At least 19 records

The Chemistry, Formation and Passivation of Solid-Electrolyte Interphase (SEI) from FSI- Breakdown at Li-metal Potential

LiFSI-based liquid electrolytes are promising for realizing high Coulombic efficiency (CE) and long cycle life of next-generation high-energy Li metal battery. Nevertheless, the fundamentals of both the chemistry and formation of solid-electrolyte interphase (SEI) in these electrolytes have remained elusive. Herein, we extensively combine electrochemistry and X-ray photoelectron spectroscopy (XPS) to illustrate the reaction pathways of electrolyte decomposition, especially FSI- breakdown, as well as the dissolution trend of various inorganic SEI components. The SEI-forming reactions at Cu/electrolyte interface manifest a potential (E) dependence, driven by direct electron-transfer (ET) and Li underpotential-deposition (Li UPD) at high and low E regions, respectively. By closely correlating the XPS data obtained with and without solvent washing, we demonstrate that not all the products derived from SEI reactions are incorporated into forming a passivating surface layer, with a notable portion dissolving into liquid electrolyte instead. Importantly, high-CE electrolyte dictated by the chemical identity of solvent, is found to exhibit minimized interfacial reactivity of SEI formation enabling more effective interphasial passivation, via preferential integration of passivating ingredients such as LiF. Overall, this work formulates a systematic understating of bridging the SEI chemistry, formation and passivation while identifying key characteristics of high-performance electrolyte for guiding future design.

Bao, Zhenan [SLAC National Accelerator Laboratory

Evolution and Degradation Patterns of Electrochemical Cells Based on the Analysis of Interfacial Phenomena at Li Metal Anode/Electrolyte Interfaces

In this work, we report the results of a theoretical–computational analysis of the solid electrolyte interphase (SEI) growth and degradation dynamics occurring in lithium metal batteries during cycling. We use ab initio-kinetic Monte Carlo simulations to generate a synthetic data set, which is analyzed by machine learning methods. We aim to determine: (i) how modifications in interfacial interaction energies between solid electrolyte interphase (SEI) blocks and between Li ions and SEI facets impact the Coulombic efficiency (CE) of the battery and (ii) what factors, including reactions, microscopic transport, and other interfacial events, may lead to cell performance “failure” during prolonged charge and discharge cycles, signaled as a sharp decay in the CE over cycling. The demonstration of our approach is done on a cell including a Li metal surface interfacing with a previously introduced state-of-the-art electrolyte, and the idea can be applied to any electrochemical system. Outcomes include the identification of the leading chemical, physical, and structural variables causing cell failure and relating them to the electrolyte formulation, thus paving the way to future more refined analysis and electrolyte design.

batteries

Surprising Relationship between Silicon Anode Calendar Aging and Electrolyte Components in a Localized High-Concentration Electrolyte System

Although localized high-concentration electrolytes (LHCEs) have been shown to improve the calendar lifetime of silicon anodes, the roles of the electrolyte constituents in calendar aging are not well understood. Here, in this work, we utilize a voltage hold protocol and an LHCE with varying molar ratios of lithium bis(fluorosulfonyl)imide (LiFSI), tetramethylene sulfone (TMS), and 1,1,2,2-tetrafluoroethyl-2,2,3,3-tetrafluoropropyl ether (TTE) to probe the component roles during aging. Interestingly, the estimated calendar lifetime and irreversible lithium losses from the V-hold experiments are independent of the electrolyte formulations. Contrarily, the solid electrolyte interphase (SEI) composition depends on the electrolyte formulation. X-ray photoelectron spectroscopy shows that TMS-coordinated species decompose to form insoluble alkanes and lithium hydroxide (LiOH), while lithium fluoride (LiF) originates from the anion-coordination complex. The SEI composition does not appear to play a significant role in the silicon anode passivity, as measured by parasitic current, suggesting that the SEI-electrolyte interactions dictate the calendar aging mechanisms.

