Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “polysiloxane composites”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Easy-Processable and Aging-Free All-Polymer Polysiloxane Composites

In this work, we report all-polymer polysiloxane composites that overcome the long-standing processing problems of silica-reinforced silicone rubbers. Polystyrene fillers are dispersed with styrene/dimethylsiloxane symmetric diblock and triblock copolymers that control the filler morphology, filler–matrix interactions, and filler–filler interactions. Surprisingly, the composites not only rival the traditional silica-reinforced polysiloxane in mechanical properties of cured materials but also have better processability and stability than the silica-filled compound before curing. Large amplitude oscillatory shear experiments demonstrate that the triblock copolymer addition strongly affects the rheological properties. We hypothesize that the bridges and entangled loops that were formed by the triblock copolymer can connect different PS domains to provide additional reinforcement. The aging effect that originates from PDMS chain adsorption on the filler particle surface is also avoided because of the thermodynamic repulsion between PS and PDMS phases.

36 MATERIALS SCIENCE↗

Curable polysiloxane compositions and slippery materials and coatings and articles made therefrom

The present teachings generally provide curable polysiloxane compositions including a base resin including a surface active polymer. Articles of manufacture including the curable polysiloxane compositions and slippery coatings and materials also are provided. The compositions may be used to provide slippery, lubricious, or repellent materials and coatings and may provide anti-fouling function. The compositions can provide anti-fouling or foul-release function on open surfaces, internal surfaces, membranes; to provide pinning free or low contact angle hysteresis surfaces; to provide homogeneous interface to suppress nucleation; to provide a barrier layer such as anti-corrosion; to provide anti-stain, anti-smudge, anti-fingerprint, anti-soil function.

Kim, Philseok↗

Curable polysiloxane compositions and slippery materials and coatings and articles made therefrom

The present teachings generally provide curable polysiloxane compositions including a base resin including a surface active polymer. Articles of manufacture including the curable polysiloxane compositions and slippery coatings and materials also are provided. The compositions may be used to provide slippery, lubricious, or repellent materials and coatings and may provide anti-fouling function. The compositions can provide anti-fouling or foul-release function on open surfaces, internal surfaces, membranes; to provide pinning free or low contact angle hysteresis surfaces; to provide homogeneous interface to suppress nucleation; to provide a barrier layer such as anti-corrosion; to provide anti-stain, anti-smudge, anti-fingerprint, anti-soil function.

Kim, Philseok↗

Cellulosic gels, films and composites including the gels, and methods of forming same

Disclosed are cellulose-based 5 flexible aerogels and xerogels containing bacterial cellulose nanorods, ribbons, fibers, and the like, wherein the gels have tunable optical, heat transfer, and stiffness properties. Further disclosed are highly transparent and flexible cellulose nanofiber-polysiloxane composite aerogels featuring enhanced mechanical robustness, tunable optical anisotropy, and low thermal conductivity.

Smalyukh, Ivan I.↗

3D Printing of High Viscosity Reinforced Silicone Elastomers

Recent advances in additive manufacturing, specifically direct ink writing (DIW) and ink-jetting, have enabled the production of elastomeric silicone parts with deterministic control over the structure, shape, and mechanical properties. These new technologies offer rapid prototyping advantages and find applications in various fields, including biomedical devices, prosthetics, metamaterials, and soft robotics. Stereolithography (SLA) is a complementary approach with the ability to print with finer features and potentially higher throughput. However, all high-performance silicone elastomers are composites of polysiloxane networks reinforced with particulate filler, and consequently, silicone resins tend to have high viscosities (gel- or paste-like), which complicates or completely inhibits the layer-by-layer recoating process central to most SLA technologies. Herein, the design and build of a digital light projection SLA printer suitable for handling high-viscosity resins is demonstrated. Further, a series of UV-curable silicone resins with thiol-ene crosslinking and reinforced by a combination of fumed silica and MQ resins are also described. The resulting silicone elastomers are shown to have tunable mechanical properties, with 100–350% elongation and ultimate tensile strength from 1 to 2.5 MPa. Three-dimensional printed features of 0.4 mm were achieved, and complexity is demonstrated by octet-truss lattices that display negative stiffness.

