Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “steam oxidation”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

High Pressure Steam Oxidation of Alloys for Advanced Ultra-Supercritical Conditions

A steam oxidation test was conducted at 267 ± 17 bar and 670°C for 293 hr. A comparison test was run at 1 bar. All of the alloys showed an increase in scale thickness and oxidation rate with pressure, and TP304H and IN625 had very large increases. Fine-grained TP304H at 267 bar behaved like a coarse grained alloy, indicative of high pressure increasing the critical Cr level needed to form and maintain a chromia scale. At 267 bar H230, H263, H282, IN617 and IN740 had kp values a factor of one–to-two orders of magnitude higher than at 1 bar. IN625 had a four order of magnitude increase in kp at 267 bar compared to 1 bar. Possible causes for increased oxidation rates with increased pressure were examined, including increased solid state diffusion within the oxide scale and increased critical Cr content to establish and maintain a chromia scale.

Steam, Oxidation, Superalloy, Pressure, Advanced U↗

Steam Oxidation of Advanced Steam Turbine Alloys

Power generation from coal using ultra supercritical steam results in improved fuel efficiency and decreased greenhouse gas emissions. Results of ongoing research into the oxidation of candidate nickel-base alloys for ultra supercritical steam turbines are presented. Exposure conditions range from moist air at atmospheric pressure (650°C to 800°C) to steam at 34.5 MPa (650°C to 760°C). Parabolic scale growth coupled with internal oxidation and reactive evaporation of chromia are the primary corrosion mechanisms.

20 FOSSIL-FUELED POWER PLANTS↗

Production of hydrogen by steam oxidation of calcium ferrite reduced with various coals

Production of H 2 by steam oxidation was demonstrated with calcium ferrite (CaFe 2 O 4 ) after coal gasification to produce CO with several types of coals. All coal types reacted with CaFe 2 O 4 to produce CO. The reduced CaFe 2 O 4 after the reaction with coal can also be oxidized with steam at 800 °C while producing of H 2 . Sub-bituminous coal and lignite coal had better reactivity with CaFe 2 O 4 than the bituminous coal. A ten-cycle test conducted with Wyodak coal/CaFe 2 O 4 at 800 °C showed stable production of H 2 during oxidation with steam. A 25-cycle steam oxidation test conducted after reduction of CaFe2O4 with lignite coal also showed a very stable performance. Steam oxidation is sufficient for maintaining the cyclic reactions. A larger scale (2 kg batch) production of CaFe 2 O 4 by wet granulation-tumbling method was successful. In conclusion, steam oxidation was demonstrated with the large-scale batch of CaFe 2 O 4 after reduction with Wyodak coal.

08 HYDROGEN↗

Task 1—Steam Oxidation (NETL-US)

The proposed steam in let temperature in the Advanced Ultra Supercritical (A·USC) steam turbine is high enough (760°C) Ihat traditional turbine casing and valve body materials such as ferr;tic/manensitic steels will not suffice due to temperature lim itations of this class of materials. Cast versions of three traditionally wrought Ni-based superalloys (Haynes 263. Haynes 282, and Nimonic 105) were evaluated for use as casing or valve components for the next generation of industrial steam turbines. The full size castings are substantia l: 2-5,000 kg each half and on the order of 100 nun thick. Experimental castings were quite a bit smaller, but section size was retained and cooling rate controlled to produce equi valem microslruclUre •. A multi_step homogenization heat treatment was d~ve loped to better disperse the al loy constituents. These castings were subsequently evaluated by characterizing their microstructure as well as their steam oxidation resistance (al 760 and 800 "C).

36 MATERIALS SCIENCE↗

Study of the scale formed on super 304H boiler tube steels after long-term steam oxidation at high temperatures

Highlights: • Steam oxidation tests were performed on the conventional and shot-peened Super304H boiler tube. • A continuous amorphous SiO{sub 2} layer separated the metal from the scale in shot-peened specimen. • The SiO{sub 2} layer enhanced the formation of dense Cr{sub 2}O{sub 3} and FeCr{sub 2}O{sub 4} layers. • The scale on shot-peened specimens is stable upon steam temperature and time increase. Steam oxidation of a Super 304H boiler tube was performed at steam temperatures of 650 °C and 700 °C for time durations up to 5000 h. The oxidation scale outcomes which formed on as-received untreated and shot-peened (SP) tubes were studied using X-ray diffraction (XRD), scanning electron microscopy (SEM), electron backscatter diffraction (EBSD), and transmission electron microscopy (TEM). γ-Grain nanocrystallization on the surface of the SP specimen generated an abundant fraction of grain boundary that guaranteed the formation of a continuous amorphous SiO{sub 2} layer at the metal-scale interface that enhanced the formation of dense Cr{sub 2}O{sub 3} and FeCr{sub 2}O{sub 4} in the scale. Scale breakaway along defects in the outer layer of the scale was accelerated by the steam temperature in the untreated specimens, whereas the scale that formed on the SP specimens appeared to be stable.

