gases tested, the only ones that gave any evidence of interacting with the polymers were SO2, NOx, HCN and NH3. Poly(imidazole)/thiophene responded to each of these gases at all relative humidities, while the other polymers gave varying response, depending upon the RH. Thus, since most of these gases were electron-accepting, the electron-donating character of poly(imidazole)/thiophene substantiates the concept of electronegativity being the operating principle for interaction effects. Of the six polymers prepared, poly(imidazole)/thiophene first showed a very good response to smoldering cotton, but it later became nonresponsive; presumably due to oxidation effects.
Coal in its plastic state (typically 400-460 C) was examined by the isothermal Gieseler plastometry of seven selected coals of widely varying plastic properties. Kinetic models were proposed for the isothermal plastometric curves. Plastic behavior was compared with a variety of laboratory analyses and characterizations of these coals, including classical coal analysis; mineral analysis; microstructural analysis (extractable fractions, surface area measurement, and petrographic analysis); and thermal analysis (thermogravimetric analysis, thermomechanical analysis, and differential scanning calorimetry). The phenomenon of a sharp, large, poorly reproducible exotherm in the differential scanning calorimetric analysis of coking coals was examined. Several coal extrudates show mineral distribution, organic maceral composition and overall calorific value to be little affected by 800 F extrusion. Volatile matter and plastic properties are moderately reduced, and the network structure (as gauged by extractables) appears to be slightly degraded in the extrusion process.
Tantalum oxide gels in the form of transparent monoliths and powder were prepared from hydrolysis of tantalum pentaethoxide under controlled conditions using different mole ratios of Ta(OC2H5)5:C2H50H:H20:HCl. Alcohol acts as the mutual solvent and HCl as the deflocculating agent. For a fixed alkoxide:water:HCl ratio, time of gel formation increased with the alcohol to alkoxide mole ratio. Thermal evolution of the physical and structural changes in the gel was monitored by differential thermal analysis, thermogravimetric analysis, x-ray diffraction, and infrared spectroscopy. On heating to approximately 400 C, the amorphous gel crystallized into the low temperature orthorhombic phase Beta-Ta2O5, which transformed into the high temperature tetragonal phase Alpha-Ta2O5 when further heated to approximately 1450 C. The volume fraction of the crystalline phase increased with the firing temperature. The Alpha-Ta205 converted back into the low temperature phase, Beta-Ta2O5, on slow cooling through the transformation temperature of 1360 C indicating a slow but reversible transformation.
Niobium pentoxide gels in the form of transparent monoliths and powder have been synthesized from the controlled hydrolysis and polycondensation of niobium pentaethoxide under different experimental conditions using various mole ratios of Nb(OC2H5)5:H2O:C2H5OH:HCl. Alcohol acted as the mutual solvent and HCl as the deflocculating agent. In the absence of HCl, precipitation of colloidal particles was encountered on the addition of any water to the alkoxide. The gels were subjected to various thermal treatments and characterized by differential thermal analysis, thermogravimetric analysis, x-ray diffraction, and infrared spectroscopy. After drying at 400 C, the gels were amorphous to x-rays. The amorphous powder crystallized into the low-temperature orthorhombic form of Nb2O5 at approximately 500 C, which transformed irreversibly into the high-temperature monoclinic alpha-Nb2O5 between 900 to 1000 C. The kinetics of crystallization of the amorphous niobium pentoxide have been investigated by non-isothermal differential scanning calorimetry. The crystallization activation energy was determined to be 399 kJ/mol.
Due to the difficulty in processing polyimides with high temperature stability and good solvent resistance, we have synthesized high performance polyimides with bicyclo(2.2.2)-oct-7-ene ring system which can easily be fabricated into films and fibers and subsequently converted to the more stable aromatic polyimides. In order to improve processability, we prepared two polyimides by reacting 1,4-phenylenediamine and 1,3phenylediamine with bicyclo(2.2.2)-7-octene-2,3,5,6-tetracarboxylic dianhydride. The polyimides were characterized by FTIR, FTNMR, solubility and thermal analysis. Thermogravimetric analysis (TGA) showed that the 1,4-phenylenediamine and 1,3-phenylenediamine containing polyimides were stable up to 460 and 379 C, respectively under nitrogen atmosphere. No melting transitions were observed for both polyimides. The 1,4-phenylenediamine containing polyimide is partially soluble in dimethyl sulfoxide, methane sulfonic acid and soluble in sulfuric acid at room temperature. The 1,3-phenylenediamine containing polyimide is partially soluble in dimethyl sulfoxide, tetramethyl urea, N,N-dimethyl acetamide and soluble in methane sulfonic acid and sulfuric acid.
Silane-endcapped polyimide high temperature adhesive formulations were prepared by reacting anhydride-terminated poly(amic acid), obtained from benzophenonetetracarboxylic dianhydride and a diamine (3,3'-, 3,4'- or 4,4'-diaminodiphenylmethane and 3,3', 3,4'- or 4,4'-diaminobenzophenone) with varying amounts of gama-aminopropyltriethoxysilane in dimethylacetamide. Resin properties were evaluated by torsional braid analysis and thermogravimetric analysis. Lap shear strengths of some of the adhesive bonds were determined at room temperature and at 177 C before and after ageing at 200 C for 2500 h and after boiling in water for 72 h.
A high-temperature linear amorphous hydrocarbon polymer synthesized cationically from 2,5-norbornadiene was studied thermomechanically with respect to physical transitions and stability in nitrogen. The glass transition temperature was determined to be 320 C (at less than 1 cps), which is probably the highest known for a linear hydrocarbon addition polymer. The thermomechanical technique of torsional braid analysis, together with thermogravimetric analysis, differential thermal analysis, infrared analysis, and solubility studies, was used to investigate the sequential events of the glass transition and degradation. The polymer is of particular interest since it is a high-temperature plastic which in the bulk form would probably need to be processed at high speeds in the vicinity of the glass transition temperature in an inert atmosphere. The presence of tertiary hydrogen atoms should render it amenable to degradation by the earth's environment.