36 MATERIALS SCIENCE↗

Highly filled carbon nanofiber reinforced polysiloxanes

Provided herein are polysiloxane-based composite materials comprising a high weight percentage of elemental components (e.g., elemental boron, elemental copper, elemental bismuth, elemental lead) and low levels of carbon nanofibers. The elemental components may be present in the composite materials at levels greater than 25% by weight. Also provided herein are methods of forming the composite materials that have desirable flexibility and shielding properties. The invention provides a versatile composite material that is compliant and moldable, while still comprising high levels of the elemental shielding components. The materials are particularly useful for applications in which radiation shielding or neutron capture are desired.

Robison, Thomas Wayne↗

Polysiloxane-based objects and 3-dimensional printing method for making the same

Disclosed herein are embodiments of an additively manufactured polysiloxane-based object, as well as composition embodiments for making such object embodiments. Also disclosed are embodiments of a method for making the additively manufactured polysiloxane-based object using the composition embodiments described herein. The disclosed composition embodiments and method embodiments provide objects that are substantially free of contaminants that deleteriously affect structural integrity and that comprise a polymer skeleton consisting of oxygen-silicon bonds wherein the silicon component can further comprise one or more branching groups.

Cluff, Kyle↗

Carbon Nanotube – Polysiloxane Nanocomposites for Ablative Thermal Protection Systems

Ultra-high temperature resins (UHTR) such as polysiloxane possess excellent characteristics for ablation including low thermal conductivity, lightweight composition, high thermal resistance, and the ability to form a durable char layer. To enhance its mechanical strength, the aerospace industry utilizes fiber reinforcement, such as carbon fiber reinforced polysiloxane (CF-polysiloxane), due to its high strength-to-weight ratio. Carbon nanotubes (CNTs) have advantages over microfibers including higher specific strength, lower density, and customizable thermal conductivity. Their nano-scale dimensions allow for a more homogenous material compared to traditional microfibers. Conventional methods of incorporating CNTs into resins often have structural defects such as voids, CNT agglomerations, and randomly dispersed CNTs, resulting in marginal improvements in properties. A novel approach known as bulk nanocomposite laminating (BNL) has been introduced involving CNT densification, resin polymer infiltration, and pressurized curing to achieve a high packing density exceeding 35% by volume. Characterization and testing to simulate re-entry conditions is performed with a sample of CNT-polysiloxane nanocomposite cured onto a CF-polysiloxane backing. These samples are subjected to ablation by an oxyacetylene flame while collecting temperature data to evaluate thermal protection properties.

Palak B Patel↗

Surface characterization of LDEF materials

The NASA Long Duration Exposure Facility (LDEF), a passive experimental satellite, was placed into low-Earth orbit by the Shuttle Challenger in Apr. 1984. The LDEF spent an unprecedented 69 months in space. The flight and recovery of the LDEF provided a wealth of information on the longterm space environmental effects of a variety of materials exposed to the low-Earth orbit environment. Surface characterization of LDEF materials included polymers, composites, thermal control paints, and aluminum. X-ray photoelectron spectroscopy (XPS), Auger electron spectroscopy (AES), scanning electron microscopy (SEM), and contact angle analysis were used to document changes in both the surface composition and surface chemistry of these materials. Detailed XPS analysis of the polymer systems, such as Kapton, polyimide polysiloxane copolymers, and fluorinated ethylene propylene thermal blankets on the backside of the LDEF revealed significant changes in both the surface composition and surface chemistry as a result of exposure to the low-Earth orbit environment. Polymer systems such as Kapton, polyimide polysiloxane copolymers, and polysulfone showed a common trend of decreasing carbon content and increasing oxygen content with respect to the control sample. Carbon 1s curve fit XPS analysis of the composite samples, in conjunction with SEM photomicrographs, revealed significant ablation of the polymer matrix resin to expose the carbon fibers of the composite during exposure to the space environment. Surface characterization of anodized aluminum tray clamps, which were located at regular intervals over the entire LDEF frame, provided the first results to evaluate the extent of contamination with respect to position on the LDEF. The XPS results clearly showed that the amount and state of both silicon and fluorine contamination were directly dependent upon the position of the tray clamp on the LDEF.