36 MATERIALS SCIENCE↗

High Temperature Steam Oxidation Testing of Candidate Accident Tolerant Fuel Cladding Materials

The Fuel Cycle Research and Development (FCRD) program’s Advanced Fuels Campaign has initiated a multifold effort aimed at facilitating development of accident tolerant fuels in order to overcome the inherent shortcomings of light water reactor (LWR) fuels when exposed to beyond design basis accident conditions. The campaign has invested in development of experimental infrastructure within the Department of Energy complex capable of chronicling the performance of a wide range of concepts under prototypic accident conditions. This report summarizes progress made at Oak Ridge National Laboratory (ORNL) and Los Alamos National Laboratory (LANL) in FY13 toward these goals. Alternative fuel cladding materials to Zircaloy for accident tolerance and a significantly extended safety margin requires oxidation resistance to steam or steam-H 2 environments at ≥1200°C for short times. At ORNL, prior work focused attention on SiC, FeCr and FeCrAl as the most promising candidates for further development. Also, it was observed that elevated pressure and H2 additions had minor effects on alloy steam oxidation resistance, thus, 1 bar steam was adequate for screening potential candidates. Commercial Fe-20Cr-5Al alloys remain protective up to 1475°C in steam and CVD SiC up to 1700°C in steam. Alloy development has focused on Fe-Cr-Mn-Si-Y and Fe-Cr-Al-Y alloys with the aluminaforming alloys showing more promise. At 1200°C, ferritic binary Fe-Cr alloys required ≥25% Cr to be protective for this application. With minor alloy additions to Fe-Cr, more than 20%Cr was still required, which makes the alloy susceptible to α’ embrittlement. Based on current results, a Fe-15Cr-5Al-Y composition was selected for initial tube fabrication and welding for irradiation experiments in FY14. Evaluations of chemical vapor deposited (CVD) SiC were conducted up to 1700°C in steam. The reaction of H 2 O with the alumina reaction tube at 1700°C resulted in Al(OH) 3 formation, which reacted with the specimen to form a liquid reaction product. This behavior was not observed at lower temperatures where gas velocity and H 2 O content showed typical effects on the reaction rate. For LANL, the capabilities for oxidation testing as well as exploration of a methodology for measurement of hydrogen production of samples during oxidation under water vapor atmospheres is discussed. Results obtained for available commercial alloys are summarized, and data highlighting the performance of molybdenum, a recently proposed cladding material, are presented. Finally, leveraging of these techniques in conjunction with current and companion FCRD programs is discussed with respect to work in FY14.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Steam Oxidation of Fossil Power Plant Materials. Collaborative Research to Enable Advanced Steam Power Cycles

Research into improved materials systems and associated manufacturing and reliability issues is a major part of initiatives to produce cleaner and cheaper energy systems in the UK and the USA. Under the auspices of a Memorandum of Understanding on Energy R&D, a work programme concerned with steam oxidation has been conducted. The focus was on the generation of definitive information regarding the oxidation behaviour in steam of current and developmental ferritic steels, austenitic steels, and nickel-based alloys required to enable advanced steam power cycles. The results were intended to provide a basis for quantifying the rate of metal loss expected under advanced steam cycle conditions, as well as understanding of the evolution of oxide scale morphologies with time and temperature to identify features that could influence scale exfoliation characteristics. This understanding and acquired data were used to develop and validate models of oxide growth and loss by exfoliation. This paper provides an overview of the activity and highlights a selection of the results coming from the programme.