Si anode

On the Efficacy of Repeat Voltage Holds for Conditioning and Calendar Life Testing of Graphite and Silicon Cells

Voltage-hold (V-hold) protocols have shown promise toward calendar lifetime analysis of cells with graphite (Gr) and silicon (Si) anodes. In this work, repeat V-holds are performed on Gr and Si cells paired with lithium iron phosphate cathodes to delineate their beneficial role in formation and conditioning. We find that V-hold at the top of charge supplements constant current cycling in conditioning the cell to higher capacities for both Gr and Si cells after the first V-hold. A reduced order model provides the irreversible capacity proportions of each V-hold. With each repeat V-hold, parasitic loss of lithium to the solid electrolyte interphase (SEI) decreases on both Gr and Si cells. Gr cells show the square-root-of-time capacity loss behavior within 200 h of V-hold, indicative of its fast relaxation and low impact of reference performance test cycles on the SEI growth. Lifetime estimates from repeat V-holds on Gr can reach years. Si exhibits longer transition times from kinetic to diffusion-limited SEI growth, evidenced by the 400 h and 200 h holds showing square-root-of-time and linear behavior, respectively. Lifetime predictions from repeat V-holds on Si only reach 1–2 months, highlighting its limitations. Recommended duration of V-holds for Si cells should be ≥400 h.

25 ENERGY STORAGE

Valuation of Anode Materials for High-Performance Lithium Batteries: From Graphite to Lithium Metal and Beyond

Lithium-ion batteries have revolutionized energy storage, yet advanced technologies such as electric vehicles and eVTOLs demand even higher performance and safety. Anodes, the negative electrodes, are crucial in enhancing batteries’ safety, lifespan, and fast-charging capabilities. This review paper comprehensively evaluates the progression of anode materials from traditional graphite to advanced anodes like lithium metal. Graphite anodes, with a capacity of 372 mAh g −1 , enabled the first commercial lithium-ion batteries, but future applications require higher energy densities and fast-charging capabilities. Emerging anode materials, including alloying, and conversion types, as well as lithium metal, offer significantly higher capacities, with lithium metal offering a theoretical capacity of 3 860 mAh g −1 . However, these advanced anodes face challenges such as volume expansion, high surface reactivity, sluggish Li+ kinetics, and unstable lithium deposition morphologies. Here, this review critically examines the electrochemical performance, interfacial properties, mechanical attributes, and stability issues of various anode materials. It further discusses solid electrolyte interphase (SEI) formation, strategies for enhancing interface stability, and the requirements of anodes for solid-state batteries. Additionally, the review explores potential solutions for limitations with each anode type, highlights innovative anode-free architectures, and evaluates the current and future trends of battery anode industries. Ultimately, this paper aims to guide the development of high-performance anode materials, paving the way for the next generation of efficient, reliable lithium batteries.

Alloying anodes

Interdependence of Support Wettability - Electrodeposition Rate- Sodium Metal Anode and SEI Microstructure

Here, this study examines how current collector support chemistry (sodiophilic intermetallic Na 2 Te vs. sodiophobic baseline Cu) and electrodeposition rate affect microstructure of sodium metal and its solid electrolyte interphase (SEI). Capacity and current (6 mAh cm -2 , 0.5–3 mA cm -2 ) representative of commercially relevant mass loading in anode-free sodium metal battery (AF-SMBs) are analyzed. Synchrotron X-ray nanotomography and grazing-incidence wide-angle X-ray scattering (GIWAXS) are combined with cryogenic ion beam (cryo-FIB) microscopy. Highlighted are major differences in film morphology, internal porosity, and crystallographic preferred orientation e.g. (110) vs. (100) and (211) with support and deposition rate. Within the SEI, sodium fluoride (NaF) is more prevalent with Te-Cu versus sodium hydride (NaH) and sodium hydroxide (NaOH) with baseline Cu. Due to competitive grain growth the preferred orientation of sodium crystallites depends on film thickness. Mesoscale modeling delineates the role of SEI (ionic conductivity, morphology) on electrodeposit growth and onset of electrochemical instability.