Wightman, J. P.↗

Dataset_for_Molecular_Motion_Below_the_Glass_Transition_A_Solid-State_NMR_Study_of_Siloxane_Polymer_Dynamics Study

This dataset contains solid-state 1H and 13C NMR relaxometry data, differential scanning calorimetry (DSC) data, and size exclusion chromatography (SEC/GPC) data supporting the study of sub-glass-transition (sub-Tg) molecular dynamics in a composition- and sequence-controlled series of diphenyl-substituted polysiloxanes (PDMS, 14Ph, 33Ph, 50Ph, 67Ph, and 100Ph; 0–100% diphenylsiloxane content by mole).All solid-state NMR data were acquired on a 200 MHz Bruker Avance III HD spectrometer using a static 7 mm HX probe or a 4 mm HX probe under 4 kHz magic-angle spinning. Raw Bruker TopSpin experiment folders are included for: (1) variable-temperature 1H lineshape measurements used to determine linewidth (FWHM) as a function of temperature across the glass transition; (2) 1H T1 (saturation recovery with solid-echo detection), probing nanosecond-scale dynamics near the 1H Larmor frequency; (3) 1H T1rho (direct spin-lock, 62.5 kHz), probing microsecond-scale segmental dynamics; (4) 13C-detected Lee–Goldburg cross-polarization 1H T1rho (LGCPH T1rho) for 33Ph and 50Ph, resolving aromatic and aliphatic proton environments; and (5) 13C T1 relaxation for 33Ph and 50Ph. Differential scanning calorimetry data (TA Instruments DSC 25, −150 to +120 °C, up to +300 °C for 100Ph, 10 °C/min) are included for all six compositions and support the glass-transition temperatures in Table 1 and Figure 1. Size exclusion chromatography data (Agilent 1200 Series, PL-Gel 300 mixed-C column, THF mobile phase, polystyrene calibration standards) are included for the three synthesized copolymers (33Ph, 50Ph, 67Ph) and support the number-average molecular weights in Table 1. Processed data include per-composition relaxation-time summaries (Excel), curve-fitting and Bloembergen-Purcell-Pound (BPP) model analysis notebooks (Jupyter/Python), and Igor Pro (.pxp) master files used to generate the manuscript's figures.

Bloembergen-Purcell-Pound theory↗

Processing and Characterization of Basalt Fiber Reinforced Ceramic Composites for High Temperature Applications Using Polymer Precursors

The development of high temperature structural composite materials has been very limited due to the high cost of the materials and the processing needed. Polymer Derived Ceramics (PDCs) begin as a polymer matrix, which allows a shape to be formed prior to the cure, and is then pyrolized in order to obtain a ceramic with the associated thermal and mechanical properties. The two PDCs used in this development are polysiloxane and polycarbosilane. Basalt fibers are used for the reinforcement in the composite system. The use of basalt in structural and high temperature applications has been under development for over 50 years, yet there has been little published research on the incorporation of basalt fibers as a reinforcement in composites. Continuous basalt fiber reinforced PDCs have been fabricated and tested for the applicability of this composite system as a high temperature structural composite material.

