Recent advances in oxidative degradation of plastics
Oxidative degradation is a powerful method to degrade plastics into oligomers and small oxidized products.
SEARCH · Engineering Papers
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Oxidative degradation is a powerful method to degrade plastics into oligomers and small oxidized products.
The oxidative degradation of PMR (for polymerization of monomeric reactants) polyimides at elevated temperatures was followed by cross-polarized magic angle spinning (CP-MAS) NMR. Labeling of selected sites in the polymers with C-13 allowed for direct observation of the transformations arising from oxidation processes. The formation of several degradation products has been proposed to be occurring in the cross-links derived from the nadic end caps on oxidation. Model compounds have been synthesized and characterized by CPMAS NMR with both normal and delayed decoupling to distinguish between protonated and unprotonated carbons. Comparison of these spectra to predicted chemical shifts of proposed products for the aged polymer provides further insight to degradation occurring in the cross-linked moieties.
Experimental study conducted on thermo-oxidative degradation of composite-material specimens made of silicon carbide fibers in matrices of reaction-bonded silicon nitride. In SiC/Si3N4 composites of study, interphase is 3-micrometers-thick carbon-rich coat on surface of each SiC fiber. Thermo-oxidative degradation of these composites involves diffusion of oxygen through pores of composites to interphases damaged by oxidation. Nondestructive tests reveal critical exposure times.
Radiation-initiated crosslinking of polyethylene has proven to be an effective method of reducing creep and wear. This has allowed polyethylene to find widespread use in engineering and medical sectors where extreme conditions would otherwise cause it to degrade. However, despite their resilience, irradiated polyethylene products are still vulnerable to oxidative degradation in some long-term applications. A good deal of literature exists to discuss the effects that irradiation and oxidative degradation have on polyethylene’s mechanical properties, but not much literature exists to describe the microscopic properties that make irradiated polyethylene susceptible to this process. This review presents a micro-scale look at polyethylene’s morphology and chemistry, with the intention of describing which characteristics make the material more or less favorable for oxidation. By describing the factors that make irradiated polyethylene vulnerable to oxidation in the first place, the hope is to provide insight on how to mitigate oxidation in future applications.
Thermal oxidative degradation studies were performed on unbranched perfluoroalkylethers at 288 C in oxygen. Metals and alloys studied included Ti, Al, and Ti (4 Al, 4 Mn). The mechanism of degradation was by chain scission. Ti and Al promoted less degradation than Ti (4 Al, 4 Mn). The two inhibitors investigated (a perfluorophenyl phosphine and a phosphatriazine) reduced degradation rates by several orders of magnitude. Both inhibitors were effective for the same duration (75 to 100 hours). The phosphatriazine appeared to provide more surface protection.
The mechanisms operative in thermal oxidative degradation of Fomblin Z and hexafluoropropene oxide derived fluids and the effect of alloys and additives upon these processes are investigated. The nature of arrangements responsible for the inherent thermal oxidative instability of the Fomblin Z fluids is not established. It was determined that this behavior is not associated with hydrogen end groups or peroxy linkages. The degradation rate of these fluids at elevated temperatures in oxidizing atmospheres is dependent on the surface/volume ratio. Once a limiting ratio is reached, a steady rate appears to be attained. Based on elemental analysis and oxygen consumption data, CF2OCF2CF2O2, no. CF2CF2O, is one of the major arrangements present. The action of the M-50 and Ti(4 Al, 4 Mn) alloys is much more drastic in the case of Fomblin Z fluids than that observed for the hexafluoropropene derived materials. The effectiveness of antioxidation anticorrosion additives, P-3 and phospha-s-triazine, in the presence of metal alloys is very limited at 316 C; at 288 C the additives arrested almost completely the fluid degradation. The phospha-s-triazine appears to be at least twice as effective as the P-3 compound; it also protected the coupon better. The Ti(4 Al, 4 Mn) alloy degraded the fluid mainly by chain scission processes this takes place to a much lesser degree with M-50.
Thermal oxidative degradation studies were performed on unbranched perfluoroalkylethers at 288 C in oxygen. Metals and alloys studied included Ti, Al, and Ti (4 Al, 4 Mn). The mechanism of degradation was by chain scission. Ti and Al promoted less degradation than Ti (4 Al, 4 Mn). The two inhibitors investigated (a perfluorophenyl phosphine and a phosphatriazine) reduced degradation rates by several orders of magnitude. Both inhibitors were effective for the same duration (75 to 100 hours). The phosphatriazine appeared to provide more surface protection.
Values of global kinetic constants for pyrolysis, thermal oxidative degradation, and char oxidation of a cellulosic paper were determined by a derivative thermal gravimetric study. The study was conducted at heating rates of 0.5, 1, 1.5, 3, and 5 C/min in ambient atmospheres of nitrogen, 0.28, 1.08, 5.2 percent oxygen concentrations, and air. Sample weight loss rate, concentrations of CO, CO2, and H2O in the degradation products, and oxygen consumption were continuously measured during the experiment. Values of activation energy, preexponential factor, orders of reaction, and yields of CO, CO2, H2O, total hydrocarbons, and char for each degradation reaction were derived from the results. Heat of reaction for each reaction was determined by differential scanning calorimetry. A comparison of the calculated CO, CO2, H2O, total hydrocarbons, sample weight loss rate, and oxygen consumption was made with the measured results using the derived kinetic constants, and the accuracy of the values of kinetic constants was discussed.