36 MATERIALS SCIENCE

The Impact of Lithium Anode Interface on Capacity Fade in Polymer Electrolyte-Based Solid-State Batteries

This study investigates the Li stripping-plating morphology and failure mechanisms in full cells consisting of a solid polymer electrolyte (SPE) with two commercial Li anodes: Li chip and Li foil. The primary identified failure mechanism of the SPE cell is capacity fade, regardless of the Li manufacturer. While the cathode’s role in capacity fade is evident, the Li anode significantly influences cycling performance, with Li foil cells cycling 50% longer than Li chip cells, a statistical difference. Further, post-mortem scanning electron microscopy and X-ray photoelectron spectroscopy results attribute the Li chip’s faster capacity fade to a loss of contact and continuous growth of the solid electrolyte interphase (SEI). Conversely, Li foil maintains consistent contact with the solid polymer, displaying a thin and stable SEI. Additionally, failure mechanisms between a gel electrolyte in previous work and the dry SPE are compared.

25 ENERGY STORAGE

Multi-phase characterization of pitch-carbon coated nano-silicon anodes for lithium-ion batteries

Silicon (Si) is a leading next-generation Li-ion battery anode candidate that meets rigorous performance demands for portable power including enhanced power and energy density with robust cycling performance. However, a series of complex and interrelated reactions lead to reduced calendar life in Si-containing systems and therefore challenge practical adoption. In the present work, we probe the mechanisms underlying observed performance improvements by adding a pitch-carbon coating onto nano-Si material. We pair solid-phase (X-ray photoemission spectroscopy, Fourier-transform infrared), semi-volatile phase (solid-phase microextraction-gas chromatography-mass spectrometry), and gas-phase (gas chromatography-flame-ionization detector) characterization signals to comprehensively evaluate the impact of pitch-carbon coating on the evolution of the Si solid-electrolyte interphase (SEI) and the associated impacts on electrode/electrolyte reactivity. The pitch-carbon is found to serve as a physicochemical barrier, reducing the electro-active surface area for Si/electrolyte reactivity and preventing Si oxidation. Further, the pitch-carbon coating promotes the evolution of a more-favorable SEI by subsuming substantial functionality typically associated with the fluoroethylene carbonate (FEC) electrolyte additive - such as alkoxide scavenging and suppression of transesterification pathways - and by shifting the competitive electrolyte degradation pathways' favorability. The multi-phase characterization approach enables holistic end-products evaluation from complex (electro)chemical interfacial reactions, which informs a robust interpretation of the carbon coating's role in electrochemical performance improvements. The present mechanistic evaluation aids the rational design for improved nano-Si materials.

25 ENERGY STORAGE

A quantitative figure of merit for battery SEI films and their use as functional solid-state electrolytes

As a key passivation film that governs battery operation, the solid electrolyte interphase (SEI) has long been credited for enabling high-performance batteries or blamed for their eventual death. However, qualitative descriptions of the SEI often found in the literature (e.g., “conductive,” “passivating”) highlight our incomplete understanding of this layer, where even the most basic properties foundational to SEI function remain difficult to measure. Here, we quantify SEI conductivities and SEI transference numbers using a separator-free Cu|SEI|Li architecture that treats the SEI as a functional solid-state electrolyte (SSE). We find that while any SEI property alone (e.g., electronic conductivity) is weakly correlated (R 2 < 0.67) with battery performance (e.g., Coulombic efficiency), a strong correlation (R 2 > 0.99) can be achieved by defining the “SEI cT number” as a product between the SEI transference number (T) and the ratio of SEI conductivities (c). Analogous to the thermoelectric figure of merit (i.e., zT ), SEI cT quantitatively benchmarks the holistic impact of SEI properties on battery performance and underscores the pitfalls of citing such properties in isolation. Perhaps most strikingly, we demonstrate that Li metal deposition and stripping at room temperature is possible in our separator-free Cu|SEI|Li cell, confirming that the SEI can function precisely as an SSE. Together, these results enrich our understanding of the SEI, not just as a passivation layer but as a functional structure that can potentially have important implications for solid-state batteries.