High Temperature Composites↗

Tracking copper nanofiller evolution in polysiloxane during processing into SiOC ceramic

Polymer-derived ceramics (PDCs) remain at the forefront of research for a variety of applications including ultra-high-temperature ceramics, energy storage and functional coatings. Despite their wide use, questions remain about the complex structural transition from polymer to ceramic and how local structure influences the final microstructure and resulting properties. This is further complicated when nanofillers are introduced to tailor structural and functional properties, as nanoparticle surfaces can interact with the matrix and influence the resulting structure. The inclusion of crystalline nanofiller produces a mixed crystalline–amorphous composite, which poses characterization challenges. With this study, we aim to address these challenges with a local-scale structural study that probes changes in a polysiloxane matrix with incorporated copper nanofiller. Composites were processed at three unique temperatures to capture mixing, pyrolysis and initial crystallization stages for the pre-ceramic polymer. We observed the evolution of the nanofiller with electron microscopy and applied synchrotron X-ray diffraction with differential pair distribution function (d-PDF) analysis to monitor changes in the matrix's local structure and interactions with the nanofiller. The application of the d-PDF to PDC materials is novel and informs future studies to understand interfacial interactions between nanofiller and matrix throughout PDC processing.

Chemistry↗

Outgassing of casted and 3D printed silicones

Outgassing of 3D printed and casted silica-filled silicones was studied using a standard ASTM E-595 procedure and a modified Soreq’s method that allows very sensitive measurements of the outgassing kinetics even at low temperatures, 20 – 50 °C. We studied three different silica-filled silicones, non-porous cased M9787, and 3D printed LL50 and 40P materials. The present report shows that vacuum outgassing products of polysiloxane-based materials include multiple species. In addition to chemisorbed and physisorbed water outgassing, previously studied by TPD, polymer fragments of varying sizes evaporate as well. The chemical composition of the condensable volatile species collected on a Germanium substrate, was analyzed by FTIR. It was shown that all studied materials produce mostly PDMS-based outgassing products that form stable droplet-like structure on the Ge substrate. The highest amount of the condensable volatile species was measured for LL50. Isothermal TGA in nitrogen atmosphere of the LL50 material was compared to the standard vacuum outgassing. The results of TGA showed lower mass loss and higher water regain. The kinetics of the outgassing at relatively low temperatures of 20, 30 and 50 °C was studied using Thermoelectric Quartz Crystal Microbalance (TQCM). The TQCM surface was held at -10 °C to enhance condensation of the outgassed moisture. The analysis presented here, when combined with the extensive previous work on moisture outgassing, provides a better understanding of the aging mechanism of polysiloxane-based materials. In this work we show that outgassing techniques, usually applied for qualification of polymers for space-related applications, may be used as a complementary method to study thermal degradation and aging of silica-based silicones. Our results indicate that the long-term degradation mechanics and thermal degradation products depend primarily on the chemical composition of silicone-based material and only slightly affected by the manufacturing process. Surprisingly, the surface-to-volume ratio of the 3D printed vs. casted/molded materials showed only minor effect on the outgassing kinetic parameters.

36 MATERIALS SCIENCE↗

Tailoring Silicon Oxycarbide Glasses for Oxidative Stability

Blackglas(Trademark) polysiloxane systems produce silicon oxycarbide glasses by pyrolysis in inert atmosphere. The silicon oxycarbides evidence oxidative degradation that limits their lifetime as composite matrices. The present study characterizes bonding rearrangements in the oxycarbide network accompanying increases in pyrolysis temperature. It also addresses the changes in susceptibility to oxidation due to variations in the distribution of Si bonded species obtained under different processing conditions. The study is carried out using Si-29 nuclear magnetic resonance (NMR) spectroscopy and a design of experiments approach to model the oxidation behavior. The NMR results are compared with those obtained by thermogravimetric analysis (TGA). Samples pyrolyzed under inert conditions are compared to those pyrolyzed in reactive ammonia environments.

