Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “non-metallic inclusion”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

Effectiveness of Shot Peening In Suppressing Fatigue Cracking At Non-Metallic Inclusions In Udimet(Registered Trademark)720

The fatigue lives of modern powder metallurgy disk alloys can be reduced over an order of magnitude by cracking at inherent non-metallic inclusions. The objective of this work was to study the effectiveness of shot peening in suppressing LCF crack initiation and growth at surface nonmetallic inclusions. Inclusions were carefully introduced at elevated levels during powder metallurgy processing of the nickel-base disk superalloy Udimet 720. Multiple strain-controlled fatigue tests were then performed on machined specimens with and without shot peened test sections at 427 C and 650 C. The low cycle fatigue lives and failure initiation sites varied as functions of inclusion content, shot peening, and fatigue conditions. A large majority of the failures in as-machined specimens with the introduced inclusions occurred at cracks initiating from inclusions intersecting the specimen surface. These inclusions reduced fatigue life by up to 100X, when compared to lives of material without inclusions residing at specimen surface. Large inclusions produced the greatest reductions in life for tests at low strain ranges and high strain ratios. Shot peening improved life in many cases by reducing the most severe effects of inclusions.

Barrie, Robert L.↗

Effectiveness of Shot Peening in Suppressing Fatigue Cracking at Non-Metallic Inclusions in Udimet(trademark) 720

The fatigue lives of modern powder metallurgy disk alloys can be reduced by over an order of magnitude by surface cracking at inherent non-metallic inclusions. The objective of this work was to study the effectiveness of shot peening in suppressing LCF crack initiation and growth at surface nonmetallic inclusions. Inclusions were carefully introduced at elevated levels during powder metallurgy processing of the nickel-base disk superalloy Udimet 720. Multiple strain-controlled fatigue tests were then performed on machined specimens at 427 and 650 C in peened and unpeened conditions. Analyses were performed to compare the low cycle fatigue lives and failure initiation sites as a function of inclusion content, shot peening, and fatigue conditions. A large majority of the failures in as-machined specimens with introduced inclusions occurred at cracks initiating from inclusions intersecting the specimen surface. The inclusions could reduce fatigue life by up to 100X. Large inclusions had the greatest effect on life in tests at low strain ranges and high strain ratios. Shot peening can be used to improve life in these conditions by reducing the most severe effects of inclusions.

Barrie, Robert L.↗

Interaction of Porosity with a Planar Solid/Liquid Interface

In this paper, an investigation of the interaction between gas porosity and a planar solid/liquid (SL) interface is reported. A two-dimensional numerical model able to accurately track sharp SL interfaces during solidification of pure metals and alloys is proposed. The finite difference method and a rectangular undeformed grid are used for computation. The SL interface is described through the points of intersection with the grid lines. Its motion is determined by the thermal and solute gradients at each particular point. Changes of the interface temperature because of capillarity or solute redistribution as well as any perturbation of the thermal and solute field produced by the presence of non-metallic inclusions can be computed. To validate the model, the dynamics of the interaction between a gas pore and a solidification front in metal alloys was observed using a state of the art X-ray Transmission Microscope. The experiments included observation of the distortion of the SL interface near a pore, real-time measurements of the growth rate and the change in shape of the porosity during interaction with an advancing SL interface in pure Al and Al-0.25 wt% Au alloy. In addition, porosity induced solute segregation patterns surrounding a pore were also quantified.

Catalina, Adrian V.↗

Interaction of Porosity with a Planar Solid/Liquid Interface

In this article, an investigation of the interaction between gas porosity and a planar solid/liquid (SL) interface is reported. A two-dimensional numerical model able to accurately track sharp SL interfaces during solidification of pure metals and alloys is proposed. The finite-difference method and a rectangular undeformed grid are used for computation. The SL interface is described through the points of intersection with the grid lines. Its motion is determined by the thermal and solute gradients at each particular point. Changes of the interface temperature because of capillarity or solute redistribution as well as any perturbation of the thermal and solute field produced by the presence of non-metallic inclusions can be computed. To validate the model, the dynamics of the interaction between a gas pore and a solidification front in metal alloys was observed using a state of the art X-ray transmission microscope (XTM). The experiments included observation of the distortion of the SL interface near a pore, real-time measurements of the growth rate, and the change in shape of the porosity during interaction with the SL interface in pure Al and Al-0.25 wt pct Au alloy. In addition, porosity-induced solute segregation patterns surrounding a pore were also quantified.