Science & Technology - Other Topics

Binary Cation Matrix Electrolyte and Its Effect on Solid Electrolyte Interphase Suppression and Evolution of Si Anode

An unstable solid electrolyte interphase (SEI) has been recognized as one of the biggest challenges to commercializing silicon (Si) anodes for high-energy-density batteries. This work thoroughly investigates a binary cation matrix of Mg 2+ +Li + electrolyte and its role in SEI development, suppression, and evolution of a Si anode. Findings demonstrate that introducing Mg ions dramatically reduces the SEI growth before lithiation occurs, primarily due to the suppression of solvent reduction, particularly ethylene carbonate (EC) reduction. The Mg 2+ alters the Li + cation solvation environment as EC preferably participates in the oxophyllic Mg 2+ solvation sheath, thereby altering the solvent reduction process, resulting in a distinct SEI formation mechanism. The initial SEI formation before lithiation is reduced by 70% in the electrolyte with the presence of Mg 2+ cations. While the SEI continues to develop in the postlithiation, the inclusion of Mg ions results in an approximately 80% reduction in the postlithiation SEI growth. Continuous electrochemical cycling reveals that Mg 2+ plays a crucial role in stabilizing the deep-lithiated Si phases, which effectively mitigates side reactions, resulting in controlled SEI growth and stable interphase while eliminating complex Li x Si y formation. Mg ions promote the development of a notably more rigid and homogeneous SEI, characterized by a reduced dissipation (ΔD) in the Mg 2+ +Li + ion matrix compared to the solely Li + system. In conclusion, this report reveals how the Mg 2+ +Li + ion matrix affects the SEI evolution, viscoelastic properties, and electrochemical behavior at the Si interface in real time, laying the groundwork for devising strategies to enhance the performance and longevity of Si-based next-generation battery systems.

25 ENERGY STORAGE

Deconvoluting Effects of Lithium Morphology and SEI Stability at Moderate Current Density Using Interface Engineering

Lithium (Li)-morphology and solid electrolyte interphase (SEI) are among the most significant performance regulators in Li-metal batteries (LMBs). While both Li-morphology and SEI composition play key roles in the cyclability of LMBs, less is understood about the individual contributions of each factor to overall Li reversibility, particularly at a practical current density (1 mA cm −2 ) at which the kinetics of both factors are not naturally separated. Herein, an interface engineering approach is introduced to deconvolute the impacts of Li-morphology and SEI composition on battery performance. By using interfacial nanofilms with differing resistivity (resistive HfO 2 versus conductive ZnO), the morphology of Li is varied, and by virtue of similar acidic character of the nanofilms, the formation of anion-rich SEIs is maintained. It is established that although the surface acidity of the thin films enables preformation of a more anion-rich SEI, it is not preserved after Li plating. It is further shown that resistance-controlled, low-surface-area Li-morphology exhibits up to threefold increase in stable cycle life when tested in multiple electrolytes. Overall, these findings explain why Li-morphological control is more advantageous for performance improvement than preformed SEI modulation due to the inherent challenges in SEI preservation.

36 MATERIALS SCIENCE

Solid State Multinuclear Magnetic Resonance Investigation of Electrolyte Decomposition Products on Lithium Ion Electrodes

Solid electrolyte interphase (SEI) formation in lithium ion cells prepared with advanced electrolytes is investigated by solid state multinuclear (7Li, 19F, 31P) magnetic resonance (NMR) measurements of electrode materials harvested from cycled cells subjected to an accelerated aging protocol. The electrolyte composition is varied to include the addition of fluorinated carbonates and triphenyl phosphate (TPP, a flame retardant). In addition to species associated with LiPF6 decomposition, cathode NMR spectra are characterized by the presence of compounds originating from the TPP additive. Substantial amounts of LiF are observed in the anodes as well as compounds originating from the fluorinated carbonates.

