Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “photovoltaic modules”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Encapsulation and backsheet adhesion metrology for photovoltaic modules

Photovoltaic modules are designed to operate for decades in terrestrial environments. However, mechanical stress, moisture, and ultraviolet radiation eventually degrade protective materials in modules, particularly their adhesion properties, eventually leading to reduced solar cell performance. Despite the significance of interfacial adhesion to module durability, currently there is no reliable technique for characterizing module adhesion properties. We present a simple and reproducible metrology for characterizing adhesion in photovoltaic modules that is grounded in fundamental concepts of beam and fracture mechanics. Using width-tapered cantilever beam fracture specimens, interfacial adhesion was evaluated on relevant interfaces of encapsulation and backsheet structures of new and 27-year-old historic modules. The adhesion energy, Gc [J/m 2 ], was calculated from the critical value of the strain energy release rate, G, using G = βP 2 , where β (a mechanical and geometric parameter of the fracture specimen) and P (the experimentally measured critical load) are constants. Under some circumstances where testing may result in cracking of brittle layers in the test specimen, measurement of the delamination length in addition to the critical load was necessary to determine G. Relative to new module materials, backsheet adhesion was 95% and 98% lower for historic modules that were exposed (operated in the field) and unexposed (stored on-site, but out of direct sunlight), respectively. Encapsulation adhesion was 87-94% lower in the exposed modules and 31% lower in the unexposed module. As a result, the metrology presented here can be used to improve module materials and assess long-term reliability.

14 SOLAR ENERGY↗

Understanding interfacial chemistry of positive bias high-voltage degradation in photovoltaic modules

Photovoltaic module degradation from a high system voltage is a prevalent degradation mode in the field, where the enabling degradation mechanisms are inherently dependent on the voltage bias polarity of the installed system. In this study, the effects of positive bias on module performance are confirmed and the underlying chemical degradation processes are more thoroughly investigated to reveal different degradation pathways from those previously reported in negative bias studies. When cells are under +1000 V stress, crystalline silicon mini-modules with poly(ethylene-co-vinyl acetate) (EVA) encapsulant demonstrated a significant photocurrent loss due to EVA discoloration and delamination from increased chemical reactivity at the front-side EVA/cell metallization interface. Brown discoloration of the EVA encapsulant near the cell gridlines is linked to an electrochemical reaction at the Ag gridlines under hot and humid conditions (85 °C, 85% relative humidity). Chemical compositional analysis using X-ray photoelectron spectroscopy (XPS) confirmed that the discoloration is attributed to the formation of silver sulfide (Ag 2 S) and/or silver oxide (Ag 2 O) species at the EVA/Ag gridline interface. The subsequent migration of Ag ions from the cell gridlines into the bulk of the EVA was evident from XPS depth profiling and optical microscopy. However, the Ag signal was not detected at the EVA/glass interface, inferring limited ionic transport through the nominally 0.45 mm thick encapsulant. For the samples studied herein, the sulfur is believed by the process of elimination to come from the ambient air, diffusing into the module through the permeable polymer backsheet.

14 SOLAR ENERGY↗

Evaluating the causes of cost reduction in photovoltaic modules

Photovoltaic (PV) module costs have declined rapidly over forty years but the reasons remain elusive. Here we advance a conceptual framework and quantitative method for quantifying the causes of cost changes in a technology, and apply it to PV modules. Our method begins with a cost model that breaks down cost into variables that changed over time. Cost change equations are then derived to quantify each variable's contribution. We distinguish between changes observed in variables of the cost model – which we term low-level mechanisms of cost reduction – and research and development, learning-by-doing, and scale economies, which we refer to as high-level mechanisms. We find that increased module efficiency was the leading low-level cause of cost reduction in 1980–2012, contributing almost 25% of the decline. Government-funded and private R&D was the most important high-level mechanism over this period. After 2001, however, scale economies became a more significant cause of cost reduction, approaching R&D in importance. Policies that stimulate market growth have played a key role in enabling PV's cost reduction, through privately-funded R&D and scale economies, and to a lesser extent learning-by-doing. The method presented here can be adapted to retrospectively or prospectively study many technologies, and performance metrics besides cost.

14 SOLAR ENERGY↗

Photovoltaic module and interlocked stack of photovoltaic modules

One embodiment relates to an arrangement of photovoltaic modules configured for transportation. The arrangement includes a plurality of photovoltaic modules, each photovoltaic module including a frame. A plurality of individual male alignment features and a plurality of individual female alignment features are included on each frame. Adjacent photovoltaic modules are interlocked by multiple individual male alignment features on a first module of the adjacent photovoltaic modules fitting into and being surrounded by corresponding individual female alignment features on a second module of the adjacent photovoltaic modules. Other embodiments, features and aspects are also disclosed.