Manganese (Mn)-oxides regulate carbon (C) cycling in soils by sorbing and oxidizing organic compounds. The composition of soil organic matter varies widely, and little is known about the reactivity of individual organic compounds with structurally diverse Mn-oxides under various environmentally relevant pH conditions. Here, in this study, we examined the affinity of six organic compounds for three Mn-oxides, comprised of layer (birnessite and hydrous Mn oxide HMO) or tunnel (cryptomelane) structures, at acidic (pH 4), slightly acidic (pH 6), and slightly alkaline (pH 8) conditions. Cryptomelane, with a higher specific surface area and point of zero charge, showed higher reactivity than that of HMO and birnessite. Interestingly, these Mn-oxides, although different in structures, decomposed each organic compound to form the same products. Citrate, pyruvate, ascorbate, and catechol induced reduction and dissolution of Mn-oxides. After the reaction, the average oxidation state of Mn in the solids was much lower at pH 4 than at pH 6 and 8, suggesting more reduction under more acidic conditions. Even when reacting with phthalate and propanol, which only sorbed to Mn-oxides but did not degrade, there was proton-promoted Mn dissolution under acidic conditions. These results suggest the significance of environmental pH and mineral structures in affecting the Mn–organic interactions and provide fundamental insights into a better understanding of the roles of Mn-oxides in regulating soil C cycling.
Direct air capture (DAC) processes for extraction of CO 2 from ambient air are unique among chemical processes in that they operate outdoors with minimal feed pretreatments. Here, the impact of humidity on the oxidative degradation of a prototypical solid supported amine sorbent, poly(ethylenimine) (PEI) supported on Al 2 O 3 , is explored in detail. By combining CO 2 adsorption measurements, oxidative degradation rates, elemental analyses, solid-state NMR and in situ IR spectroscopic analysis in conjunction with 18 O labeling of water, a comprehensive picture of sorbent oxidation is achieved under accelerated conditions. Here we demonstrated that the presence of water vapor can play an important role in accelerating the degradation reactions. From the study we inferred the identity and kinetics of formation of the major oxidative products, and the role(s) of humidity. Our data are consistent with a radical mediated autooxidative degradation mechanism.
Here thermo-oxidative degradation of thermoplastic-based composites filled with two types of carbon filler including bituminous (Pittsburgh No.8, P8) and sub-bituminous (Powder River Basin, PRB) coals were investigated using differential scanning calorimetry (DSC) and thermogravimetric analysis. Oxidation induction time (OIT) and activation energy (AE) for coal plastic composites (CPCs), HDPE, and commercially available wood plastic composites (WPCs) were determined using isothermal and isoconversional kinetic methods. OIT values for CPC increased with coal content, indicating higher thermo-oxidative stability. AE values obtained using isothermal method were 52–116 kJ/mol for all CPC formulations, 32 kJ/mol for HDPE, and 33–114 kJ/mol for WPCs. AEs for CPCs obtained using isoconversional methods were not constant but rather dependent on the degree of degradation with CPC/ P8 coal possessing higher overall AE. Incorporating coal into HDPE increased thermo-oxidative stability of the resulting composite, indicating coal potentially acts as a natural primary and secondary antioxidant for polymer materials.
Abstract Direct air capture (DAC) processes for extraction of CO 2 from ambient air are unique among chemical processes in that they operate outdoors with minimal feed pretreatments. Here, the impact of humidity on the oxidative degradation of a prototypical solid supported amine sorbent, poly(ethylenimine) (PEI) supported on Al 2 O 3 , is explored in detail. By combining CO 2 adsorption measurements, oxidative degradation rates, elemental analyses, solid‐state NMR and in situ IR spectroscopic analysis in conjunction with 18 O labeling of water, a comprehensive picture of sorbent oxidation is achieved under accelerated conditions. We demonstrated that the presence of water vapor can play an important role in accelerating the degradation reactions. From the study we inferred the identity and kinetics of formation of the major oxidative products, and the role(s) of humidity. Our data are consistent with a radical mediated autooxidative degradation mechanism.