Hurwitz, F. I.↗

One-Component, Vinyl-Functional Fluorosilicone Pastes for Direct Ink Write Additive Manufacturing

In this study, one-component (“all-in-one”) fluorosilicone pastes specifically designed for application in direct ink write (DIW) additive manufacturing (AM) have been developed. They consist of vinyl-functional, methyltrifluoropropyl-containing (MeTfpS) terpolysiloxane base polymer(s), hydrosilyl-functional cross-linker(s), UV-sensitive hydrosilylation catalyst, thixotropic additive, and trimethylsilylated fumed silica filler, with other additives that are optional. Their base polymers were completely amorphous and linear, with molecular weights (M n ) ranging from approximately 7000 to 50,000 and specifically targeted for the viscosity range ideal for DIW. These polymers were prepared by anionic ring-opening polymerizations (A-ROP) of appropriate mixtures of cyclic siloxanes initiated by oligomeric, difunctional tetramethylammonium silanolate in the presence of a difunctional tetramethyldivinyldisiloxane end-blocker and molecular weight regulator. Two series of these terpolymers were prepared: one containing 5 mol % MeTfpS repeat units but varying degrees of polymerization (DP) from 80 to 600 and the other containing 5, 10, and 15 mol % MeTfpS at a constant DP of 600. All polymers contained mostly random distributions of MeTfpS repeat units. The pastes were prepared by speed-mixing, ready for use in DIW, they exhibited ideal thixotropy, long-term (over a year) rheological stability, and can be quickly (within seconds) and permanently cured by room-temperature, UV-activated hydrosilylation in air. The resulting elastomers showed base polymer molecular weight- and composition-dependent stress-induced crystallization (SIC) at higher molecular weights and lower trifluoropropyl contents and tunable Shore A hardness (30A–40A) typical for soft polysiloxane rubbers. Preliminary DIW tests indicated excellent printability with high precision of printed shapes and clearly present these one-component pastes as prime candidates for simple and practical printing of silicone elastomer objects.

36 MATERIALS SCIENCE↗

Poly(aryl ethers) and related polysiloxane copolymer molecular coatings: Preparation and radiation degradation

The radiation degradation of poly(arylene ether sulfones) and related materials is studied. These basic studies are important both as a means to developing stronger, more stable matrix resins for composite materials, as well as to improve the data base in regard to chemical structure-physical property relationships. Thirty homo and copolymers were synthesized, at least partially characterized and, in several cases suitable film casting techniques were developed. Four samples were chosen for initial radiation degradation. Poly(dimethyl siloxane) soft bocks/segments can preferentially migrate to the surface of copolymer films. Since siloxanes are utilized as thermal control coatings, this form of 'molecular' coating is of interest. The chemistry for preparing such copolymers with any of the polymers described was demonstrated.

Mcgrath, J. E.↗

Siloxane-modified polycarbosilane flexible Prepregs for fabrication of ceramic matrix composites via compression molding and PIP densification

For this work, the development of ceramic matrix composites (CMCs) using 5 harness satin carbon fiber fabric impregnated with commercial polycarbosilane precursor plasticized by siloxane copolymer was investigated aiming to improve wetting behavior and shape conformability. The polycarbosilane precursor and polysiloxane plasticizer were mixed at varying weight ratios to obtain flexible preceramic resin prepreg cloths. 13 plies of preceramic polymer prepreg cloths were stacked in 0/90° layup and cured by compression molding, followed by densified via PIP process. The CMCs were densified with eight PIP cycles followed by final crystallization at 1600 °C. The CMCs made with 10 wt% polysiloxane loading showed lower viscosity of the prepreg resin as well as higher strength and displacement to failure compared to those fabricated from unplasticized polycarbosilane prepolymer. In contrast, at higher concentration of plasticizer, viscosity of the prepreg resin increased, and the CMC became more brittle; however, it exhibited considerably higher thermal conductivity.

Carbosilane↗