Li-ion battery electrolytes

Lithium‐Containing Hybrid SEI Layer Enabling High Mass Loading and Anode‐Less Sodium Metal Batteries

Abstract The continuous rupturing and rebuilding of unstable solid electrolyte interphase (SEI) layer during cycling would block Na + diffusion and induce Na dendrite formation, ultimately limiting the practical application of high‐energy‐density sodium metal batteries. Herein, a hybrid SEI layer containing Li‐species is dexterously constructed on the surface of sodium metal anode. Li‐containing inorganic components (Li 3 N, LiF, and Li 2 CO 3 ) are introduced to stabilize the Na/electrolyte interface and enhance the mechanical and diffusion kinetic properties of the SEI layer, which can reduce the side reactions and gas generation, regulate Na + flux during cycling and promote rapid Na + migration for uniform dendrite‐free Na deposition. As a result, the constructed Na symmetric cells achieve low overpotential and long cycle life of 5900, 1800, and 500 h at current densities of 3, 10, and 30 mA cm −2 , respectively. Furthermore, the full cells paired with the Na₃V₂(PO₄)₃ cathode demonstrate high specific capacity and excellent cycle stability, even at an ultra‐high cathode loading of 39.3 mg cm −2 and a low N/P ratio (negative/positive electrode capacity ratio of 1.21).

Xia, Li [State Key Laboratory of Physical Chemistr

The Promise of Alloy Anodes for Solid-State Batteries

Solid-state batteries are anext-generation technology that could featureimproved safety and energy density, but reliably integrating high-capacity electrode materials to enable high energy while retaining stablelong-termcycling remains a challenge. Anode materials that alloy with lithium, such as silicon, tin, and aluminum,offer high capacity that canyield high-energy battery cells. The use of alloy anodes in solid-state batteries potentially offers major mechanistic benefits compared to other anode contendersand battery systems, such as lithium metal in solid-state architectures or alloys in liquid-electrolyte batteries. This perspective discusseskey advantagesof alloy anode materials for solid-state batteries, including the avoidance of the short circuiting observed with lithium metal and the chemo-mechanical stabilization of the solid-electrolyte interphase (SEI). We further discuss open research questions and challenges in engineering alloy-anode-based solid-state batteries, with the goal of advancing our understanding and control of alloy anode materialswithin solid-state architectures toward commercial application.

John A Lewis

Lithium‐Containing Hybrid SEI Layer Enabling High Mass Loading and Anode‐Less Sodium Metal Batteries

The continuous rupturing and rebuilding of unstable solid electrolyte interphase (SEI) layer during cycling would block Na + diffusion and induce Na dendrite formation, ultimately limiting the practical application of high-energy-density sodium metal batteries. Herein, a hybrid SEI layer containing Li-species is dexterously constructed on the surface of sodium metal anode. Li-containing inorganic components (Li 3 N, LiF, and Li 2 CO 3 ) are introduced to stabilize the Na/electrolyte interface and enhance the mechanical and diffusion kinetic properties of the SEI layer, which can reduce the side reactions and gas generation, regulate Na + flux during cycling and promote rapid Na + migration for uniform dendrite-free Na deposition. As a result, the constructed Na symmetric cells achieve low overpotential and long cycle life of 5900, 1800, and 500 h at current densities of 3, 10, and 30 mA cm −2 , respectively. Furthermore, the full cells paired with the Na₃V₂(PO₄)₃ cathode demonstrate high specific capacity and excellent cycle stability, even at an ultra-high cathode loading of 39.3 mg cm −2 and a low N/P ratio (negative/positive electrode capacity ratio of 1.21).