The objective of this contract was to investigate the mechanisms operative in thermal and thermal oxidative degradation of Fomblin Z and hexafluoropropene oxide derived fluids and the effect of alloys and additives upon these processes. The nature of arrangements responsible for the inherent thermal oxidative instability of the Fomblin Z fluids has not been established. It was determined that this behavior was not associated with hydrogen end-groups or peroxy linkages. The degradation rate of these fluids at elevated temperatures in oxidizing atmospheres was found to be dependent on the surface/volume ratio. Once a limiting ratio was reached, a steady rate appeared to be attained. Based on elemental analysis and oxygen consumption data, -CF2OCF2CF2O-, not -CF2CF2O-, is one of the major arrangements present. The action of the M-50 and Ti(4 Al, 4 Mn) alloys was found to be much more drastic in the case of Fomblin Z fluids than that observed for the hexalfuoropropane oxide derived materials. The effectiveness of antioxidation/anticorrosion additives, P-3 and phospha-s-triazine, in the presence of metal alloys was very limited at 316 C; at 288 C the additives arrested almost completely the fluid degradation. The phospha-s-triazine appeared to be at least twice as effective as the P-3 compound; it also protected the coupon better. The Ti(4 Al, 4 Mn) alloy degraded the fluid mainly by chain scission processes; this took place to a much lesser degree with M-50.
Phenolic aldehydes generated from lignin in fossil woods and carbonaceous sediments by oxidative degradation
Presentation Outline: Background and motivation Component design (ASME rules) Graphite degradation Oxidation Irradiation MOOSE modeling Oxidation modeling Graphite component stress modeling Oxidized conditions Irradiated conditions Future work
The oxidative degradation of PMR (for polymerization of monomeric reactants) polyimides at elevated temperatures was followed by cross-polarized magic angle spinning (Cp-MAS) NMR. C-13 labeling of selected sites in the polymers allowed for direct observation of the transformations arising from oxidation processes. As opposed to model compound studies, the reactions were followed directly in the polymer. The labeling experiments confirm the previously reported oxidation of the methylene carbon to ketone in the methylenedianiline portion of the polymer chain. They also show the formation of two other oxidized species, acid and ester, from this same carbon. In addition, the technique provides the first evidence of the kind of degradation reactions that are occurring in the nadic end caps. Several PMR formulations containing moieties determined to be present after oxidation, as suggested by the labeling study, were synthesized. Weight loss, FTIR, and natural abundance NMR of these derivatives were followed during aging. In this way, weight loss could be related to the observed transformations.
We report manganese (Mn) oxides have a high surface area and redox potential that facilitate sorption and/or oxidation of organic carbon (OC), but their role in regulating soil C storage is relatively unexplored. Small OC compounds with distinct structures were reacted with Mn(III/IV)-oxides to investigate the effects of OC/Mn molar ratios on Mn–OC interaction mechanisms. Dissolved and solid-phase OC and Mn were measured to quantify the OC sorption to and/or the redox reaction with Mn-oxides. Mineral transformation was evaluated using X-ray diffraction and X-ray absorption spectroscopy. Higher OC/Mn ratios resulted in higher sorption and/or redox transformation; however, interaction mechanisms differed at low or high OC/Mn ratios for some OC. Citrate, pyruvate, ascorbate, and catechol induced Mn-oxide dissolution. The average oxidation state of Mn in the solid phase did not change during the reaction with citrate, suggesting ligand-promoted mineral dissolution, but decreased significantly during reactions with the other compounds, suggesting reductive dissolution mechanisms. Phthalate primarily sorbed on Mn-oxides with no detectable formation of redox products. Mn–OC interactions led primarily to C loss through OC oxidation into inorganic C, except phthalate, which was predominantly immobilized in the solid phase. Together, these results provided detailed fundamental insights into reactions happening at organo–mineral interfaces in soils.
There is a growing interest in developing a methodology for effectively cleaving carbon–carbon (C–C) bonds in polymer backbones through bioconversion processes that utilize microorganisms and their enzymes. This upsurge of interest is driven by the goal of achieving a circular economy. Polyolefin post-consumer plastics are a substantial source of carbon, but the recycling potential is severely limited. Upcycling routes are needed for converting polyolefin post-consumer plastics into value-added products while concurrently mitigating adverse environmental effects. These materials contain carbon-based chemicals that can, in principle, serve as the feedstock for microbial metabolism. Some microbes have been reported to grow on polyolefin plastics, but the rate of biodegradation is insufficient for industrial processes. In this study, low-density polyethylene (LDPE) films were subjected to two mild ozone-based oxidation treatments, which facilitated biodegradation. The degree of oxidation was determined by Fourier transform infrared spectroscopy via analysis of the carbonyl index (1,710/1,460 cm −1 ), which ranged from 0.3 to 2.0, and also via analysis of the carboxylic acid content. Following oxidation of the films, studies were conducted to investigate the ability of a panel of polyvinyl alcohol-degrading microbes to degrade the oxidized films. A defined minimal medium was used to cultivate and assess microbial growth on the oxidized films. Following 45 days of cultivation, the most effective strains were further cultivated up to three additional generations on the oxidized film substrates to improve their ability to degrade the oxidized LDPE films. After these enrichments, we identified a strain from the third generation of Pseudomonas sp. Rh926 that exhibited significant cell growth and reduced the oxidized LDPE film mass by 25% in 30 days, demonstrating an enhanced capacity for degrading the oxidized LDPE films.