14 SOLAR ENERGY↗

Effects of Photovoltaic Module Materials and Design on Module Deformation Under Load

Static structural finite element models of an aluminum-framed crystalline silicon (c-Si) photovoltaic (PV) module and a glass-glass thin film PV module were constructed and validated against experimental measurements of deflection under uniform pressure loading. Parametric analyses using Latin Hypercube Sampling (LHS) were performed to propagate simulation input uncertainties related to module material properties, dimensions, and manufacturing tolerances into expected uncertainties in simulated deflection predictions. This exercise verifies the applicability and validity of finite element modeling for predicting mechanical behavior of solar modules across architectures and enables computational models to be used with greater confidence in assessment of module mechanical stressors and design for reliability. Sensitivity analyses were also performed on the uncertainty quantification data sets using linear correlation coefficients to elucidate the key parameters influencing module deformation. This information has implications on which materials or parameters may be optimized to best increase module stiffness and reliability, whether the key optimization parameters change with module architecture or loading magnitudes, and whether parameters such as frame design and racking must be replicated in reduced-scale reliability studies to adequately capture full module mechanical behavior.

14 SOLAR ENERGY↗

Decay of Electrostatic Force of Dust Particles on Photovoltaic Modules

Photovoltaic (PV) energy yield loss due to solar module soiling has become increasingly important as solar module deployment is now at the hundreds of gigawatts scale and continues to grow rapidly. We have reported on direct measurements-using atomic force microscopy (AFM)-of strong electric-field-induced attraction and adhesion force (Fes) of dust particles onto solar panel that are 1 to 2 orders of magnitude stronger than the van der Waals and water capillary forces, corroborated by observing the increase in system voltage-induced soiling rate. Here, we report another characteristic of Fes on soiling-long lasting or slow decay after turning off the high voltage applied to solar panels. The Fes decay time varies in a wide time range of 1 to 10 hours, depending on two factors: 1) either/both the cell or/and particle were charged with high voltage before the voltages were turned off; and 2) how the cell was connected to the ground after the voltage was turned off-either connected through the power supply electronics, directly connected to the ground, or electrically floated. The Fes decay is understood in terms of 1) net electrical charge dissipations in both particle and cell, 2) thermal disordering of dipole polarization in the module glass dielectrics, and 3) charge redistribution by the electrostatic interaction of particle and module glass. This long-lasting Fes for hours can significantly affect the solar panel soiling after sunset, especially combined with water condensation.

14 SOLAR ENERGY↗

Long-lasting strong electrostatic attraction and adhesion forces of dust particles on photovoltaic modules

Photovoltaic (PV) energy-yield loss due to solar module soiling has become increasingly important as solar module deployment is now at the hundreds of gigawatts scale and continues to grow rapidly. The electrostatic attraction and adhesion force (F es ) of dust particles by the high voltages from solar panels have been reported to be 1 to 2 orders of magnitude stronger than the van der Waals and water capillary forces, which has been corroborated by observing the increase in system voltage-induced soiling rate by setting up an outdoor test. Here, we report another characteristic of F es on soiling - long-lasting or slow decay after turning off the high voltage applied to solar panels. The F es decay time varies across a wide time range of 1 to 10 h, depending on two factors: 1) whether the cell, the particle, or both were charged with high voltage before the voltages were turned off; and 2) how the cell was connected to the ground after the voltage was turned off - either connected through the power-supply electronics, directly connected to the ground, or electrically floated. The Fes decay is understood in terms of 1) net electrical charge dissipations in both particle and cell, 2) thermal disordering of dipole polarization in the module glass dielectrics, and 3) charge redistribution by the electrostatic interaction of particle and module glass. This long-lasting F es for hours can affect the solar panel soiling after sunset, and it can have an even greater effect when combined with water condensation at night.

14 SOLAR ENERGY↗

Photovoltaic module and interlocked stack of photovoltaic modules

One embodiment relates to an arrangement of photovoltaic modules configured for transportation. The arrangement includes a plurality of photovoltaic modules, each photovoltaic module including a frame having at least a top member and a bottom member. A plurality of alignment features are included on the top member of each frame, and a plurality of alignment features are included on the bottom member of each frame. Adjacent photovoltaic modules are interlocked by the alignment features on the top member of a lower module fitting together with the alignment features on the bottom member of an upper module. Other embodiments, features and aspects are also disclosed.