Diffusion kinetic

All-organic self-separating three-dimensionally nanoarchitected electrochemical energy storage devices

This work realizes a three-dimensionally (3D) nanoarchitected, all organic, "self-separating" lithium-ion electrochemical energy storage (EES) device that is cycled as a solid-state full cell. The device is enabled by a monolithic carbon anode with a co-continuous pore network, derived from the structure direction of resols by an ultra-large molar mass block copolymer (BCP), poly(styrene-block-2-dimethylaminoethyl methacrylate) (SA). Electropolymerization of a single-phase conductive and redox-active material, poly((2,3-dihydrothieno[3,4-b][1,4]dioxin-2-yl)methyl 9,10-dioxo-9,10-dihydroanthracene-2-carboxylate) (PAQEDOT), into the pore space provides the cathode of the cell. The device is electronically contacted to the relevant electrode network enabled by the co-continuous nature of each electrode. Electrochemical processing via cycling against external lithium in an electrolyte generates a solid electrolyte interphase (SEI) as a separator and lithiates the cell electrodes, after which the EES device is cycled in the solid state. While the full cell does not demonstrate high cyclability, the best full cell demonstrates a discharge capacity of 267 milliamp hours per gram (mAh/g). This work marks, to the best of knowledge of the authors, the first example of an all-organic materials derived 3D nanoarchitected EES device, as well as the first design of "self-separating" cell fabrication. Furthermore, generalization of the design to another co-continuous carbon form factor is demonstrated.

FOS: Physical sciences

Heterogeneous Solid Electrolyte Interphase Interactions Dictate Interface Instability in Sodium Metal Electrodes

Sodium (Na) metal batteries have attracted recent attention due to their low cost and high abundance of Na. However, the advancement of Na metal batteries is impeded due to key challenges such as dendrite growth, solid electrolyte interphase (SEI) fracture, and low Coulombic efficiency. This study examines the coupled electro‐chemo‐mechanical interactions governing the electrodeposition stability and morphological evolution at the Na/electrolyte interface. The SEI heterogeneities influence transport and reaction kinetics leading to the formation of current and stress hotspots during Na plating. Further, it is demonstrated that the heterogeneity‐induced Na metal evolution and its influence on the stress distribution critically affect the mechanical overpotential, contributing to a faster SEI failure. The analysis reveals three distinct failure mechanisms—mechanical, transport, and kinetic—that govern the onset of instabilities at the interface. Finally, a comprehensive comparative study of SEI failure in Na and lithium (Li) metal anodes illustrates that the electrochemical and mechanical characteristics of the SEI are crucial in tailoring the anode morphology and interface stability. This work delineates mechanistic stability regimes cognizant of the SEI attributes and underlying failure modes and offers important guidelines for the design of artificial SEI layers for stable Na metal electrodes.

25 ENERGY STORAGE

Direct regeneration of degraded LiFePO4 cathodes via a separator-enabled prelithiation strategy

A persistent challenge in lithium-ion batteries is the loss of active lithium due to the solid electrolyte interphase (SEI) formation and associated side reactions. While prelithiation employing lithium replenishment separator (LRS) has been proven effective in compensating for lithium loss, previous studies have largely been accompanied by gas evolution or solid residue formation during the prelithiation process. To surmount this challenge, we present a LRS based on 4-fluoro-1,2-dihydroxybenzene lithium salt (LiDF), capable of mitigating lithium loss while producing decomposition products that integrate directly into the electrolyte as functional additives which can assist with the stability of the SEI, free from gas or solid formation, thus establishing a sustainable and environmentally benign strategy for lithium compensation. Incorporation of the LRS enables the pristine LiFePO4||graphite (Gr) full cell to achieve 10.8% higher capacity than the cell with a polypropylene separator (PPS) after 200 cycles at 0.5C. Remarkably, the degraded LiFePO4 (D-LFP)||Gr full cell with the LRS exhibits a 135.8% capacity improvement over the PPS-based cell after 500 cycles. These findings establish the LRS as a powerful approach for both boosting high-performance lithium-ion batteries and recovering the capacity of degraded batteries.

Tao, Fujun