Characterization of Saltstone Grout Line Samples
During a prestart recirculation operation in the Saltstone Processing Facility (SPF), operations staff noticed hardened scaling falling into the hopper. As a result, SPF operators and Saltstone Engineering decided to postpone operation and conduct a process room hopper cleanout. During the cleanout effort personnel noted greater than normal buildup of damp solid material in the transfer line. A borescope investigation was conducted and confirmed buildup was present throughout the transfer line to the downstream valves. Savannah River National Laboratory personnel were asked to characterize the scale material and samples collected from the saltstone grout line and provide recommendations and/or further guidance as to whether additional corrosion testing is needed for useful equipment operating life information. Based on the samples characterized results, the plug material contained only the 60:40 slag:fly ash saltstone. Portland cement in the original 10:45:45 Portland cement:slag:fly ash mix may result in a less abrasive slurry compared to the 60:40 slag:fly ash mix because the slag is > 95 % crushed angular, sharp edged glass. Saltstone grout erosion and corrosion testing of A36 carbon steel is needed to determine if the 60:40 mix is more abrasive and corrosive for A36 carbon steel than the 10:45:45 mix.