20 FOSSIL-FUELED POWER PLANTS↗

Hydrogen measurement during steam oxidation using coupled thermogravimetric analysis and quadrupole mass spectrometry

An analytical technique is presented with the goal of measuring reaction kinetics during steam oxidation reactions for three cases in which obtaining kinetics information often requires a prohibitive amount of time and cost. The technique presented relies on coupling thermogravimetric analysis (TGA) with a quantitative hydrogen measurement technique using quadrupole mass spectrometry (QMS). The first case considered is in differentiating between the kinetics of steam oxidation reactions and those for simultaneously reacting gaseous impurities such as nitrogen or oxygen. The second case allows one to independently measure the kinetics of oxide and hydride formation for systems in which both of these reactions are known to take place during steam oxidation. The third case deals with measuring the kinetics of formation for competing volatile and non-volatile oxides during certain steam oxidation reactions. In order to meet the requirements of the coupled technique, a methodology is presented which attempts to provide quantitative measurement of hydrogen generation using QMS in the presence of an interfering fragmentation species, namely water vapor. This is achieved such that all calibrations and corrections are performed during the TGA baseline and steam oxidation programs, making system operation virtually identical to standard TGA. Benchmarking results showed a relative error in hydrogen measurement of 5.7–8.4% following the application of a correction factor. Lastly, suggestions are made for possible improvements to the presented technique so that it may be better applied to the three cases presented.

36 MATERIALS SCIENCE↗

Nondestructive hydrogen analysis of steam-oxidized Zircaloy-4 by wide-angle neutron scattering

In this study, a nondestructive neutron scattering method to precisely measure the hydrogen content in high-temperature steam-oxidized Zircaloy-4 cladding was developed. Zircaloy-4 cladding was used to produce hydrided specimens with hydrogen content up to ≈500 wppm. Following hydrogen charging, the hydrogen content of the hydrided specimens was measured using the vacuum hot extraction method, by which the samples with desired hydrogen concentrations were selected for the neutron study. The hydrided samples were then oxidized in steam up to ≈6.0wt. % at 1100°C. Optical microscopy shows that our hydriding procedure results in uniform distribution of circumferential hydrides across the wall thickness, and uniform oxide layers were formed on the sample surfaces by the steam oxidation. Small- and wide-angle neutron scattering were simultaneously performed to provide a quick (less than an hour per sample) measurement of the hydrogen content in various types of hydrided and oxidized Zircaloy-4. Our study demonstrates that the hydrogen in pre-oxidized Zircaloy-4 cladding can be measured very accurately by both small- and wide-angle neutron scattering. For steam-oxidized samples, the small-angle neutron scattering is contaminated with coherent scattering from additional structural features induced by the steam oxidation. However, the scattering intensity of the wide-angle neutron scattering increases proportionally with the hydrogen charged in the samples. The hydrogen content and wide-angle neutron scattering intensity are highly linearly correlated for the oxidized cladding samples examined in this work, and can be used to precisely determine the hydrogen content in steam-oxidized Zircaloy-4 samples. Hydrogen contents determined by neutron scattering of oxidation samples were also found to be consistent with the results of chemical analysis within acceptable margins for error.

36 MATERIALS SCIENCE↗

Steam Oxidation Testing in the Severe Accident Test Station

After the March 2011 accident at Fukushima Daiichi, Oak Ridge National Laboratory (ORNL) began conducting high temperature steam oxidation testing of candidate materials for accident tolerant fuel (ATF) cladding in August 2011 [1-11]. The ATF concept is to enhance safety margins in light water reactors (LWR) during severe accident scenarios by identifying materials with 100× slower steam oxidation rates compared to current Zr-based alloys. In 2012, the ORNL laboratory equipment was expanded and made available to the entire ATF community as the Severe Accident Test Station (SATS) [4,12]. Compared to the current UO2/Zr-based alloy fuel system, an ATF alternative would significantly reduce the rate of heat and hydrogen generation in the core during a coolant-limited severe accident [13-14]. The steam oxidation behavior of candidate materials is a key metric in the evaluation of ATF concepts and also an important input into models [15-17]. However, initial modeling work of FeCrAl cladding has used incomplete information on the physical properties of FeCrAl. Also, the steam oxidation data being collected at 1200°-1700°C is unique as no prior work has considered steam oxidation of alloys at such high temperatures. Also, because many accident scenarios include steadily increasing temperatures, the required data are not traditional isothermal exposures but exposures with varying “ramp” rates. In some cases, the steam oxidation behavior has been surprising and difficult to interpret. Thus, more fundamental information continues to be collected. In addition, more work continues to focus on commercially-manufactured tube material. This report summarizes recent work to characterize the behavior of candidate alloys exposed to high temperature steam, evaluate steam oxidation behavior in various ramp scenarios and continue to collect integral data on FeCrAl compared to conventional Zr-based cladding.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Steam Oxidation Testing in the Severe Accident Test Station