14 SOLAR ENERGY↗

Thermal and Electrical Effects of Partial Shade in Monolithic Thin-Film Photovoltaic Modules

Photovoltaic cells can be damaged by reverse bias stress, which arises during service when a monolithically integrated thin-film module is partially shaded. We introduce a model for describing a module's internal thermal and electrical state, which cannot normally be measured. Using this model and experimental measurements, we present several results with relevance for reliability testing and module engineering: Modules with a small breakdown voltage experience less stress than those with a large breakdown voltage, with some exceptions for modules having light-enhanced reverse breakdown. Masks leaving a small part of the masked cells illuminated can lead to very high temperature and current density compared to masks covering entire cells.

14 SOLAR ENERGY↗

Simulation of an active cooling system for photovoltaic modules

Photovoltaic cells are devices that convert solar radiation directly into electricity. However, solar radiation increases the photovoltaic cells temperature [1] [2]. The temperature has an influence on the degradation of the cell efficiency and the lifetime of a PV cell. This work reports on a water cooling technique for photovoltaic panel, whereby the cooling system was placed at the front surface of the cells to dissipate excess heat away and to block unwanted radiation. By using water as a cooling medium for the photovoltaic solar cells, the overheating of closed panel is greatly reduced without prejudicing luminosity. The water also acts as a filter to remove a portion of solar spectrum in the infrared band but allows transmission of the visible spectrum most useful for the PV operation. To improve the cooling system efficiency and electrical efficiency, uniform flow rate among the cooling system is required to ensure uniform distribution of the operating temperature of the PV cells. The aims of this study are to develop a 3D thermal model to simulate the cooling and heat transfer in Photovoltaic panel and to recommend a cooling technique for the PV panel. The velocity, pressure and temperature distribution of the three-dimensional flow across the cooling block were determined using the commercial package, Fluent. The second objective of this work is to study the influence of the geometrical dimensions of the panel, water mass flow rate and water inlet temperature on the flow distribution and the solar panel temperature. The results obtained by the model are compared with experimental results from testing the prototype of the cooling device.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Advances in Coring Procedures of Silicon Photovoltaic Modules

We describe advances on procedures used for the coring of silicon photovoltaic modules. These procedures involve coring specific locations, starting from the back of the modules, and removing selected parts of the cell structure, while preserving the front tempered glass. The standard coring procedures had to be modified from case to case due to the different cell structures and measurement requirements. We provide examples of the characterization of the cored samples by scanning electron microscopy and energy-dispersive X-ray spectroscopy. Finally, we describe a simple process to create small openings at specific locations on the back of photovoltaic modules to allow for efficiency-related measurement of individual cells and groups of cells.

41 EE - Solar Energy Technologies Office (EE-4S)↗

Photovoltaic Module Imaging for Hail Damage Assessment with Multi-Year Follow Up

Outdoor-aged photovoltaic modules that have experienced golf-ball sized hail are characterized by flash testing and photoluminescence, electroluminescence, thermal, and ultraviolet fluorescence imaging. These measurements were performed immediately after the hailstorm and then again after another two years and four years in the field. The modules originally experienced different ranges of hail damage with some having cracks on approximately half of the cells and some having few to no cracked cells. Flash testing shows that the hail-damaged modules with the most cracked cells have 3 to 4% less power than those with the least damage. After four more years in the outdoor climate of Golden, Colorado since the hailstorm, all of the modules still exhibit similar relative power and amounts of cell cracking, suggesting that the hail damage has only initially reduced power but has not yet increased the degradation rate.

electroluminescence↗

Electrochemical mechanisms of leakage-current-enhanced delamination and corrosion in Si photovoltaic modules

This paper analyzes the mechanisms for corrosion and delamination observed in Si photovoltaic modules subjected to high temperature and humidity with a negative-ground bias testing. Based on the thermodynamic data, the ionic component of the leakage current causes reduction reactions of water on the cathodic metallization, producing hydrogen gas and hydroxide ions. Ag fingers are strong catalysts for this reduction reaction compared to other materials used in solar cells and can be the initiation sites of corrosion and delamination caused by the electrochemical reactions. The produced hydrogen gas accumulates inside the module potentially producing a high gas pressure that can promote delamination, which is often preferentially initiated on metallization where the adhesion strength is lower [1], [2], [3]. The local basicity near the metal surface increases due to the hydroxide ion generation. Thus, the environment inside the encapsulant can be alkaline despite the presence of acetic acid decomposition products from the encapsulant. Corrosion of materials such as Si used in solar cells occurs and the extent depends on their corrosion resistance to the alkaline solution. This suggests that corrosion and delamination are interactive and promote the formation and propagation of one another.