Catalina, Adrian V.↗

Integration of Product, Package, Process, and Environment: A Food System Optimization

The food systems slated for future NASA missions must meet crew nutritional needs, be acceptable for consumption, and use resources efficiently. Although the current food system of prepackaged, moderately stabilized food items works well for International Space Station (ISS) missions, many of the current space menu items do not maintain acceptability and/or nutritive value beyond 2 years. Longer space missions require that the food system can sustain the crew for 3 to 5 years without replenishment. The task "Integration of Product, Package, Process, and Environment: A Food System Optimization" has the objective of optimizing food-product shelf life for the space-food system through product recipe adjustments, new packaging and processing technologies, and modified storage conditions. Two emergent food processing technologies were examined to identify a pathway to stable, wet-pack foods without the detrimental color and texture effects. Both microwave-assisted thermal sterilization (MATS) and pressure-assisted thermal stabilization (PATS) were evaluated against traditional retort processing to determine if lower heat inputs during processing would produce a product with higher micronutrient quality and longer shelf life. While MATS products did have brighter color and better texture initially, the advantages were not sustained. The non-metallized packaging film used in the process likely provided inadequate oxygen barrier. No difference in vitamin stability was evident between MATS and retort processed foods. Similarly, fruit products produced using PATS showed improved color and texture through 3 years of storage compared to retort fruit, but the vitamin stability was not improved. The final processing study involved freeze drying. Five processing factors were tested in factorial design to assess potential impact of each to the quality of freeze-dried food, including the integrity of the microstructure. The initial freezing rate and primary freeze drying temperature and pressure were linked to final product quality in freeze-dried corn, indicating processing modifications that could lead to improved product shelf life. Storage temperatures and packaging systems were also assessed for the impact to food quality. Reduced temperature storage had inconclusive impact to the progression of rancidity in butter cookies. Frozen storage was detrimental to fruit and vegetable textural attributes but refrigerated storage helped to sustain color and organoleptic ratings for plant-based foods. With regard to packaging systems, the metallized film overwrap significantly decreased the progression of the rancidity of butter cookies as compared to the highest barrier non-metallized film. The inclusion of oxygen scavengers resulted in noticeable moisture gains in butter cookies over time, independent of packaging film systems. Neither emergent processing technology nor the freeze dry optimization resulted in compelling quality differences from current space food provisions such that a five-year shelf life is likely with these processing changes alone. Using a combination of refrigeration and PATS processing is expected to result in organoleptically-acceptable fruit quality for most fruits through five years. The vitamin degradation will be aided somewhat by the cold temperatures but, given the labile nature of vitamin C, a more stable fortification method, such as encapsulation, should also be investigated to ensure vitamin delivery throughout the product life. Similarly, significant improvement to the packaging film used in the MATS processing, optimization of formulation for dielectric properties, vitamin fortification, and reduced temperature storage should be investigated as a hurdle approach to reach a five year shelf life in wet-pack entrees and soups. Baked goods and other environmentally-sensitive spaceflight foods will require an almost impenetrable barrier to protect the foods from oxygen and moisture ingress but scavengers and reduced storage temperature did not improve baked good shelf life and are not recommended at this time for these foods.

Cooper, Maya R.↗

Crack barriers improve the mechanical and thermal properties of non-metallic sinter materials

Means of improving the tensile strength of ceramic composites by introducing ductile intermediate layers capable of absorbing the elastic energy at the rupture front are studied. Tests with an Al203 laminate with niobium inclusions showed that crack propagation could be successfully precluded by dissipation of the energy by deformation and/or delamination at the inclusion/matrix interface.

Gruenthaler, K. H.↗