Since 2011, Oak Ridge National Laboratory (ORNL) has been conducting high temperature steam oxidation testing of candidate alloys for accident tolerant fuel (ATF) cladding. These concepts are designed to enhance safety margins in light water reactors (LWR) during severe accident scenarios. In the US ATF community, the Severe Accident Test Station (SATS) has been evaluating candidate materials (including coatings) since 2012. Compared to the current UO 2 /Zr-based alloy fuel system, alternative cladding materials need to offer slower oxidation kinetics and a smaller enthalpy of oxidation in order to significantly reduce the rate of heat and hydrogen generation in the core during a coolant-limited severe accident. The steam oxidation behavior of candidate materials is a key metric in the evaluation of ATF concepts and also an important input into models. However, prior modeling work of FeCrAl cladding has used incomplete information on the physical properties of FeCrAl. Also, the steam oxidation data being collected at 1200°-1700°C is unique as no prior work has considered steam oxidation of alloys at such high temperatures. In some cases, the results have been difficult to interpret and more fundamental information is needed such as the stability of alumina in flowing steam at 1400°-1500°C. This report summarizes recent work to measure the steam oxidation kinetics of candidate alloys, the evaporation rate of alumina in steam and the development of integral data on FeCrAl compared to conventional Zr-based cladding.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Hydrogen Production by Steam Oxidation of Reduced CaFe 2 O 4 during Chemical Looping Coal Gasification: Equilibrium and Kinetic Analysis

CaFe 2 O 4 reduced during chemical looping coal gasification can be oxidized with steam for production of hydrogen. The conversion and equilibrium data of the oxidation of reduced CaFe 2 O 4 with steam were analyzed using steam concentrations of 10–25 vol % with a balance of helium and the temperature range of 1023–1123 K. Experimental data were evaluated to characterize H 2 production rates and oxidation isotherms. The film diffusion was the controlling step for the oxygen uptake process, and its parameters were determined on the basis of the uptake rate model. The steady-state oxygen uptake data were also evaluated with Langmuir, Temkin, Freundlich, and Dubinin–Radushkevich isotherms. The Langmuir isotherm model correlated the oxidation isotherms best, and the peak uptake capacity decreased with increasing temperatures, which suggests an exothermic process. In conclusion, the negative Gibbs free energy values (–Δ G °) implied the spontaneous nature of the uptake process at 1023–1123 K.

01 COAL, LIGNITE, AND PEAT↗

Enhanced steam oxidation resistance of uranium nitride nuclear fuel pellets

Here, the steam oxidation resistance of UN and UN-(20 vol%)ZrN fuel pellets is evaluated to enhance understanding of steam corrosion mechanisms in advanced nuclear fuel materials. In situ neutron diffraction shows the modified UN fuel pellets form a (U 0.77 ,Zr 0.23 )N solid-solution and the sole crystalline oxidation product detected in bulk is (U 0.77 ,Zr 0.23 )O 2 . U 2 N 3 is not detected in significant quantities during the steam oxidation of UN or (U 0.77 ,Zr 0.23 )N and stable lattice parameters show that hydriding does not take place. Steam oxidation rates, obtained via sequential Rietveld refinement show how (U 0.77 ,Zr 0.23 )N has a higher activation energy (79 ± 1 kJmol -1 vs. 50 ± 5 kJmol -1 ), higher onset temperature (430 °C vs. 400 °C) and slower reaction rates for steam oxidation up to 616 °C, than pure UN. Throughout, both UN and (U 0.77 ,Zr 0.23 )N exhibit linear (non-protective) oxidation kinetics, signifying that degradation of the fuel pellets is caused by the evolution of gaseous products at the interface followed by oxide scale spallation. This quantitative and mechanistic understanding of material degradation enables better defined operating regimes and points towards (U,Zr)N solid solutions as a promising strategy for the design of advanced nuclear fuel materials with enhanced steam corrosion resistance.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

In situ investigations of the hydrogen uptake of zirconium alloys during steam oxidation - 2016-0041

The hydrogen uptake during steam oxidation of Zircaloy-4 and E110 was investigated in situ in the temperature range of 1,000-1,300 deg. C. The procedure to determine hydrogen concentrations from the neutron radiographs measured is explained in detail. Very fast hydrogen absorption (less than 10 s) was observed directly after starting the steam injection. The maximal hydrogen concentration reached increased with increasing temperatures. A slight release of hydrogen was observed after this first fast hydrogen uptake. The hydrogen concentration depended on time with a power of -1/8. An enhanced hydrogen uptake occurred if the oxidation switched into the breakaway mode. The hydrogen concentration increased by nearly one order of magnitude. (authors)

36 MATERIALS SCIENCE↗