14 SOLAR ENERGY↗

Generalized Spatio-Temporal Model of Backsheet Degradation From Field Surveys of Photovoltaic Modules

Photovoltaic (PV) module backsheets degrade at different rates because of the specific polymeric materials and the local exposure environments of the installations. Studies of real-world backsheet degradation provide valuable information to understand backsheet degradation and failure. Field surveys of PV module backsheets were conducted on 1310 modules in four commercial PV power plant sites with different exposure times. The backsheet's local exposure environment is determined by its location along the rack length and depth, the modules' elevation above the ground, and the ground cover albedo. Backsheets that are installed at the ends of the module rack length exhibit larger degradation rates (with yellowness index difference of 1.14 $\pm$ 0.45 and 7.80 $\pm$ 1.3 for backsheets of poly (ethylene terephthalate) and poly (ethylene naphthalate) as the air-side layer, respectively) than backsheets in the center section of the rack. A generalized spatio-temporal model was developed to predict the large-scale backsheet degradation of different backsheet polymers across time/age and location in the PV power plant rack. The model utilizes a cubic-spline relationship between backsheet degradation and rack length, and a quadratic relationship between backsheet discoloration and rack depth. This generalized spatio-temporal model predicts the outdoor backsheet degradation with an adjusted- $R^2$ range between 0.31 to 0.89. The similarity between this model and the spatial variation of the rear-side irradiance, indicates that the irradiance plays a significant role in outdoor backsheet degradation. The generalized spatio-temporal model can be used to evaluate large scale PV backsheet performance, as well as a guidance for PV site designers and operations and maintenance crews.

14 SOLAR ENERGY↗

Durability of Poly(Methyl Methacrylate) Lenses Used in Concentrating Photovoltaic Modules: Preprint

Concentrating photovoltaic (CPV) technology has recently gained interest based on their expected low levelized cost of electricity, high efficiency, and scalability. Many CPV systems use Fresnel lenses made of poly(methyl methacrylate)(PMMA) to obtain a high optical flux density. The optical and mechanical durability of such components, however, are not well established relative to the desired service life of 30 years. Specific reliability issues may include: reduced optical transmittance, discoloration, hazing, surface erosion, embrittlement, crack growth, physical aging, shape setting (warpage), and soiling. The initial results for contemporary lens- and material-specimens aged cumulatively to 6 months are presented. The study here uses an environmental chamber equipped with a xenon-arc lamp to age specimens at least 8x the nominal field rate. A broad range in the affected characteristics (including optical transmittance, yellowness index, mass loss, and contact angle) has been observed to date, depending on the formulation of PMMA used. The most affected specimens are further examined in terms of their visual appearance, surface roughness (examined via atomic force microscopy), and molecular structure (via Fourier transform infrared spectroscopy).

14 SOLAR ENERGY↗

Creep in Photovoltaic Modules: Examining the Stability of Polymeric Materials and Components

Interest in renewable energy has motivated the implementation of new polymeric materials in photovoltaic modules. Some of these are non-cross-linked thermoplastics, in which there is a potential for new behaviors to occur, including phase transformation and visco-elastic flow. Differential scanning calorimetry and rheometry data were obtained and then combined with existing site-specifictime-temperature information in a theoretical analysis to estimate the displacement expected to occur during module service life. The analysis identified that, depending on the installation location, module configuration and/or mounting configuration, some of the thermoplastics are expected to undergo unacceptable physical displacement. While the examples here focus on encapsulation materials,the concerns apply equally to the frame, junction-box, and mounting-adhesive technologies.

14 SOLAR ENERGY↗

Review of Potential–Induced Degradation in Bifacial Photovoltaic Modules

Bifacial modules are increasingly deployed in the field and are expected to represent half of the market share within 10 years. Their rear structure differs from monofacial modules to allow additional light absorption. However, it brings new reliability challenges to address. In particular, the risk of potential-induced degradation (PID) is increased as both module sides are impacted. Different PID processes have been identified in the literature: shunting type (PID-s), polarization type (PID-p), Na penetration type, and corrosion type (PID-c). Their occurrence depends on the photovoltaic system configuration as well as the module's materials. Apart from PID-s, PID processes are not well understood and extensive research is needed to elucidate the PID scenario and underlying mechanisms. Herein, current knowledge about PID processes and their impact on the main bifacial modules in the market are gathered with the aim to guide future research. Bifacial module technologies and leakage current paths leading to PID are described. Indoor and outdoor PID testing methods are detailed. For each bifacial module technology, the PID processes are investigated with their indicators, mechanism and recovery process. Furthermore, PID-impacting factors and limitation solutions are finally reported and a state of the art on PID modeling is presented.

14 SOLAR ENERGY↗